Ti 15333 Ti-15V-3O-3Sn-3Al) Titanium Alloy Plate Manufacturer - Daxun Alloy
As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.
- Plate Grade:Ti15333 / UNS R58153
- Plate Production type:cold rolling, hot rolling, forging.
- Features:High strength, Lightweight, High-temperature resistance
- Surface:bright, polished, pickled, sandblasted, etc.
- Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request
————Daxun produces titanium sheets in China to meet the diverse and ——demanding needs of customers!
Providing High-quality Ti 15333 Titanium Plates to Serve Customers Worldwide
TI15333 plate is a high-performance α-β phase titanium alloy plate developed for mission-critical industrial scenarios, characterized by its precisely controlled chemical composition and superior comprehensive mechanical properties. he material exhibits excellent corrosion resistance, with a corrosion rate of less than 0.1 mm/year in 3.5% NaCl solution and stable performance under continuous operating temperatures up to 350°C, effectively resisting pitting, crevice corrosion, and stress corrosion cracking in harsh environments. It strictly complies with ASTM B265 and AMS 4911 standards, ensuring consistent dimensional tolerance (±0.05 mm for thickness ≥5 mm) and metallurgical uniformity, while its low oxygen content (<0.18%) enhances weldability and fatigue resistance, supporting reliable fabrication of complex structural components.
Where is Ti15333 titanium plate used?
TI15333 Plate is widely adopted in industries with stringent material performance requirements. In the aerospace sector, it is a key material for airframe structural parts such as wing spars and fuselage frames, as well as aero-engine static components, where its high strength-to-weight ratio contributes to aircraft fuel efficiency, and its thermal stability withstands cyclic temperature fluctuations during takeoff and landing. In the oil and gas industry, it is used for subsea wellhead housings, riser connectors, and offshore platform load-bearing structures, capable of resisting corrosion from H₂S-containing sour service environments and seawater without relying on heavy protective coatings. Within the medical device field, it is processed into orthopedic implant components like hip stems and spinal fixation plates, meeting ISO 10993-5 biocompatibility standards to ensure minimal tissue reaction and good osseointegration. Additionally, it finds application in high-end chemical processing equipment (such as reactor vessels and heat exchanger tubes) and marine propulsion systems, where its corrosion resistance and mechanical stability support long-term, low-maintenance operation.
Compared to other titanium grades
Compared to pure titanium (such as Grade 2), Ti-15333 is significantly stronger. Pure titanium’s strengths lie in corrosion resistance and ease of formability, but its strength is average. Ti-15333 is designed for high strength and is suitable for aircraft structural components or high-performance springs.
Compared to the most commonly used titanium alloy grade, Ti-6Al-4V (Grade 5), Ti-15333’s strength lies in its improved cold working properties, meaning it can be easily shaped at room temperature, such as by bending or stamping. While Ti-6Al-4V offers excellent overall properties, cold working is much more difficult.
Finally, compared to another high-strength alloy, Beta C, both are beta alloys, but their focus is different. Beta C offers extreme corrosion resistance, making it particularly suitable for use in chemical environments. Ti-15333, on the other hand, focuses on a balance between high strength and good formability.
Data
- Parameter
- Physical Properties
- Mechanical Properties
| Element | Content (%) |
| Titanium(Ti) | 75 |
| Vanadium(V) | 15 |
| Chromium(Cr) | 3 |
| Aluminum(Al) | 3 |
| Tin(Sn) | 3 |
| Iron(Fe) | ≤ 0.25 |
| Oxygen(O) | ≤ 0.13 |
| Carbon(C) | ≤ 0.05 |
| Nitrogen(N) | ≤ 0.05 |
| Hydrogen(H) | ≤ 0.015 |
| Eigentum | Wert |
|---|---|
| Density (g/cm³) | 4.8 |
| Melting Point (°C) | 1600-1650 |
| Wärmeleitfähigkeit (W/m-K) | 6.7-8.0 |
| Specific Heat (J/kg·K) | 510 |
| Electrical Resistivity (μΩ·m) | 1.30 |
| Coefficient of Thermal Expansion (10^-6/K) | 8.6-9.4 |
| Eigentum | Wert |
|---|---|
| Zugfestigkeit (MPa) | 1100-1200 |
| Yield Strength (MPa) | 950-1050 |
| Dehnung (%) | 10-15 |
| Reduction of Area (%) | 25-35 |
| Hardness (HB) | 350-400 |
| Fatigue Strength (MPa) | 550-650 |
| Shear Strength (MPa) | 670-770 |
| Impact Toughness (J) | 40-60 |
Choose Daxun to help your project take off.

Fast delivery
Daxun provides customers with timely and fast delivery of ti15333 titanium plate products. Behind the speed is the system support from professional production capacity, and information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected.
Custom Cutting
Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:
- Water jet cutting
- Laser cutting
- Plasma cutting
- Wire cutting
- Bending
- Slitting
- Sawing


Verpackung
We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
• Boxes and crates
• Shrinkwrap
• Wooden pallets
• Wooden boxes
Technical Support
If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.

Daxun Ti15333 Titanium sheet Let your brand improve rapidly
- Other Titanium Plate Grades
| Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of Plate, Bar and Tube. | |
| Products/Processing Standard | Grade/Size |
| Titanium Plate, Sheet, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136 | GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Thickness:( 0.0197”-6”)Max Width: 12 feet,Max Length: 50 feet) |
| AMS-T-9046 | |
| Titanium and Titanium alloy sheet, plate | |
| Commercially pure titanium (CP) | |
| Code designation | Yield strength |
| minimum, ksi 1 / | |
| CP-1 Gr1 | 70 |
| CP-2 Gr2 | 55 |
| CP-3 Gr3 | 40 |
| CP-4 Gr4 | 25 |
| Alpha titanium alloys(A) | |
| Code designation | Zusammensetzung |
| A-1 | 5A1-2.5Sn |
| A-2 | 5A1-2.5Sn(ELI) 2 / |
| A-3 | 6A1-2Cb-1Ta-0.8Mo |
| A-4 | 8A1-1Mo-1V |
| Alpha-beta titanium alloys(AB) | |
| Code designation | Zusammensetzung |
| AB-1 Gr5 | 6A1-4V |
| AB-2 Gr5 | 6A1-4V(ELI) |
| AB-3 | 6A1-6V-2Sn |
| AB-4 | 6A1-2Sn-4Zr-2Mo |
| AB-5 | 3A1-2.5V |
| AB-6 | 8Mn |
| Beta titanium alloys(B) | |
| Code designation | Zusammensetzung |
| B-1 | 13V-11Cr-3A1 |
| B-2 | 11.5Mo-6Zr-4.5Sn |
| B-3 | 3A1-8V-6Cr-4Mo-4Zr |
| B-4 | 8Mo-8V-2Fe-3A1 |
| Processing: | |
| Warmwalzen | Kaltwalzen |
| Available Grades: | |
| CP Grade 1 | Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2) |
| CP Grade 2 | Grade 6Al-4V ELI (Formerly Grade 23) |
| Grade 7 | Grade 6Al-6V-2Sn (6-62) |
| Grade 19 | Grade 8Al-1Mo-1V (8-1-1) |
| Grade 5 (6Al-4V) | Grade 9 (3Al-2.5V) |
| Grade 6 (5Al-2.5Sn) | CP Grade 3 |
| Anwendung | |
| Chemische Industrie | Desalination Of Sea Water |
| Petrochemical Industry | Luft- und Raumfahrt |
| Machining Field, Automobile Field | Mobile Phone Component Field. |
Recent hot case projects and products






Verwandte Produkte (7)
Ti15333, also known by its UNS number R51853 or its commercial name TB5, is a metastable beta titanium alloy. Its nominal composition is Ti-15V-3Cr-3Sn-3Al. It is specifically designed for excellent cold formability, making it distinct from the more common alpha-beta alloys like Ti-6Al-4V.
Ti15333 is prized for its unique combination of properties:
- Exceptional Cold Formability: It can be cold formed by up to 70-90% in the solution-treated condition, allowing for the creation of complex shapes that are difficult or impossible with other titanium alloys.
- High Strength: After a simple aging heat treatment, it can achieve high tensile strength, typically over 1080 MPa (156 ksi).
- Low Elastic Modulus: It has a lower modulus (~80 GPa) compared to other titanium alloys, giving it high elasticity and excellent spring-back. This makes it ideal for flexible components and springs.
- Good Weldability: It can be readily welded in the solution-treated condition.
- Corrosion Resistance: Like most titanium alloys, it offers outstanding resistance to corrosion in many environments.
Ti15333 is typically processed in two stages:
- Solution Treatment (Annealing): The material is heated to approximately 790-815°C (1450-1500°F), held for a short time, and then rapidly cooled (air or water quench). This puts the alloy into a soft, ductile condition, optimal for cold forming.
- Aging (Precipitation Hardening): After forming, the part is aged at a lower temperature, typically between 480-595°C (900-1100°F), for 2-24 hours. This process precipitates fine alpha particles within the beta matrix, significantly increasing the material’s strength.
Absolutely. We provide customization for thickness (2mm-100mm), length/width (up to 3000mm×1500mm), and cut-to-size services based on CAD drawings. For complex shapes (e.g., curved plates for aerospace components), we support cold forming or hot forming with post-processing to maintain mechanical properties.
Yes. Its alloy composition enables excellent resistance to sour service corrosion (H₂S-containing environments). Testing shows a corrosion rate of <0.1 mm/year in 3.5% NaCl solution (simulating seawater) and no stress corrosion cracking in H₂S partial pressures up to 0.1 MPa, meeting NACE MR0175 standards for oilfield materials.
Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email (Daxunalloy@gmail.com) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week
We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.
We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.
Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.