x
همین امروز استعلام خود را ارسال کنید
استعلام سریع

SS 416 stainless steel bars and round bars China supplier

شرکت داکسون به‌عنوان یکی از تأمین‌کنندگان و صادرکنندگان پیشرو فولاد ضدزنگ در چین، میله‌های فولاد ضدزنگ را عرضه می‌کند.میلگرد (میلگرد گرد) به سراسر جهان.
  • Grade: AISI 416-Y1Cr13
  • تولید: نورد گرم، کشش سرد، آهنگری
  • استانداردها: ASTM, ASME, GB, DIN, JIS, ISO
  • 416 stainless steel round bar is easy to process
  • It is magnetic in both annealed and hardened conditions
  • Different heating methods produce a variety of properties

The machinability of most free cutting steels, Stainless Steel 416 Bright Bar (SS 416 Bright Bar) can be enhanced by the addition of sulphur which results in the presence of manganese sulphides. Considering the national and international quality of raw materials, we also offer UNS S41600 Round Bar in customized sizes and thicknesses as per the specific needs of our valued clients at market leading prices.

416 Global leader in stainless rod and Round Bar fabrication services

Grade 416 stainless steel has the highest machinability of any stainless steel, accounting for nearly 85% of easily machinable carbon steels. For most other easily machinable steels, the addition of sulfur improves machinability by forming manganese sulfide inclusions; however, this sulfur addition reduces corrosion resistance, weldability, and formability to levels lower than those of the non-easy machinable equivalent steel, grade 410. Grade 416 stainless steel is sometimes used unhardened or hardened and severely tempered due to its inexpensive cost and simplicity of machining. Martensitic stainless steels are tailored for high hardness, with some compromises on other qualities. Fabrication procedures must accommodate poor weldability and, in most cases, allow for a final hardening and tempering heat treatment. Corrosion resistance is lower than that of normal austenitic grades, and its usable working temperature range is limited by loss of ductility at subzero temperatures and loss of strength at high temperatures owing to over-tempering.

شبکه مراکز خدمات ما محصولات میلگرد فولاد ضدزنگ را برای تأمین سریع و آماده میلگرد در ابعاد و آلیاژهای رایج موجود دارد. ما همچنین میله‌های فولادی ضدزنگ با ابعاد سفارشی تولید می‌کنیم و در صورت کمتر بودن مقادیر از حداقل‌های کارخانه، می‌توانیم برنامه‌های موجودی را برای تحویل سریع و به‌موقع تنظیم کنیم. شرکت Daxun Alloys میلگردهای گرد فولادی ضدزنگ با قطرهای بین ۱/۱۶ تا ۲۶ اینچ را موجود دارد. میلگردهای گرد تقریباً در همه گریدهای فولاد ضدزنگ موجود هستند، از جمله 302، 303، 304/L، 309/S، 310/S، 316/L، 317/L، 321، 321/H، 347، 347H، 410، 416، 420، 440C، 17-4PH، دوبلکس 2205 و آلیاژ 20. میلگردهای گرد استیل ضد زنگ حرارت‌دیده در گریدهای 17-4PH، تمپر H900 (به درخواست)، H1025، H1150، Double H1150 و H1150M عرضه می‌شوند. سایر تمپرهای حرارت‌دیده نیز بنا به درخواست قابل تولید هستند. ما استیل‌های ضد زنگ سری 400 زیر را موجود داریم: 410، 430 و 416. ما همچنین میلگردهای گرد استنلس استیل با کیفیت دقیق و یاتاقانی 303، 304 و 316/L را نیز عرضه می‌کنیم. بخش عمده‌ای از موجودی ما شامل گریدهای میلگرد ماشین‌کاری‌شده منحصربه‌فرد ما است: میلگردهای گرد استنلس استیل که بر اساس استانداردهای یکنواخت ذوب می‌شوند تا قابلیت ماشین‌کاری را افزایش داده و هزینه کل هر قطعه را کاهش دهند. ماشین‌آلات پردازش میلگرد استنلس استیل ما به شرکت داکسون آلیاژز (Daxun Alloys) این امکان را می‌دهد که بر اساس مشخصات دقیق مشتریان خود تولید کند.

بیشتر بخوانید

داده‌ها

ASTM A479 416 Round Bar Specification ASTM A479 / ASTM A479 /ASTM A182 / ASME SA479 / ASME SA479 / ASME SA182
ASTM A479 416 Round Bar Manufacturing Process Hot Rolled / Cold Rolled / Hot Forging / Rolling / Machining
ASTM A479 416 Round Bar Other Grades 202 / 304 / 304L / 304H / 309S / 310S / 316 / 316L / 316Ti / 317L / 321 / 321H / 347 / 347H / 904L etc.
UNS No. – UNS S30400, UNS S30403, UNS S31008, UNS S31620, UNS S31603, UNS S31603, UNS S31635, UNS S31703, UNS S32100, UNS S34700, UNS S34709, UNS S8904
DIN / EN No. – 1.4301, 1.4307, 1.4845, 1.4401, 1.4404, 1.4571, 1.4438, 1.4541, 1.4550, 1.4551, 1.4539
AFNOR: Z2 CN 18.10, Z 6 CND 17-11, Z 2 CND 17-12,Z3 CrNi 22.05 AZ
EURONORM: FeMi35Cr20Cu4Mo2, FeMi35Cr20Cu4Mo2, X1CrNiMo17 12 2, X3CrNiMo17 12 2, FeMi35Cr20Cu4Mo2, X2CrNiMoN 22.5.3
ASTM A479 416 Round Bar Dimension Round Bars : Outside Diameter in the range of 4mm to 500mm
Bright Bars : Outside Diameter in the range of 4mm to 200mm
Hex Bars : 18mm to 57mm (11/16″ to 2-3/4″)
Square Bars : 18mm to 57mm (11/16″ to 2-3/4″)
Flat Bars : 1/2″to 10″in thickness range of 2mm to 150mm, Custom Size Stainless Steel Flats available
ASTM A479 416 Round Bar Length 2 meters to 7.5 meters ( 8 feet to 24 feet), or Custom Length as per Requirement
ASTM A479 416 Round Bar Forms and Shape Round, Square, Hex (A/F), Rectangle, Billet, Ingot, HRAP, Bright, Shaft, Forging Etc.
ASTM A479 416 Round Bar Finish سیاه، براق صیقلی، تراش‌خورده‌ی زبر، پرداخت شماره ۴، پرداخت مات، پرداخت BA
ASTM A479 416 Round Bar Dimension Standard ASTM A 484 / ISO h11 / ISO K12 Tolerances F8 / h8, h9, h10, h11, h12, k12, k13, A-484, EN-10060, DIN-1013 etc.
ASTM A479 416 Round Bar Heat Treatment Condition A in which the bars are Annealed
Condition H in which the bars are Hardened and Tempered at a relative Temperature
Condition T in which the bars are Hardened and Tempered at a relatively High Temperature
Condition S in which the bars are Strain Hardened or relatively Light Cold Worked
Condition B in which the bars are Relatively severe Cold worked.
Solution Annealed, Aging and Double Aging
ASTM A479 416 Round Bar Surface Finish Centreless Ground & Belt Polished, up to Ra value = 0.2 um (12 RMS), and Grit Polished of up to 180 to 600
ASTM A479 416 Round Bar Chamfering Available in 30°, 45° & 60° through fully automatic, both-end chamfering machine
ASTM A479 416 Round Bar Other Testing NACE MR0175, IGC TEST, Intergranular Corrrosion Test as per ASTM A262 Practice E, Charpy Impact Test, Macro, Grain Size, Hardness, Magnetic Particle Inspection (MPI), 100% tested thru Digital Ultrasonic Flaw Detector, as per ASTM A-388, EN 10308 (class 1to4),API 6A/ISO 10423:2003-PSL3,SEP 1920:1984 ( class A,B,C), MIL STD 2154 etc.
ASTM A479 416 Round Bar Value Added Services Rolling, Drill, Punch, CNC Machining, Sand Blasting, Shot Blasting, Heat Treatment, Anti-rust Paint, Polishing
ASTM A479 416 Round Bar Packaging Loose / Carrate / Wooden Pallet / Wooden Box / Plastic Cloth Wraps
ASTM A479 416 Round Bar Shipment & Transportation از طریق جاده – کامیون/قطار بار جزئی، بار کامل، از طریق دریا – کشتی معمولی بارتکه‌تکه / FCL (بار کامل کانتینر) / LCL (بار کمتر از کانتینر) / کانتینر ۲۰ فوت / کانتینر ۴۰ فوت / کانتینر ۴۵ فوت / کانتینر مکعب بلند / کانتینر سقف باز، از طریق هوا – هواپیمای باری، هواپیمای مسافربری و باربری
ASTM A479 416 Round Bar Material Test Certificate Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS, Bureau of CHINA Standards BIS Approved ETC
ASTM A479 416 Round Bar Documentation Commercial Invoice which includes HS Code / Packing List including net weight and gross weight, number of boxes, Marks and Numbers / Certificate of Origin legalized/attested by Chamber of Commerce or Embassy / Fumigation Certificates / Raw Material Test Reports / Material Traceability Records / Quality Assurance Plan (QAP) / Heat Treatment Charts / Test Certificates certifying NACE MR0103, NACE MR0175 / Material Test Certificates (MTC) as per EN 10204 3.1 and EN 10204 3.2 / Guarantee Letter / NABL approved Laboratory Test Reports / Welding Procedure Specification/Procedure Qualification Record, WPS/PQR / Form A for the purposes of the Generalized System of Preferences (GSP)
Chemical Composition Limits
Weight% C P سی ام‌ان S کروم آهن Se
Alloy 416 Type 1 0.15 max 0.060 max 1 max 1.25 max 0.40 max 11.50-13.50 bal 0.18-0.35
Alloy 416 Type 2 0.15 max 0.060 max 1 max 2.50 max 0.40 max 11.50-13.50 bal –
مواد Tempering Temp °F (°C) 0.2 % Yield Strength (Mpa) Tensile Strength (Mpa) % Elongation in 2″ % Reduction of Area Hardness Brinell
SS 416 300 (149) 1034 1344 10 40 390
SS 416 500 (260) 979 1276 13 45 375
SS 416 700 (371) 1007 1310 13 48 390
SS 416 900 (482) 896 1158 14 50 341
SS 416 1000 (538) 793 1000 15 50 300
SS 416 1100 (593) 689 862 17 53 262
SS 416 1200 (650) 586 758 18 55 225
STANDARD WERKSTOFF NR. بدون سرویس جی‌آی‌اس بی‌اس آفنور انگلیسی
SS 416 1.4005 S41600 SUS 416 416S21 – X12CrS13

