x
Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat

CP Grade 3 Titanium Plate Manufacturer - Daxun Alloy

As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.

  • Plate Grade:R50550 / CP TI50A
  • Plate Production type:cold rolling, hot rolling, forging.
  • Features:High strength, Lightweight, High-temperature resistance
  • Surface:bright, polished, pickled, sandblasted, etc.
  • Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request

————Daxun produces titanium sheets in China to meet the diverse and ——demanding needs of customers!

Providing High-quality CP Grade 3 Titanium Plates to Serve Customers Worldwide

CP Grade 3 Titanium plate is a commercially pure titanium grade known for its excellent balance of strength and ductility. It offers higher mechanical properties compared to Grades 1 and 2, making it ideal for applications requiring moderate strength and good formability. This grade features outstanding corrosion resistance, especially in marine and chemical environments, along with low density and high toughness.

Key Characteristics:
  • Composition: CP Grade 3 is primarily titanium (typically ~99.1%), with small amounts of oxygen, iron, carbon, nitrogen, and hydrogen. The oxygen content is the main factor influencing its strength.
  • Mechanical Properties: It offers higher tensile and yield strength than Grades 1 and 2, making it suitable for applications requiring more robust performance while still maintaining good ductility.
  • Ketahanan Korosi: Like all CP titanium grades, Grade 3 provides outstanding resistance to corrosion, especially in oxidizing environments such as those containing chlorides or seawater.
  • Fabrication: It can be welded, formed, and machined using conventional methods, which enhances its versatility in manufacturing.
  • Biocompatibility: The material is biocompatible, allowing its use in medical implants and other healthcare applications.
Common Applications:
  • Aerospace: For components that need a mix of strength, light weight, and corrosion resistance.
  • Chemical Processing: Equipment exposed to corrosive environments.
  • Marine Engineering: Parts subject to seawater corrosion.
  • Medical Devices: Implants and surgical tools due to its biocompatibility.

 

CP Grade 3 vs. Other Titanium Grades

CP Grade 3 Titanium plate serves as a powerful middle-ground option in the titanium family. It delivers significantly higher strength than the softer, more formable Grades 1 and 2, making it suitable for components that face greater mechanical stress. Crucially, it achieves this strength boost while retaining excellent corrosion resistance and good weldability, a key advantage over the even stronger but less ductile CP Grade 4.

When compared to the popular alloy Grade 5 (Ti-6Al-4V), CP Grade 3 is less strong and not heat-treatable. However, it is far easier to form and fabricate, and it provides superior corrosion resistance in many reducing chemical environments. This makes CP Grade 3 the ideal choice when your project requires a step up in strength from the basic CP grades but cannot sacrifice the ease of manufacturing and outstanding durability needed for demanding aerospace, marine, and chemical processing applications.

Baca Lebih Lanjut

Data

Elemen Konten (%)
Titanium (Ti) Balance (~99.1%)
Oksigen (O) 0.10 – 0.27
Besi (Fe) ≤ 0.30
Carbon © ≤ 0.08
Nitrogen (N) ≤ 0.05
Hidrogen (H) ≤ 0.015
Properti Nilai
Kepadatan ~4.51 g/cm³
Titik Leleh ~1660–1670 °C
Modulus Elastisitas ~103–107 GPa
Konduktivitas Termal ~21.9 W/m·K (at 25°C)
Tahanan Listrik ~420 nΩ·m
Properti Nilai
Kekuatan Tarik ~450–485 MPa
Kekuatan Hasil ~380–415 MPa
Perpanjangan ~20–30%
Kekerasan (Brinell) ~200–240 HB

Pilih Daxun untuk membantu proyek Anda berjalan.

Pengiriman cepat

At Daxun Alloys Co., Ltd., we specialize in the rapid supply of premium CP Grade 3 titanium plates to meet your urgent project needs. With our extensive inventory and efficient logistics network, we ensure prompt delivery without compromising on quality. Whether you require standard sizes or custom-cut solutions, our team is committed to providing reliable, on-time service to support your manufacturing and engineering schedules.

Pemotongan Khusus

Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:

  • Pemotongan jet air
  • Pemotongan laser
  • Plasma cutting
  • Wire cutting
  • Bending
  • Menggorok
  • Menggergaji

Pengemasan

We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- Kotak dan peti
• Shrinkwrap
- Palet kayu
- Kotak kayu

Dukungan Teknis

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.

