Titanium Plate and Sheet

Titanium plate and sheet supplier from China since 2003.
CP Grade 1–4 and titanium alloy, hot rolled, cold rolled, and forged.

Daxun has a full range of pure titanium plates

  • Grade:CP Grade 1 to Grade 18
  • Type: Titanium and titanium alloy plates
  • Hot rolled titanium plate 3.0mm-100mm
  • Cold rolled titanium plate with thickness 0.3mm to 3.2mm
  • Forged titanium plate: thickness 20mm-380mm
  • Standards:ASTM AMS ASME GB GJB DIN JIS

Send your grade, thickness, and specification, and we’ll confirm availability, pricing, and lead time.

Applications and Usage for Titanium Sheet and Plate

Since 2003, Daxun’s titanium sheet and plate have been supplied for chemical processing, marine, medical, and architectural applications. Medical-grade material — CP Grade 1–4 and Ti-6Al-4V ELI — is produced to ASTM F67 and ISO 5832-2 for orthopedic and dental implant use. CP Grade 5 (Ti-6Al-4V) is also supplied for automotive and sports equipment applications where high strength-to-weight ratio matters. Commercially pure grades hold up to service temperatures with a melting range around 3,000°F (1,650°C), making titanium a reliable choice where corrosion resistance and thermal stability both matter. Send your grade and application, and we’ll confirm the right specification for your project.

Daxun’s titanium plates are built for demanding applications where strength, toughness, and corrosion resistance matter most. From marine engineering to chemical processing and medical device manufacturing, our material is produced under strict quality control and advanced processing technology, so every plate meets the specification your application requires. Send your grade, thickness, and application, and we’ll confirm the right material for your project.

Baca Lebih Lanjut

Characteristics of various titanium plates

Each titanium plate material has its own different usage scenarios.

cp1
titanium sheet grade 1

Industrial pure titanium plate, easy to weld, corrosion-resistant, and can work at 300°C for a long time.

cp6
titanium plate grade 2

Industrial pure titanium plate, easy to stretch and bend, can work at 300℃ for a long time.

cp3
Titanium alloy plate

High strength, light weight, good neutralizing performance, and can work at 400℃ for a long time

cp7
titanium sheet grade 5

High temperature resistance and high strength, suited to demanding structural applications.

Forged titanium plates have good strength and toughness, and the grains are refined.

Titanium grade 5 belongs to α+β type titanium alloy and has good comprehensive properties.

cp8
Titanium Clad Steel Plate

Titanium and steel plate composite materials for power plant chimneys

Low density, corrosion resistance, acid and alkali resistance, light weight and easy to process.

Low density, corrosion resistance, acid and alkali resistance, light weight and easy to process.

cp12
titanium sheet grade 12

Grade 12 titanium plates have better corrosion resistance than industrial pure titanium plates

Ti 6Al-4V sheet has been widely used in aerospace and military fields

Ti 6Al-4V plates and plates are α+β titanium alloys and have good overall properties.

12 Products Found.

Titanium plate production flow

With our reliable titanium plates, their properties can be customized to suit your application.

  • titanium sponge
    Choose titanium sponge

    Choose titanium sponge that meets your smelting requirements

  • ronglian
    carry out smelting

    The third smelting uses EB furnace and vacuum consumable furnace.

  • zhazhi
    Rolled

    After heating, it undergoes several rounds of rolling, then trimming and straightening to become a titanium plate.

  • biaomian
    Surface treatment

    We can pickle, polish, sandblast to get a better surface

  • xiuzheng
    Board trimming

    Remove burrs and defects to improve the quality and finish of the board, making it flatter and smoother.

  • jianyan
    Inspection and delivery

    To ensure product quality, inspections ensure products meet quality standards.

Main features of titanium plate

Ringan

Titanium has a density of approximately 4.51 g/cm³ — about 60% of steel’s density at comparable strength.

Corrosion resistant

A stable, self-healing oxide layer gives titanium excellent resistance to seawater, chlorides, and most acids — significantly outperforming stainless steel in chloride-rich environments.

Non-magnetik

Suitable for applications where magnetic interference must be avoided.

kekuatan tinggi

Titanium alloys such as Ti-6Al-4V offer strength comparable to many steels at roughly half the weight.

Commercially Pure Titanium and Titanium Alloys

Pure Titainium:

CP Grade 1, CP Grade 2, CP Grade 3, CP Grade 4

Titanium Alloys:

CP Grade5 , Ti 6AL-4V,Ti15333,Ti 4AL-3.5V

Other Available Titanium Product Grade:

Grade7, Grade 9, Grade 11, Grade 12, Grade 16, Grade 17, Grade 18 , Grade 23

scx

SPECIFICATIONS

 

  • UNS R50250
  • UNS R50400
  • UNS R50550
  • UNS R50700
  • 3.7035
  • ASME SB 265
  • ASTM B265
  • ASTM B348
  • ASTM F67
  • ISO 5832-2

 

PHYSICAL PROPERTIES For CP 1, 2, 3, 4:

 

Melting Range: 3,000-3,040°F, (1,649 – 1,671°C)

Density: 0.163 lbs/in³; 4.51 gm/cm³

Beta Transus Temperature (typical, per ASTM B265):
CP Grade 1: approx. 1,634°F (890°C)
CP Grade 2: approx. 1,679°F (915°C)
CP Grade 3: approx. 1,688°F (920°C)
CP Grade 4: approx. 1,742°F (950°C)

Actual beta transus temperature varies with oxygen content and
composition — confirm against the mill test certificate for your specific
heat.

Forged titanium plate

Forged titanium plate offers refined grain structure and improved mechanical properties compared to rolled plate, suited to medical device and energy equipment applications requiring higher strength and toughness.

Titanium plate heat treatment

Heat Treatment Processes We Offer:

Stress Relief Annealing

Solution Annealing with Air or Water Quenching

Solution Treating + Aging (STA)

Other Processes Available upon Request

Titanium Plate Quality Inspection

Every titanium plate undergoes chemical composition analysis, mechanical property testing, non-destructive testing, and corrosion resistance verification before shipment. Inspection reports are available in accordance with EN 10204 3.1/3.2 upon request.

Corrosion Resistant Information

Titanium’s corrosion resistance comes from a thin, stable oxide layer that
forms naturally on the surface and self-repairs when scratched or exposed.

Nominal Composition Forms Coil Lembar Piring
CP Kelas 1 Ti

√

√

√

CP Kelas 2 Ti

√

√

√

CP Kelas 3 Ti

√

√

√

CP Grade 4

CP Grade 5

Ti

Ti

√

√

√

√

√

√

CP Grade 7 Ti (Gr2) 0.2 Pd

√

√

**
CP Grade 11 Ti (Gr1) 0.2 Pd

√

√

**
CP Grade 16 Ti (Gr2) 0.05 Pd

√

√

**
CP Grade 17 Ti (Gr1) 0.05 Pd

√

√

**
* Produced to ASTM, AMS, ASME and MIL Specifications.
** Inquire with your sales representative.

 

SIZES,TOLERANCES

Lembar
Width** (in) Thickness (in)
24″ – 48″ Up to 0.1874″
Strip
Width (in) Thickness (in)
0.250″ – 24″ 0.001″ – 0.1874″
Piring
Width (in) Thickness (in)
96″ 0.1875″ – 4.0″ x 360″ max

* Sizes and tolerances vary. Inquire with your sales representative.

Product technical details and mechanical properties

For specific technical details, please view the individual product pages. We also could provide a design and fabrication handbook for industrial applications workbooks, Technical Data Sheets, certification, and price quotes. For non- commercially pure titanium, we will give exact alloying elements, metals, materials, and grades, oxygen, nitrogen for each product.

Who is Daxun Alloy?

Daxun Alloy supplies titanium plate, titanium alloy (including Grade 5 and other alloy grades), and stainless steel products, with procurement, processing, and logistics handled under one roof to simplify sourcing for our customers.

Visit Our Factory in China

We can arrange a factory visit, or a video call if an in-person visit
isn’t possible, so you can see how your order is being manufactured.

Safety Data Sheet-Titanium
  • Full SDS (Safety Data Sheet) available to ensure safe use and compliance.

  • Each batch can be supplied with an SDS, meeting international standards.

  • SDS available upon request, supporting global compliance and safety.

Similar products

Daxun also produces titanium pipe, rod, and rolled rings. Send us your requirement and we’ll confirm availability.

Paduan Daxun

Regarding titanium plates, we can handle any type of inquiry. Please feel free to ask us. We will make recommendations based on each client’s needs.

Q1: Which international standards do your titanium plates comply with?

A1: Our titanium plates meet ASTM B265, AMS, ISO, GB/T, and GOST standards. Specific standards can also be supplied upon request.

Q2: Can you provide Mill Test Certificates (MTC) and inspection reports?

Yes. Every shipment includes a mill test certificate, and inspection reports are available in accordance with EN 10204 3.1/3.2 upon request.

Q3: How do you guarantee the mechanical properties and chemical composition?

Every batch undergoes chemical composition analysis, mechanical testing, and non-destructive testing before shipment, verified against the applicable ASTM, AMS, or GB/T specification for your order.

Q4: What are the common sizes and tolerances of your titanium plates? Can they be customized?

Standard plate is available up to 96″ wide, 0.1875″–4.0″ thick, and up to 360″ in length. Custom sizes and tolerances can be confirmed against your specification — send your drawing or requirements for a quote.

Q5: What are the main applications of titanium plates?

Chemical processing, marine engineering, medical devices, and architecture, with CP Grade 5 (Ti-6Al-4V) also used in automotive and
sports equipment applications.

Q6: What surface finishes are available?

Pickled, polished, and sandblasted finishes are available — confirm the required finish with your order.

Q7: What is the typical delivery time?

In-stock items ship in 1–3 days. Custom orders typically take 7–15 days depending on grade, size, and quantity.

Q8: How do you ensure safe packaging and transportation?

Titanium plate is packed to prevent damage in transit, with packaging method matched to the product and shipping method. We offer sea, land, and air shipping depending on order urgency.

T9: Berapa jumlah pesanan minimum (MOQ)?

Minimum order quantity is 100kg. Contact us if your requirement is below this threshold — we may still be able to help.

Q10: Do you provide heat treatment or additional processing services?

Yes. Available heat treatment processes include stress relief annealing, solution annealing (air or water quench), and solution treating + aging (STA). Other processes are available on request.

Q11: Which titanium grades and alloys do you supply?

Commercially pure titanium CP Grade 1 through 4, and titanium alloys including Grade 5 (Ti-6Al-4V), Ti-15-3-3-3, and Ti-6Al-4V ELI, along with other grades including 7, 9, 11, 12, 16, 17, 18, and 23.

Q12: How do you ensure corrosion resistance of titanium plates?

Titanium’s corrosion resistance comes from a stable, self-healing oxide layer that forms naturally on the surface. Material is supplied to
the specified grade and standard to ensure this performance is consistent batch to batch.

Q13: Can you manufacture according to customer drawings?

Yes. Send your drawing with required dimensions, tolerances, and grade, and we’ll confirm feasibility, pricing, and lead time.

Q14: What factors influence the pricing of titanium plates?

Pricing depends on grade, thickness, size, quantity, surface finish, and any additional processing or heat treatment required. Send your
specification for a quote.

Q15: Do you support common international trade terms?

Yes — quotes can be provided on FOB, CFR, CIF, or other terms as required for your order.

Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat