  • Grade: AISI 304/S30400
  • Fabrication : tôles laminées à froid, tôles laminées à chaud, tôles forgées
  • Norme : ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Type : tôles minces laminées à froid, tôles épaisses laminées à chaud
  • Surface : 2B, NO.1, NO.4, HL, BA, 8K, etc.
  • Longueur : 2438mm3048mm6000mm peut être personnalisé
  • Origin: TISCO, Baosteel, Posco, Tsingshan, Delong

Leader mondial des services de fabrication de tôles en acier inoxydable

304 is one of the most popular grades of stainless steel because of its high strength, excellent corrosion resistance, and excellent formability. This grade has a low carbon content and excellent ductility. It can be cold worked by roll forming, deep drawing, and bending. This grade is suitable for forming complex shapes. You will see this grade in the oil and gas industry and the food service industry.Our 304 series is a standout product available in thicknesses from 0.4mm to 120mm.

Daxun is your trusted stainless steel sheet supplier.By choosing our 304stainless steel plates, you are investing in a material that guarantees long life, reliability and superior performance. Don’t compromise on quality – choose our stainless steel solutions and experience the difference they can make in your projects. Contact us today for more details or to order your required specifications and quantities.

Lire la suite

Données

Stainless Plate and sheet Type Plate, Sheet, Strip, Coils, Foils, Flats, Clad Plate, Plain Sheet, Rolling Sheet, Rolling Plate, Flat Shim, Flat Sheet, Shim Sheet, Rolls, Blank (Circle), sheared, annealed, soft annealed, descaled, tread plate, Checker Plate
Standard ASTM A240 / ASME SA240 ASTM/ASME A240/480,JIS 4305,DIN EN 10088-2JIS, AISI, ASTM, GB, DIN, EN, etc
Stainless Steel Plate and sheet Length 1000mm-13000mm or as required
304 Stainless Plate Width 1000mm-1219mm-1500mm-1800mm-2000mm-2500mm or as required
UNS 304 Plate Thickness 0.3 to 120mm or as required
ASTM A240 Stainless Steel 304 Plate Process Hot/ Cold Rolled/forging
UNS 304 Plate surface No.1, No. 2D, No. 2B, BA, No.3, No.4, No.6, No.7, 2B, 2D, BA NO(8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met with Plastic Coated), No.1 finish hot rolled ASTM A240Stainless Steel 304 Plate, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc.
Stainless 304 Sheet ASTM ASTM A240
Stainless 304 Sheet AMS ASTM 240
Tolerances of width and thickness ASTM-ASME-GB-EN-DIN-JIS
 304 Stainless Plate standards and approvals EN ISO 18286 EN 10051 EN 10088-1 ISO 15510 EN ISO 9445 ASTM A 480 ASTM A 959 ASME IID
304 Plate & Sheet Sizes 1000 x 2000 mm, 1220 x 2440 mm, 1500 x 3000 mm, 2000 x 2000 mm, 2000 x 4000 mm,1500*6000,Cold rolled 304 Stainless Plate 0.5-6.4 mm,Hot rolled 304 Stainless Plate 3.0–60.0 mm
UNS 304 Plate Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard ASTM A240Stainless Steel 304 Sheet suppliers
Cutting To provide a comprehensive service, we use a variety of cutting methods, including:Laser Plate Cutting,Plasma Plate Cutting,Oxy-propane Flame Cutting
Profils plasmatiques As per customer’s drawings
Value added services for 304 Stainless Plate Laser cutting, Waterjet cutting, Plasma cutting, Bending and mechanical processing, edge preparation, welding, sawing and shearing.
Fabricant POSCO, Aperam, ATI, ThyssenKrupp, Baosteel, TISCO, ArcelorMittal, VDM, Nippon Metal, Outokumpu, Tsingshan, Delong.
China 304 Stainless Plate Manufacturer ASTM A240Stainless Steel 304 Plate: material 3/16″ [5.00 mm] and over in thickness and over 10″ [250 mm] in width;304 Stainless Sheet: material under 3/16″ [5.00 mm] in thickness and 24″ [600 mm] and over in width;Steel Stainless 304 Clad plate: Steel Stainless 304 Clad plate is a composite steel plate made by bonding 304 Stainless 304 Plate, etc.ASTM A240Stainless Steel 304 Strip: cold-rolled material under 3/16″ [5.00 mm] in thickness and under 24″ [600 mm] in width.
304 Plate Origin CHINA
Packing of 304 plate Bundles with waterproof cloth outside or plywood box
Test UT, SGS testing, TUV etc
Why buy 304 Sheet from DAXUN? Free quote、Free sample、EN 10204 3.1、Mill Test Certificate is supplied with shipment、 TestGrade: AISI 304/S30400
Fabrication : tôles laminées à froid, tôles laminées à chaud, tôles forgées
Norme : ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
Type : tôles minces laminées à froid, tôles épaisses laminées à chaud
Surface : 2B, NO.1, NO.4, HL, BA, 8K, etc.
Length: 2438mm/3048mm/6000mm can be customized
Origin: TISCO, Baosteel, Posco, Tsingshan, Delong
Standard Werkstoff Nr. UNS JIS BS GOST AFNOR FR CN
SS 304 1.4301 S30400 SUS 304 304S31 08Х18Н10 Z7CN18-09 X5CrNi18-10 06Cr19Ni10
Grade C Mn Si P S Cr Ni N
304 ≤0.08% ≤2.0% ≤ 0.75% ≤0.045% ≤0.030% 18%-20% 8.0%-10.5% ≤0.10%
Type Limite d'élasticité 0.2% offset (KSI) Résistance à la traction (KSI) % Allongement (2″ Longueur de la jauge)
304 Ann 30 min. 75 min. 40 min.
304 ¼ Dur 75 min. 125 min. 12 min.
304 ½ Dur 110 min. 150 min. 7 min.
304L Ann 25 min. 70 min. 40 min.
304L ¼ Dur 75 min. 125 min. 12 min.
304L ½ Dur 110 min. 150 min. 6 min.
304 & 304L
Densité (lb./ in^2) @ RT 0.29
Module d'élasticité en traction (psi x 10^6) 28
Chaleur spécifique (BTU/o F/lb.) 32 à 212 oF 0.12
Conductivité thermique (BTU/hr/ft^2/ft) 212oF 9.4
932oF 12.4
Coefficient moyen de dilatation thermique (po x 10^-6 par o F) 32 à 212oF 9.2
32 à 600oF 9.9
32 à 1 000oF 10.2
32 à 1 200oF 10.4
Résistivité électrique (micro ohms - cm) à 70oF 72
Gamme de points de fusion (oF) 2550 à 2650
Résistance à l'oxydation - Service continu(oF) 1,650
Résistance à l'oxydation - Service intermittent(oF) 1,500

