| Product Parameters: Stainless Steel Angle bar | |
| Taille | 20×20×3;25×25×3、25×25×4;30×30×3、30×30×4、30×30×5、30×30×6;40×40×3、40×40×4、40×40×5、40×40×6;50×50×4、50×50×5、50×50×6;60×60×5、60×60×6;65×65×5、65×65×6、65×65×7、65×65×8;70×70×6、70×70×7、 |
| 70×70×8;75×75×6、75×75×7、75×75×8、75×75×9;80×80×8、80×80×9、80×80×10;100×100×8、100×100×9、100×100×10、100×100×12 *Sizes from 100×100 to 150×150 can be customized. | |
| Surface | Décapage 8K, NO.1, NO.4, hairline, etc. |
| longueur | 6000mm ou sur mesure |
| Grade | 304 201 304L 310S 316L 321 904L 2205 2507 S32750 S32760 etc. |
| Normes | ASTM A276, ASTM A484M, DIN 1028, EN10056, GB4227 |
| Caractéristiques | Anti-corrosion (le degré dépend des alliages contenus), résistance à la chaleur, bonnes propriétés de travail à froid et à chaud, bonne ténacité, bonnes performances globales et application étendue. |
Daxun offers stainless steel angle steel in different sizes, material grades, profiles, finishes and other specifications. We can also produce custom stainless steel angles based on your specific needs or applications.
Stainless Steel Angle Steel Grade
Each type of stainless steel angle steel has its own different usage scenarios.
Cliquez sur l'image pour obtenir plus d'informations sur ce produit
Cliquez sur l'image pour obtenir plus d'informations sur ce produit
Cliquez sur l'image pour obtenir plus d'informations sur ce produit
Cliquez sur l'image pour obtenir plus d'informations sur ce produit
Cliquez sur l'image pour obtenir plus d'informations sur ce produit
Cliquez sur l'image pour obtenir plus d'informations sur ce produit
Cliquez sur l'image pour obtenir plus d'informations sur ce produit
Cliquez sur l'image pour obtenir plus d'informations sur ce produit
Performance of stainless steel angle steel
The chemical composition on stainless steel angle bars protects them from rust. Their corrosion resistance is enhanced by the necessary polished finish, making them ideal for architectural use.
Since stainless steel angles have a low melting point, no special tools are required. They are also durable and long-lasting materials, allowing industries to save on work and maintenance costs.
The smarter option material SS angles have far lesser drawbacks than other alloys. They provide excellent value, cost-effectiveness, and durability. SS is an easy-to-clean metal material.
Stainless steel angle material is an excellent choice for a variety of applications such as manufacturing. They are simple to use and ideal for large-scale industrial and complex uses.
Vaste stock de matériel de choix
Daxun dispose de stocks d'acier inoxydable pour les qualités et les tailles courantes afin de répondre rapidement à la demande de ses clients : TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc.


Common areas of stainless steel angle steel
- Stainless steel angle bars are hot-rolled and pickled, making them versatile for use in a wide range of construction and engineering projects. They are commonly used in structures like house beams, bridges, power transmission towers, and shipyards.
Peut être transformé à la largeur souhaitée
1. Prix et qualité compétitifs de notre propre usine
2. Approuvé par ISO9001, CE, SGS chaque année
3. Meilleur service avec une réponse dans les 24 heures
4. Paiement flexible par T/T, L/C, paypal, etc.
5. Capacité de production régulière
6. Livraison rapide et emballage standard pour l'exportation
7. OEM/ODM

Informations techniques
Chez Daxun, nous choisissons différents emballages pour différents produits en acier inoxydable, notamment : papier kraft, boîtes en bois, sacs tissés, palettes en bois, sur la base des normes industrielles les plus strictes afin de garantir que les marchandises arrivent entre vos mains en bon état.
Tous nos matériaux en acier inoxydable sont certifiés par différentes normes industrielles telles que ISO9001:2008, ISO14001:2014, AAA Certification, CQGC Certifications, etc. Notre société est également certifiée par le système de gestion de la qualité ISO9001:2015.
Chez Daxun, nous disposons d'un laboratoire et d'un équipement de test pour garantir que nos matériaux en acier inoxydable sont de poids réel et de bonne qualité avant l'expédition. Notre équipe de contrôle de la qualité effectue également des inspections strictes et 100% à tous les stades de la production.
Notre soutien et nos services ne se limitent pas au début de nos transactions. Même si vous avez reçu vos commandes, Daxun continuera à fournir d'excellents services après-vente. Nous continuerons à fournir une assistance et une garantie pour vos commandes.
Application cases of stainless steel angle in different industries
Stainless steel angles are widely used in the construction field and can be used for exterior wall supports, interior decoration, roofing materials, building structures, etc. Stainless steel is corrosion-resistant and has high strength, which can meet the design requirements of different buildings.
