Daxun Alloy - Hastelloy C-22 pipe made in China
As a leading supplier of Hastelloy C-22 pipes in China, Daxun provides high-performance alloy tubes to the world.
- Hastelloy C-22 types: Seamless tube, welded tube, forged tube
- Certification : ASTM,SGS,ISO,CE
- Delivery Time : 7-15 days
- Surface finish: Annealed, polished etc.
- MOQ : ≥300kg
————Daxun produces hastelloy pipe in China to meet the diverse and ——نیازهای سختگیرانه مشتریان!
Characteristics & Properties of Hastelloy C-22
Hastelloy C-22(UNS N06022) alloy is an all-around nickel-chromium-molybdenum-tungsten alloy with better overall corrosion resistance than other existing nickel-chromium-molybdenum alloys, including Hastelloy C-276, C-4 alloy and 625 alloy. Hastelloy C-22 alloy has good resistance to pitting, crevice corrosion and stress corrosion cracking. It has excellent resistance to oxidizing aqueous media, including wet chlorine, nitric acid or mixed acids containing oxidizing acids with chloride ions. At the same time, Hastelloy C-22 alloy also has ideal resistance to reducing and oxidizing environments encountered in the process. Relying on this versatile performance, it can be used in some troublesome environments or in factories with multiple production purposes. Hastelloy C-22 alloy has an exceptional resistance to various chemical environments, including strong oxidizing substances such as ferric chloride, cupric chloride, chlorine, hot contaminated solutions (organic and inorganic), formic acid, acetic acid, acetic anhydride, seawater and salt solutions. Hastelloy C-22 alloy has the ability to resist the formation of grain boundary precipitation in the heat-affected zone of welding, so that it can also be used in many chemical processes in the welded state.
Corrosion resistance
The corrosion resistance of Hastelloy C-22 is its most outstanding feature, and it is suitable for a variety of corrosive environments:
Oxidizing media: such as nitric acid, chromic acid, hypochlorite, etc.
Reducing media: such as sulfuric acid, hydrochloric acid, phosphoric acid, etc.
Local corrosion: It has strong resistance to pitting, crevice corrosion and stress corrosion cracking (SCC).
Mixed acid environment: complex media such as sulfuric acid + hydrochloric acid, nitric acid + hydrofluoric acid.
High temperature corrosion: It can still maintain good corrosion resistance at high temperatures.
Comparison with other alloys
Compared with Hastelloy C-276, C-22 has a higher chromium content and stronger oxidation resistance.
Compared with stainless steel, C-22 has significantly better pitting and crevice corrosion resistance in chloride environments.
Processing performance
Hastelloy C-22 has good processing performance, but its high strength and work hardening tendency should be noted:
Cold processing: It can be processed by cold rolling, cold drawing, etc., but attention should be paid to work hardening.
Hot working: The hot working temperature range is 950-1200°C, and overheating should be avoided.
Welding: TIG (tungsten inert gas shielded welding), MIG (metal inert gas shielded welding), plasma arc welding and other methods can be used. Heat treatment is usually not required after welding, but heat input needs to be controlled to avoid intergranular corrosion.
Application areas
Hastelloy C-22 is widely used in the following fields:
Chemical industry: used to manufacture reactors, heat exchangers, pipelines, valves and other equipment, especially in strong acid, strong alkali and mixed acid environments.
Oil and gas: used for downhole tools, valves, pumps, pipelines, etc., to resist corrosion from hydrogen sulfide, carbon dioxide and chlorides.
Environmental protection field: used for flue gas desulfurization (FGD) systems, wastewater treatment equipment, etc.
Pharmaceutical industry: used for high-purity equipment to resist corrosive media.
Nuclear industry: used for nuclear waste treatment equipment to resist corrosion from radioactive media.
Hastelloy C-22 Parameters
- ترکیب شیمیایی
- Physical properties
- خواص مکانیکی
| نی | کروم | مو | W | آهن | Co |
| 56% | 20-22.5% | 12.5-14.5% | 2.5-3.5% | 2-6% | ≤2.5% |
| امان | سی | C | P | S | |
| ≤0.5% | ≤0.08% | ≤0.015% | ≤0.02% | ≤0.02% |
| مالکیت | تراکم | نقطه ذوب | Thermal Expansion Coefficient | هدایت حرارتی | مقاومت الکتریکی | Elastic Modulus |
| ارزش | 8.69 g/cm³ | 1325-1370°C | 12.8 μm/m·°C | 10.1 W/m·K | 1.25 μΩ·m | 206 GPa |
| مالکیت | Room Temperature (20°C) | High Temperature (600°C) | Test Standard/Notes |
| مقاومت کششی | ≥690 MPa | ≥380 MPa | ASTM E8/E8M |
| Yield Strength (0.2%) | ≥310 MPa | ≥220 MPa | ASTM E8/E8M |
| Elongation | ≥45% | ≥30% | 50 mm gauge length |
| سختی (برینل) | ≤220 HB | – | ASTM E10 |
داکسون را انتخاب کنید تا به پروژهتان کمک کند اوج بگیرد.

Advanced Production:Hastelloy alloy pipe
Hastelloy C22 alloy is an all-around nickel-chromium-molybdenum-tungsten alloy with good resistance to pitting, crevice corrosion and stress corrosion cracking. It has excellent resistance to oxidative aqueous media, including wet chlorine, nitric acid or mixed acids of oxidizing acids containing chloride ions. At the same time, Hastelloy C22 alloy also has ideal resistance to reducing and oxidizing environments encountered in the process. Relying on this versatile performance, it can be used in some troublesome environments or in factories for a variety of production purposes.
Hastelloy C-22 Pipe Features
Hastelloy C22 alloy has an exceptional resistance to various chemical environments, including strong oxidizing substances, such as ferric chloride, cupric chloride, chlorine, thermally contaminated solutions (organic and inorganic), formic acid, acetic acid, acetic anhydride, seawater and salt solutions, etc. Hastelloy C22 alloy has the ability to resist the formation of grain boundary precipitation in the heat affected zone of welding, so that it can also be used in many chemical processes in the welding state.


کیفیت، تحویل، بازرسی
Daxun conducts a series of quality assurance tests on Hastelloy C-22 pipes. These tests include flattening test, flaring test, ultrasonic flaw detection, crevice corrosion resistance test, mechanical property test, hardness test, material positive identification, and expansion test, etc. All these tests are designed to ensure that the Hastelloy C-22 pipes meet the requirements of the intended applications. During the production process, we meticulously measure the outer diameter, wall thickness, and surface quality of the products. Our standard delivery time is 5 – 7 days, and for special sizes, it is 15 – 20 days.
- زمان تحویل ما دقیقاً مطابق قرارداد است.
- از آژانسهای ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
- از نمونههای رایگان برای آزمایش مشتری پشتیبانی کنید.
- حمایت از بازرسی کارخانهای حضوری یا ویدیویی
بستهبندی
داکسون آلیاژ بهترین کیفیت بستهبندی را تضمین میکند، زیرا بستهبندی نقش مهمی در حملونقل بینالمللی دارد که کالاها از مسیرهای مختلف عبور میکنند تا به مقصد نهایی برسند؛ بنابراین ما توجه ویژهای به بستهبندی داریم. ما کالاهای خود را بسته به محصول به روشهای مختلف بستهبندی میکنیم. روشهای بستهبندی محصولات ما عبارتند از:
• جعبهها و صندوقها
• سلفون منقبضشونده
• پالتهای چوبی
• جعبههای چوبی


پشتیبانی فنی
If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. [همین حالا با ما تماس بگیرید]Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.
Daxun is a trustworthy stainless steel tube manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel tubes have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
محصولات مرتبط (8)
لطفاً فرم صفحه “تماس با ما” را پر کنید یا با مدیر فروش ما به شماره +86 13382898899 تماس بگیرید. ما در اسرع وقت با شما تماس خواهیم گرفت. واتساپ ما آنلاین است و ایمیل (Daxunalloy@gmail.com) ظرف ۶ ساعت بررسی میشود. به هر پرسش یا پیام بهسرعت پاسخ داده خواهد شد. علاوه بر این، ما هر هفته اطلاعات بازار را با مشتریان خود به اشتراک میگذاریم.
ما میتوانیم نمونههای ورق فولاد ضدزنگ را برای بررسی کیفیت در اختیار شما قرار دهیم. نمونه رایگان است و شما فقط هزینه حمل را پرداخت میکنید.
ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشتهایم.
The minimum order quantity for our Hastelloy products is 300kg
سفارشهای آزمایشی را میتوان ظرف یک هفته تحویل داد. برای سفارشهای معمولی تقریباً دو هفته زمان لازم است.