Grade 9 Ti-3Al-2.5V Titanium Alloy Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:Grade 9 – UNS R56320
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Titanium tube density The density of grade 9 titanium is 4.48 g/cm3
  • Standards:ASTM B381、AMS 4920、ASTM B265

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

Grade 9 Titanium Alloy Pipe Manufacturer - Daxun Alloy

Provide High Quality Grade 9 Titanium Pipe to Customers Around The World
Grade 9 titanium pipe is a versatile alpha-beta alloy (Ti-3Al-2.5V), offering an optimal balance between pure titanium’s formability and Grade 5’s strength. It features moderate strength, exceptional weldability, and outstanding corrosion resistance in diverse environments. Its density (4.48 g/cm³) is approximately 60% that of steel, yet it delivers strength comparable to some steels, making it ideal for weight-sensitive applications. The alloy excels in durability across harsh conditions, including seawater, chemical processing, and extreme temperatures, while maintaining excellent fracture toughness and fatigue resistance.

Where is Grade 9 titanium pipe used?
In aerospace, it’s used for hydraulic and fuel lines, ducting systems, and airframe components—reducing weight without sacrificing structural integrity. کارخانه‌های فرآوری شیمیایی rely on it for heat exchangers, reactor tubing, and piping systems handling corrosive acids, alkalis, and chlorides due to its inertness. Marine and offshore industries use it for seawater cooling systems, desalination plants, and subsea equipment, leveraging its unparalleled seawater corrosion resistance. Oil and gas operations employ it in downhole tubing, risers, and Christmas tree components for high-pressure sour gas environments. Additionally, sports equipment manufacturers utilize it for high-performance bicycle frames, golf shafts, and racing components, where its strength-to-weight ratio and fatigue resistance are critical. It also serves in power generation (condenser tubing) and industrial heat transfer systems, combining longevity with thermal efficiency.

Key Performance:

Strength-Ductility Balance:

  • Tensile Strength: 620 MPa (annealed state) – Lower than Grade 23 but 30% stronger than pure titanium (Grade 1-4).
  • Elongation: ≥15% – Superior ductility vs. Grade 5 (≥10%), enabling complex forming and high fatigue resistance.
  • Density: 4.48 g/cm³ – 60% lighter than steel, ideal for weight-sensitive applications.

Corrosion Resistance:

  • Resists pitting/crevice corrosion in seawater, chlorides, and acidic/alkaline environments (e.g., HCl, H₂SO₄).
  • Outperforms stainless steel in marine/chemical processing, with no galvanic corrosion risk.

Weldability & Processability:

  • Welding: Exceptional compatibility with TIG, laser, and electron-beam welding – minimal post-weld cracking risk.
  • Forming: Cold-workable into tubes, sheets, and complex shapes; machinability comparable to Grade 5.
  • Heat Treatment: Stress-relieved at 480–650°C to optimize mechanical properties.

Application Advantages:

  • Aerospace: Hydraulic tubing, ducting – weight reduction without sacrificing fatigue life.
  • Marine: Heat exchangers, desalination plants – seawater immunity extends service life.
  • Chemical: Reactors, piping systems – handles sour gas (H₂S) and strong acids.
  • Industrial: High-pressure cylinders, sports equipment (bike frames, golf shafts) – lightweight durability.
بیشتر بخوانید

داده‌ها

عنصر Composition Range (wt.%)
تیتانیوم Balance (>90%)
آل 2.50–3.50%
V 2.00–3.00%
آهن ≤0.25%
O ≤0.13%
C ≤0.08%
N ≤0.03%
H ≤0.015%
سایر ≤0.4% (single element)

Key Characteristics

  • نسبت قدرت به وزن: Higher than pure titanium (Grades 1–4) but lower than Ti-6Al-4V (Grade 5).
  • مقاومت در برابر خوردگی: Excellent in marine, chemical, and chloride environments.
  • سازگاری زیستی: Non-toxic and MRI-compatible, but less commonly used in implants than Grade 23.
  • Formability: Superior to Grade 5; suitable for complex forming, welding, and machining.

 کاربردهای معمول

  • هوافضا: Hydraulic tubing, aircraft fittings, fasteners.
  • Marine: Heat exchangers, seawater components, propeller shafts.
  • Medical: Surgical instruments, non-implantable devices.
  • Industrial: Chemical processing equipment, pressure vessels.

