x
Senden Sie Ihre Anfrage noch heute
Schnelles Angebot

SS 416 stainless steel bars and round bars China supplier

As a leading stainless steel supplier and exporter in China, Daxun supplies stainless steel barsRod (Round Bar)to all over the world.
  • Grade: AISI 416-Y1Cr13
  • Manufacturing: hot rolled, cold drawn, forged
  • Standards: ASTM, ASME, GB, DIN, JIS, ISO
  • 416 stainless steel round bar is easy to process
  • It is magnetic in both annealed and hardened conditions
  • Different heating methods produce a variety of properties

The machinability of most free cutting steels, Stainless Steel 416 Bright Bar (SS 416 Bright Bar) can be enhanced by the addition of sulphur which results in the presence of manganese sulphides. Considering the national and international quality of raw materials, we also offer UNS S41600 Round Bar in customized sizes and thicknesses as per the specific needs of our valued clients at market leading prices.

416 Global leader in stainless rod and Round Bar fabrication services

Grade 416 stainless steel has the highest machinability of any stainless steel, accounting for nearly 85% of easily machinable carbon steels. For most other easily machinable steels, the addition of sulfur improves machinability by forming manganese sulfide inclusions; however, this sulfur addition reduces corrosion resistance, weldability, and formability to levels lower than those of the non-easy machinable equivalent steel, grade 410. Grade 416 stainless steel is sometimes used unhardened or hardened and severely tempered due to its inexpensive cost and simplicity of machining. Martensitic stainless steels are tailored for high hardness, with some compromises on other qualities. Fabrication procedures must accommodate poor weldability and, in most cases, allow for a final hardening and tempering heat treatment. Corrosion resistance is lower than that of normal austenitic grades, and its usable working temperature range is limited by loss of ductility at subzero temperatures and loss of strength at high temperatures owing to over-tempering.

Our network of service centers stock stainless steel bar products for fast, ready supply of bar in common sizes and alloys.We also produce custom-sized stainless steel rods and can arrange inventory schedules for quick turnaround in a timely manner if quantities are below factory minimums.Daxun Alloys stocks stainless steel round bars with diameters ranging from 1/16″ to 26″. Round bars are available in nearly every grade of stainless steel, including 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205, and Alloy 20. Heat treated stainless steel round bars are offered in 17-4PH, H900 temper (on request), H1025, H1150, Double H1150, and H1150M. Other heat-treated tempers can be manufactured upon request. We stock the following 400 series stainless steels: 410, 430, and 416. We also carry 303, 304, and 316/L precision and bearing quality stainless steel round bars. The majority of our inventory consists of our unique machined bar grades: stainless steel round bars that are melted to consistent standards to increase machinability and lower total cost per component. Our stainless steel bar processing machinery allows Daxun Alloys to produce to our customers’ exact specifications.