داکسون را انتخاب کنید و مشتریان خود را راضی کنید.

همین حالا با داکسون تماس بگیرید

Quick response-416 Stainless Steel Rod

We provide customers with timely and fast delivery of 416 stainless steel bar products. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to ports and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.

همین حالا با داکسون تماس بگیرید

مزایای داکسون

  • انواع: ما طیف گسترده‌ای از اندازه‌ها و درجه‌ها را ارائه می‌دهیم، از جمله سری ۳۰۰، ۴۰۰، ۶۰۰ و غیره.
  • انعطاف‌پذیری: چه به میله‌های نورد گرم یا کشش سرد نیاز داشته باشید، طول میله‌های فولاد ضدزنگ ما برای برآورده کردن نیازهای خاص پروژه شما طراحی شده‌اند.
  • Quality Standards: Our 416 Stainless Steel Rod meet strict ASTM, ISO9001, GB, NSF/ANSI standards to ensure reliability and performance.
  • سفارش‌های سفارشی: به دنبال اندازه‌های ویژه میله‌های فولاد ضدزنگ هستید؟ ما گزینه‌های متنوعی برای سفارشی‌سازی میله‌های فولاد ضدزنگ با قیمت‌های رقابتی و سفارش آنلاین آسان ارائه می‌دهیم.
همین حالا با داکسون تماس بگیرید

416 Stainless Steel Rod packaging

We pay attention to every process to ensure quality. The 416 round steel packaging we usually adopt is to pack the stainless steel round bars with environmentally friendly plastic bags and then put them into fumigation-free wooden boxes or wooden pallets. Customized packaging such as OEM can also be negotiated. We provide almost everything to meet your round bar packaging requirements. We attach great importance to packaging. The round bars are packed in wooden corrugated boxes, wrapped with plastic packaging and bubble film on the outside.

همین حالا با داکسون تماس بگیرید

کیفیت، تحویل، بازرسی

  • داکسون همچنین چندین آزمون تضمین کیفیت را انجام می‌دهد. این آزمون‌ها شامل آزمون صاف‌کاری، آزمون فرورفتگی و مقاومت، آزمون مکانیکی، آزمون سختی، شناسایی مثبت مواد، آزمون انبساط و غیره هستند. تمام این آزمون‌ها تضمین می‌کنند که ماده برای کاربرد مورد نظر مناسب است.
  • در طول فرآیند تولید، قطر، ضخامت و سطح محصول را اندازه‌گیری می‌کنیم. زمان تحویل استاندارد ما ۷ تا ۱۵ روز است؛ به جز برای برخی محصولات با اندازه‌های ویژه که زمان تحویل آن‌ها تا ۲۰ روز افزایش می‌یابد.
    زمان تحویل ما دقیقاً مطابق قرارداد است.
  • از آژانس‌های ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
  • از ارائه نمونه‌های رایگان به مشتریان برای آزمایش پشتیبانی کنید.
  • حمایت از بازرسی کارخانه‌ای حضوری یا ویدیویی
همین حالا با داکسون تماس بگیرید

پشتیبانی فنی

اگر به هرگونه پشتیبانی فنی اضافی نیاز دارید، متالورژیست مقیم ما و کارکنان آگاه ما با کمال میل آماده کمک‌رسانی هستند. علاوه بر این، داکسون دارای آزمایشگاه آزمون معتبر است—نخستین در صنعت موجودی چندفلزی و پلاستیکی. به نظر ما، این امر تعهد تزلزل‌ناپذیر ما به کیفیت و فلسفه ما به‌عنوان یک تأمین‌کننده تمام‌خدمت را نشان می‌دهد.

همین حالا با داکسون تماس بگیرید

416 Stainless Steel Rod Ordering Information

Purchase orders for 416 round bars shall include quantity, PSL grade, type or category, API5L reference, diameter, surface finish, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish, or end treatment. Bars are solution bright annealed.

SS 416 Stainless Steel Rod Features

مقاومت بالا
مقاومت در برابر خوردگی
مقاومت در برابر حرارت
مقاومت در برابر دمای پایین
حفاظت از محیط زیست
عملکرد جوشکاری

داکسون آلیاژ به برند شما کمک می‌کند تا به‌سرعت پیشرفت کند.

انتخاب ایالت تحویل وضعیت سطح
کوبیده شده سیاه
صیقلی‌شده
نورد گرم سیاه
صیقلی‌شده
درخشان
شور شده
کشش سرد صیقلی‌شده
درخشان
توجه:
۱. در صورتی که به وضعیت تحویل متفاوتی از موارد فوق نیاز دارید، لطفاً با ما هماهنگ فرمایید.
۲. در صورت هرگونه پرسش یا سفارش، لطفاً ما را از هرگونه نیاز اضافی که در اینجا ذکر نشده است، مطلع سازید.
مواد در حالت آنیل‌شده در محلول ممکن است به روش زیر با افزایش سن سخت‌تر شوند: * نشان‌دهندهٔ افزایش سن دوگانه است.
وضعیت H900 (H480) H925 (H495) H1025 (H550) H1075 (H580) H1100 (H595) H1150 (H620) H1150M (H620M)* بیشتر H1150D (H620D)* بیشتر
تا حرارت دهید ±۱۵ درجه فارنهایت ۹۰۰ درجه فارنهایت ۹۲۵ درجه فارنهایت ۱۰۲۵ درجه فارنهایت ۱۰۷۵ درجه فارنهایت ۱۱۰۰ درجه فارنهایت ۱۱۵۰ درجه فارنهایت ۱۴۰۰ درجه فارنهایت ۱۱۵۰ درجه فارنهایت ۱۱۵۰ درجه فارنهایت ۱۱۵۰ درجه فارنهایت
±۹ درجه سانتی‌گراد ۴۸۰ درجه سانتی‌گراد ۴۹۵ درجه سانتی‌گراد ۵۵۰ درجه سانتی‌گراد ۵۸۰ درجه سانتی‌گراد ۵۹۵ درجه سانتی‌گراد ۶۲۰ درجه سانتی‌گراد ۷۶۰ درجه سانتی‌گراد ۶۲۰ درجه سانتی‌گراد ۶۲۰ درجه سانتی‌گراد ۶۲۰ درجه سانتی‌گراد
برای ساعت‌ها نگه دارید 1 4 4 4 4 4 2 4 4 4
خنک تا زیر هوا هوا هوا هوا هوا هوا هوا هوا هوا هوا
۹۰ درجه فارنهایت (۳۲ درجه سانتی‌گراد)

Types of SS 416 Stainless Steel Rods (6)

اطلاعات موجود برای مرجع و دانلود

Stainless Steel Rod Production

داکسون یک تولیدکننده قابل اعتماد میله‌ها و شمش‌های فولاد ضد زنگ است.

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless rod  are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 416 Stainless Steel Rod have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

پروژه‌ها و محصولات داغ اخیر

میله‌ی فولاد ضدزنگ
میله‌ی فولاد ضدزنگ با قطر بزرگ
میله‌ی صیقلی فولاد ضدزنگ
میله‌ی فولاد ضدزنگ
میله‌ی فولاد ضدزنگ
میله‌ی دقیق از فولاد ضدزنگ
میله‌ی فولاد ضدزنگ
می‌توانم چند نمونه بگیرم؟

We can provide 416 Stainless Steel Rod samples for you to check the quality. Sample is free and you just pay the freight.

تا کنون به کدام کشورها صادرات داشته‌اید؟

ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشته‌ایم.

حداقل مقدار سفارش شما چیست؟

Our MOQ is 1 ton for 416 Stainless Steel Rod.

زمان تحویل شما چقدر است؟

سفارش‌های آزمایشی را می‌توان ظرف یک هفته تحویل داد. برای سفارش‌های معمولی تقریباً دو هفته زمان لازم است.

همین امروز استعلام خود را ارسال کنید
استعلام سریع