 

مالکیت Value (Imperial) Value (Metric)
تراکم 0.160 lb/in³ 4.43 g/cm³
نقطه ذوب 3,000–3,050°F 1,650–1,680°C
هدایت حرارتی 6.5 Btu/(hr·ft·°F) 11.2 W/(m·K)
Coefficient of Thermal Expansion 5.3 × 10⁻⁶/°F 9.5 × 10⁻⁶/K
مقاومت الکتریکی 120 µΩ·cm 120 nΩ·m

داکسون را انتخاب کنید تا به پروژه‌تان کمک کند اوج بگیرد.

همین حالا با داکسون تماس بگیرید

Advanced Production:Titanium seamless pipe

Titanium seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities. Hot rolled tube/hot extruded titanium seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm. Cold rolled titanium seamless tube: cold processed tubes are supplied after heat treatment, surface etching, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm.

همین حالا با داکسون تماس بگیرید

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

همین حالا با داکسون تماس بگیرید

گزارش‌های آزمون

Our Grade 9 titanium tubing comes with an extensive range of certification and testing documentation tailored to meet your specific project requirements. We supply detailed material traceability records, comprehensive chemical composition analysis, and mechanical property certifications that demonstrate the exceptional performance characteristics of our titanium products. Each tube shipment includes quality assurance documentation covering dimensional verification, surface inspection reports, and welding procedure specifications when applicable.

همین حالا با داکسون تماس بگیرید

Applications and standards

Titanium Grade 9 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
همین حالا با داکسون تماس بگیرید

کیفیت، تحویل، بازرسی

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 9 Titanium Welded Pipe and Grade 9 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • زمان تحویل ما دقیقاً مطابق قرارداد است.
  • از آژانس‌های ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
  • از نمونه‌های رایگان برای آزمایش مشتری پشتیبانی کنید.
  • حمایت از بازرسی کارخانه‌ای حضوری یا ویدیویی
همین حالا با داکسون تماس بگیرید

بسته‌بندی

داکسون آلیاژ بهترین کیفیت بسته‌بندی را تضمین می‌کند، زیرا بسته‌بندی نقش مهمی در حمل‌ونقل بین‌المللی دارد که کالاها از مسیرهای مختلف عبور می‌کنند تا به مقصد نهایی برسند؛ بنابراین ما توجه ویژه‌ای به بسته‌بندی داریم. ما کالاهای خود را بسته به محصول به روش‌های مختلف بسته‌بندی می‌کنیم. روش‌های بسته‌بندی محصولات ما عبارتند از:
• جعبه‌ها و صندوق‌ها
• سلفون منقبض‌شونده
• پالت‌های چوبی
• جعبه‌های چوبی

همین حالا با داکسون تماس بگیرید

پشتیبانی فنی

اگر به هرگونه پشتیبانی فنی اضافی نیاز دارید، متالورژیست مقیم ما و کارکنان آگاه ما با کمال میل آماده کمک‌رسانی هستند. علاوه بر این، داکسون دارای آزمایشگاه آزمون معتبر است—نخستین در صنعت موجودی چندفلزی و پلاستیکی. به نظر ما، این امر تعهد تزلزل‌ناپذیر ما به کیفیت و فلسفه ما به‌عنوان یک تأمین‌کننده تمام‌خدمت را نشان می‌دهد.

Daxun Grade 9 Titanium TUBE Let your brand improve rapidly

Grade 9 titanium tube form (4)

پروژه‌ها و محصولات داغ اخیر

Grade 9 Titanium pipe and tube
Grade 9 Titanium pipe and tube
Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
How does Grade 9 titanium compare to Grade 5 in terms of performance?

While Grade 5 titanium offers higher strength, Grade 9 provides better formability, weldability, and corrosion resistance. Grade 9 is often preferred for tubing applications due to its excellent balance of properties and easier fabrication characteristics.

What sizes of Grade 9 titanium tubes do you supply?

We offer Grade 9 titanium tubes in a wide range of outside diameters from 6mm to 120mm, with wall thicknesses from 0.5mm to 10mm. We can supply both seamless and welded tubes, with lengths up to 6 meters or as specified by customer requirements.

Can you provide custom specifications for Grade 9 titanium tubes?

Yes, we can produce Grade 9 titanium tubes to your specific requirements including custom dimensions, special tolerances, unique tempers, and specific surface finishes. Please provide your technical specifications, and our engineering team will work with you to meet your exact needs.

How do you ensure the quality of your Grade 9 titanium tubes?

All our Grade 9 titanium tubes undergo comprehensive quality control including dimensional checks, surface inspection, and mechanical testing. We provide complete material traceability and full documentation including chemical analysis, mechanical properties, and conformity certificates with every shipment.

کلاس‌های بالاتر تیتانیوم چه تفاوتی با کلاس‌های پایین‌تر دارند؟

در داکسون، ما طیف گسترده‌ای از گریدهای آلیاژ تیتانیوم از گرید ۱ تا گرید ۱۲ را ارائه می‌دهیم.

گریدهای ۱ تا ۴ تیتانیوم خالص هستند، در حالی که گریدهای بالاتر آلیاژ هستند.

کلاس‌های آلیاژ به‌خاطر نسبت بالای استحکام به وزن‌شان محبوب هستند.

رایج‌ترین گرید آلیاژ تیتانیومی که می‌یابیم، گرید ۵ است. اگرچه همچنان غنی از تیتانیوم است، این گرید یکی از قابل‌اعتمادترین‌هاست زیرا می‌تواند دماهای تا ۶۰۰ درجه فارنهایت را تحمل کند و در شرایط شدید دوام بیاورد.

در صنایعی مانند صنایع هوافضا و دریایی، به دلیل مقاومت در برابر سایش و خوردگی، گریدهای بالاتر ترجیح داده می‌شوند.

برعکس، گریدهای پایین‌تر عمدتاً به دلیل استحکام کمتر برای جوشکاری استفاده می‌شوند.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

آیا درجه تیتانیوم بر هزینه تأثیر دارد؟

اگرچه درجه تیتانیوم کمی هزینه را افزایش می‌دهد، اما هزینه کل عمدتاً به شکل و فرم تیتانیومی که نیاز دارید بستگی دارد.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

متأسفانه بدون اطلاع کافی از پروژه شما و کاربرد تیتانیوم، تعیین قیمت به‌صورت آنلاین دشوار است.

خوشبختانه تیم کارشناسان ما همیشه در خدمت شماست تا در زمینه نیازهای تیتانیومی‌تان به شما کمک و مشاوره دهد. با ارسال ایمیل به daxunalloy@gmail.com، ما قادر خواهیم بود با ارائه مشاوره و برآورد دقیق هزینه به شما پاسخ دهیم.

حتماً تا حد امکان اطلاعاتی دربارهٔ گرید، شکل و مقدار تیتانیومی که نیاز دارید ارائه دهید تا نیازهایتان بهتر درک شود.

از کجا می‌توانم دربارهٔ گریدهای تیتانیوم بیشتر بیاموزم؟

تیم DAXUN باتجربه، آگاه و خوش‌برخورد است. با سال‌ها تجربه در این صنعت، آن‌ها همه چیز را درباره تیتانیوم، از کاربردها و مزایا گرفته تا گریدهای مختلف آن، می‌دانند.

برای دریافت به‌روزرسانی‌های منظم درباره تیتانیوم، کاربردها و مصارف آن در صنایع مختلف، حتماً وبلاگ ما را بررسی کنید. کارشناسان ما راهنماهای ساده‌ای نوشته‌اند که همیشه می‌توانید هنگام پرسش به آن‌ها مراجعه کنید.

اگر همچنان با مشکل مواجه هستید، با ما تماس بگیرید؛ خوشحال می‌شویم به شما کمک کنیم.

با ارسال ایمیل به daxunalloy@gmail.com، پاسخ سریعی دریافت خواهید کرد. لطفاً در سؤال خود تا حد امکان جزئیات بیشتری درج کنید تا بتوانیم راه‌حل مناسبی پیشنهاد دهیم.

می‌توانم چند نمونه بگیرم؟

We can providetitanium tube for you to check the quality. Sample is free and you just pay the freight.

تا کنون به کدام کشورها صادرات داشته‌اید؟

ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشته‌ایم.

زمان تحویل شما چقدر است؟

سفارش‌های آزمایشی را می‌توان ظرف یک هفته تحویل داد. برای سفارش‌های معمولی تقریباً دو هفته زمان لازم است.

همین امروز استعلام خود را ارسال کنید
استعلام سریع