United StatesChinaJISISO NumberSymbolEuropean
UNS(AISI)GBFR
S20100201S35350SUS2014372-201-00-IX12CrMnNiN17-7-51.4372
S20200202S35450SUS2024373-202-00-IX12CrMnNiN18-9-51.4373
S30100301S30110SUS3014319-301-00-IX5CrNi17-71.4319
S30153*S30153SUS301L4318-301-53-IX2CrNiN18-71.4318
***SUS301J1––*
S30200302S30120SUS3024325-302-00-EX9CrNi18-91.4325
S30215302BS30240SUS302B4326-302-15-IX12CrNiSi18-9-3*
S30300303S30317SUS3034305-303-00-IX10CrNiS18-91.4305
S30323303SeS30327SUS303Se4625-303-23-XX12CrNiSe18-9*
–*–SUS303Cu4667-303-76-JX12CrNiCuS18-9-3*
S30400304S30408SUS3044301-304-00-IX5CrNi18-101.4301
–*S30488SUS304Cu4649-304-76-JX6CrNiCu19-9-1*
S30403304LS30403SUS304L4307-304-03-IX2CrNi18-91.4307
S30403304LS304034306-304-03-IX2CrNi19-111.4306
–*S304034650-304-75-EX2CrNiCu19-101.465
S30451304NS30458SUS304N14315-304-51-IX5CrNiN19-91.4315
S30452**SUS304N2––*
S30453304LNS30453SUS304LN4311-304-53-IX2CrNiN18-91.4311
–*S30480SUS304J14567-304-76-IX6CrNiCu17-8-21.4567
–*–SUS304J24617-201-76-JX6CrNiMnCu17-8-4-2*
S30431*S30480SUS304J34567-304-98-XX6CrNiCu18-9-21.4567
S30500305S30510SUS3054303-305-00-IX6CrNi18-121.4303
***SUS305J1––*
S30908309SS30908SUS309S4950-309-08-EX6CrNi23-131.495
S31008310SS31008SUS310S4951-310-08-IX6CrNi25-201.4951
S31008310SS310084845-310-08-EX8CrNi25-211.4845
S31254*S31252SUS312L4547-312-54-IX1CrNiMoCuN20-18-71.4547
–*–SUS315J14660-315-77-IX6CrNiCuSiMo19-10-3-2*
–*–SUS315J24648-315-77-IX6CrNiSiCuMo19-13-3-3-1*
S31600316S31608SUS3164401-316-00-IX5CrNiMo17-12-21.4401
S31600316S316084436-316-00-IX3CrNiMo17-12-31.4436
–*–SUS316F4494-316-74-JX6CrNiMoS17-12-3*
S31603316LS31603SUS316L4404-316-03-IX2CrNiMo17-12-21.4404
S31603316LS316034432-316-03-IX2CrNiMo17-12-31.4432
S31603316LS316034436-316-91-IX2CrNiMo18-14-31.4435
S31651316NS31658SUS316N4495-316-51-JX6CrNiMoN17-12-3*
S31653316LNS31653SUS316LN4406-316-53-IX2CrNiMoN17-11-21.4406
S31653316LNS316534429-316-53-IX2CrNiMoN17-12-31.4429
S31635*S31668SUS316Ti4571-316-35-IX6CrNiMoTi17-12-21.4571
–*–SUS316J14465-316-76-JX6CrNiMoCu18-12-2-2*
–*S31683SUS316J1L4647-316-75-XX2CrNiMoCu18-14-2-2*
S31700317S31708SUS3174445-317-00-UX6CrNiMo19-13-4*
S31703317LS31703SUS317L4438-317-03-IX2CrNiMo19-14-41.4438
S31753*S31753SUS317LN4434-317-53-IX2CrNiMoN18-12-41.4434
–*S31794SUS317J14476-317-92-XX3CrNiMo18-16-5*
–*–SUS317J24496-309-51-JX4CrNiMoN25-14-1*
N08367,*–SUS836L4478-083-67-UX2NiCrMoN25-21-7*
S32053
N08904*S39042SUS890L4539-089-04-IX1NiCrMoCu25-20-51.4539
S32100321S32168SUS3214541-321-00-IX6CrNiTi18-101.4541
S32109**X7CrNiTi18-101.4541
S34700347S34778SUS3474550-347-00-IX6CrNiNb18-101.455
S34709**X7CrNiNb18-101.4912
S38400384S38408SUS3844389-384-00-IX3NiCr18-16*
S30430S30430S30488SUSXM74567-304-30-IX3CrNiCu18-9-41.4567
S30500*S38148SUSXM15J14884-305-00-XX6CrNiSi18-13-4*
S82122**SUS821L1**–
S32304*S23043SUS323L4362-323-04-1X2CrNiN23-41.4362
S32900329–SUS329J14480-329-00-UX6CrNiMo26-4-2*
S32205,*S22053SUS329J3L4462-318-03-IX2CrNiMoN22-5-31.4462
S31803
S31260,*S22583SUS329J4L4481-312-60-JX2CrNiMoN25-7-3*
S32506
S32750*S25073SUS327L4410-327-50-EX2CrNiMoN25-7-41.441
S40500405S11348SUS4054002-405-00-IX6CrAl131.4002
–*S11203SUS410L4030-410-90-XX2Cr12*
S42900429S11510SUS4294012-429-00-XX10Cr15*
S43000430S11710SUS4304016-430-00-IX6Cr171.4016
S43020430FS11717SUS430F4004-430-20-IX7CrS17*
–*–SUS430LX4520-430-70-IX2CrTi171.452
S43940*S118734509-439-40-XX2CrTiNb181.4509
S43035439S118634510-430-35-IX3CrTi171.451
–*–4511-430-71-IX3CrNb171.4511
–*–SUS430J1L4664-430-75-JX2CrCuTi18*
S43400434S11790SUS4344113-434-00-IX6CrMo17-11.4113
S43600436S11862SUS436L4513-436-00-JX2CrMoNbTi18-1*
–*–SUS436J1L4609-436-77-JX2CrMo19*
–**SUS443J1–––
S44400444S11972SUS4444521-444-00-IX2CrMoTi18-21.4521
***SUS445J1––*
***SUS445J2––*
S44700*S13091SUS447J14135-447-92-CX1CrMo30-2*
S44627*S12791SUSXM274131-446-92-CX1CrMo26-1*
S40300403*SUS403––*
S41000410S41010SUS4104006-410-00-IX12Cr131.4006
–*–4024-410-09-EX15Cr131.4024
S41008*S41008SUS410S4000-410-08-IX6Cr131.4
–*–SUS410F24642-416-72-JX13CrPb13*
–*S45710SUS410J14119-410-92-CX13CrMo13*
S41600416S41617SUS4164005-416-00-IX12CrS131.4005
S42000420S42020SUS420J14021-420-00-IX20Cr131.4021
S42000420S42030SUS420J24028-420-00-IX30Cr1314,028
S42020420FS42037SUS420F4029-420-20-IX33CrS131.4029
–*–SUS420F24643-420-72-JX33CrPb13*
S43100431S43120SUS4314057-431-00-XX17CrNi16-21.4057
S44002440AS44070SUS440A4040-440-02-XX68Cr17*
S44003440BS44080SUS440B4041-440-03-XX85Cr17*
S44004440CS44096SUS440C4023-440-04-IX110Cr17*
–*S44097SUS440F4025-440-74-XX110CrS17*
S17400630S51740SUS6304542-174-00-IX5CrNiCuNb16-41.4542
S17700631S51700SUS6314568-177-00-IX7CrNiAl17-71.4568
***SUS631J1––*
***SUS632J1––*

 

Titanium Product List

GradeUNS NumberComposition/Description
Première annéeUNS R50250Unalloyed titanium
Niveau 2UNS R50400Unalloyed titanium
Grade 2HUNS R50400Unalloyed titanium (Grade 2 with 58 ksi (400 MPa) minimum UTS)
Niveau 3UNS R50550Unalloyed titanium
Grade 4UNS R50700Unalloyed titanium
Grade 5UNS R56400Titanium alloy (6% aluminum, 4% vanadium)
Grade 6UNS R54520Titanium alloy (5% aluminum, 2.5% tin)
7e annéeUNS R52400Unalloyed titanium plus 0.12 to 0.25% palladium
Grade 7HUNS R52400Unalloyed titanium plus 0.12 to 0.25% palladium (Grade 7 with 58 ksi (400 MPa) minimum UTS)
9e annéeUNS R56320Titanium alloy (3.0% aluminum, 2.5% vanadium)
Grade 11UNS R52250Unalloyed titanium plus 0.12 to 0.25% palladium
Grade 12UNS R53400Titanium alloy (0.3% molybdenum, 0.8% nickel)
Grade 13UNS R53413Titanium alloy (0.5% nickel, 0.05% ruthenium)
Grade 14UNS R53414Titanium alloy (0.5% nickel, 0.05% ruthenium)
Grade 15UNS R53415Titanium alloy (0.5% nickel, 0.05% ruthenium)
Grade 16UNS R52402Unalloyed titanium plus 0.04 to 0.08% palladium
Grade 16HUNS R52402Unalloyed titanium plus 0.04 to 0.08% palladium (Grade 16 with 58 ksi (400 MPa) minimum UTS)
Grade 17UNS R52252Unalloyed titanium plus 0.04 to 0.08% palladium
Grade 18UNS R56322Titanium alloy (3% aluminum, 2.5% vanadium) plus 0.04 to 0.08% palladium