Daxun is a 316/316L stainless steel channel supplier in China
En tant que principal fournisseur et exportateur de profilés en acier inoxydable en Chine, Daxun fournit des profilés en acier inoxydable dans le monde entier.
- Brand: S31600 (316) – S31603 (316L)
- Delivery status: hot rolling, laser fusion, press bending
- Surface treatment: pickling, bright, polished, mirror, hairline
- Standards: ASTM A276, ASTM A484M, DIN 1028, EN10056, GB4227
- With full traceability and original factory test reports.
- building structure, architectural structure, engineering structure
Introduction to Austenitic Stainless Steel
Austenitic stainless steel is a type of stainless steel alloy that contains a high percentage of chromium and nickel. Known for its excellent corrosion resistance, high ductility and good formability, austenitic stainless steel is used in a wide range of industries. Its unique combination of properties makes it ideal for applications in the construction, automotive and food processing industries. This type of stainless steel stands out for its ability to withstand harsh environments while maintaining its structural integrity and aesthetics.
Données
- Paramètres
- Élément
- Propriétés mécaniques
- PROPRIÉTÉS PHYSIQUES
- Tous les équivalents
| standard | ASTM、EN、DIN、JIS、ASME、BS、GB等, |
| aspect | C5-C30 |
| alloy | 201、310、304、304L、316、316L |
| type | U-slot, C-slot, |
| longueur | 1.0-12.0 m |
| l'épaisseur | 3mm to 25mm |
| Customization options | Oui |
| tolerance | ± ¼”, ± 1/16” |
| Finition | Grinding machine, brush, mirror, polishing |
| Chemical composition: ASTM A240, A666 | ||
| element | Type 316 | Type 316L |
| carbon | Max. 0.08. | Max. 0.030. |
| manganese | 2.00 max. | 2.00 max. |
| sulfur | Max. 0.030. | Max. 0.030. |
| phosphorus | Max. 0.045. | Max. 0.045. |
| silicon | Max 0.75. | Max 0.75. |
| chromium | 16.0 – 18.0 | 16.0 – 18.0 |
| nickel | 10.00 – 14.00 | 10.00 – 14.00 |
| molybdenum | 2.00 – 3.00 | 2.00 – 3.00 |
| nitrogen | Max 0.10. | Max 0.10. |
| type | Yield Strength 0.2% Deviation (KSI) | Tensile Strength(KSI) | % Elongation (2″ Gauge Length) |
| 316 | 30 mins | 75 minutes | 40 mins |
| 316L | 25 mins | 70 minutes | 40 mins |
| Density (psi) @ RT | 0.29 | |
| Tensile modulus (psi x 10^6) | XXVIII | |
| Specific heat (BTU/o F/lb.) | 32 to 212 degrees Fahrenheit | 0.12 |
| Thermal Conductivity (BTU/hour/square foot/foot) | 212 degrees Fahrenheit | 9.4 |
| 932 degrees Fahrenheit | 12.4 | |
| Average Coefficient of Thermal Expansion (inches x 10^-6 per oF) | 32 à 212oF | 8.9 |
| 32 à 600oF | 9 | |
| 32 à 1 000oF | 9.7 | |
| 32 à 1 200oF | 10.3 | |
| Resistivity (microohm-cm) | At 70oF | 29.4 |
| Melting Point Range (°F) | 2500 – 2550 |
| grade | China | UNS Number | Old England | Normes européennes | Swedish SS | Japan JIS | ||
| Bachelor’s degree | kindness | No | Nom | |||||
| 316 | 06Cr17Ni12Mo2 | S31600 | 304S11 | 58E | 1.4401 | X5CrNiMo17-12-2 | 2347 | Stainless Steel 316 |
Choisissez Daxun et faites en sorte que vos clients soient satisfaits.

Composition and Properties
Austenitic stainless steels typically contain 16-18% chromium, 10-14% nickel and 2-3% molybdenum. The addition of molybdenum significantly improves the corrosion resistance of the alloy, especially in chloride-rich environments. This composition not only provides excellent corrosion resistance, but also outstanding mechanical properties such as high tensile strength, good ductility and excellent weldability. These properties make austenitic stainless steels a versatile material suitable for a variety of demanding applications.
Corrosion Resistance and Heat Resistance
Austenitic stainless steel is known for its excellent corrosion resistance, especially in acidic and chloride environments. This makes it ideal for applications that require high strength and maximum corrosion resistance. In addition, it is resistant to stress corrosion cracking, further increasing its durability in harsh conditions. Austenitic stainless steel also has good heat resistance and can withstand temperatures up to approximately 870°C. This combination of properties ensures that it performs reliably in both high temperature and corrosive environments.

