Daxun is a 316/316L stainless steel angle steel supplier in China
As a leading stainless steel angle steel supplier and exporter in China, Daxun supplies stainless steel angle steel to all over the world.
- Grade: S31600(316)-S31603(316L)
- Equal Angle Steel/Unequal Angle Steel
- Process: hot rolling and laser welding
- Easy to weld and process
- Length can be cut to size
- Daxun specializes in custom stainless steel angles with fast delivery and competitive prices. Contact Daxun today.
Global leader in stainless steel angle fabrication services
304/304L and 316/316L Stainless Steel Angles
As China’s premier supplier of specialty metals, you can trust Daxun for all of your stainless steel angle needs. Our stainless steel angle selection includes 304/304L and 316/316L stainless steel angles. Our extensive product line offers durability and versatility, making it the perfect solution for your structural and fabrication needs.
Our stainless steel angles are available in 304/304L and 316/316L, all from fully certified factories. Our comprehensive product line is both durable and adaptable, ideal for structural and fabrication applications. As a leading stainless steel angle manufacturer, we offer a wide range of specialty angles and L-shaped angles. Daxun offers stainless steel angles in any length, up to 6 meters. The following stainless steel grades are also available: 304/304L and 316/316L. Stainless steel angles are most commonly used for supports or frames, but are also used in food equipment, building supports, structural supports, and medical equipment.
Can be welded and processed using simple procedures, 304/304L stainless steel angles are suitable for many environments, such as general industrial projects, chemical projects. While 316/316L angles are marine grade and have strong corrosion resistance in more demanding conditions.
The surface treatment we use on our stainless steel angles is hot rolling, annealing, and pickling. This surface treatment maximizes corrosion resistance and gives the angles a unique “stainless” appearance.
The two manufacturing methods are laser melting and hot rolling. Hot rolling produces stainless steel angles at a lower price. They usually have rounded or tapered edges. On the other hand, laser melted stainless steel angles have consistent sharp and square corners. They also have a sandblasted, smoother surface. Laser melted stainless steel angles have a smoother surface quality than hot rolled stainless steel angles.
Daxun Alloy manufactures laser melted and hot rolled stainless steel angles in metric and imperial sizes. We can ship them all over the world.
Données
- Paramètres
- Élément
- Propriétés mécaniques
- PROPRIÉTÉS PHYSIQUES
- Tous les équivalents
| Standard | ASTM、EN、DIN、JIS, ASME, BS, GBetc, |
| Dimensions | ∠20*20*3mm-∠200*200*24mm |
| Alliage | 201, 310, 304, 304L, 316, 316L |
| Type | Equal, Unequal |
| Longueur | 1.0-12.0m |
| Épaisseur | 3mm-25mm |
| Options personnalisées | Oui |
| Tolérances | ± ¼”, ± 1/16” |
| Finition | Moulin, brosse, miroir, poli |
| CHEMICAL COMPOSITION: ASTM A240, A666 | ||
| Élément | Type 316 | Type 316L |
| Carbone | 0,08 max. | 0,030 max. |
| Manganèse | 2.00 max. | 2.00 max. |
| Soufre | 0,030 max. | 0,030 max. |
| Phosphore | 0,045 max. | 0,045 max. |
| Silicium | 0.75 max. | 0.75 max. |
| Chrome | 16.0 – 18.0 | 16.0 – 18.0 |
| Nickel | 10.00 – 14.00 | 10.00 – 14.00 |
| Molybdène | 2.00 – 3.00 | 2.00 – 3.00 |
| Azote | 0.10 max. | 0.10 max. |
| Type | Limite d'élasticité 0.2% offset (KSI) | Résistance à la traction (KSI) | % Allongement (2″ Longueur de la jauge) |
| 316 | 30 min. | 75 min. | 40 min. |
| 316L | 25 min. | 70 min. | 40 min. |
| Densité (lb./ in^2) @ RT | 0.29 | |
| Module d'élasticité en traction (psi x 10^6) | 28 | |
| Chaleur spécifique (BTU/o F/lb.) | 32 à 212 oF | 0.12 |
| Conductivité thermique (BTU/hr/ft^2/ft) | 212oF | 9.4 |
| 932oF | 12.4 | |
| Coefficient moyen de dilatation thermique (po x 10^-6 par o F) | 32 à 212oF | 8.9 |
| 32 à 600oF | 9 | |
| 32 à 1 000oF | 9.7 | |
| 32 à 1 200oF | 10.3 | |
| Résistivité électrique (micro ohms - cm) | à 70oF | 29.4 |
| Gamme de points de fusion (oF) | 2500 – 2550 |
| Grade | UNS No | Old British | Euronorm | Swedish SS | Japanese JIS | ||
| BS | En | No | Nom | ||||
| 316l | S31603 | 316S11 | – | 1.4404 | X2CrNiMo17-12-2 | 2348 | SUS 316L |
Choisissez Daxun et faites en sorte que vos clients soient satisfaits.

Réponse rapide
Nous assurons une livraison rapide et en temps voulu des produits en acier inoxydable pour les clients ayant des besoins urgents. Cette rapidité s'explique par le soutien du système, du flux d'informations à la logistique et au flux de capitaux. Par exemple, en termes de flux d'informations, les données des commandes de Daxun sont transmises au système logistique en temps réel et les données sont connectées de manière transparente ; en termes de logistique, le centre de traitement est proche des autoroutes, des rivières et des mers, avec une programmation raisonnable, une réponse rapide, un stockage et un lien de transport, et un chargement efficace, ce qui garantit que la tâche est accomplie dans les délais prévus.
Avantages de Daxun
Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel uses the ERP system to achieve full traceability of each angle steel, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.


Emballage
Daxun Alloy garantit la meilleure qualité d'emballage, car celui-ci joue un rôle important dans le fret international, où les marchandises passent par différents canaux avant d'atteindre leur destination finale ; nous accordons donc une attention particulière à l'emballage. Nous emballons nos marchandises de différentes manières, en fonction du produit. Nous emballons nos produits de différentes manières, notamment :
- Boîtes et caisses
- Emballage rétractable
- Palettes en bois
- Boîtes en bois
Qualité, livraison, inspection
- Daxun effectue également plusieurs tests d'assurance qualité. Ces tests comprennent le test d'aplatissement, le test de piqûre et de résistance, le test mécanique, le test de dureté, l'identification positive du matériau, le test d'expansion, etc. Tous ces tests garantissent que le matériau est adapté à l'application requise.
- Au cours du processus de production, nous mesurons le diamètre, l'épaisseur et la surface du produit. Notre délai de livraison standard est de 7 à 15 jours, sauf pour certains produits de taille spéciale, pour lesquels le délai de livraison peut atteindre 20 jours.
Nos délais de livraison sont strictement conformes au contrat. - Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
- Fournir des échantillons gratuits aux clients pour qu'ils les testent
- Soutien à l'inspection sur site ou à l'inspection vidéo en usine


Informations sur les commandes
Les bons de commande doivent indiquer la quantité, le grade, le type ou la catégorie, la référence API5L, l'épaisseur, la largeur, la longueur et toutes les pièces jointes ou exigences supplémentaires relatives à la composition chimique, aux propriétés mécaniques, au traitement thermique, aux essais supplémentaires, au processus de fabrication, au revêtement de surface ou à la finition. Contactez Daxun dès maintenant, nous répondrons à votre email dans les plus brefs délais.
Support technique
Si vous avez besoin d'une assistance technique supplémentaire, notre métallurgiste résident et notre personnel compétent se feront un plaisir de vous aider. En outre, Daxun dispose d'un laboratoire d'essai certifié, une première dans l'industrie des stocks multimétaux et plastiques. Ceci, à notre avis, démontre notre dévouement inébranlable à la qualité et notre philosophie en tant que fournisseur de services complets.

SS 316-316L Stainless Steel angle Features
Daxun Alloy Permettez à votre marque de s'améliorer rapidement
- Tableau de spécification
| Angle – Steel Data | |||||||||||||
| EQUAL AND UNEQUAL ANGLE | |||||||||||||
| ANGLE is available in other sizes on request | |||||||||||||
| Description | Width (W) | Depth (D) | Épaisseur | Standard | Weight per | Surface | |||||||
| (mm) | (mm) | (T) (mm) | Longueur | Metre | Area per | ||||||||
| (kg/m) | Metre | ||||||||||||
| (m²/m) | |||||||||||||
| ANGLE 20 X 20 X 3.0mm | 20 | 20 | 3 | 6.0 metres | 0.98 | 0.0897 | |||||||
| ANGLE 25 X 25 X 3.0mm | 25 | 25 | 3 | 7.5 metres | 1.12 | 0.0953 | |||||||
| ANGLE 25 X 25 X 5.0mm | 25 | 25 | 5 | 7.5 metres | 1.65 | 0.0953 | |||||||
| ANGLE 25 X 25 X 6.0mm | 25 | 25 | 6 | 7.5 metres | 2.08 | 0.0953 | |||||||
| ANGLE 30 X 30 X 2.5mm | 30 | 30 | 2.5 | 6.0 metres | 1.06 | 0.117 | |||||||
| ANGLE 30 X 30 X 3.0mm | 30 | 30 | 3 | 7.5 metres | 1.35 | 0.115 | |||||||
| ANGLE 30 X 30 X 5.0mm | 30 | 30 | 5 | 7.5 metres | 2.01 | 0.115 | |||||||
| ANGLE 30 X 30 X 6.0mm | 30 | 30 | 6 | 7.5 metres | 2.56 | 0.115 | |||||||
| ANGLE 40 X 40 X 2.5mm | 40 | 40 | 2.5 | 6.0 metres | 1.43 | 0.157 | |||||||
| ANGLE 40 X 40 X 3.0mm | 40 | 40 | 3 | 7.5 metres | 1.83 | 0.155 | |||||||
| ANGLE 40 X 40 X 4.0mm | 40 | 40 | 4 | 6.0 metres | 2.2 | 0.155 | |||||||
| ANGLE 40 X 40 X 5.0mm | 40 | 40 | 5 | 9.0 metres | 2.73 | 0.155 | |||||||
| ANGLE 40 X 40 X 6.0mm | 40 | 40 | 6 | 9.0 metres | 3.5 | 0.155 | |||||||
| ANGLE 45 X 45 X 3.0mm | 45 | 45 | 3 | 9.0 metres | 2.06 | 0.175 | |||||||
| ANGLE 45 X 45 X 5.0mm | 45 | 45 | 5 | 9.0 metres | 3.1 | 0.175 | |||||||
| ANGLE 45 X 45 X 6.0mm | 45 | 45 | 6 | 9.0 metres | 3.97 | 0.175 | |||||||
| ANGLE 50 X 50 X 2.5mm | 50 | 50 | 2.5 | 9.0 metres | 1.81 | 0.197 | |||||||
| ANGLE 50 X 50 X 3.0mm | 50 | 50 | 3 | 7.5 metres | 2.31 | 0.195 | |||||||
| ANGLE 50 X 50 X 4.0mm | 50 | 50 | 4 | 9.0 metres | 2.79 | 0.195 | |||||||
| ANGLE 50 X 50 X 5.0mm | 50 | 50 | 5 | 9.0 metres | 3.48 | 0.195 | |||||||
| ANGLE 50 X 50 X 6.0mm | 50 | 50 | 6 | 9.0 metres | 4.46 | 0.195 | |||||||
| ANGLE 50 X 50 X 8.0mm | 50 | 50 | 8 | 9.0 metres | 5.68 | 0.195 | |||||||
| ANGLE 55 X 55 X 5.0mm | 55 | 55 | 5 | 9.0 metres | 3.84 | 0.215 | |||||||
| ANGLE 55 X 55 X 6.0mm | 55 | 55 | 6 | 9.0 metres | 4.93 | 0.215 | |||||||
| ANGLE 65 X 50 X 5.0mm | 65 | 50 | 5 | 9.0 metres | 4.02 | 0.225 | |||||||
| ANGLE 65 X 50 X 6.0mm | 65 | 50 | 6 | 9.0 metres | 5.16 | 0.225 | |||||||
| ANGLE 65 X 50 X 8.0mm | 65 | 65 | 8 | 9.0 metres | 6.59 | 0.225 | |||||||
| ANGLE 65 X 65 X 4.0mm | 65 | 65 | 4 | 9.0 metres | 3.69 | 0.255 | |||||||
| ANGLE 65 x 65 x 5.0mm | 65 | 65 | 5 | 9.0 metres | 4.56 | 0.255 | |||||||
| ANGLE 65 X 65 X 6.0mm | 65 | 65 | 6 | 9.0 metres | 5.87 | 0.255 | |||||||
| ANGLE 65 X 65 X 8.0mm | 65 | 65 | 8 | 9.0 metres | 7.51 | 0.255 | |||||||
| ANGLE 65 X 65 X 10.0mm | 65 | 65 | 10 | 9.0 metres | 9.02 | 0.255 | |||||||
| ANGLE 75 X 50 X 5.0mm | 75 | 50 | 5 | 9.0 metres | 4.4 | 0.244 | |||||||
| ANGLE 75 X 50 X 6.0mm | 75 | 50 | 6 | 9.0 metres | 5.66 | 0.244 | |||||||
| ANGLE 75 X 50 X 8.0mm | 75 | 50 | 8 | 9.0 metres | 7.23 | 0.244 | |||||||
| ANGLE 75 X 75 X 4.0mm | 75 | 75 | 4 | 9.0 metres | 4.29 | 0.295 | |||||||
| ANGLE 75 X 75 X 5.0mm | 75 | 75 | 5 | 9.0 metres | 5.27 | 0.292 | |||||||
| ANGLE 75 X 75 X 6.0mm | 75 | 75 | 6 | 9.0 metres | 6.81 | 0.292 | |||||||
| ANGLE 75 X 75 X 8.0mm | 75 | 75 | 8 | 9.0 metres | 8.73 | 0.292 | |||||||
| ANGLE 75 X 75 X 10.0mm | 75 | 75 | 10 | 9.0 metres | 10.5 | 0.292 | |||||||
| ANGLE 90 X 90 X 6.0mm | 90 | 90 | 6.0 | 9.0 metres | 8.22 | 0.352 | |||||||
| ANGLE 90 X 90 X 8.0mm | 90 | 90 | 8.0 | 9.0 metres | 10.6 | 0.352 | |||||||
| ANGLE 90 X 90 X 10.0mm | 90 | 90 | 10.0 | 9.0 metres | 12.7 | 0.352 | |||||||
| ANGLE 100 X 75 X 6.0mm | 100 | 75 | 6.0 | 9.0 metres | 7.98 | 0.342 | |||||||
| ANGLE 100 X 75 X 8.0mm | 100 | 75 | 8.0 | 9.0 metres | 10.3 | 0.342 | |||||||
| ANGLE 100 X 75 X 10.0mm | 100 | 75 | 10.0 | 9.0 metres | 12.4 | 0.342 | |||||||
| ANGLE 100 X 100 X 10.0mm | 100 | 100 | 10.0 | 9.0 metres | 14.2 | 0.392 | |||||||
| ANGLE 100 X 100 X 12.0mm | 100 | 100 | 12.0 | 9.0 metres | 17.7 | 0.392 | |||||||
| ANGLE 100 X 100 X 4.0mm | 100 | 100 | 4.0 | 9.0 metres | 5.78 | 0.395 | |||||||
| ANGLE 100 X 100 X 6.0mm | 100 | 100 | 6.0 | 9.0 metres | 9.16 | 0.392 | |||||||
| ANGLE 100 X 100 X 8.0mm | 100 | 100 | 8.0 | 9.0 metres | 11.8 | 0.392 | |||||||
| ANGLE125 X 75 X 6.0mm | 125 | 75 | 6.0 | 9.0 metres | 9.16 | 0.392 | |||||||
| ANGLE 125 X 75 X 8.0mm | 125 | 75 | 8.0 | 9.0 metres | 11.8 | 0.392 | |||||||
| ANGLE 125 X 75 X 10.0mm | 125 | 75 | 10.0 | 9.0 metres | 14.2 | 0.392 | |||||||
| ANGLE 125 X 75 X 12.0mm | 125 | 75 | 12.0 | 9.0 metres | 17.7 | 0.392 | |||||||
| ANGLE 125 X 125 X 8.0mm | 125 | 125 | 8.0 | 9.0 metres | 14.9 | 0.491 | |||||||
| ANGLE 125 X 125 X 10.0mm | 125 | 125 | 10.0 | 9.0 metres | 18 | 0.491 | |||||||
| ANGLE 125 X 125 X 12.0mm | 125 | 125 | 12.0 | 9.0 metres | 22.5 | 0.491 | |||||||
| ANGLE 125 X 125 X 16.0mm | 125 | 125 | 16.0 | 9.0 metres | 29.1 | 0.491 | |||||||
| ANGLE 150 X 90 X 8.0mm | 150 | 90 | 8.0 | 9.0 metres | 14.3 | 0.471 | |||||||
| ANGLE 150 X 90 X 12.0mm | 150 | 90 | 12.0 | 9.0 metres | 21.6 | 0.471 | |||||||
| ANGLE 150 X 90 X 16.0mm | 150 | 90 | 16.0 | 9.0 metres | 27.9 | 0.471 | |||||||
| ANGLE 150 X 100 X 10.0mm | 150 | 100 | 10.0 | 9.0 metres | 18 | 0.491 | |||||||
| ANGLE 150 X 100 X 12.0mm | 150 | 100 | 12.0 | 9.0 metres | 22.5 | 0.491 | |||||||
| ANGLE 150 X 150 X 10.0mm | 150 | 150 | 10.0 | 9.0 metres | 21.9 | 0.59 | |||||||
| ANGLE 150 X 150 X 12.0mm | 150 | 150 | 12.0 | 9.0 metres | 27.3 | 0.59 | |||||||
| ANGLE 150 X 150 X 16.0mm | 150 | 150 | 16.0 | 9.0 metres | 35.4 | 0.59 | |||||||
| ANGLE 150 X 150 X 19.0mm | 150 | 150 | 19.0 | 9.0 metres | 42.1 | 0.59 | |||||||
| ANGLE 150 X 90 X 10.0mm | 150 | 90 | 10.0 | 9.0 metres | 17.3 | 0.471 | |||||||
| ANGLE 200 x 200 x 13.0mm | 200 | 200 | 13.0 | 9.0 metres | 40 | 0.788 | |||||||
| ANGLE 200 X 200 X 16.0mm | 200 | 200 | 16.0 | 9.0 metres | 48.7 | 0.788 | |||||||
| ANGLE 200 X 200 X 20.0mm | 200 | 200 | 20.0 | 9.0 metres | 60.1 | 0.788 | |||||||
| ANGLE 200 X 200 X 26.0mm | 200 | 200 | 26.0 | 9.0 metres | 76.8 | 0.788 | |||||||
SS 316/316L Stainless Steel Angle Surface Type (3)
Informations disponibles pour référence et téléchargement
Daxun is a trustworthy stainless steel Angle manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel angles have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
Projets et produits récents
Produits apparentés (8)
Leading stainless steel angle Suppliers in China
Daxun est engagée dans le commerce international depuis plus de dix ans. En 2023, le volume des exportations a dépassé 100 millions de dollars américains, et le volume des exportations s'est classé parmi les principaux fabricants chinois d'acier inoxydable. Daxun améliore constamment ses compétences en matière de services. Pour servir le marché mondial, elle a établi trois installations de services d'exportation en Chine, coopérant avec des sociétés d'ingénierie, des aciéries et des sociétés de commerce international. Daxun fournit des services de chaîne d'acier inoxydable et a établi des relations de coopération à long terme avec des dizaines d'aciéries de renom dans le monde entier. Le stock comprend 50 000 tonnes d'acier inoxydable conventionnel et 20 000 tonnes d'acier duplex, d'alliages à base de nickel, d'acier résistant à la chaleur et d'autres métaux. Les matériaux en acier inoxydable de Daxun sont de qualité stable, et les variétés, les spécifications et les poids de livraison sont strictement conformes aux normes.
316 Stainless Steel Angle
- 316 Stainless Steel Angle is an austenitic chromium nickel angle shape containing molybdenum which provides superior corrosion resistance and increased strength at elevated temperatures when compared to 304 Stainless.
- Because of the 4% molybdenum concentration, the 316 material is resistant to chloride ion stress corrosion. Stainless Steel 304 Unequal Angle Sizes vary depending on the application needs. Angles are used to hold components together using a grip. There are also angles with bolt holes for screws and bolts. The 316 Stainless Steel Unequal Angle is suitable for more corrosive applications than the 304 angles. The Stainless Steel Unequal Angle is just as frequent as the Equal Angle. They are utilized in a variety of applications, including brackets, trim, and reinforcements. Please contact us for more information about the angles and their costs.
Caractéristiques
- Cold Working: Good
- Corrosion Resistance: Excellent
- Heat Resistance: Good
- Heat Treatment: Poor
- Hot Working: Fair
- Machinability: Good
- Weldability: Very Good
Why should you buy stainless steel angles from Daxun?
Daxun’s objective is to supply you with the highest quality and most durable stainless steel angles and steel. We provide hundreds of stainless steel angles in various leg lengths, thicknesses, and material grades. Our 316/316L and 304/304L stainless steel angles are made at our well-equipped production facility using high-quality raw materials and cutting-edge technology, overseen by qualified workers. Some other significant benefits of partnering with us include:
- When you purchase any steel products from us, you get the products directly from the manufacturer.
- Our employees are dedicated to providing the lowest prices and fastest shipping times so that you can start your project right away!
- We have a skilled, capable workforce for quality checks, packaging, and shipping.
- We follow multiple quality check levels, which helps ensure that the products are of the highest standards.
- We have a qualified and dedicated support team available 24×7 to help you out if any issues arise.
Suppliers from China Make Stainless Steel Angles to Size
- Daxun is a leading supplier of stainless steel products in China. With high-quality products and customized services, we can meet all your stainless steel angle needs. Order online or by phone and get it delivered in as fast as 15 days.
304 and 316 Grade Stainless Steel Angles
- This versatile right angle steel has a wide range of applications and is available in grades 304 /30L and 316 /316L. Grade 304 is the most versatile and commonly used grade of stainless steel angle steel and is suitable for most general applications. It is easy to weld and has good formability and corrosion resistance. Sometimes called 18/8 stainless steel because its composition includes 18% chromium and 8% nickel, grade 304 is well suited to most applications.
- Grade 316 is more suitable for harsh environments, such as exposure to salt water and areas with high industrialization. Due to the higher nickel content and the addition of molybdenum to the metal, it has higher corrosion resistance than grade 304, especially to chlorides and chlorinated solutions. It also has good weldability, but is more difficult to process than grade 304.
There are two basic processes for manufacturing stainless steel angles:
- laser melting and hot rolling. Hot rolled stainless steel angles are less expensive. They typically have rounded or tapered edges. On the other hand, laser melted stainless steel angles have consistent sharp and square corners. They also include sandblasting and a smoother finish. The surface of laser melted stainless steel angles is smoother than that of hot rolled stainless steel angles.
Choose Your Size and Size
- We offer a wide variety of stainless steel angles, so whatever your needs, we have you covered. Grade 304 stainless steel angles come in a variety of sizes with thicknesses from 3mm-16mm and lengths of 1m, 3m, or 6m.
- Our grade 316 angles come in thicknesses from 3mm-16mm and lengths of 1m, 3m, or 6m. Angles are available in a variety of sizes.
Talk to Your Preferred Stainless Steel Angle Supplier
- It couldn’t be easier to buy the stainless steel angles you need, as well as all of our other products, through our website. Alternatively, you can call our sales team in China at +8613382898899 to place your order and they will be happy to process your order. If you have any questions, you can even send an email to daxunalloy@gmail.com and our team will get back to you as soon as possible.
Veuillez remplir le formulaire de la page “Contactez-nous” ou appeler notre responsable des ventes au “+86 13382898899”, nous vous contacterons dans les plus brefs délais. Notre WhatsApp est en ligne, et l'email (Daxunalloy@gmail.com) sera vérifié dans les 6 heures. Chaque demande ou message recevra une réponse rapide. En outre, nous partageons chaque semaine des informations sur le marché avec nos clients
Des échantillons peuvent être fournis gratuitement, mais les frais de transport sont à la charge du client et seront remboursés après coopération.
Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.
Our MOQ is 1 ton for 316L Stainless Steel Angle.
Nous disposons d'une organisation complète allant de l'achat des matières premières au traitement et à l'organisation de l'expédition. Tout au long de la chaîne, le personnel documentaire et le service de contrôle de la qualité vérifient et contrôlent les produits en fonction d'exigences précises.
Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.