Choisissez Daxun et faites en sorte que vos clients soient satisfaits.

Contacter Daxun maintenant

Livraison rapide

Daxun provides customers with timely and fast delivery of stainless steel plate products. Behind the speed is the system support from production capacity, information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.

Contacter Daxun maintenant

Réponse rapide

Daxun saves customers time, materials and stress, and ultimately saves them costs. With its professional advantages, Daxun can provide the most cost-optimized material recommendations based on customer needs, and can also reduce costs for customers through continuous processing, nesting processing, etc.

Contacter Daxun maintenant

Usinage avancé

Our advanced nesting processing method improves material utilization and cutting utilization. At the same time, Daxun can also achieve continuous cost reduction and efficiency improvement by promoting lean improvement activities, and return the benefits to customers.

Contacter Daxun maintenant

304 stainless steel plate packaging

Daxun Alloy ensures the best quality of 304 stainless steel sheet packaging, because packaging plays an important role in international freight, and the goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways according to the products. We pack our products in many ways, such as:
- Boîtes et caisses
- Papier kraft + palettes en bois
- Emballage rétractable
- Palettes en bois sans fumigation
- Boîtes en bois sans fumigation

Contacter Daxun maintenant

304 Stainless Steel Sheet Processing:

  • Traitement de la gravure
  • Traitement des soudures
  • Traitement du pliage
  • Traitement du gaufrage
  • Traitement par sablage
  • Traitement par polissage
  • Traitement du poinçonnage
  • Traitement de l'estampage
Contacter Daxun maintenant

SS 304 Plate Surface Treatment

1D : la surface est mate et la forme des particules est discontinue.
2D : Blanc avec un ton argenté.
2B : gris argenté avec une meilleure brillance et planéité que la surface 2D.
Ba : Surface proche d'un miroir avec une brillance et une réflectivité excellentes.
No.3 : Bonne brillance et surface rugueuse.
No.4 : La surface présente des lignes fines et une bonne brillance.
HL : Gris argenté avec des cheveux dorés.
8K : Surface miroir.