Emballage
Daxun Alloy garantit la meilleure qualité d'emballage, car celui-ci joue un rôle important dans le fret international, où les marchandises passent par différents canaux avant d'atteindre leur destination finale ; nous accordons donc une attention particulière à l'emballage. Nous emballons nos marchandises de différentes manières, en fonction du produit. Nous emballons nos produits de différentes manières, notamment :
- Boîtes et caisses
- Emballage rétractable
- Palettes en bois
- Boîtes en bois
Qualité, livraison, inspection
- At Daxun, we carry out several quality checks to ensure product reliability. These checks include tests for flattening, corrosion resistance, mechanical properties, hardness, material verification, and expansion. Each test guarantees that our stainless steel meets the needs of your applications.During production, we monitor the diameter, thickness, and surface quality carefully. Our standard delivery time is between 7-15 days, with special sizes taking up to 20 days. All deliveries are made on time, strictly following the contract terms.
- Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
- Fournir des échantillons gratuits aux clients pour qu'ils les testent
- Soutien à l'inspection sur site ou à l'inspection vidéo en usine

Informations sur les commandes
To reach us, please fill out the form on the “Contact Us” page or call our sales manager at +86 13382898899. We will respond as soon as possible. You can also contact us through WhatsApp or email us at Daxunalloy@gmail.com, which is checked every 6 hours. We reply promptly to all messages. We also share market updates with our customers each week to keep them informed.
Support technique
Si vous avez besoin d'une assistance technique supplémentaire, notre métallurgiste résident et notre personnel compétent se feront un plaisir de vous aider. En outre, Daxun dispose d'un laboratoire d'essai certifié, une première dans l'industrie des stocks multimétaux et plastiques. Ceci, à notre avis, démontre notre dévouement inébranlable à la qualité et notre philosophie en tant que fournisseur de services complets.

SS 316-316L Austenitic Stainless Steel Channel Features
Daxun Alloy Permettez à votre marque de s'améliorer rapidement
- Tableau de spécification
- Galerie
| Tableau des dimensions de la section transversale, de la surface de la section transversale et du poids théorique des profilés en acier | ||||||||
| modèle | taille | Espace sectionnel | Poids théorique | |||||
| h | b | d | t | r | r 1 | |||
| (mm) | (cm2) | (kg/m) | ||||||
| 5 | 50 | 37 | 4.5 | 7 | 7 | 3.5 | 6.925 | 5.44 |
| 6.3 | 63 | 40 | 4.8 | 7.5 | 7.5 | 3.8 | 8.446 | 6.63 |
| 6.5 | 65 | 40 | 4.3 | 7.5 | 7.5 | 3.8 | 8.292 | 6.51 |
| 8 | 80 | 43 | 5 | 8 | 8 | 4 | 10.24 | 8.04 |
| 10 | 100 | 48 | 5.3 | 8.5 | 8.5 | 4.25 | 12.74 | 10 |
| 12 | 120 | 53 | 5.5 | 9 | 9 | 4.5 | 15.36 | 12.1 |
| 12.6 | 126 | 53 | 5.5 | 9 | 9 | 4.5 | 15.69 | 12.3 |
| 14a | 140 | 58 | 6 | 9.5 | 9.5 | 4.8 | 18.51 | 14.5 |
| 14b | 60 | 8 | 21.31 | 16.7 | ||||
| 16a | 160 | 63 | 6.5 | 10 | 10 | 5 | 21.95 | 17.2 |
| 16b | 65 | 8.5 | 25.15 | 19.8 | ||||
| 18a | 180 | 68 | 7 | 10.5 | 10.5 | 5.2 | 25.69 | 20.2 |
| 18b | 70 | 9 | 29.29 | 23 | ||||
| 20a | 200 | 73 | 7 | 11 | 11 | 5.5 | 28.83 | 22.6 |
| 20b | 75 | 9 | 32.83 | 25.8 | ||||
| 22a | 220 | 77 | 7 | 11.5 | 11.5 | 5.8 | 31.83 | 25 |
| 22b | 79 | 9 | 36.23 | 28.5 | ||||
| 24a | 240 | 78 | 7 | 12 | 12 | 6 | 34.21 | 26.9 |
| 24b | 80 | 9 | 39.01 | 30.6 | ||||
| 24c | 82 | 11 | 43.81 | 34.4 | ||||
| 25a | 250 | 78 | 7 | 12 | 12 | 6 | 34.91 | 27.4 |
| 25b | 80 | 9 | 39.91 | 31.3 | ||||
| 25c | 82 | 11 | 44.91 | 35.3 | ||||
| 27a | 270 | 82 | 7.5 | 12.5 | 12.5 | 6.2 | 39.27 | 30.8 |
| 27b | 84 | 9.5 | 44.67 | 35.1 | ||||
| 27c | 86 | 11.5 | 50.07 | 39.3 | ||||
| 28a | 280 | 82 | 7.5 | 12.5 | 12.5 | 6.2 | 40.02 | 31.4 |
| 28b | 84 | 9.5 | 45.62 | 35.8 | ||||
| 28c | 86 | 11.5 | 51.22 | 40.2 | ||||
| 30a | 300 | 85 | 7.5 | 13.5 | 13.5 | 6.8 | 43.89 | 34.5 |
| 30b | 87 | 9.5 | 49.89 | 39.2 | ||||
| 30c | 89 | 11.5 | 55.89 | 43.9 | ||||
| 32a | 320 | 88 | 8 | 14 | 14 | 7 | 48.5 | 38.1 |
| 32b | 90 | 10 | 54.9 | 43.1 | ||||
| 32c | 92 | 12 | 61.3 | 48.1 | ||||
| 36a | 360 | 96 | 9 | 16 | 16 | 8 | 60.89 | 47.8 |
| 36b | 98 | 11 | 68.09 | 53.5 | ||||
| 36c | 100 | 13 | 75.29 | 59.1 | ||||
| 40a | 400 | 100 | 10.5 | 18 | 18 | 9 | 75.04 | 58.9 |
| 40b | 102 | 12.5 | 83.04 | 65.2 | ||||
| 40c | 104 | 14.5 | 91.04 | 71.5 | ||||
SS 316 /316L Stainless Steel Channel Type (3)
Informations disponibles pour référence et téléchargement
Daxun est un fabricant digne de confiance de profilés en acier inoxydable.
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified to ISO9001, SGS, CE, OQC and more international quality standards. Stainless steel is an iron alloy known for its specific composition and unique properties, especially 316 stainless steel, which is classified as austenitic, non-magnetic and highly corrosion-resistant. We also conduct strict quality control to ensure that stainless steel channels have fewer defects. At Daxun, you can rest assured that all products are durable, high-quality and excellent in performance.
Projets et produits récents
Daxun est engagée dans le commerce international depuis plus de dix ans. En 2023, le volume des exportations a dépassé 100 millions de dollars américains, et le volume des exportations s'est classé parmi les principaux fabricants chinois d'acier inoxydable. Daxun améliore constamment ses compétences en matière de services. Pour servir le marché mondial, elle a établi trois installations de services d'exportation en Chine, coopérant avec des sociétés d'ingénierie, des aciéries et des sociétés de commerce international. Daxun fournit des services de chaîne d'acier inoxydable et a établi des relations de coopération à long terme avec des dizaines d'aciéries de renom dans le monde entier. Le stock comprend 50 000 tonnes d'acier inoxydable conventionnel et 20 000 tonnes d'acier duplex, d'alliages à base de nickel, d'acier résistant à la chaleur et d'autres métaux. Les matériaux en acier inoxydable de Daxun sont de qualité stable, et les variétés, les spécifications et les poids de livraison sont strictement conformes aux normes.
Our stock of stainless steel channels includes hot rolled channels and laser fused channels, and we have the sizes and grades you need for immediate shipment. Grades include: 316 and 304. We also stock specialty products, non-standard sizes, and offer a quick turnaround finish service for commercial customers.
Whether you are looking for a large stock, or a smaller requirement from one of our domestic customers, we are here to help. Our friendly and experienced team can help you decide which size, grade and finish will suit you best. So for more information, help and advice please email: daxunalloy@gmail.com
- ASTM A276, ASTM A484M, DIN 1028, EN10056, GB4227
Corrosion resistance (depending on alloy content), heat resistance, good hot and cold working properties, toughness and excellent overall performance. Suitable for a wide range of applications. In addition, these materials are highly durable even in harsh environments, making them ideal for industrial use. They also have good weldability and formability, which makes them easier to form into different shapes and structures, providing flexibility for custom projects. Austenitic stainless steels such as 316 have lower thermal conductivity compared to ferritic steels, which affects their expansion and melting points, making them perform well in extreme temperature conditions.
- ASTM A276
- ASTM A484
- ASTM A479
- ASME SA479
-
ASTM A1069/A1069M/11
- ASTM A276
- ASTM A484
- ASTM A479/A479
Samples can be provided free of charge, but the freight is borne by the customer and will be refunded after cooperation.
Our minimum order quantity for stainless steel channels is 1 ton.
Trial orders can be shipped within a week, regular orders take about two weeks.