L'acier inoxydable présente les avantages suivants : résistance à la corrosion, absence de rouille, absence de décoloration, élimination facile des aliments attachés, bonnes propriétés mécaniques à haute et basse température. Il est largement utilisé dans les machines alimentaires, telles que les systèmes sanitaires, les réservoirs de fluides, les réservoirs de stockage des aliments, les échangeurs de chaleur, les récipients sous vide, etc.
L'acier inoxydable présente une bonne solidité, une bonne ténacité et une bonne résistance à la corrosion, et il est largement utilisé dans les pièces structurelles des avions. Par exemple, la structure des ailes, les supports du fuselage, les sièges et d'autres composants sont tous fabriqués en acier inoxydable.
Stainless steel angles are also used in the manufacture and maintenance of oil refining equipment, and the brackets used in the petrochemical industry are all made of stainless steel angles.
Principales applications : revêtement d'aile, longerons d'aile, bandes de bord supérieur et inférieur du longeron d'aile, âme, longerons de fuselage, rails de siège, poutre de quille, cadres latéraux, revêtement de fuselage, panneaux de la paroi inférieure du fuselage, longerons du plancher principal, etc.
Stainless steel angle steel is widely used in the shipbuilding industry. The stainless steel angle supplied by Daxun are used in the shipbuilding and petroleum industries. They have high strength, good toughness, and are resistant to seawater corrosion, fatigue, and wear.
SS316L est la principale nuance d'acier inoxydable austénitique utilisée dans les installations offshore, où elle améliore la résistance à des températures élevées et protège les structures contre les environnements acides sévères. L'acier UNS S32205 est la nuance d'acier inoxydable duplex la plus couramment utilisée pour les installations offshore.
The main application of stainless steel angle steel in electricity is the support of power station equipment. The excellent corrosion resistance and high strength of stainless steel make it the preferred material for power generation components.
Mechanical Information
- Stock
- Tolérance
- État de livraison
| Gamme de tailles | |||||||
| Hot-rolled equal-leg angle bar | |||||||
| Désignation | Masse | Désignation | Masse | Désignation | Masse | Désignation | Masse |
| 20x20x3 | 0.88 | 70x70x5 | 5.37 | 120x120x8 | 14.7 | 180x180x16 | 43.5 |
| 25x25x3 | 1.12 | 70x70x6 | 6.38 | 120x120x9 | 16.5 | 180x180x17 | 46 |
| 25x25x4 | 1.45 | 70x70x7 | 7.38 | 120x120x10 | 18.2 | 180x180x18 | 48.6 |
| 25x25x5 | 1.78 | 70x70x8 | 8.37 | 120x120x11 | 19.9 | 180x180x19 | 51.1 |
| 30x30x3 | 1.36 | 70x70x9 | 9.32 | 120x120x12 | 21.6 | 180x180x20 | 53.7 |
| 30x30x4 | 1.78 | 70x70x10 | 10.3 | 120x120x13 | 23.3 | 200x200x13 | 39.8 |
| 30x30x5 | 2.18 | 75x75x4 | 4.65 | 120x120x14 | 25 | 200x200x14 | 42.7 |
| 35x35x3 | 1.6 | 75x75x5 | 5.76 | 120x120x15 | 26.6 | 200x200x15 | 45.6 |
| 35x35x3.5 | 1.85 | 75x75x6 | 6.85 | 120x120x16 | 28.3 | 200x200x16 | 48.5 |
| 35x35x4 | 2.09 | 75x75x7 | 7.93 | 130x130x8 | 16 | 200x200x17 | 51.4 |
| 35x35x5 | 2.57 | 75x75x8 | 8.99 | 130x130x9 | 17.9 | 200x200x18 | 54.3 |
| 38x38x4.5 | 2.56 | 75x75x9 | 10 | 130x130x10 | 19.8 | 200x200x19 | 57.1 |
| 38x38x6 | 3.33 | 75x75x10 | 11.1 | 130x130x11 | 21.7 | 200x200x20 | 59.9 |
| 40x40x3 | 1.84 | 76x76x5 | 5.84 | 130x130x12 | 23.6 | 200x200x21 | 62.8 |
| 40x40x4 | 2.42 | 76x76x6.5 | 7.49 | 130x130x13 | 25.4 | 200x200x22 | 65.6 |
| 40x40x5 | 2.97 | 76x76x8 | 9.11 | 130x130x14 | 27.2 | 200x200x23 | 68.3 |
| 40x40x6 | 3.52 | 76x76x9.5 | 10.7 | 130x130x15 | 29 | 200x200x24 | 71.1 |
| 45x45x3 | 2.09 | 80x80x5 | 6.17 | 130x130x16 | 30.8 | 200x200x25 | 73.9 |
| 45x45x4 | 2.74 | 80x80x6 | 7.34 | 140x140x9 | 19.3 | 200x200x26 | 76.6 |
| 45x45x4.5 | 3.06 | 80x80x7 | 8.49 | 140x140x10 | 21.4 | 200x200x27 | 79.3 |
| 45x45x5 | 3.38 | 80x80x8 | 9.63 | 140x140x11 | 23.4 | 200x200x28 | 82 |
| 45x45x6 | 4 | 80x80x9 | 10.8 | 140x140x12 | 25.4 | 250x250x17 | 64.4 |
| 45x45x7 | 4.6 | 80x80x10 | 11.9 | 140x140x13 | 27.5 | 250x250x18 | 68.1 |
| 50x50x3 | 2.33 | 90x90x5 | 6.97 | 140x140x14 | 29.4 | 250x250x19 | 71.7 |
| 50x50x4 | 3.06 | 90x90x6 | 8.3 | 140x140x15 | 31.4 | 250x250x20 | 75.3 |
| 50x50x5 | 3.77 | 90x90x7 | 9.61 | 140x140x16 | 33.3 | 250x250x21 | 78.9 |
| 50x50x6 | 4.47 | 90x90x8 | 10.9 | 140x140x18 | 37.2 | 250x250x22 | 82.5 |
| 50x50x7 | 5.15 | 90x90x9 | 12.2 | 150x150x10 | 23 | 250x250x23 | 86.1 |
| 50x50x8 | 5.82 | 90x90x10 | 13.4 | 150x150x11 | 25.2 | 250x250x24 | 89.7 |
| 50x50x9 | 6.47 | 90x90x11 | 14.7 | 150x150x12 | 27.3 | 250x250x25 | 93.2 |
| 55x55x4 | 3.38 | 90x90x16 | 20.7 | 150x150x13 | 29.5 | 250x250x26 | 96.7 |
| 55x55x5 | 4.18 | 100x100x6 | 9.26 | 150x150x14 | 31.6 | 250x250x27 | 101 |
| 55x55x6 | 4.95 | 100x100x7 | 10.7 | 150x150x15 | 33.8 | 250x250x28 | 104 |
| 60x60x4 | 3.7 | 100x100x8 | 12.2 | 150x150x16 | 35.9 | 250x250x29 | 107 |
| 60x60x5 | 4.57 | 100x100x9 | 13.6 | 150x150x17 | 38 | 250x250x30 | 111 |
| 60x60x6 | 5.42 | 100x100x10 | 15 | 150x150x18 | 40.1 | 250x250x31 | 114 |
| 60x60x7 | 6.26 | 100x100x11 | 16.4 | 150x150x19 | 42.1 | 250x250x32 | 118 |
| 60x60x8 | 7.09 | 100x100x12 | 17.8 | 150x150x20 | 44.2 | 250x250x33 | 121 |
| 60x60x10 | 8.69 | 100x100x13 | 19.2 | 160x160x12 | 29.3 | 250x250x34 | 124 |
| 63x63x5 | 4.82 | 100x100x14 | 20.6 | 160x160x13 | 31.6 | 250x250x35 | 128 |
| 63x63x6 | 5.72 | 100x100x15 | 21.9 | 160x160x14 | 33.9 | 300x300x25 | 112 |
| 63x63x6.5 | 6.17 | 100x100x16 | 23.2 | 160x160x15 | 36.2 | 300x300x26 | 116 |
| 65x65x4 | 4.02 | 110x110x6 | 10.2 | 160x160x16 | 38.4 | 300x300x27 | 121 |
| 65x65x5 | 4.97 | 110x110x7 | 11.8 | 160x160x17 | 40.7 | 300x300x28 | 125 |
| 65x65x6 | 5.91 | 110x110x8 | 13.4 | 160x160x18 | 42.9 | 300x300x29 | 129 |
| 65x65x7 | 6.83 | 110x110x9 | 15 | 160x160x19 | 45.1 | 300x300x30 | 133 |
| 65x65x8 | 7.73 | 110x110x10 | 16.6 | 160x160x20 | 47.3 | 300x300x31 | 138 |
| 65x65x9 | 8.62 | 110x110x11 | 18.2 | 180x180x13 | 35.7 | 300x300x32 | 142 |
| 65x65x10 | 9.49 | 110x110x12 | 19.7 | 180x180x14 | 38.3 | 300x300x33 | 146 |
| 65x65x11 | 10.3 | 120x120x7 | 12.9 | 180x180x15 | 40.9 | ||
| Hot-rolled unequal-leg angle bar | |||||||
| Désignation | Masse | Désignation | Masse | Désignation | Masse | Désignation | Masse |
| 30x20x3 | 1.12 | 100x50x6 | 6.84 | 125x75x8 | 12.2 | 150x90x10 | 18.2 |
| 30x20x4 | 1.46 | 100x50x8 | 8.97 | 125x75x10 | 15 | 150x90x11 | 19.9 |
| 40x20x4 | 1.77 | 100x65x7 | 8.77 | 125x75x12 | 17.8 | 150x90x12 | 21.6 |
| 40x25x4 | 1.93 | 100x65x8 | 9.94 | 130x90x10 | 16.6 | 150x90x15 | 26.6 |
| 45x30x4 | 2.25 | 100x65x9 | 11.1 | 130x90x12 | 19.7 | 150x100x10 | 19 |
| 50x30x5 | 2.96 | 100x65x10 | 12.3 | 130x90x14 | 22.8 | 150x100x12 | 22.5 |
| 60x30x5 | 3.36 | 100x65x11 | 13.4 | 135x65x8 | 12.2 | 150x100x14 | 26.1 |
| 60x40x5 | 3.76 | 100x65x12 | 14.5 | 135x65x10 | 15 | 200x100x10 | 23 |
| 60x40x6 | 4.46 | 100x75x8 | 10.6 | 140x90x8 | 14 | 200x100x12 | 27.3 |
| 65x50x5 | 4.35 | 100x75x10 | 13 | 140x90x10 | 17.4 | 200x100x14 | 31.6 |
| 70x50x6 | 5.41 | 100x75x12 | 15.4 | 140x90x12 | 20.6 | 200x100x15 | 33.8 |
| 75x50x6 | 5.65 | 110x70x10 | 13.4 | 140x90x14 | 23.8 | 200x100x16 | 35.9 |
| 75x50x8 | 7.39 | 110x70x11 | 15.9 | 150x75x9 | 15.4 | 200x150x12 | 32 |
| 80x40x6 | 5.41 | 120x80x8 | 12.2 | 150x75x10 | 17 | 200x150x15 | 39.6 |
| 80x40x8 | 7.07 | 120x80x10 | 15 | 150x75x12 | 20.2 | ||
| 80x60x7 | 7.36 | 120x80x12 | 17.8 | 150x75x15 | 24.8 | ||
| Tolérance | |||||||||
| Side Width Tolerance for Width | Épaisseur | ||||||||
| 3 4 5 6 7 8 9 10 | |||||||||
| Tolerance for Thickness | |||||||||
| 20 | ±1.5 | ±0.4 | |||||||
| 25 | ±1.5 | ±0.5 | ±0.5 | ||||||
| 30 | ±2.0 | ±0.5 | ±0.5 | ±0.5 | ±0.5 | ||||
| 40 | ±2.0 | ±0.6 | ±0.6 | ±0.6 | ±0.6 | ||||
| 50 | ±2.0 | ±0.6 | ±0.6 | ±0.6 | |||||
| 60 | ±3.0 | ±0.6 | ±0.6 | ||||||
| 65 | ±3.0 | ±0.6 | ±0.6 | ±0.7 | ±0.7 | ||||
| 70 | ±3.0 | ±0.7 | ±0.7 | ±0.7 | |||||
| 75 | ±3.0 | ±0.7 | ±0.7 | ±0.7 | ±0.7 | ||||
| 80 | ±3.0 | ±0.7 | ±0.7 | ±0.7 | ±0.7 | ||||
| 90 | ±3.0 | ±0.7 | ±0.7 | ±0.8 | |||||
| 100 | ±4.0 | ±0.7 | ±0.7 | ±0.8 | |||||
| Choix de l'État de livraison | État de surface |
| Laminés à chaud | Mariné |
| Sablage | |
| Poli | |
| Remarque : | |
| 1. Si vous avez besoin d'un autre pays de livraison que ceux mentionnés ci-dessus, veuillez nous le confirmer. | |
| 2. En cas de demande ou de commande, veuillez nous faire part de toute exigence supplémentaire non indiquée ici. | |
Produit connexe
Daxun Alloy
Regarding stainless steel angle, we can handle any type of inquiry. Please feel free to ask us. We will make recommendations based on each client’s needs.
Oui, nous disposons de spécifications et d'un inventaire complets et pouvons rapidement répondre à vos besoins.
Oui, il peut être personnalisé. Vous pouvez nous contacter et nous envoyer les spécifications et quantités personnalisées.
Nos méthodes de transport comprennent généralement le transport maritime, le transport terrestre et le transport maritime. Ils vous permettent d'arriver à destination rapidement et en toute sécurité.
Parce que notre production est élevée, le coût sera beaucoup plus faible, donc le prix est bas.
We can provide stainless steel angle samples for you to check the quality. Sample is free and you just pay the freight.
Nous attachons une grande importance à la qualité de nos produits et avons passé plusieurs tests de qualité.