Daxun CP Grade 3 Titanium sheet Let your brand improve rapidly

Selain produk yang tercantum di bawah ini, produk logam lain yang tersedia tidak tercantum di sini. Produk logam lain yang dapat diproduksi dan dipasok DAXUN termasuk Tantalum, Niobium, Zirkonium, Hafnium, Nikel, Tembaga, dll., Yang sebagian besar dalam bentuk Plat, Batang dan Tabung.
Standar Produk/Pemrosesan Kelas / Ukuran
Plat Titanium, Lembaran, Kumparan- ASME SB265, AMS 4911, AMS 4919, AMS 4914, ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7, GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3 (Ketebalan: (0,0197 ”-6”) Lebar Maksimum: 12 kaki, Panjang Maksimum: 50 kaki)
AMS-T-9046
Lembaran paduan Titanium dan Titanium, pelat
Titanium murni komersial (CP)
Penunjukan kode Kekuatan luluh
minimum, ksi 1 /
CP-1 Gr1 70
CP-2 Gr2 55
CP-3 Gr3 40
CP-4 Gr4 25
Paduan titanium alfa (A)
Penunjukan kode Komposisi
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn (ELI) 2 /
A-3 6A1-2Cb-1Ta-0.8Mo
A-4 8A1-1Mo-1V
Paduan titanium alfa-beta (AB)
Penunjukan kode Komposisi
AB-1 Gr5 6A1-4V
AB-2 Gr5 6A1-4V (ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
Paduan titanium beta (B)
Penunjukan kode Komposisi
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
Pemrosesan:
Penggulungan Panas Penggulungan Dingin
Nilai yang Tersedia:
CP Kelas 1 Kelas 6Al-2Sn-4Zr-2Mo (6-2-4-2)
CP Kelas 2 Kelas 6Al-4V ELI (Sebelumnya Kelas 23)
Kelas 7 Kelas 6Al-6V-2Sn (6-62)
Kelas 19 Kelas 8Al-1Mo-1V (8-1-1)
Kelas 5 (6Al-4V) Kelas 9 (3Al-2.5V)
Kelas 6 (5Al-2.5Sn) CP Kelas 3
Aplikasi
Industri Kimia Desalinasi Air Laut
Industri Petrokimia Dirgantara
Bidang Permesinan, Bidang Otomotif Bidang Komponen Telepon Seluler.

Proyek dan produk hot case terbaru

CP Grade 3 Titanium Titanium Plate and sheet
Naval vessels
Plat dan lembaran Titanium
Aviation and Aerospace
Plat dan lembaran Titanium
Military armor
Plat dan lembaran Titanium
Guidance components
Plat dan lembaran Titanium
Industri energi baru
Plat dan lembaran Titanium
Teknik Kelautan
What is the main difference between CP Grade 3 and the more common Grade 2 titanium? How do I choose?

The primary difference is strength. CP Grade 3 offers significantly higher tensile and yield strength than Grade 2, making it suitable for components that must withstand greater mechanical stress. It still maintains excellent corrosion resistance and good weldability.

How to choose:

  • Choose Grade 2 if your project demands excellent formability and cost-effectiveness with moderate strength.
  • Choose CP Grade 3 if your parts need to endure medium to high mechanical loads without sacrificing corrosion resistance or weldability.
Do you offer cutting services for CP Grade 3 titanium plates? Can I get custom sizes?

Yes, we provide professional custom cutting services. To minimize your material waste and machining time, we can cut the titanium plates to your exact specifications based on your drawings or dimensions. Please provide your detailed requirements when requesting a quote, and our team will offer the best solution.

Are your CP Grade 3 titanium plates certified to international standards? Can you provide a Material Test Report (MTR)?

Absolutely. All our CP Grade 3 titanium plates comply with international standards such as ASTM B265 / ASME SB265. With every shipment, we can provide a certified Material Test Report (MTR) detailing the chemical composition and mechanical properties, ensuring full traceability and quality assurance.

How is the weldability of CP Grade 3 titanium? Does it require special procedures?

CP Grade 3 titanium has excellent weldability. We recommend using TIG (Gas Tungsten Arc Welding) or MIG (Gas Metal Arc Welding). The most critical step is to provide proper shielding with an inert gas (typically argon) to protect the weld pool from atmospheric contamination. With correct protection, the weld’s performance will be as strong as the base material.

Bagaimana cara mendapatkan penawaran atau memahami informasi pasar secepatnya?

Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email (Daxunalloy@gmail.com) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week

Bisakah saya mendapatkan beberapa sampel?

We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.

Negara mana saja yang sudah Anda ekspor?

Kami telah mengekspor ke lebih dari 42 negara, seperti Kanada, Chili, Kuwait, Jerman, Korea Selatan, Arab Saudi, Singapura, dll.

Berapa lama waktu pengiriman Anda?

Pesanan percobaan dapat dikirim dalam waktu satu minggu. Untuk pesanan reguler, kira-kira membutuhkan waktu dua minggu.

Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat