Grade 12 (Ti-0.3Mo-0.8Ni) Titanium Alloy Plate Manufacturer - Daxun Alloy
As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.
- Plate Grade:Grade 12 UNS R53400
- Plate Production type:cold rolling, hot rolling, forging.
- Standard:ASTM B265
- Features:High strength, Lightweight, High-temperature resistance
- Surface:bright, polished, pickled, sandblasted, etc.
- Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request
————Daxun produces titanium sheets in China to meet the diverse and ——les besoins exigeants des clients!
Providing High-quality Grade 12 Titanium Plate to Serve Customers Worldwide
Grade 12 titanium (Ti Grade 12 / UNS R53400) is a nickel-molybdenum-enhanced, commercially pure (CP) titanium alloy specifically engineered for superior corrosion resistance in moderately aggressive environments. It consists of titanium (≥99%) with strategic additions of 0.6–0.9% nickel (Ni) and 0.2–0.4% molybdenum (Mo), which significantly improves its corrosion performance. This nickel-molybdenum modification enhances resistance to reducing acids (e.g., sulfuric, hydrochloric), chloride solutions, and crevice corrosion—conditions where standard CP grades like Grade 2 would show limited performance. While maintaining the inherent advantages of titanium—low density (~4.5 g/cm³), high strength-to-weight ratio, excellent weldability, and biocompatibility—Grade 12 offers improved strength and better corrosion resistance at elevated temperatures (up to ~315°C/600°F) compared to other CP grades. Its passive oxide layer, reinforced by the nickel-molybdenum addition, provides robust protection against chemical attack, making it an excellent choice for applications requiring enhanced corrosion performance without the premium cost of palladium-containing alloys.
Where is Grade 12 titanium used?
Grade 12 titanium is widely utilized in chemical processing for components such as heat exchangers, piping systems, and vessels handling chlorides, organic acids, and reducing media. In marine and offshore applications, it serves in seawater cooling systems, heat rejection equipment, and components exposed to brackish water. The alloy also performs exceptionally well in oil and gas production, particularly in downhole equipment and sour gas environments where hydrogen sulfide resistance is critical. Additionally, Grade 12 finds applications in pollution control systems, pulp and paper processing, and heat management systems. Its cost-effective balance between corrosion resistance and mechanical properties—offering performance superior to standard CP grades but at a lower cost than palladium-enhanced alloys—provides excellent lifecycle value by reducing maintenance requirements and extending service life in corrosive environments. This combination of performance and economics makes Grade 12 titanium a preferred material for demanding applications where both reliability and cost-effectiveness are essential considerations.
Données
- Paramètres
- Propriétés physiques
- Propriétés mécaniques
| Élément | Minimum (%) | Maximum (%) |
|---|---|---|
| Titane (Ti) | Équilibre | Équilibre |
| Molybdène (Mo) | 0.25 | 0.40 |
| Nickel (Ni) | 0.60 | 0.90 |
| Fer (Fe) | — | 0.30 |
| Oxygène (O) | — | 0.25 |
| Carbone © | — | 0.08 |
| Azote (N) | — | 0.03 |
| Hydrogène (H) | — | 0.015 |
| Autres éléments | — | 0.40 (total) |
| Propriété | Value/Range | Unit |
|---|---|---|
| Densité | 4.48 | g/cm³ |
| Point de fusion | 1650 ± 20 | °C |
| Conductivité thermique | 7.2 (at 25°C) | W/m·K |
| Chaleur spécifique | 560 (at 25°C) | J/kg·K |
| Résistivité électrique | 1.7 | μΩ·m |
| Magnetic Susceptibility | Paramagnetic | — |
| Propriété | Minimum Requirement | Typical Value | Unit | Test Method |
|---|---|---|---|---|
| Résistance à la traction | 483 | 520–620 | MPa | ASTM E8/E8M |
| Limite d'élasticité (décalage de 0,2%) | 345 | 380–480 | MPa | ASTM E8/E8M |
| Élongation | 18 | 22–30 | % | ASTM E8/E8M |
| Dureté | ≤ 200 (HV) | 150–180 (HV) | Vickers | ASTM E10 |
| Résistance aux chocs | Not specified | 40–60 | J | ASTM E23 |
Elevated Temperature Performance
| Temperature (°C) | Résistance à la traction (MPa) | Limite d'élasticité (MPa) | Élongation (%) |
|---|---|---|---|
| 100 | 450–500 | 320–370 | 20–25 |
| 200 | 400–450 | 280–330 | 18–23 |
| 300 | 350–400 | 240–290 | 15–20 |
Choisissez Daxun pour faire décoller votre projet.

Common applications
Grade 12 titanium plates and sheets are primarily used in applications that require excellent corrosion resistance in reducing environments, combined with higher strength than pure titanium grades and good weldability.
- Applications include chemical processing equipment such as heat exchangers, pressure vessels, and piping systems that handle hot chlorides and acids.
- Industrial applications include components for pulp and paper manufacturing, where resistance to corrosive chemicals and high temperatures is essential.
- Marine and offshore equipment, including seawater cooling systems, heat exchangers, and components exposed to brackish water environments.
- Oil and gas industry components, particularly for equipment used in sour gas environments containing hydrogen sulfide.
- Power generation equipment, including condenser tubing and other components that operate in corrosive high-temperature environments.
Livraison rapide
Daxun provides customers with timely and fast delivery of grade 12 titanium plate products. Behind the speed is the system support from professional production capacity, and information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected.


Custom Cutting
Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:
- Water jet cutting
- Laser cutting
- Plasma cutting
- Wire cutting
- Bending
- Refendage
- Sciage
Emballage
We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- Boîtes et caisses
- Emballage sous film plastique
- Palettes en bois
- Boîtes en bois


Support technique
If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.
Daxun Grade 12 Titanium sheet Let your brand improve rapidly
- Other Titanium Plate Grades
| Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of Plate, Bar and Tube. | |
| Norme relative aux produits/transformations | Qualité/taille |
| Titanium Plate, Sheet, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136 | GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Epaisseur :( 0.0197”-6”)Largeur maximale : 12 pieds,Longueur maximale : 50 pieds) |
| AMS-T-9046 | |
| Titanium and Titanium alloy sheet, plate | |
| Titane commercialement pur (CP) | |
| Désignation du code | Limite d'élasticité |
| minimum, ksi 1 / | |
| CP-1 Gr1 | 70 |
| CP-2 Gr2 | 55 |
| CP-3 Gr3 | 40 |
| CP-4 Gr4 | 25 |
| Alliages de titane alpha(A) | |
| Désignation du code | Composition |
| A-1 | 5A1-2,5Sn |
| A-2 | 5A1-2,5Sn(ELI) 2 / |
| A-3 | 6A1-2Cb-1Ta-0,8Mo |
| A-4 | 8A1-1Mo-1V |
| Alliages de titane alpha-bêta (AB) | |
| Désignation du code | Composition |
| AB-1 Gr5 | 6A1-4V |
| AB-2 Gr5 | 6A1-4V(ELI) |
| AB-3 | 6A1-6V-2Sn |
| AB-4 | 6A1-2Sn-4Zr-2Mo |
| AB-5 | 3A1-2,5V |
| AB-6 | 8Mn |
| Alliages de titane bêta(B) | |
| Désignation du code | Composition |
| B-1 | 13V-11Cr-3A1 |
| B-2 | 11,5Mo-6Zr-4,5Sn |
| B-3 | 3A1-8V-6Cr-4Mo-4Zr |
| B-4 | 8Mo-8V-2Fe-3A1 |
| Traitement : | |
| Laminage à chaud | Laminage à froid |
| Classes disponibles : | |
| CP grade 1 | Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2) |
| CP grade 2 | Grade 6Al-4V ELI (anciennement grade 23) |
| 7e année | Grade 6Al-6V-2Sn (6-62) |
| 19e année | Grade 8Al-1Mo-1V (8-1-1) |
| Grade 5 (6Al-4V) | 9e année (3Al-2,5V) |
| Grade 6 (5Al-2.5Sn) | CP grade 3 |
| Application | |
| Industrie chimique | Dessalement de l'eau de mer |
| Industrie pétrochimique | Aérospatiale |
| Domaine de l'usinage, domaine de l'automobile | Téléphone mobile Champ des composants. |
Projets et produits récents






Produits apparentés (7)
Grade 12 titanium is a titanium alloy containing 0.3% molybdenum and 0.8% nickel, which provides enhanced strength and superior corrosion resistance compared to commercially pure titanium grades. This combination offers excellent weldability, formability, and stability at elevated temperatures while maintaining good ductility.
While Grade 12 titanium has a higher initial cost than stainless steels, it offers a lower total cost of ownership in corrosive applications due to its extended service life and reduced maintenance requirements. Compared to other titanium grades, Grade 12 is typically priced between Grade 2 and Grade 7 titanium.
Grade 12 titanium maintains its properties at temperatures up to approximately 425°C (800°F). Beyond this temperature, the material may begin to experience reduced mechanical properties, though it still performs better than many competing alloys in high-temperature corrosive environments.
All our Grade 12 titanium plates are supplied with full material test certificates including chemical analysis, mechanical properties, and dimensional verification. We comply with ASTM B265, AMS 4901, and other international standards as required by our customers.
We supply Grade 12 titanium plates in thicknesses ranging from 0.5mm to 100mm, with standard plate dimensions of 1m x 2m or 1.5m x 3m. Custom sizes and thicknesses can be produced to meet specific project requirements.
Veuillez remplir le formulaire de la page “Contactez-nous” ou appeler notre responsable des ventes au “+86 13382898899”, nous vous contacterons dans les plus brefs délais. Notre WhatsApp est en ligne, et l'email (Daxunalloy@gmail.com) sera vérifié dans les 6 heures. Chaque demande ou message recevra une réponse rapide. En outre, nous partageons chaque semaine des informations sur le marché avec nos clients
We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.
Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.
Our MOQ is 1 ton for titanium sheet.
Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.