304 plate stainless steel Features

Haute résistance
Résistance à la corrosion
Résistance à la chaleur
Résistance aux basses températures
Protection de l'environnement
Performance de soudage

Let your brand improve rapidly

Tolérance pour la tôle 2B
Taille Rang de tolérance
Groupe 1 Groupe 2 Groupe 3
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
Tolérance pour la tôle laminée à chaud n° 1
Taille Rang de tolérance
Groupe 1 Groupe 2 Groupe 3
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
16 15.2~ 15.5 15.5~ 15.7 15.7~ 16.1
18 17.2~ 17.5 17.5~ 17.7 17.7~ 18.1
20 19.2~ 19.5 19.5~ 19.7 19.7~ 20.1
30 29.2~ 29.5 29.5~ 29.7 29.7-30.1
40 39.2~ 39.5 39.5~ 39.7 39.7~ 40.1
50 49.2~ 49.5 49.5~ 49.7 49.7~ 50.1
60 59.2~ 59.5 59.5~ 59.7 59.7~ 60.1
Choix de l'État de livraison État de surface
Laminés à froid 2B
2D
BA
Ligne de démarcation des cheveux
N° 3
N°4
6K
8K
Remarque :
1. Si vous avez besoin d'un autre pays de livraison que ceux mentionnés ci-dessus, veuillez nous le confirmer.
2. En cas de demande ou de commande, veuillez nous faire part de toute exigence supplémentaire non indiquée ici.
État de livraison
Choix de l'État de livraison État de surface
Laminés à chaud N°1
N° 3
N°4
6K
8K
Mariné
Remarque :
1. Si vous avez besoin d'un autre pays de livraison que ceux mentionnés ci-dessus, veuillez nous le confirmer.
2. En cas de demande ou de commande, veuillez nous faire part de toute exigence supplémentaire non indiquée ici.
Grade Type Épaisseur Surface
Austénitique 304/304H/304L/304J1 0,25-150 mm 2B/BA/NO.4/8K/SB/HL/NO.1
321 0,4-80 mm 2B/BA/NO.4/8K/SB/HL/NO.1
316/316L/317L/316Ti 0.3-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
Ferrite 430 0,4-3,0 mm 2B/BA/NO.4/8K/SB/HL
Ferrite ultra pure 443 0,4-2,0 mm 2B
436L/439/444/441 0,5-3,0 mm 2B、2D
409L 0,4-2,5 mm 2B、2D
Grade Type Épaisseur Original
Acier résistant à la chaleur 309S 0,5-40 mm CHN
310S 0,5-40 mm CHN
Acier duplex 2101 1,5-50 mm CHN
2304 3.0-50mm CHN
2205 0,5-60 mm CHN
2507 1.0-60mm SWE / JPN / CHN
Acier super austénitique N08904 0,6-50 mm SWE / JPN / CHN
S31254 0,5-50 mm SWE / JPN / CHN
N08926 0,5-50 mm SWE / JPN / CHN
N08367 0,5-50 mm SWE / JPN / CHN
Alliage base nickel N08031 1.0-50mm US / JPN / GER
N08810/N08800 0,8-50 mm US / JPN / CHN
N08028 1.0-20mm US / GER / JPN
N08020 1.0-20mm US / GER / JPN
N08825 0,8-40 mm US / GER / SWE / JPN / CHN
N10276 0,5-50 mm US / GER / JPN
N06022 1.0-50mm US / GER / JPN
N06625 0,8-20 mm US / GER / CHN
N04400 1.0-20mm US / GER / JPN
N06600 1.0-50mm US / GER / JPN / CHN
N02201 0,5-20 mm US / JPN
Titane TA1/Gr1 0,5-50 mm JPN / CHN
TA2/Gr2 0,5-50 mm JPN / CHN
Matériel de soudage ERNiCrMo-13 1.2、2.4mm GER
ERNiCrMo-3 2,4 mm GER
ERNiCrMo-4 2,4 mm ÉTATS-UNIS

Daxun est un fabricant de plaques d'acier inoxydable digne de confiance.

En tant que fabricant professionnel, Daxun s'assure que tous les produits qu'il fabrique sont de haute qualité. Par conséquent, nous veillons à ce que toutes les plaques d'acier inoxydable soient certifiées ISO9001, SGS, CE, OQC et autres normes de qualité internationales. Chez Daxun, vous avez l'assurance que tous les produits sont durables, de haute qualité et très performants.

Projets et produits récents

304 plate stainless steel
astm a240 plate stainless steel
304 flat stainless steel plate
304 stainless steel sheet suppliers
304 2b stainless steel sheet
304 stainless steel sheet price
Puis-je obtenir des échantillons ?

Nous pouvons vous fournir des échantillons de tôles d'acier inoxydable pour vous permettre de vérifier la qualité. L'échantillon est gratuit et vous ne payez que les frais de transport.

Quels sont les pays que vous avez déjà exportés ?

Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.

Quel est votre MOQ ?

Notre MOQ est de 1 tonne pour les tôles d'acier inoxydable.

Quel est le délai de livraison ?

Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.

Envoyez votre demande dès aujourd'hui
Devis rapide