x
Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat

Daxun 304 stainless steel plate and sheet China supplier

As China’s leading stainless steel plate supplier and exporter, Daxun provides stainless steel plates to the world.
  • Grade: AISI 304/S30400
  • Manufaktur: pelat canai dingin, pelat canai panas, pelat tempa
  • Standar: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Jenis: pelat tipis canai dingin, pelat tebal canai panas
  • Permukaan: 2B, NO.1, NO.4, HL, BA, 8K, dll.
  • Panjang: 2438mm3048mm6000mm dapat disesuaikan
  • Asal TISCO, Baosteel, Posco, Tsingshan, Delong

Pemimpin global dalam layanan fabrikasi lembaran baja tahan karat

304 is one of the most popular grades of stainless steel because of its high strength, excellent corrosion resistance, and excellent formability. This grade has a low carbon content and excellent ductility. It can be cold worked by roll forming, deep drawing, and bending. This grade is suitable for forming complex shapes. You will see this grade in the oil and gas industry and the food service industry.Our 304 series is a standout product available in thicknesses from 0.4mm to 120mm.

Daxun is your trusted stainless steel sheet supplier.By choosing our 304stainless steel plates, you are investing in a material that guarantees long life, reliability and superior performance. Don’t compromise on quality – choose our stainless steel solutions and experience the difference they can make in your projects. Contact us today for more details or to order your required specifications and quantities.

Baca Lebih Lanjut

Data

Stainless Plate and sheet Type Pelat, Lembaran, Strip, Gulungan, Foil, Flat, Pelat Berpakaian, Lembaran Polos, Lembaran Bergulir, Pelat Bergulir, Shim Datar, Lembaran Datar, Lembaran Shim, Gulungan, Kosong (Lingkaran), dicukur, dianil, dianil lunak, kerak, pelat tapak, Pelat Pemeriksa
Standar ASTM A240 / ASME SA240 ASTM/ASME A240/480,JIS 4305,DIN EN 10088-2JIS, AISI, ASTM, GB, DIN, EN, etc
Stainless Steel Plate and sheet Length 1000mm-13000mm atau sesuai kebutuhan
304 Stainless Plate Width 1000mm-1219mm-1500mm-1800mm-2000mm-2500mm atau sesuai kebutuhan
UNS 304 Plate Thickness 0,3 hingga 120mm atau sesuai kebutuhan
ASTM A240 Stainless Steel 304 Plate Process Canai Panas / Dingin / penempaan
UNS 304 Plate surface No.1, No. 2D, No. 2B, BA, No.3, No.4, No.6, No.7, 2B, 2D, BA NO(8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met with Plastic Coated), No.1 finish hot rolled ASTM A240Stainless Steel 304 Plate, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc.
Stainless 304 Sheet ASTM ASTM A240
Stainless 304 Sheet AMS ASTM 240
Toleransi lebar dan ketebalan ASTM-ASME-GB-EN-DIN-JIS
 304 Stainless Plate standards and approvals EN ISO 18286 EN 10051 EN 10088-1 ISO 15510 EN ISO 9445 ASTM A 480 ASTM A 959 ASME IID
304 Plate & Sheet Sizes 1000 x 2000 mm, 1220 x 2440 mm, 1500 x 3000 mm, 2000 x 2000 mm, 2000 x 4000 mm,1500*6000,Cold rolled 304 Stainless Plate 0.5-6.4 mm,Hot rolled 304 Stainless Plate 3.0–60.0 mm
UNS 304 Plate Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard ASTM A240Stainless Steel 304 Sheet suppliers
Pemotongan To provide a comprehensive service, we use a variety of cutting methods, including:Laser Plate Cutting,Plasma Plate Cutting,Oxy-propane Flame Cutting
Profil plasma As per customer’s drawings
Value added services for 304 Stainless Plate Pemotongan laser, pemotongan waterjet, pemotongan plasma, pembengkokan dan pemrosesan mekanis, persiapan tepi, pengelasan, penggergajian dan pemotongan.
Produsen POSCO, Aperam, ATI, ThyssenKrupp, Baosteel, TISCO, ArcelorMittal, VDM, Nippon Metal, Outokumpu, Tsingshan, Delong.
China 304 Stainless Plate Manufacturer ASTM A240Stainless Steel 304 Plate: material 3/16″ [5.00 mm] and over in thickness and over 10″ [250 mm] in width;304 Stainless Sheet: material under 3/16″ [5.00 mm] in thickness and 24″ [600 mm] and over in width;Steel Stainless 304 Clad plate: Steel Stainless 304 Clad plate is a composite steel plate made by bonding 304 Stainless 304 Plate, etc.ASTM A240Stainless Steel 304 Strip: cold-rolled material under 3/16″ [5.00 mm] in thickness and under 24″ [600 mm] in width.
304 Plate Origin CHINA
Packing of 304 plate Bundel dengan kain tahan air di luar atau kotak kayu lapis
Tes UT, pengujian SGS, TUV dll
Why buy 304 Sheet from DAXUN? Free quote、Free sample、EN 10204 3.1、Mill Test Certificate is supplied with shipment、 TestGrade: AISI 304/S30400
Manufaktur: pelat canai dingin, pelat canai panas, pelat tempa
Standar: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
Jenis: pelat tipis canai dingin, pelat tebal canai panas
Permukaan: 2B, NO.1, NO.4, HL, BA, 8K, dll.
Length: 2438mm/3048mm/6000mm can be customized
Asal TISCO, Baosteel, Posco, Tsingshan, Delong
Standar Werkstoff Nr. UNS JIS BS GOST AFNOR EN CN
SS 304 1.4301 S30400 SUS 304 304S31 08Х18Н10 Z7CN18‐09 X5CrNi18-10 06Cr19Ni10
Kelas C Mn Si P S Cr Ni N
304 ≤0.08% ≤2.0% ≤ 0.75% ≤0.045% ≤0.030% 18%-20% 8.0%-10.5% ≤0.10%
Jenis Kekuatan Hasil 0,2% offset (KSI) Kekuatan Tarik (KSI) % Elongation(2″ Gauge length)
304 Ann 30 min. 75 menit. 40 min.
304 ¼ Hard 75 menit. 125 menit. 12 min.
304 ½ Hard 110 menit. 150 menit. 7 min.
304L Ann 25 menit. 70 min. 40 min.
304L ¼ Hard 75 menit. 125 menit. 12 min.
304L ½ Hard 110 menit. 150 menit. 6 min.
304 & 304L
Kepadatan (lb./ in^2) @ RT 0.29
Modulus Elastisitas dalam Ketegangan (psi x 10^6) 28
Panas Spesifik (BTU/o F/lb.) 32 hingga 212 oF 0.12
Konduktivitas Termal (BTU/jam/ft^2/ft) 212oF 9.4
932oF 12.4
Koefisien Ekspansi Termal Rata-rata (dalam. x 10^-6 per o F) 32 hingga 212oF 9.2
32 hingga 600oF 9.9
32 hingga 1.000oF 10.2
32 to 1,200oF 10.4
Resistivitas Listrik (mikro ohm - cm) pada suhu 70oF 72
Rentang Titik Leleh (oF) 2550 to 2650
Ketahanan Oksidasi - Layanan Berkelanjutan (oF) 1,650
Ketahanan Oksidasi - Layanan Terputus-putus (oF) 1,500

