x
Envoyez votre demande dès aujourd'hui
Devis rapide

Grade 9 (Ti-3Al-2.5V) Titanium Alloy Plate Manufacturer - Daxun Alloy

As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.

  • Plate Grade:Grade 9 UNS R56320
  • Plate Production type:cold rolling, hot rolling, forging.
  • Standard:ASTM B 265,ASME SB265,AMS491 etc
  • Features:High strength, Lightweight, High-temperature resistance
  • Surface:bright, polished, pickled, sandblasted, etc.
  • Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request

————Daxun produces titanium sheets in China to meet the diverse and ——les besoins exigeants des clients!

Providing High-quality Grade 9 Titanium Plate to Serve Customers Worldwide

Grade 9 titanium plate is a high-performance near-alpha titanium alloy with a nominal composition of Ti-3Al-2.5V. It is based on pure titanium (Grades 1-4) reinforced with appropriate amounts of aluminum and vanadium, achieving an excellent balance of strength and toughness. Compared to pure titanium, Grade 9 boasts significantly higher strength and yield strength while maintaining good ductility and toughness. It is particularly renowned for its excellent weldability and cold formability. This material also offers lightweight, excellent corrosion resistance (especially in chloride environments), and good biocompatibility. It is both strong and durable, yet can withstand a variety of harsh operating conditions, making it an ideal choice for applications requiring high performance and reliability.

Where is Grade 9 titanium plate used?

In the aerospace industry, Grade 9 titanium plate is widely used in the manufacture of aircraft structures, fasteners, hydraulic systems, and engine components. Its combination of high strength and low density effectively reduces aircraft weight and improves fuel efficiency. In marine engineering and shipbuilding, its exceptional resistance to seawater corrosion makes it the material of choice for ship hull structures, desalination equipment, heat exchangers, and offshore platform components, ensuring long-term reliability in harsh marine environments. In the medical industry, Grade 9 titanium plate, due to its excellent biocompatibility and moderate strength, is widely used in the manufacture of orthopedic implants (such as plates and screws), dental implants, and surgical instruments. Furthermore, Grade 9 titanium plate demonstrates its unique value and adaptability in high-end sports equipment (such as bicycle frames and golf club heads), chemical equipment (corrosion-resistant reactors and heat exchangers), and precision mechanical components requiring lightweight and high strength.

Données

Élément Gamme de composition (wt.%)
Ti Solde (>90%)
Al 2.50-3.50%
V 2.00-3.00%
Fe ≤0.25%
O ≤0.13%
C ≤0.08%
N ≤0.03%
H ≤0.015%
Autres ≤0.4% (élément unique)

Caractéristiques principales

  • Rapport résistance/poids: Plus élevé que le titane pur (grades 1-4) mais moins élevé que le Ti-6Al-4V (grade 5).
  • Résistance à la corrosion: Excellent dans les environnements marins, chimiques et chlorés.
  • Biocompatibilité: Non toxique et compatible avec l'IRM, mais moins couramment utilisé dans les implants que le grade 23.
  • Formabilité: Supérieure à la qualité 5 ; convient aux opérations complexes de formage, de soudage et d'usinage.

 Applications typiques

  • Aérospatiale: Tubes hydrauliques, raccords aéronautiques, fixations.
  • Marine: Échangeurs de chaleur, composants pour l'eau de mer, arbres d'hélice.
  • Médical: Instruments chirurgicaux, dispositifs non implantables.
  • Industriel: Équipements de traitement chimique, appareils à pression.
Propriété Valeur (impériale) Valeur (métrique)
Densité 0,160 lb/in³ 4,43 g/cm³
Point de fusion 3,000-3,050°F 1,650-1,680°C
Conductivité thermique 6,5 Btu/(hr-ft-°F) 11,2 W/(m-K)
Coefficient de dilatation thermique 5.3 × 10-⁶/°F 9.5 × 10-⁶/K
Résistivité électrique 120 µΩ-cm 120 nΩ-m

Propriétés à température ambiante (état recuit)

Propriété Valeur (impériale) Valeur (métrique)
Résistance à la traction 130-140 ksi 895-965 MPa
Limite d'élasticité (décalage de 0,2%) 120-125 ksi 825-860 MPa
Élongation 10-15% 10-15%
Réduction de la surface 25-30% 25-30%
Dureté (Brinell) 280-320 HB 290-330 HBW
Module d'élasticité 16,5 × 10⁶ psi 114 GPa

Performance à haute température

Température (°F) Résistance à la traction (ksi) Limite d'élasticité (ksi)
400°F (200°C) 115-125 105-110
600°F (315°C) 100-110 90-95
800°F (425°C) 85-95 75-80

Choisissez Daxun pour faire décoller votre projet.

Common applications

Grade 9 titanium plates and sheets are primarily used for components that require an excellent balance of strength, ductility, and corrosion resistance, offering superior weldability and formability compared to other titanium alloys.

  1. Applications include aerospace components such as airframe structures, pressure vessels, and engine components that require moderate strength but exceptional corrosion resistance.
  2. Industrial applications include chemical processing equipment, heat exchangers, and marine components due to their outstanding resistance to corrosive environments.
  3. Oil and gas industry components, including downhole drilling equipment and subsea systems, where both strength and corrosion resistance are critical.
  4. Medical implants and surgical instruments, particularly where biocompatibility and moderate strength are required.
  5. Performance automotive components, including exhaust systems, suspension parts, and high-performance vehicle frames that benefit from titanium’s strength-to-weight ratio.

Livraison rapide

Daxun provides customers with timely and fast delivery of grade 9 titanium plate products. Behind the speed is the system support from professional production capacity, and information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected.

titanium plate

Custom Cutting

Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:

  • Water jet cutting
  • Laser cutting
  • Plasma cutting
  • Wire cutting
  • Bending
  • Refendage
  • Sciage

Emballage

We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- Boîtes et caisses
- Emballage sous film plastique
- Palettes en bois
- Boîtes en bois

Support technique

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.

Daxun Grade 9 Titanium sheet Let your brand improve rapidly

Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of Plate, Bar and Tube.
Norme relative aux produits/transformations Qualité/taille
Titanium Plate, Sheet, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Epaisseur :( 0.0197”-6”)Largeur maximale : 12 pieds,Longueur maximale : 50 pieds)
AMS-T-9046
Titanium and Titanium alloy sheet, plate
Titane commercialement pur (CP)
Désignation du code Limite d'élasticité
minimum, ksi 1 /
CP-1 Gr1 70
CP-2 Gr2 55
CP-3 Gr3 40
CP-4 Gr4 25
Alliages de titane alpha(A)
Désignation du code Composition
A-1 5A1-2,5Sn
A-2 5A1-2,5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0,8Mo
A-4 8A1-1Mo-1V
Alliages de titane alpha-bêta (AB)
Désignation du code Composition
AB-1 Gr5 6A1-4V
AB-2 Gr5 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2,5V
AB-6 8Mn
Alliages de titane bêta(B)
Désignation du code Composition
B-1 13V-11Cr-3A1
B-2 11,5Mo-6Zr-4,5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
Traitement :
Laminage à chaud Laminage à froid
Classes disponibles :
CP grade 1 Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2)
CP grade 2 Grade 6Al-4V ELI (anciennement grade 23)
7e année Grade 6Al-6V-2Sn (6-62)
19e année Grade 8Al-1Mo-1V (8-1-1)
Grade 5 (6Al-4V) 9e année (3Al-2,5V)
Grade 6 (5Al-2.5Sn) CP grade 3
Application
Industrie chimique Dessalement de l'eau de mer
Industrie pétrochimique Aérospatiale
Domaine de l'usinage, domaine de l'automobile Téléphone mobile Champ des composants.

Projets et produits récents

Grade 9 Titanium Plate and sheet
Naval vessels
Grade 9 Titanium Plate and sheet
Aviation and Aerospace
Titanium Plate and sheet
Armure militaire
Titanium Plate and sheet
Guidance components
Titanium Plate and sheet
Nouvelle industrie de l'énergie
Titanium Plate and sheet
Génie maritime
What makes Grade 9 titanium different from other titanium alloys?

Grade 9 titanium (Ti-3Al-2.5V) offers an optimal balance between strength, ductility, and corrosion resistance. It contains 3% aluminum and 2.5% vanadium, which gives it approximately 20-30% higher strength than pure titanium (Grade 1-4) while maintaining excellent formability and weldability that surpasses many other titanium alloys.

What are the main advantages of using Grade 9 titanium plates in industrial applications?

Grade 9 titanium plates provide exceptional corrosion resistance, high strength-to-weight ratio, excellent weldability, and good formability. These properties make them ideal for applications requiring durability in harsh environments while reducing overall weight, which can lead to improved fuel efficiency in transportation applications.

What are the recommended machining practices for Grade 9 titanium plates?

Machining Grade 9 titanium requires slower speeds, lower feed rates, and ample coolant compared to steel or aluminum. Using sharp, high-quality carbide tools with rigid setups is essential. The material has a tendency to work-harden, so maintaining positive cutting action and avoiding dwell times is important for successful machining.

How does Grade 9 titanium perform in marine environments compared to other alloys?

Grade 9 titanium excels in marine environments, offering outstanding resistance to seawater corrosion, crevice corrosion, and stress corrosion cracking. Unlike many stainless steels that may require regular maintenance or replacement in marine applications, Grade 9 titanium can provide decades of service with minimal degradation, making it cost-effective despite higher initial material costs.

Is Grade 9 titanium suitable for welding and fabrication processes?

Yes, Grade 9 titanium is highly suitable for welding and fabrication. It can be welded using TIG, MIG, plasma arc, and electron beam welding processes. The alloy requires proper shielding from atmospheric contamination during welding, but generally offers excellent weldability without the need for post-weld heat treatment in most applications.

Comment obtenir un devis OU comprendre les informations du marché le plus rapidement possible ?

Veuillez remplir le formulaire de la page “Contactez-nous” ou appeler notre responsable des ventes au “+86 13382898899”, nous vous contacterons dans les plus brefs délais. Notre WhatsApp est en ligne, et l'email (Daxunalloy@gmail.com) sera vérifié dans les 6 heures. Chaque demande ou message recevra une réponse rapide. En outre, nous partageons chaque semaine des informations sur le marché avec nos clients

Puis-je obtenir des échantillons ?

We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.

Quels sont les pays que vous avez déjà exportés ?

Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.

Quel est votre MOQ ?

Our MOQ is 1 ton for titanium sheet.

Quel est le délai de livraison ?

Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.

Envoyez votre demande dès aujourd'hui
Devis rapide