Daxun is an excellent manufacturer of CP Grade 4 titanium rods and bars.

  • Titanium bar grade: UNS R50700
  • Titanium bar types: rolled bars, drawn bars, forged titanium bars
  • Main standards: ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
  • High corrosion resistance, excellent weldability, superior strength, lightweight, and outstanding performance in aggressive environments.

The global leader in commercially titanium alloy rod manufacturing services

Daxun, specializing in the production of alloy titanium rods for extreme environments

CP Grade 4 titanium bar represents the highest strength variant within the commercially pure titanium family, combining exceptional mechanical properties with outstanding corrosion resistance. As an unalloyed titanium grade, it maintains the inherent biocompatibility and weldability of pure titanium while delivering significantly enhanced tensile strength, with minimum yield strength reaching 480 MPa and ultimate tensile strength exceeding 550 MPa. This unique combination makes CP Grade 4 titanium bars particularly valuable in applications demanding both structural integrity and environmental durability.

The chemical composition of CP Grade 4 titanium bar consists primarily of titanium with controlled amounts of oxygen (0.40% maximum), iron (0.50% maximum), carbon (0.08% maximum), and nitrogen (0.05% maximum). The elevated oxygen content compared to other CP grades directly contributes to its superior strength characteristics. These bars exhibit excellent ductility, allowing for various forming processes while maintaining their enhanced mechanical properties, making them suitable for cold working, machining, and fabrication into complex components.

Key Application Areas

  • Aerospace: Used for critical structural components, aircraft fasteners, and springs where high strength-to-weight ratio is essential.
  • Chemical Processing: Ideal for pump shafts, valve components, and heat exchanger parts exposed to aggressive media.
  • Marine Engineering: Employed for hardware and components that require long-term durability in seawater.
  • Medical Implants: Utilized for surgical instruments and implant devices that demand both high strength and biocompatibility.

Manufacturing & Product Forms

  • Production Processes: Can be produced through hot rolling, forging, or extrusion, followed by annealing.
  • Available Forms: Supplied in various shapes, including round, square, hexagonal, and flat bars.
  • Custom Dimensions: Available in a wide range of sizes, with options for custom dimensions to meet specific project needs.
  • Machining: Can be effectively machined using appropriate tooling and cooling strategies, though it requires more robust parameters than lower titanium grades.
Spesifikasi Details
Bahan CP Grade 4 Titanium Bar
Standar ASTM B348, ASTM F67, AMS 4921, ISO 5832-2
Dimensions EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN
Diameter Range 0.125″ – 14″ (3.175mm – 355.6mm), custom
Length Range Up to 240″ (6096mm), custom
Form Round Bar, Square Bar, Hexagonal Bar
Permukaan akhir Cold drawn, Centerless Ground, Polished, Rough Turned, Black, NO.4 Finish, BA Finish, Matt Finish
Kondisi Annealed, Hardened & tempered
Toleransi Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm)
Form Titanium square bars, titanium ingots, titanium round bars, rectangular titanium bars, triangular titanium bars, forged titanium bars, titanium hexagonal bars

Data

Elemen Minimum Maximum
Titanium (Ti) 99.2 -
Oksigen (O) 0.35 0.40
Besi (Fe) - 0.50
Carbon © - 0.08
Nitrogen (N) - 0.05
Hidrogen (H) - 0.015
Properti Minimum Value Unit
Kekuatan Tarik Tertinggi 550 MPa
Yield Strength (0.2% offset) 480 MPa
Perpanjangan 15 %
Reduction of Area 30 %
Brinell Hardness 320 HBW
Modulus of Rigidity 44 GPa

 

Properti Nilai Unit
Kepadatan 4.51 g/cm³
Titik Leleh 1668 °C
Modulus Elastisitas 105 GPa
Konduktivitas Termal 16.4 W/m·K
Tahanan Listrik 560 nΩ·m
Specific Heat 0.52 J/g·K

Pilih Daxun untuk membantu proyek Anda berjalan.

Hubungi Daxun sekarang

Daxun Factory Advantages

Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

Hubungi Daxun sekarang

CP Grade 4 Titanium Rod Production Method

Daxun produces high-quality titanium bars with high performance, and can also manufacture according to customer’s agreement:

  • Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.
Hubungi Daxun sekarang

Kualitas, pengiriman, inspeksi

Daxun performs several quality assurance tests, these tests include mechanical tests like area tensile, chemical analysis, material positive identification – PMI test, micro and macro testing, intergranular corrosion (IGC) test, ultrasonic flaw detection test, pitting and resistance test, hardness test, material positive identification, expansion test etc. All these tests ensure that the CP Grade 4 Titanium Rod and CP Grade 4 Titanium Round Bar material is suitable for the required application. During the production process, we measure the diameter, thickness and surface of the product.

  • Waktu pengiriman kami benar-benar sesuai dengan kontrak.
  • Mendukung agen pihak ketiga pelanggan untuk pergi ke pabrik untuk pemeriksaan
  • Support free samples for customer testing
  • Mendukung inspeksi pabrik di tempat atau video
Hubungi Daxun sekarang

Pengemasan

Daxun Alloy memastikan kualitas kemasan terbaik karena memainkan peran penting dalam pengiriman internasional di mana barang melewati berbagai saluran untuk mencapai tujuan akhir, jadi kami memberikan perhatian khusus pada pengemasan. Kami mengemas barang-barang kami dengan berbagai cara tergantung pada produknya. Kami mengemas produk kami dengan berbagai cara seperti:
- Kotak dan peti
- Kecilkan bungkus
- Palet kayu
- Kotak kayu

Hubungi Daxun sekarang

Dukungan Teknis

Jika Anda memerlukan bantuan teknis tambahan, ahli metalurgi dan staf kami yang berpengetahuan luas akan dengan senang hati membantu. Selain itu, Daxun memiliki laboratorium pengujian bersertifikat-yang pertama dalam industri inventaris multi-logam dan plastik. Ini, menurut pendapat kami, menunjukkan dedikasi kami yang tak tergoyahkan terhadap kualitas dan filosofi kami sebagai pemasok layanan penuh.

Daxun CP Grade 4 Titanium Rods help your brand improve quickly

NOMINAL SIZE
h5
h6
h7
h8
h9
H10
H11
h12
DIAMETER mm
~ to 3 +0.004/0 +0.006/0 +0.01/0 +0.014/0 +0.025/0 +0.04/0 +0.06/0 +0.1/0
over 3 to 6 +0.005/0 +0.008/0 +0.012/0 +0.018/0 +0.03/0 +0.048/0 +0.075/0 +0.12/0
over 6 to 10 +0.006/0 +0.009/0 +0.015/0 +0.022/0 +0.036/0 +0.058/0 +0.09/0 +0.15/0
over 10 to 18 +0.008/0 +0.011/0 +0.018/0 +0.027/0 +0.043/0 +0.07/0 +0.11/0 +0.18/0
over 18 to 30 +0.009/0 +0.013/0 +0.021/0 +0.033/0 +0.052/0 +0.084/0 +0.13/0 +0.21/0
over 30 to 50 +0.011/0 +0.016/0 +0.025/0 +0.039/0 +0.062/0 +0.1/0 +0.16/0 +0.25/0
over 50 to 80 +0.013/0 +0.019/0 +0.03/0 +0.046/0 +0.074/0 +0.12/0 +0.19/0 +0.3/0
over 80 to 120 +0.015/0 +0.022/0 +0.035/0 +0.054/0 +0.087/0 +0.14/0 +0.22/0 +0.35/0
over 120 to 180 +0.018/0 +0.025/0 +0.04/0 +0.063/0 +0.1/0 +0.16/0 +0.25/0 +0.4/0
over 180 to 250 +0.02/0 +0.029/0 +0.046/0 +0.072/0 +0.115/0 +0.185/0 +0.29/0 +0.46/0

Proyek dan produk hot case terbaru

Grade 7 Titanium rod and bar
Batang dan batang titanium
Batang dan batang titanium
Batang dan batang titanium
Batang dan batang titanium
Batang dan batang titanium
What makes CP Grade 4 titanium bar different from other commercially pure grades?

CP Grade 4 is the strongest of all the commercially pure titanium grades. Its key differentiator is its higher oxygen content, which gives it a minimum yield strength of 480 MPa, significantly higher than CP Grade 2 (275 MPa). This makes it the preferred choice when high strength and durability are critical, while still maintaining excellent corrosion resistance.

What are the most common applications for CP Grade 4 titanium bar?

Due to its high strength-to-weight ratio and biocompatibility, CP Grade 4 titanium bar is widely used in the aerospace industry for fasteners and springs, in chemical processing for pump and valve components, in marine engineering for durable hardware, and in the medical field for surgical instruments and implants that require superior structural integrity.

Is CP Grade 4 titanium bar difficult to machine or weld?

While it is more challenging to machine than lower grades due to its strength, it can be effectively machined with proper tooling and cooling. It is also readily weldable using standard methods like TIG welding, but it requires an inert gas shield (like argon) to protect the weld area from atmospheric contamination and prevent embrittlement.

Why should I choose CP Grade 4 titanium over stainless steel?

The primary advantage is its superior corrosion resistance, especially in chloride environments like seawater, where stainless steel is prone to pitting and stress corrosion cracking. CP Grade 4 also offers a much better strength-to-weight ratio. Although the initial cost is higher, its extended service life and reduced maintenance in harsh environments often result in a lower total cost of ownership.

Bagaimana cara mendapatkan penawaran atau memahami informasi pasar secepatnya?

Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email (Daxunalloy@gmail.com) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week

Bisakah saya mendapatkan beberapa sampel?

We can provide titanium rod samples for you to check the quality. Sample is free and you just pay the freight.

Negara mana saja yang sudah Anda ekspor?

Kami telah mengekspor ke lebih dari 42 negara, seperti Kanada, Chili, Kuwait, Jerman, Korea Selatan, Arab Saudi, Singapura, dll.

Berapa lama waktu pengiriman Anda?

Pesanan percobaan dapat dikirim dalam waktu satu minggu. Untuk pesanan reguler, kira-kira membutuhkan waktu dua minggu.

Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat