Daxun Alloy - Hastelloy C2000 pipe made in China
As a leading supplier of Hastelloy C2000 pipes in China, Daxun provides high-performance alloy tubes to the world.
- Hastelloy C2000 types: Seamless tube, welded tube, forged tube
- Certification : ASTM,SGS,ISO,CE
- Délai de livraison : 7-15 jours
- Finition de la surface : Recuit, poli, etc.
- MOQ : ≥300kg
————Daxun produit des tubes en hastelloy en Chine pour répondre aux besoins divers et variés des consommateurs. ——les besoins exigeants des clients!
Caractéristiques et propriétés de l'Hastelloy C2000
Hastelloy C2000 pipe is a nickel-based alloy pipe with excellent performance, which plays an important role in many industrial fields.It entered the market in late 1995 and has been highly recognized by the market for its versatility.
In terms of composition, it cleverly combines multiple key elements such as nickel, chromium, and molybdenum. Nickel gives the pipe good toughness and basic corrosion resistance; chromium enhances its corrosion resistance in oxidizing environments, enabling it to resist the erosion of various oxidizing media; molybdenum significantly improves the pipe’s resistance to pitting and crevice corrosion in reducing acids, greatly expanding its application range.
Hastelloy C2000 pipe has extremely excellent corrosion resistance. Whether facing harsh chemical media such as strong acids and alkalis, or in extreme environments such as high temperature and high pressure, it can maintain stable chemical properties and effectively resist corrosion. In the chemical industry, many chemical reaction processes will produce extremely corrosive substances, which ordinary pipes cannot withstand, but Hastelloy C2000 pipes can operate stably for a long time to ensure the normal operation of production equipment.
Its mechanical properties are also excellent. It has high strength and good toughness, and can withstand certain pressure and impact without deformation or rupture. This makes it an ideal choice for some occasions that require high mechanical properties of pipes, such as high-pressure pipeline systems and large reaction vessels.
In practical applications, Hastelloy C2000 pipes are widely used. In the petrochemical industry, it is often used in pipeline systems that transport various corrosive media to ensure the safety and stability of the petrochemical production process; in the field of marine engineering, due to its excellent seawater corrosion resistance, it is widely used in seawater desalination equipment, offshore platform pipelines and other facilities; in the power industry, it can be used to manufacture key components such as boiler feed water pipelines to ensure efficient power production.
However, due to the special material and properties of Hastelloy C2000 pipes, its processing difficulty is relatively large. During the welding process, it is necessary to strictly control the welding process parameters and use appropriate welding methods and materials to ensure the welding quality. Otherwise, welding defects are prone to occur, affecting the performance and service life of the pipe.
Paramètres de l'Hastelloy C2000
- Composition chimique
- Propriétés physiques
- Propriétés mécaniques
| Ni | Cr | Mo | W | Cu | Fe | C | Mn |
| 55% - 62% | 15% - 23%| | 6% - 16% | 2% - 4.5% | 1,3% - 1,9% | ≤3.0% | ≤0.01% - 0.25% | ≤0.5% |
| Si | P | S | Al | Ti | Nb | Co | |
| ≤0.08% - 0.080% | ≤0.02% | ≤0.08% | ≤0.3 – 0.5%≤0.2 – 0.5% | ≤3% | ≤2% |
| Propriété | Densité | Point de fusion | Capacité thermique spécifique | Conductivité thermique | Résistivité électrique | Coefficient de dilatation thermique | Module d'élasticité | Dureté | Température de fonctionnement |
| Valeur | 8,4 - 10,6 g/cm³ | 1280 - 1350°C | 0,102 - 0,46 J/(g-°C) | 7 - 13 W/m-K | 1,4 - 1,6 Ω-mm²/m | 12,4 - 20,0 μm/(m-°C) | 206 GPa | 132 - 247 HB | -196°Cà650°C |
| Propriété | Résistance à la traction | Limite d'élasticité | Élongation | Réduction de la surface | Résistance aux chocs | Dureté |
| Valeur | 752 - 1090MPa | 345 - 750MPa | 20% - 62% | ≥40% | ≥90J | 132 - 247HB |
Choisissez Daxun pour faire décoller votre projet.

Production avancée : tube en alliage d'Hastelloy
Hastelloy C2000 alloy is an all-around nickel-chromium-molybdenum-tungsten alloy with good resistance to pitting, crevice corrosion and stress corrosion cracking. It has excellent resistance to oxidative aqueous media, including wet chlorine, nitric acid or mixed acids of oxidizing acids containing chloride ions. At the same time, Hastelloy C2000 alloy also has ideal resistance to reducing and oxidizing environments encountered in the process. Relying on this versatile performance, it can be used in some troublesome environments or in factories for a variety of production purposes.
Hastelloy C-2000 Pipe Features
Hastelloy C2000 alloy has an exceptional resistance to various chemical environments, including strong oxidizing substances, such as ferric chloride, cupric chloride, chlorine, thermally contaminated solutions (organic and inorganic), formic acid, acetic acid, acetic anhydride, seawater and salt solutions, etc. Hastelloy C2000 alloy has the ability to resist the formation of grain boundary precipitation in the heat affected zone of welding, so that it can also be used in many chemical processes in the welding state.


Qualité, livraison, inspection
Daxun conducts a series of quality assurance tests on Hastelloy C2000 pipes. These tests include flattening test, flaring test, ultrasonic flaw detection, crevice corrosion resistance test, mechanical property test, hardness test, material positive identification, and expansion test, etc. All these tests are designed to ensure that the Hastelloy C2000 pipes meet the requirements of the intended applications. During the production process, we meticulously measure the outer diameter, wall thickness, and surface quality of the products. Our standard delivery time is 5 – 7 days, and for special sizes, it is 15 – 20 days.
- Nos délais de livraison sont strictement conformes au contrat.
- Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
- Prise en charge d'échantillons gratuits pour les essais des clients
- Soutien à l'inspection sur site ou à l'inspection vidéo en usine
Emballage
Daxun Alloy garantit la meilleure qualité d'emballage, car celui-ci joue un rôle important dans le fret international, où les marchandises passent par différents canaux avant d'atteindre leur destination finale ; nous accordons donc une attention particulière à l'emballage. Nous emballons nos marchandises de différentes manières, en fonction du produit. Nous emballons nos produits de différentes manières, notamment :
- Boîtes et caisses
- Emballage rétractable
- Palettes en bois
- Boîtes en bois


Support technique
Si vous avez besoin d'une assistance technique supplémentaire, notre métallurgiste résident et notre personnel compétent se feront un plaisir de vous aider. [Nous contacterEn outre, Daxun s'enorgueillit de posséder un laboratoire d'essai certifié, une première dans l'industrie des stocks multimétaux et plastiques. Ceci, à notre avis, démontre notre dévouement inébranlable à la qualité et notre philosophie en tant que fournisseur de services complets.
Daxun est un fabricant de tubes en acier inoxydable digne de confiance.
En tant que fabricant professionnel, Daxun s'assure que tous les produits qu'il fabrique sont de haute qualité. Par conséquent, nous veillons à ce que tous les tubes en titane soient certifiés ISO9001, SGS, CE, OQC et autres normes de qualité internationales. Nous effectuons également un contrôle de qualité strict afin de garantir que les tubes en acier inoxydable présentent moins de défauts. Chez Daxun, vous pouvez être assuré que tous les produits sont durables, de haute qualité et d'excellentes performances.
Produits apparentés (8)
Veuillez remplir le formulaire de la page “Contactez-nous” ou appeler notre responsable des ventes au “+86 13382898899”, nous vous contacterons dans les plus brefs délais. Notre WhatsApp est en ligne, et l'email (Daxunalloy@gmail.com) sera vérifié dans les 6 heures. Chaque demande ou message recevra une réponse rapide. En outre, nous partageons chaque semaine des informations sur le marché avec nos clients
Nous pouvons vous fournir des échantillons de tôles d'acier inoxydable pour vous permettre de vérifier la qualité. L'échantillon est gratuit et vous ne payez que les frais de transport.
Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.
La quantité minimale de commande pour nos produits en Hastelloy est de 300 kg.
Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.