x
Envoyez votre demande dès aujourd'hui
Devis rapide

CP Grade 4 Titanium Plate Manufacturer - Daxun Alloy

As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.

  • Plate Grade:UNS R50700
  • Plate Production type:cold rolling, hot rolling, forging.
  • Features:High strength, Lightweight, High-temperature resistance
    • Surface:bright, polished, pickled, sandblasted, etc.
  • Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request

————Daxun produces titanium sheets in China to meet the diverse and ——les besoins exigeants des clients!

Providing High-quality CP Grade 4 Titanium Plates to Serve Customers Worldwide

CP Grade 4 Titanium Plate stands as the strongest of the commercially pure (CP) titanium grades, offering an exceptional combination of high strength and outstanding corrosion resistance. This grade is distinguished by its higher allowable oxygen content, which directly contributes to its superior mechanical properties compared to other CP titanium grades, making it a highly sought-after material for demanding industrial applications.

In terms of specifications, CP Grade 4 conforms to standards like ASTM B265 and AMS 4901. Its chemical composition is tightly controlled, featuring a maximum oxygen content of 0.40%, which is the key to its enhanced strength. This results in a minimum tensile strength of 550 MPa (80,000 psi) and a minimum yield strength of 480 MPa (70,000 psi), while still maintaining a respectable elongation of 15-25%. With a density of approximately 4.51 g/cm³, it provides a high strength-to-weight ratio, a characteristic benefit of all titanium alloys.

Applications of CP Grade 4 Titanium Plate

The robust properties of CP Grade 4 titanium plate make it an ideal choice for a wide range of critical applications. It is extensively used in the aerospace industry for components such as jet engine parts and airframe fasteners where both strength and reliability are paramount. Its excellent resistance to corrosive environments, including seawater and industrial chemicals, makes it a staple in marine engineering, chemical processing equipment, and desalination plants. Furthermore, its biocompatibility allows for its use in certain medical implants, and it is also found in demanding sectors like pulp and paper production and corrosive waste disposal systems.

For projects that require a material that bridges the gap between the lower-strength CP grades and the more complex titanium alloys, CP Grade 4 titanium plate is often the perfect solution. It delivers superior performance in harsh environments without the need for alloying, ensuring long-term durability and structural integrity. This makes it a versatile and valuable material for any engineer or procurement manager looking to specify high-performance titanium for their products.

Compared with other pure titanium grades

The core difference between CP Grade 4 and the other commercially pure (CP) titanium grades (Grades 1, 2, and 3) is a trade-off between strength and formability, which is controlled by their oxygen content.

  • Grade 1: The softest and most ductile (easiest to form). It has the lowest strength.
  • Grade 2: The most common “workhorse” grade. It offers the best all-around balance of strength and formability.
  • Grade 3: Stronger than Grade 2, but less formable. It’s used less frequently.
  • Grade 4: The strongest of all the CP grades. However, it is also the least formable and the most difficult to cold-work.

In short, as you move from Grade 1 to Grade 4, strength increases, but formability decreases.

So, the choice depends on your project’s priority: if you need maximum strength for a less complex shape, choose Grade 4. If you need to form the material into complex shapes, Grade 1 or 2 would be a better choice.

Lire la suite

Données

Élément Maximum Content (%)
Azote (N) 0.05
Carbone © 0.08
Hydrogène (H) 0.015
Fer (Fe) 0.50
Oxygène (O) 0.40
Titane (Ti) Équilibre
Propriété Valeur
Densité 4.51 g/cm³ (0.163 lb/in³)
Point de fusion 1660°C (3020°F)
Conductivité thermique ~16.4 W/m·K (114 BTU·in/hr·ft²·°F)
Résistivité électrique 5.4 × 10⁻⁵ Ω·cm
Coefficient of Thermal Expansion (20–100°C) 8.6 µm/m·°C
Propriété Valeur
Résistance à la traction, ultime 550 MPa (80,000 psi) min
Résistance à la traction, limite d'élasticité 480 MPa (70,000 psi) min
Allongement à la rupture 15–25%
Module d'élasticité ~104 GPa (15,100 ksi)
Dureté, Vickers ~280 HV

Choisissez Daxun pour faire décoller votre projet.

Livraison rapide

At Daxun Alloys Co., Ltd., we specialize in the rapid supply of premium CP Grade 4 titanium plates to meet your urgent project needs. With our extensive inventory and efficient logistics network, we ensure prompt delivery without compromising on quality. Whether you require standard sizes or custom-cut solutions, our team is committed to providing reliable, on-time service to support your manufacturing and engineering schedules.

Custom Cutting

Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:

  • Water jet cutting
  • Laser cutting
  • Plasma cutting
  • Wire cutting
  • Bending
  • Refendage
  • Sciage

Emballage

We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- Boîtes et caisses
- Emballage sous film plastique
- Palettes en bois
- Boîtes en bois

Support technique

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.

Daxun CP Grade 4 Titanium sheet Let your brand improve rapidly

Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of Plate, Bar and Tube.
Norme relative aux produits/transformations Qualité/taille
Titanium Plate, Sheet, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Epaisseur :( 0.0197”-6”)Largeur maximale : 12 pieds,Longueur maximale : 50 pieds)
AMS-T-9046
Titanium and Titanium alloy sheet, plate
Titane commercialement pur (CP)
Désignation du code Limite d'élasticité
minimum, ksi 1 /
CP-1 Gr1 70
CP-2 Gr2 55
CP-3 Gr3 40
CP-4 Gr4 25
Alliages de titane alpha(A)
Désignation du code Composition
A-1 5A1-2,5Sn
A-2 5A1-2,5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0,8Mo
A-4 8A1-1Mo-1V
Alliages de titane alpha-bêta (AB)
Désignation du code Composition
AB-1 Gr5 6A1-4V
AB-2 Gr5 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2,5V
AB-6 8Mn
Alliages de titane bêta(B)
Désignation du code Composition
B-1 13V-11Cr-3A1
B-2 11,5Mo-6Zr-4,5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
Traitement :
Laminage à chaud Laminage à froid
Classes disponibles :
CP grade 1 Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2)
CP grade 2 Grade 6Al-4V ELI (anciennement grade 23)
7e année Grade 6Al-6V-2Sn (6-62)
19e année Grade 8Al-1Mo-1V (8-1-1)
Grade 5 (6Al-4V) 9e année (3Al-2,5V)
Grade 6 (5Al-2.5Sn) CP grade 3
Application
Industrie chimique Dessalement de l'eau de mer
Industrie pétrochimique Aérospatiale
Domaine de l'usinage, domaine de l'automobile Téléphone mobile Champ des composants.

Projets et produits récents

CP Grade 4 Titanium Titanium Plate and sheet
Naval vessels
Titanium Plate and sheet
Aviation and Aerospace
Titanium Plate and sheet
Armure militaire
Titanium Plate and sheet
Guidance components
Titanium Plate and sheet
Nouvelle industrie de l'énergie
Titanium Plate and sheet
Génie maritime
What is CP Grade 4 Titanium and why is it special?

CP Grade 4 is the strongest of all the commercially pure (CP) titanium grades. Its high strength comes from a higher oxygen content, making it an excellent choice when you need more durability than Grade 2 or 3 titanium, but don’t want to move to a more complex alloy. It combines superior strength with outstanding corrosion resistance.

How does Grade 4 Titanium compare to stainless steel?

While both are corrosion resistant, Grade 4 titanium offers a significantly higher strength-to-weight ratio—it’s about 40% lighter than stainless steel but can be just as strong. It also provides far superior resistance to chlorides (like saltwater) and many industrial chemicals, making it ideal for marine and chemical environments where stainless steel might fail.

Is Grade 4 Titanium difficult to weld or machine?

It can be welded using standard titanium welding procedures (like TIG or MIG) with proper inert gas shielding. For machining, it requires sharp tools, slower speeds, and ample coolant, much like other titanium grades. It’s more challenging than stainless steel but very manageable with the right equipment and techniques.

What industry standards do your Grade 4 Titanium Plates meet?

Our Grade 4 Titanium plates fully comply with major international standards, including ASTM B265 (for plate, sheet, and strip) and AMS 4901. We can provide material test certificates (MTCs) to verify the chemical composition and mechanical properties upon request.

What sizes and surface finishes can you supply?

We typically stock Grade 4 Titanium plates in a range of standard thicknesses and widths. Common finishes include hot-rolled, pickled, or polished. For specific dimensions or custom fabrication, please contact our sales team with your requirements, and we will be happy to assist you.

Comment obtenir un devis OU comprendre les informations du marché le plus rapidement possible ?

Veuillez remplir le formulaire de la page “Contactez-nous” ou appeler notre responsable des ventes au “+86 13382898899”, nous vous contacterons dans les plus brefs délais. Notre WhatsApp est en ligne, et l'email (Daxunalloy@gmail.com) sera vérifié dans les 6 heures. Chaque demande ou message recevra une réponse rapide. En outre, nous partageons chaque semaine des informations sur le marché avec nos clients

Puis-je obtenir des échantillons ?

We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.

Quels sont les pays que vous avez déjà exportés ?

Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.

Quel est le délai de livraison ?

Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.

Envoyez votre demande dès aujourd'hui
Devis rapide