Weiterlesen

Data

ASTM A479 416 Round Bar Specification ASTM A479 / ASTM A479 /ASTM A182 / ASME SA479 / ASME SA479 / ASME SA182
ASTM A479 416 Round Bar Manufacturing Process Hot Rolled / Cold Rolled / Hot Forging / Rolling / Machining
ASTM A479 416 Round Bar Other Grades 202 / 304 / 304L / 304H / 309S / 310S / 316 / 316L / 316Ti / 317L / 321 / 321H / 347 / 347H / 904L etc.
UNS No. – UNS S30400, UNS S30403, UNS S31008, UNS S31620, UNS S31603, UNS S31603, UNS S31635, UNS S31703, UNS S32100, UNS S34700, UNS S34709, UNS S8904
DIN / EN No. – 1.4301, 1.4307, 1.4845, 1.4401, 1.4404, 1.4571, 1.4438, 1.4541, 1.4550, 1.4551, 1.4539
AFNOR: Z2 CN 18.10, Z 6 CND 17-11, Z 2 CND 17-12,Z3 CrNi 22.05 AZ
EURONORM: FeMi35Cr20Cu4Mo2, FeMi35Cr20Cu4Mo2, X1CrNiMo17 12 2, X3CrNiMo17 12 2, FeMi35Cr20Cu4Mo2, X2CrNiMoN 22.5.3
ASTM A479 416 Round Bar Dimension Round Bars : Outside Diameter in the range of 4mm to 500mm
Bright Bars : Outside Diameter in the range of 4mm to 200mm
Hex Bars : 18mm to 57mm (11/16″ to 2-3/4″)
Square Bars : 18mm to 57mm (11/16″ to 2-3/4″)
Flat Bars : 1/2″to 10″in thickness range of 2mm to 150mm, Custom Size Stainless Steel Flats available
ASTM A479 416 Round Bar Length 2 meters to 7.5 meters ( 8 feet to 24 feet), or Custom Length as per Requirement
ASTM A479 416 Round Bar Forms and Shape Round, Square, Hex (A/F), Rectangle, Billet, Ingot, HRAP, Bright, Shaft, Forging Etc.
ASTM A479 416 Round Bar Finish Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish
ASTM A479 416 Round Bar Dimension Standard ASTM A 484 / ISO h11 / ISO K12 Tolerances F8 / h8, h9, h10, h11, h12, k12, k13, A-484, EN-10060, DIN-1013 etc.
ASTM A479 416 Round Bar Heat Treatment Condition A in which the bars are Annealed
Condition H in which the bars are Hardened and Tempered at a relative Temperature
Condition T in which the bars are Hardened and Tempered at a relatively High Temperature
Condition S in which the bars are Strain Hardened or relatively Light Cold Worked
Condition B in which the bars are Relatively severe Cold worked.
Solution Annealed, Aging and Double Aging
ASTM A479 416 Round Bar Surface Finish Centreless Ground & Belt Polished, up to Ra value = 0.2 um (12 RMS), and Grit Polished of up to 180 to 600
ASTM A479 416 Round Bar Chamfering Available in 30°, 45° & 60° through fully automatic, both-end chamfering machine
ASTM A479 416 Round Bar Other Testing NACE MR0175, IGC TEST, Intergranular Corrrosion Test as per ASTM A262 Practice E, Charpy Impact Test, Macro, Grain Size, Hardness, Magnetic Particle Inspection (MPI), 100% tested thru Digital Ultrasonic Flaw Detector, as per ASTM A-388, EN 10308 (class 1to4),API 6A/ISO 10423:2003-PSL3,SEP 1920:1984 ( class A,B,C), MIL STD 2154 etc.
ASTM A479 416 Round Bar Value Added Services Rolling, Drill, Punch, CNC Machining, Sand Blasting, Shot Blasting, Heat Treatment, Anti-rust Paint, Polishing
ASTM A479 416 Round Bar Packaging Loose / Carrate / Wooden Pallet / Wooden Box / Plastic Cloth Wraps
ASTM A479 416 Round Bar Shipment & Transportation By Road – Truck / Train Partial Load, Full Load, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes
ASTM A479 416 Round Bar Material Test Certificate Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS, Bureau of CHINA Standards BIS Approved ETC
ASTM A479 416 Round Bar Documentation Commercial Invoice which includes HS Code / Packing List including net weight and gross weight, number of boxes, Marks and Numbers / Certificate of Origin legalized/attested by Chamber of Commerce or Embassy / Fumigation Certificates / Raw Material Test Reports / Material Traceability Records / Quality Assurance Plan (QAP) / Heat Treatment Charts / Test Certificates certifying NACE MR0103, NACE MR0175 / Material Test Certificates (MTC) as per EN 10204 3.1 and EN 10204 3.2 / Guarantee Letter / NABL approved Laboratory Test Reports / Welding Procedure Specification/Procedure Qualification Record, WPS/PQR / Form A for the purposes of the Generalized System of Preferences (GSP)
Chemical Composition Limits
Weight% C P Si Mn S Cr Fe Se
Alloy 416 Type 1 0.15 max 0.060 max 1 max 1.25 max 0.40 max 11.50-13.50 bal 0.18-0.35
Alloy 416 Type 2 0.15 max 0.060 max 1 max 2.50 max 0.40 max 11.50-13.50 bal –
Material Tempering Temp °F (°C) 0.2 % Yield Strength (Mpa) Tensile Strength (Mpa) % Elongation in 2″ % Reduction of Area Hardness Brinell
SS 416 300 (149) 1034 1344 10 40 390
SS 416 500 (260) 979 1276 13 45 375
SS 416 700 (371) 1007 1310 13 48 390
SS 416 900 (482) 896 1158 14 50 341
SS 416 1000 (538) 793 1000 15 50 300
SS 416 1100 (593) 689 862 17 53 262
SS 416 1200 (650) 586 758 18 55 225
STANDARD WERKSTOFF NR. UNS JIS BS AFNOR EN
SS 416 1.4005 S41600 SUS 416 416S21 – X12CrS13

Choose Daxun and make your customers satisfied.

Contact Daxun now

Quick response-416 Stainless Steel Rod

We provide customers with timely and fast delivery of 416 stainless steel bar products. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to ports and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.

Contact Daxun now

Daxun Advantages

  • Varieties: We offer a wide range of sizes and grades, including 300 series, 400, 600 series, and more.
  • Flexibility: Whether you need hot-rolled or cold-drawn bars, our stainless steel bar lengths are designed to meet your specific project requirements.
  • Quality Standards: Our 416 Stainless Steel Rod meet strict ASTM, ISO9001, GB, NSF/ANSI standards to ensure reliability and performance.
  • Custom Orders: Looking for special sizes of stainless steel bars? We offer a variety of stainless steel bar customization options with competitive prices and convenient online ordering.
Contact Daxun now

416 Stainless Steel Rod packaging

We pay attention to every process to ensure quality. The 416 round steel packaging we usually adopt is to pack the stainless steel round bars with environmentally friendly plastic bags and then put them into fumigation-free wooden boxes or wooden pallets. Customized packaging such as OEM can also be negotiated. We provide almost everything to meet your round bar packaging requirements. We attach great importance to packaging. The round bars are packed in wooden corrugated boxes, wrapped with plastic packaging and bubble film on the outside.

Contact Daxun now

Quality, delivery, inspection

  • Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    Our delivery time is strictly in accordance with the contract.
  • Support customer third-party agencies to go to the factory for inspection
  • Support free samples to customers for testing
  • Support on-site or video factory inspection
Contact Daxun now

Technical Support

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Contact Daxun now

416 Stainless Steel Rod Ordering Information

Purchase orders for 416 round bars shall include quantity, PSL grade, type or category, API5L reference, diameter, surface finish, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish, or end treatment. Bars are solution bright annealed.

SS 416 Stainless Steel Rod Features

High strength
Corrosion resistance
Heat resistance
Low temperature resistance
Environmental protection
Welding performance

Daxun Alloy Let your brand improve rapidly

Delivery State Choice Surface Condition
Forged Black
Poliert
Hot Rolled Black
Poliert
Bright
Pickled
Cold Drawn Poliert
Bright
Note:
1. If you require different deliver state than the above listed, kindly confirm with us.
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here.
Material in the solution annealed condition may be age hardened as follows:-*Denotes Double Overaged
Condition H900 (H480) H925 (H495) H1025 (H550) H1075 (H580) H1100 (H595) H1150 (H620) H1150M (H620M)* Plus H1150D (H620D)* Plus
Heat to ±15oF 900oF 925 oF 1025oF 1075oF 1100oF 1150oF 1400oF 1150oF 1150oF 1150oF
±9oC 480oC 495oC 550oC 580oC 595oC 620oC 760oC 620oC 620oC 620oC
Hold for Hours 1 4 4 4 4 4 2 4 4 4
Cool to Below Air Air Air Air Air Air Air Air Air Air
90oF (32oC)

Types of SS 416 Stainless Steel Rods (6)

Information available for reference and download

Stainless Steel Rod Production

Daxun is a trustworthy stainless steel rod and bar manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless rod  are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 416 Stainless Steel Rod have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

Recent hot case projects and products

Edelstahlstange
large diameter stainless steel rod
SS 416 stainless steel rod
Stainless Steel Polished rod
Edelstahlstange
Stainless steel rod
SS 416 stainless rod
Stainless steel precision rod
Stainless steel rod
Kann ich ein paar Muster bekommen?

We can provide 416 Stainless Steel Rod samples for you to check the quality. Sample is free and you just pay the freight.

Which countries have you already exported?

We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.

What is your MOQ?

Our MOQ is 1 ton for 416 Stainless Steel Rod.

How long is your delivery time?

Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.

Senden Sie Ihre Anfrage noch heute
Schnelles Angebot