x
Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat
  • Hastelloy Pipe
  • Hastelloy Pipe
  • Hastelloy Pipe
  • Hastelloy Pipe
  • Hastelloy Pipe
  • Hastelloy Pipe
  • Hastelloy Pipe
  • Hastelloy Pipe
  • Hastelloy Pipe
  • Hastelloy Pipe

Daxun Alloy - Hastelloy C-22 pipe made in China

As a leading supplier of Hastelloy C-22 pipes in China, Daxun provides high-performance alloy tubes to the world.
  • Hastelloy C-22 types: Seamless tube,  welded tube, forged tube
  • Certification : ASTM,SGS,ISO,CE
  • Delivery Time : 7-15 days
  • Surface finish: Annealed, polished etc.
  • MOQ : ≥300kg

————Daxun produces hastelloy pipe in China to meet the diverse and ——demanding needs of customers!

Characteristics & Properties of Hastelloy C-22

Hastelloy C-22(UNS N06022) alloy is an all-around nickel-chromium-molybdenum-tungsten alloy with better overall corrosion resistance than other existing nickel-chromium-molybdenum alloys, including Hastelloy C-276, C-4 alloy and 625 alloy. Hastelloy C-22 alloy has good resistance to pitting, crevice corrosion and stress corrosion cracking. It has excellent resistance to oxidizing aqueous media, including wet chlorine, nitric acid or mixed acids containing oxidizing acids with chloride ions. At the same time, Hastelloy C-22 alloy also has ideal resistance to reducing and oxidizing environments encountered in the process. Relying on this versatile performance, it can be used in some troublesome environments or in factories with multiple production purposes. Hastelloy C-22 alloy has an exceptional resistance to various chemical environments, including strong oxidizing substances such as ferric chloride, cupric chloride, chlorine, hot contaminated solutions (organic and inorganic), formic acid, acetic acid, acetic anhydride, seawater and salt solutions. Hastelloy C-22 alloy has the ability to resist the formation of grain boundary precipitation in the heat-affected zone of welding, so that it can also be used in many chemical processes in the welded state.

Corrosion resistance
The corrosion resistance of Hastelloy C-22 is its most outstanding feature, and it is suitable for a variety of corrosive environments:
Oxidizing media: such as nitric acid, chromic acid, hypochlorite, etc.
Reducing media: such as sulfuric acid, hydrochloric acid, phosphoric acid, etc.
Local corrosion: It has strong resistance to pitting, crevice corrosion and stress corrosion cracking (SCC).
Mixed acid environment: complex media such as sulfuric acid + hydrochloric acid, nitric acid + hydrofluoric acid.
High temperature corrosion: It can still maintain good corrosion resistance at high temperatures.

Comparison with other alloys
Compared with Hastelloy C-276, C-22 has a higher chromium content and stronger oxidation resistance.
Compared with stainless steel, C-22 has significantly better pitting and crevice corrosion resistance in chloride environments.

Processing performance
Hastelloy C-22 has good processing performance, but its high strength and work hardening tendency should be noted:
Cold processing: It can be processed by cold rolling, cold drawing, etc., but attention should be paid to work hardening.
Hot working: The hot working temperature range is 950-1200°C, and overheating should be avoided.
Welding: TIG (tungsten inert gas shielded welding), MIG (metal inert gas shielded welding), plasma arc welding and other methods can be used. Heat treatment is usually not required after welding, but heat input needs to be controlled to avoid intergranular corrosion.
Application areas
Hastelloy C-22 is widely used in the following fields:
Chemical industry: used to manufacture reactors, heat exchangers, pipelines, valves and other equipment, especially in strong acid, strong alkali and mixed acid environments.
Oil and gas: used for downhole tools, valves, pumps, pipelines, etc., to resist corrosion from hydrogen sulfide, carbon dioxide and chlorides.
Environmental protection field: used for flue gas desulfurization (FGD) systems, wastewater treatment equipment, etc.
Pharmaceutical industry: used for high-purity equipment to resist corrosive media.
Nuclear industry: used for nuclear waste treatment equipment to resist corrosion from radioactive media.

Baca Lebih Lanjut

Hastelloy C-22 Parameters

Ni Cr Mo W Fe Co
56% 20-22.5% 12.5-14.5% 2.5-3.5% 2-6% ≤2.5%
Mn Si C P S
≤0.5% ≤0.08% ≤0.015% ≤0.02% ≤0.02%

 

Properti Kepadatan Titik Leleh Thermal Expansion Coefficient Konduktivitas Termal Tahanan Listrik Modulus Elastisitas
Nilai 8.69 g/cm³ 1325-1370°C 12.8 μm/m·°C 10.1 W/m·K 1.25 μΩ·m 206 GPa

 

Properti Room Temperature (20°C) High Temperature (600°C) Test Standard/Notes
Kekuatan Tarik ≥690 MPa ≥380 MPa ASTM E8/E8M
Yield Strength (0.2%) ≥310 MPa ≥220 MPa ASTM E8/E8M
Perpanjangan ≥45% ≥30% 50 mm gauge length
Kekerasan (Brinell) ≤220 HB – ASTM E10

 

Pilih Daxun untuk membantu proyek Anda berjalan.

Hubungi Daxun sekarang

Advanced Production:Hastelloy alloy pipe

Hastelloy C22 alloy is an all-around nickel-chromium-molybdenum-tungsten alloy with good resistance to pitting, crevice corrosion and stress corrosion cracking. It has excellent resistance to oxidative aqueous media, including wet chlorine, nitric acid or mixed acids of oxidizing acids containing chloride ions. At the same time, Hastelloy C22 alloy also has ideal resistance to reducing and oxidizing environments encountered in the process. Relying on this versatile performance, it can be used in some troublesome environments or in factories for a variety of production purposes.

Hubungi Daxun sekarang

Hastelloy C-22 Pipe Features

Hastelloy C22 alloy has an exceptional resistance to various chemical environments, including strong oxidizing substances, such as ferric chloride, cupric chloride, chlorine, thermally contaminated solutions (organic and inorganic), formic acid, acetic acid, acetic anhydride, seawater and salt solutions, etc. Hastelloy C22 alloy has the ability to resist the formation of grain boundary precipitation in the heat affected zone of welding, so that it can also be used in many chemical processes in the welding state.

Hubungi Daxun sekarang

Kualitas, pengiriman, inspeksi

Daxun conducts a series of quality assurance tests on Hastelloy C-22 pipes. These tests include flattening test, flaring test, ultrasonic flaw detection, crevice corrosion resistance test, mechanical property test, hardness test, material positive identification, and expansion test, etc. All these tests are designed to ensure that the Hastelloy C-22 pipes meet the requirements of the intended applications. During the production process, we meticulously measure the outer diameter, wall thickness, and surface quality of the products. Our standard delivery time is 5 – 7 days, and for special sizes, it is 15 – 20 days.

  • Waktu pengiriman kami benar-benar sesuai dengan kontrak.
  • Mendukung agen pihak ketiga pelanggan untuk pergi ke pabrik untuk pemeriksaan
  • Support free samples for customer testing
  • Mendukung inspeksi pabrik di tempat atau video
Hubungi Daxun sekarang

Pengemasan

Daxun Alloy memastikan kualitas kemasan terbaik karena memainkan peran penting dalam pengiriman internasional di mana barang melewati berbagai saluran untuk mencapai tujuan akhir, jadi kami memberikan perhatian khusus pada pengemasan. Kami mengemas barang-barang kami dengan berbagai cara tergantung pada produknya. Kami mengemas produk kami dengan berbagai cara seperti:
- Kotak dan peti
- Kecilkan bungkus
- Palet kayu
- Kotak kayu

Hubungi Daxun sekarang

Dukungan Teknis

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. [Hubungi Kami Sekarang]Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Daxun is a trustworthy stainless steel tube manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel tubes have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

Bagaimana cara mendapatkan penawaran atau memahami informasi pasar secepatnya?

Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email (Daxunalloy@gmail.com) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week

Bisakah saya mendapatkan beberapa sampel?

Kami dapat menyediakan sampel lembaran baja tahan karat untuk Anda periksa kualitasnya. Sampel gratis dan Anda hanya membayar ongkos kirim.

Negara mana saja yang sudah Anda ekspor?

Kami telah mengekspor ke lebih dari 42 negara, seperti Kanada, Chili, Kuwait, Jerman, Korea Selatan, Arab Saudi, Singapura, dll.

Apa MOQ Anda?

The minimum order quantity for our Hastelloy products is 300kg

Berapa lama waktu pengiriman Anda?

Pesanan percobaan dapat dikirim dalam waktu satu minggu. Untuk pesanan reguler, kira-kira membutuhkan waktu dua minggu.

Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat