Tôle d'acier inoxydable
Daxun maintains a standing inventory of 30,000 tons of stainless steel plate, divided between cold-rolled thin plate and hot-rolled medium-to-heavy plate. Surface processing services are available, including polishing, brushing, and pickling. For common grades such as 304, 316L, and 321, this stock lets us confirm availability and quote turnaround on the same day you send your specification — no need to wait on a new mill run for standard sizes.
Présentation des tôles en acier inoxydable de Daxun
| Paramètres du produit : Tôle d'acier inoxydable | |||
| Grade | 201,304,304L,316,316L,317,321,309,310S,2205,2507,904L,409,410,420,430,436,444,441,17-4 etc. | ||
| Largeur | 10mm~2500mm | ||
| Épaisseur | 0,2mm~100mm | Tolérance d'épaisseur | +/-0,03 mm |
| Standard | ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2 | ||
| Surface | 2B,BA,8K,NO.1,NO.4,NO.3,hairline,damier,or ,noir ,or rose,etc. | ||
| spécification | 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L | ||
| Origine du moulin | TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc. | ||
| Certification | ISO, SGS, BV, TUV, CE, etc. | ||
A Wide Range of Steel Grades
Daxun Alloy supplies stainless steel sheet in cold-rolled and hot-rolled
form across the austenitic, ferritic, and duplex grade range — including
304, 316L, 321, 409, 430, and 2205. Send your grade, thickness, and
application, and we’ll confirm availability and lead time.
Excellent Flatness and Thickness Accuracy
Every coil is checked for flatness and thickness against the applicable
standard tolerance (e.g. ASTM A480) before shipment, under an in-process
quality control system. Consistent tolerance is what keeps formability and
corrosion performance predictable from sheet to sheet.
Finition de surface
Automated rolling control keeps surface condition consistent across the
full range — from 2B mill finish to polished and brushed finishes.
Confirm the finish grade with your order and we’ll match it to the
applicable standard.
Stainless Steel Sheet — Grades and Finishes
Daxun supplies stainless steel sheet in austenitic grades — including 201,
304, 304L, 304J1, 321, 316, 316L, 317L, and 316Ti — with standard surface
finishes including 2B, BA, No.1, No.4, 8K, SB, and HL.
Send your grade, thickness, and finish requirement, and we’ll confirm
availability and lead time.
Nuances et caractéristiques des tôles en acier inoxydable
Chaque matériau de plaque d'acier inoxydable a ses propres scénarios d'utilisation.
Les tôles en acier inoxydable 201 sont peu coûteuses et conviennent aux matériaux de décoration des bâtiments, aux boîtiers d'équipements et de machines, etc.
Résistant à la corrosion,Convient à la décoration des bâtiments, à l'alimentation et à la médecine, aux machines et équipements, etc.
Résistant à la corrosion,Convient aux équipements chimiques, à l'alimentation et à la médecine, aux équipements mécaniques
Résistant à la corrosion,Convient à l'énergie chimique, à l'ingénierie marine, à l'équipement mécanique
Résistant à la corrosion,Convient à l'énergie chimique, à l'ingénierie marine, à l'équipement mécanique, etc.
Résistance à la corrosion,Résistance aux températures élevées,Convient à l'énergie chimique, à l'ingénierie marine, à l'équipement mécanique.
Résistance à la corrosion,Résistance aux températures élevées,Convient aux équipements de chaudière, aux équipements résistants à la chaleur, aux équipements mécaniques.
haute résistance,Convient à l'industrie du raffinage, à la pétrochimie et à l'industrie maritime.
Types de formes de tôles en acier inoxydable
Si la forme dont vous avez besoin n'est pas disponible ici, veuillez nous contacter.
L'épaisseur des tôles en acier inoxydable varie de 0,3 mm à 50 mm en fonction de l'utilisation requise. Elles sont idéales pour la construction, la construction de machines, l'équipement industriel et les matériaux décoratifs.
Les tôles ondulées en acier inoxydable sont souvent utilisées dans les matériaux de construction, tels que les panneaux de toit utilisés dans les usines. Elles possèdent d'excellentes propriétés anticorrosion, ont une longue durée de vie et sont plus durables.
Les plaques polies en acier inoxydable peuvent traiter différentes surfaces, telles que les plaques en acier inoxydable brossé, les plaques en acier inoxydable miroir et les plaques en acier inoxydable mat. Vous avez le choix entre une grande variété d'options.
Les tôles structurales en acier inoxydable conviennent pour les structures, les sols antidérapants, les panneaux décoratifs, etc. Elles sont formées à l'aide de techniques de laminage à chaud et à froid. Ces panneaux en acier sont disponibles en couleur naturelle sur demande.
Performance des tôles en acier inoxydable
Vaste stock de matériel de choix
Daxun keeps stainless steel sheet in stock across common grades and sizes, so most orders ship without waiting on a new production run — with additional grades and thicknesses available to source on request. Every order, whether from stock or sourced to spec, goes through the same inspection process and ships with a mill test certificate.
Options de finition de la tôle d'acier inoxydable
Daxun’s stainless steel sheet comes in a range of finishes: brushed (hairline/HL) for a uniform grain that hides scratches, sandblasted for an even matte surface, mirror (up to 8K) for high-gloss polish, laser-etched for permanent patterns, and embossed for raised decorative or anti-slip textures. Confirm the finish grade with your order.
Contrôle strict de la qualité
Daxun cuts and finishes stainless steel sheet to your exact size
specifications. Our quality management system is certified to ISO 9001, and
every shipment is accompanied by a mill test certificate. Material is
inspected on receipt and again before it leaves our warehouse, with full
traceability from source to delivery.
Traitement et personnalisation des plaques d'acier inoxydable
Daxun’s processing capability includes laser cutting, water jet cutting,CNC bending, and CNC shearing — covering both straight and contoured cuts, and forming to your specified angles and dimensions.Send us your drawing with the required dimensions and tolerances, and we’ll confirm feasibility, pricing, and lead time for cutting and bending to your specification.
Emballage des tôles en acier inoxydable
Daxun matches packaging to the product and shipping method — including kraft paper wrapping, wooden crates, woven bags, and wooden pallets — to protect surface finish and prevent damage in transit. Packaging is confirmed with you before shipment based on your order size and destination.
Daxun’s quality management system is certified to ISO 9001:2015. Every
shipment includes a mill test certificate, and material is traceable from
source to delivery.
Daxun maintains an in-house testing laboratory to verify that every shipment meets the specified weight and quality standard before delivery. Our quality control team performs 100% inspection at every production stage.
Our support doesn’t end when your order ships. Daxun continues to provide after-sales assistance and warranty support for every order.
Cas d'application des tôles en acier inoxydable dans différentes industries
Stainless steel plate is widely used in construction, including exterior
wall cladding, interior decoration, roofing, and structural applications.
Its corrosion resistance and mechanical strength make it suitable for both
long-term exposed applications and structural load-bearing use, while
surface finish options (brushed, mirror, embossed) support a range of
architectural design requirements.
Corrosion resistance and a smooth, easy-to-clean surface make stainless
steel plate well suited to food machinery applications — including
sanitation systems, fluid pipe troughs, food storage tanks, heat
exchangers, and vacuum vessels. Mechanical properties remain stable across
a wide temperature range, supporting both hot processing and cold storage
equipment.
Stainless steel plate offers a combination of strength, toughness, and
corrosion resistance suited to demanding structural applications.
Petroleum refining equipment manufacturing and maintenance uses medium-thick
plate and cold-rolled sheet in grades including 321 and 316L. Typical
specification for petrochemical vessel applications: SUS316, thickness
0.3-0.6mm, width 1219-1520mm, surface finish 2B/2D.
Stainless steel plate is used in shipbuilding for its resistance to
seawater corrosion, along with strength, toughness, and fatigue resistance
— properties suited to the demanding marine environment.
316L is a widely used austenitic stainless steel grade for offshore
installations, offering a stable combination of mechanical strength and
resistance to chloride-induced corrosion in marine environments.
Duplex stainless steels combine high mechanical strength with strong
resistance to stress corrosion cracking, making them well suited to
offshore applications. UNS S32205 is the most commonly used duplex grade
for offshore installations.
Stainless steel plate is used in power generation applications for its
corrosion resistance and mechanical strength, supporting components that
operate under demanding thermal and structural conditions.
Nos tôles d'acier inoxydable en stock ont les dimensions suivantes
- Fiche technique
- Tolérances et état de livraison
- Finitions de surface
| Épaisseur (mm) | Largeur (mm) | Longueur (mm) | Commentaire |
| 0.5 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 0.8 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 1.0 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 1.5 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 2.5 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 3.0 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 5.0 | 1500/1800/2000 | 3000/6000/8000 | AAA |
| 6-8.0 | 1500/1800/2000 | 3000/6000/8000 | AAA |
| 1.0-20.0 | 1500/1800/2000 | 3000/6000/8000 | AAA |
| 20.0-50.0 | 1500/1800/2000 | 3000/6000/8000 | AAA |
| 50.0+ | 1500/1800/2000 | 3000/6000/8000 | AAA |
| Tolérances | |||||
| Rang de tolérance | |||||
| Taille | Groupe 1 | Groupe 2 | Groupe 3 | État de livraison | État de surface |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 | Laminés à froid | 2B 2D BA Ligne de démarcation des cheveux N° 3 N°4 6K 8K |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 | ||
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 | ||
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 | ||
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 | ||
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 | ||
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 | ||
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 | ||
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 | ||
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 | ||
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 | ||
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 | ||
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 | État de livraison | N°1 N° 3 N°4 6K 8K Mariné |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 | ||
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 | ||
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 | ||
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 | ||
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 | ||
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 | ||
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 | ||
| Remarque : 1. Si vous avez besoin d'un autre pays de livraison que ceux mentionnés ci-dessus, veuillez nous le confirmer. 2. En cas de demande ou de commande, veuillez nous faire part de toute exigence supplémentaire non indiquée ici. |
|||||
| Désignation de la finition | Méthode et degré de finition |
| N°1 | Après le laminage à chaud, un traitement thermique, un décapage ou un autre traitement équivalent est appliqué. |
| No.2D | Le recuit et le décapage sont effectués après le laminage à froid ; le matériau est doux avec une surface d'un éclat blanc argenté ; il est utilisé pour des applications générales et l'emboutissage. |
| No.2B | Après la finition 2D, le laminage de la peau est effectué pour obtenir un lustre plus approprié ; la surface devient très exquise ; elle est utilisée pour des applications générales. |
| N° 3 | Finition intermédiaire de grain 100-120 ; utilisée pour les applications dans lesquelles le polissage de la surface est effectué après la mise en forme. |
| N°4 | Finition générale de grain 150-180 ; utilisée pour les restaurants et les équipements et outils de cuisine. |
| #240 | Finition en grain 240 ; utilisé lorsqu'une finition plus fine que le n° 4 est requise ; généralement pour les restaurants et les équipements et outils de cuisine. |
| #320 | Produit poli avec une finition au grain 320. |
| HL | Cette finition est réalisée par un polissage linéaire continu à l'aide d'un abrasif de granulométrie appropriée ; elle est principalement utilisée pour les applications architecturales. |
| BA | Obtenu en effectuant un recuit brillant après le laminage à froid, puis un laminage par passes de peau pour obtenir une réflectance encore plus grande ; offre une excellente résistance à la corrosion ; utilisé pour les appareils électroménagers, les équipements de cuisine et les automobiles. |
| 8K | Grâce à de multiples meulages, il atteint une très grande luminosité et une très grande douceur, comme un miroir. |
Produit connexe
Daxun Alloy
We handle all types of stainless steel plate inquiries — send us your
requirements and we’ll recommend the right grade and specification for
your application.
Stainless Steel Sheet Supplier in China
Daxun supplies stainless steel sheet in a range of finishes, with free
cutting service and dependable delivery — so you can source everything you
need from a single supplier.
Surface Finishes
Available finishes include brushed (hairline), sandblasted, mirror (8K),
laser-etched, and embossed.
Protective Film
Daxun’s stainless steel sheet ships with a protective film on the finished
surface, which can be peeled off after installation or fabrication to
protect against scratches and marks during handling. The reverse side is
left unfilmed.
Grade
300-series stainless steel is the most commonly used type, offering good
formability, corrosion resistance, and weldability.
Sizing and Cutting
Daxun supplies stainless steel sheet across a wide range of thicknesses and
sheet sizes, with free cutting service included on every order to meet
your exact dimensions.
How to Order
Send us your specifications by email or phone, and our team will confirm
availability, pricing, and lead time.
Courriel : daxunalloy@gmail.com
Phone: +86 133 8289 8899
We offer three shipping methods — sea, land, and air — to get your order
to you reliably.
Important Safety Note
Sheet edges are not polished, ground, or deburred and may be sharp, as with
any raw stainless steel plate. Please handle, install, and use with
appropriate care.
Oui, nous disposons de spécifications et d'un inventaire complets et pouvons rapidement répondre à vos besoins.
Oui, il peut être personnalisé. Vous pouvez nous contacter et nous envoyer les spécifications et quantités personnalisées.
Nos méthodes de transport comprennent généralement le transport maritime, le transport terrestre et le transport maritime. Ils vous permettent d'arriver à destination rapidement et en toute sécurité.
Parce que notre production est élevée, le coût sera beaucoup plus faible, donc le prix est bas.
Nous pouvons vous fournir des échantillons de tôles d'acier inoxydable pour vous permettre de vérifier la qualité. L'échantillon est gratuit et vous ne payez que les frais de transport.
Nous attachons une grande importance à la qualité de nos produits et avons passé plusieurs tests de qualité.