Grade 23 Ti 6Al-4V ELI Titanium Alloy Pipe Manufacturer
En tant que principal fournisseur de tubes en titane et en alliage de titane en Chine, Daxun fournit des tubes en titane de haute performance au monde entier.
- Tube en titane Grade:Grade 23 – UNS R56401
- Types de tubes en titane:Tube Ti sans soudure, tube Ti soudé, tube Ti forgé
- Titanium tube density The density of grade 23 titanium is 4.43 g/cm3
- Standards:ASTM B338/ASME SB338、ASTM B337/ASME SB337、ASTM B861/ASME SB861、ASTM B862/ASME SB862、AMS4911、AMS4928
----Daxun produit des tubes en titane en Chine pour répondre aux besoins divers et -- exigeants des clients!.
Provide High Quality Grade 23 Titanium Pipe to Customers Around The World
Grade 23 titanium tubing, also known as Ti-6Al-4V ELI, is a high-strength, lightweight alloy composed of titanium with 6% aluminum and 4% vanadium in an extra-low interstitial (ELI) form.It is an improved alloy based on the classic Ti-6Al-4V (grade 5) by further reducing the content of interstitial elements such as oxygen, iron, and nitrogen (such as oxygen content ≤ 0.13%).Its extra-low interstitial (ELI) composition significantly enhances fracture toughness and fatigue resistance compared to standard titanium alloys, allowing it to perform reliably under cyclic loading conditions. The alloy maintains its impressive strength-to-weight ratio even at cryogenic temperatures, unlike many metals that become brittle in extreme cold. Additionally, Grade 23 exhibits superior corrosion resistance in both acidic and chloride environments, outperforming many stainless steels and other titanium grades in aggressive chemical settings.
Where is Grade 23 titanium pipe used?
Grade 23 titanium tubing has unique applications in cutting-edge medical devices, particularly orthopedic implants such as spinal fusion cages and joint replacement components, which require lifelong biocompatibility and fatigue resistance. It is particularly well-suited for dental implant systems, where osseointegration (a direct structural connection between bone and implant) is crucial to the long-term success of the system. In aerospace, it is the material of choice for hydraulic and fuel lines in commercial and military aircraft, which must balance weight reduction with extreme pressure requirements. The material’s properties also make it an ideal choice for high-performance bicycle frames used by professional cyclists, where its vibration-absorbing properties and fatigue resistance provide a competitive advantage.
Key Notes:
ELI (Extra Low Interstitial): Grade 23 has stricter limits on oxygen, nitrogen, hydrogen, and carbon compared to standard Grade 5 (Ti-6Al-4V) to enhance ductility and biocompatibility.
Primary alloying elements: Aluminum (Al) and vanadium (V) contribute to strength and phase stability.
Impurity control: Low iron, carbon, nitrogen, and hydrogen ensure superior corrosion resistance and fatigue performance.
Key performance:
High strength + high toughness: tensile strength can reach 895-930 MPa (annealed state), elongation ≥10%, better than ordinary Grade 5, suitable for scenes with dynamic loads.
Excellent corrosion resistance: acid resistance (such as hydrochloric acid, sulfuric acid), alkali resistance, seawater resistance, outstanding performance in medical implants and chemical equipment.
Biocompatibility: non-magnetic, non-toxic, excellent compatibility with human tissue, is the preferred material for orthopedic implants.
Processability: can be formed by forging, rolling, machining, welding performance is better than ordinary titanium alloy.
Données
- Paramètres
- Propriétés mécaniques
- Propriétés physiques
| Élément | Ti | Al | V | O | Fe | C | N | H | Other elements |
| Gamme de composition (wt.%) | >89% | 5.50 – 6.75% | 3.50 – 4.50% | ≤ 0.13% | ≤ 0.25% | ≤ 0.08% | ≤ 0.05% | ≤ 0.0125% | ≤ 0.4% |
| Propriété | Valeur |
|---|---|
| Résistance ultime à la traction | 860-950 MPa |
| Limite d'élasticité | 825-860 MPa |
| Élongation | 10-15% |
| Résistance à la fatigue | ~500 MPa (at 10⁷ cycles) |
| Résistance à la rupture | 70-90 MPa√m |
| Dureté | 320-350 HV |
| Module d'élasticité | 90-110 GPa |
| Propriété | Valeur |
|---|---|
| Densité | 4,43 g/cm³ |
| Point de fusion | 1660-1680°C |
| Conductivité thermique | 7.2 W/m·K |
| Coefficient de dilatation thermique | 8.6 × 10⁻⁶ /°C |
| Résistivité électrique | 1.78 μΩ·m |
| Capacité thermique spécifique | 560 J/kg·K |
Choisissez Daxun pour faire décoller votre projet.