Pilih Daxun dan buat pelanggan Anda puas.

Hubungi Daxun sekarang

Pengiriman cepat

Daxun provides customers with timely and fast delivery of stainless steel plate products. Behind the speed is the system support from production capacity, information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.

Hubungi Daxun sekarang

Respon cepat

Daxun saves customers time, materials and stress, and ultimately saves them costs. With its professional advantages, Daxun can provide the most cost-optimized material recommendations based on customer needs, and can also reduce costs for customers through continuous processing, nesting processing, etc.

Hubungi Daxun sekarang

Pemesinan tingkat lanjut

Our advanced nesting processing method improves material utilization and cutting utilization. At the same time, Daxun can also achieve continuous cost reduction and efficiency improvement by promoting lean improvement activities, and return the benefits to customers.

Hubungi Daxun sekarang

304 stainless steel plate packaging

Daxun Alloy ensures the best quality of 304 stainless steel sheet packaging, because packaging plays an important role in international freight, and the goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways according to the products. We pack our products in many ways, such as:
- Kotak dan peti
- Kertas kraft + palet kayu
- Kecilkan bungkus
- Palet kayu bebas fumigasi
- Kotak kayu bebas fumigasi

Hubungi Daxun sekarang

304 Stainless Steel Sheet Processing:

  • Pemrosesan etsa
  • Pemrosesan pengelasan
  • Pemrosesan pembengkokan
  • Pemrosesan timbul
  • Pemrosesan sandblasting
  • Pemrosesan pemolesan
  • Pemrosesan meninju
  • Pemrosesan stamping
Hubungi Daxun sekarang

SS 304 Plate Surface Treatment

1D: Permukaannya matte dengan bentuk partikel yang terputus-putus.
2D: Putih dengan nada keperakan.
2B: Abu-abu perak dengan kilap dan kerataan yang lebih baik daripada permukaan 2D.
Ba: Dekat dengan permukaan cermin dengan kilap dan daya pantul yang istimewa.
No.3: Kilauan yang bagus dan permukaan yang kasar.
No.4: Permukaannya memiliki garis-garis halus dan kilap yang bagus.
HL: Abu-abu perak dengan rambut keemasan.
8K: Permukaan cermin.