Advanced Production
We offer a comprehensive selection of Grade 23 titanium tubing solutions, including both welded and seamless options to meet diverse industrial requirements. Our inventory features precision-engineered tubes manufactured to the highest quality standards, ensuring optimal performance in demanding applications. Whether you need welded tubes for cost-effective solutions or seamless tubes for superior pressure capabilities, our Grade 23 titanium products deliver exceptional strength-to-weight ratios, outstanding corrosion resistance, and biocompatibility for aerospace, medical, marine, and chemical processing industries.
Rapports d'essais
We provide comprehensive documentation and certification reports for all our Grade 23 titanium tubing, ensuring complete transparency and compliance with industry standards. Our documentation package includes material test reports (MTRs), chemical analysis certificates, mechanical property verification, and non-destructive testing results. Each batch of our Grade 23 titanium tubes comes with full traceability records, detailing the manufacturing process, heat treatment information, and quality assurance protocols.


Qualité, livraison, inspection
Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 23 Titanium Welded Pipe and Grade 23 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.
- Nos délais de livraison sont strictement conformes au contrat.
- Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
- Prise en charge d'échantillons gratuits pour les essais des clients
- Soutien à l'inspection sur site ou à l'inspection vidéo en usine
Support technique
Si vous avez besoin d'une assistance technique supplémentaire, notre métallurgiste résident et notre personnel compétent se feront un plaisir de vous aider. En outre, Daxun dispose d'un laboratoire d'essai certifié, une première dans l'industrie des stocks multimétaux et plastiques. Ceci, à notre avis, démontre notre dévouement inébranlable à la qualité et notre philosophie en tant que fournisseur de services complets.

Daxun Grade 23 Titanium TUBE Let your brand improve rapidly
- Galerie
Grade 23 titanium tube form (4)
Projets et produits récents
Produits apparentés (5)
Grade 23 titanium pipe (Ti-6Al-4V ELI) is an extra low interstitial version of the popular Grade 5 titanium alloy. It contains reduced levels of oxygen, iron, and other interstitial elements, which results in improved fracture toughness, better fatigue resistance, and enhanced biocompatibility while maintaining high strength-to-weight ratio.
Grade 23 titanium tubes offer excellent biocompatibility, reducing the risk of adverse reactions when implanted in the human body. They have a modulus of elasticity closer to bone than many other metals, which helps reduce stress shielding. Additionally, their superior fatigue resistance ensures long-term performance in load-bearing medical applications.
Grade 23 titanium tubes exhibit outstanding corrosion resistance in most environments, including seawater, chlorides, and acidic conditions. The protective oxide layer that forms on the surface provides exceptional resistance to pitting and crevice corrosion, making them suitable for marine and chemical processing applications.
We offer Grade 23 titanium tubes in a comprehensive range of sizes, with outer diameters from 6mm to 120mm and wall thicknesses from 0.5mm to 10mm. We can also provide custom dimensions and special tolerances to meet specific project requirements.
Yes, we can supply Grade 23 titanium tubes with various surface treatments including anodizing, passivation, polishing, and coating options. These treatments can enhance specific properties such as wear resistance, friction characteristics, or aesthetic appearance depending on your application needs.
All our Grade 23 titanium tubes undergo rigorous quality control including ultrasonic testing, eddy current inspection, and dimensional verification. We provide full material traceability and complete documentation including chemical analysis, mechanical properties, and non-destructive testing reports with every order.
Bien que la qualité du titane augmente légèrement le coût, le coût total est principalement déterminé par la forme du titane dont vous avez besoin.
DAXUN propose une large gamme de produits en titane, notamment des tubes, des bobines et des barres. La longueur, la largeur et la quantité de chaque article dont vous avez besoin influencent le montant que vous payez à la caisse.
Malheureusement, il est difficile d'établir un prix en ligne sans en savoir plus sur votre projet et sur l'utilisation du titane.
Heureusement, notre équipe d'experts est toujours là pour vous aider et vous conseiller dans vos besoins en titane. En envoyant un e-mail à daxunalloy@gmail.com, nous pourrons vous donner des conseils et un devis précis.
Veillez à inclure autant d'informations que possible sur le grade, la forme et la quantité de titane dont vous avez besoin afin d'obtenir une meilleure compréhension de vos besoins.
Veuillez remplir le formulaire de la page “Contactez-nous” ou appeler notre responsable des ventes au “+86 13382898899”, nous vous contacterons dans les plus brefs délais. Notre WhatsApp est en ligne, et l'email (Daxunalloy@gmail.com) sera vérifié dans les 6 heures. Chaque demande ou message recevra une réponse rapide. En outre, nous partageons chaque semaine des informations sur le marché avec nos clients
We can provide titanium tube samples for you to check the quality. Sample is free and you just pay the freight.
Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.