304 plate stainless steel Features

Kekuatan tinggi
Ketahanan korosi
Tahan panas
Tahan suhu rendah
Perlindungan lingkungan
Kinerja pengelasan

Let your brand improve rapidly

Toleransi untuk Lembar 2B
Ukuran Peringkat Toleransi
Kelompok 1 Kelompok 2 Kelompok 3
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
Toleransi untuk Pelat Canai Panas No.1
Ukuran Peringkat Toleransi
Kelompok 1 Kelompok 2 Kelompok 3
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
16 15.2~ 15.5 15.5~ 15.7 15.7~ 16.1
18 17.2~ 17.5 17.5~ 17.7 17.7~ 18.1
20 19.2~ 19.5 19.5~ 19.7 19.7~ 20.1
30 29.2~ 29.5 29.5~ 29.7 29.7-30.1
40 39.2~ 39.5 39.5~ 39.7 39.7~ 40.1
50 49.2~ 49.5 49.5~ 49.7 49.7~ 50.1
60 59.2~ 59.5 59.5~ 59.7 59.7~ 60.1
Pilihan Status Pengiriman Kondisi Permukaan
Digulung Dingin 2B
2D
BA
Garis rambut
No.3
No.4
6K
8K
Catatan:
1. Jika Anda memerlukan status pengiriman yang berbeda dari yang tercantum di atas, mohon konfirmasi dengan kami.
2. Jika ada pertanyaan atau pesanan, mohon beritahukan kepada kami persyaratan tambahan yang tidak disebutkan di sini.
Status Pengiriman
Pilihan Status Pengiriman Kondisi Permukaan
Canai Panas No.1
No.3
No.4
6K
8K
Acar
Catatan:
1. Jika Anda memerlukan status pengiriman yang berbeda dari yang tercantum di atas, mohon konfirmasi dengan kami.
2. Jika ada pertanyaan atau pesanan, mohon beritahukan kepada kami persyaratan tambahan yang tidak disebutkan di sini.
Kelas Jenis Ketebalan Permukaan
Austenitik 304/304H/304L/304J1 0,25-150mm 2B/BA/NO.4/8K/SB/HL/NO.1
321 0,4-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
316/316L/317L/316Ti 0,3-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
Ferit 430 0.4-3.0mm 2B/BA/NO.4/8K/SB/HL
Ferit Ultra Murni 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B 、 2D
409L 0,4-2,5 mm 2B 、 2D
Kelas Jenis Ketebalan Asli
Baja tahan panas 309S 0,5-40mm CHN
310S 0,5-40mm CHN
Baja Dupleks 2101 1,5-50mm CHN
2304 3.0-50mm CHN
2205 0,5-60mm CHN
2507 1.0-60mm SWE / JPN / CHN
Baja Austenitik Super N08904 0,6-50mm SWE / JPN / CHN
S31254 0,5-50mm SWE / JPN / CHN
N08926 0,5-50mm SWE / JPN / CHN
N08367 0,5-50mm SWE / JPN / CHN
Paduan Dasar Nikel N08031 1.0-50mm AS / JPN / GER
N08810 / N08800 0,8-50mm AS / JPN / CHN
N08028 1.0-20mm AS / JERMAN / JPN
N08020 1.0-20mm AS / JERMAN / JPN
N08825 0,8-40mm US / GER / SWE / JPN / CHN
N10276 0,5-50mm AS / JERMAN / JPN
N06022 1.0-50mm AS / JERMAN / JPN
N06625 0,8-20mm AS / GER / CHN
N04400 1.0-20mm AS / JERMAN / JPN
N06600 1.0-50mm US / GER / JPN / CHN
N02201 0,5-20mm AS / JPN
Titanium TA1/Gr1 0,5-50mm JPN / CHN
TA2/Gr2 0,5-50mm JPN / CHN
Bahan Pengelasan ERNiCrMo-13 1.2 、 2.4mm GER
ERNiCrMo-3 2.4mm GER
ERNiCrMo-4 2.4mm AS

Daxun adalah produsen pelat baja tahan karat yang dapat dipercaya

Sebagai produsen profesional, Daxun memastikan bahwa semua produk yang kami hasilkan berkualitas tinggi. Oleh karena itu, kami memastikan bahwa semua pelat baja tahan karat disertifikasi oleh ISO9001, SGS, CE, OQC, dan lebih banyak standar kualitas internasional, serta memiliki kontrol kualitas yang ketat untuk memastikan bahwa pelat baja tahan karat memiliki lebih sedikit cacat. Di Daxun, yakinlah bahwa semua produk tahan lama, berkualitas tinggi, dan berkinerja tinggi.

Proyek dan produk hot case terbaru

304 plate stainless steel
baja tahan karat pelat astm a240
304 flat stainless steel plate
304 2b stainless steel sheet
304 stainless steel sheet price
Bisakah saya mendapatkan beberapa sampel?

Kami dapat menyediakan sampel lembaran baja tahan karat untuk Anda periksa kualitasnya. Sampel gratis dan Anda hanya membayar ongkos kirim.

Negara mana saja yang sudah Anda ekspor?

Kami telah mengekspor ke lebih dari 42 negara, seperti Kanada, Chili, Kuwait, Jerman, Korea Selatan, Arab Saudi, Singapura, dll.

Apa MOQ Anda?

MOQ kami adalah 1 ton untuk lembaran baja tahan karat.

Berapa lama waktu pengiriman Anda?

Pesanan percobaan dapat dikirim dalam waktu satu minggu. Untuk pesanan reguler, kira-kira membutuhkan waktu dua minggu.

Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat