17-4PH/630 stainless steel bars and round bars
As a leading stainless steel supplier and exporter in China, Daxun supplies stainless steel barsRod (Round Bar)to all over the world.
- Grade: AISI 17-4PH-SUS630
- Manufacturing: hot rolling, cold drawing, forging
- Standard: ASTM, ASME, GB, DIN, JIS, ISO
- High strength
- High hardness
- Wear resistance
- Heat treatable
Global leader in stainless rod and Round Bar fabrication services
Daxun is a global manufacturer of SS 17-4PH/630 Round Bar/Rod range. We are a supplier, exporter and reputable distributor of high quality bars and rods.
We offer our customers bars and rods in various parameters including surface treatment, end finish, dimensions, shapes and sizes.
SS 17-4PH is a martensitic stainless steel that is hardened by precipitation. However, the alloy includes alloying elements such as nickel, copper and chromium. The alloy is widely used in the aerospace sector for fasteners and other structural components. UNS S17400 has a microstructure obtained from the alloy during the remelting process. The improved structure in the alloy improves its toughness.
Stainless steel 17-4 PH Round Bar is a popular and adaptable material in the manufacturing and engineering industries due to its excellent corrosion resistance, high strength and ease of production. The “PH” in 17-4 PH refers to precipitation hardening, which is a heat treatment procedure that improves the mechanical properties of the material.
Our network of service centers stock stainless steel bar products for fast, ready supply of bar in common sizes and alloys.We also produce custom-sized stainless steel rods and can arrange inventory schedules for quick turnaround in a timely manner if quantities are below factory minimums.Daxun Alloys stocks stainless steel round bars with diameters ranging from 1/16″ to 26″. Round bars are available in nearly every grade of stainless steel, including 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205, and Alloy 20. Heat treated stainless steel round bars are offered in 17-4PH, H900 temper (on request), H1025, H1150, Double H1150, and H1150M. Other heat-treated tempers can be manufactured upon request. We stock the following 400 series stainless steels: 410, 430, and 416. We also carry 303, 304, and 316/L precision and bearing quality stainless steel round bars. The majority of our inventory consists of our unique machined bar grades: stainless steel round bars that are melted to consistent standards to increase machinability and lower total cost per component. Our stainless steel bar processing machinery allows Daxun Alloys to produce to our customers’ exact specifications.
Data
- Parameter
- Ingredients
- Mechanical Properties
- PHYSICAL PROPERTIES
- All equivalent
- Types
| Product Parameters: Stainless Steel rod | |
| Specifications | ASTM A276, ASME SA276 / ASTM A479 ASME SA479 |
| Dimensions | EN, DIN, JIS, ASTM, BS, ASME, AISI |
| SS 17-4PH Round Bars | Outside Diameter in the range of 4mm to 500mm |
| SS 17-4PH Round Bars | Outside Diameter in the range of 4mm to 100mm |
| SS 17-4PH Round Bars | 18mm – 57mm (11/16″ to 2-3/4″) |
| Finish | Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish |
| Length | 1 to 6 Meters, Custom Cut Lengths |
| Form | Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc. |
| Carbon | 0.07% (Max) |
| Silicon | 1.00% (Max) |
| Manganese | 1.00% (Max) |
| Phosphorous | 0.040% (Max) |
| Sulfur | 0.030% (Max) |
| Chromium | 15%-17.5% |
| Molybdenum | 0.50% (Max) |
| Nickel | 3%-5% |
| Copper | 3%-5% |
| Material Type | Condition | Ultimate Tensile Strength (PSI) | 0.2% Yield Strength (PSI) | Elongation (% In 2in.) | Reduction Of Area (%) | Hardness Brinell | Hardness Rockwell |
| 17-4 PH | H900 | 190,000 | 170,000 | 10 | 40 | 388 | C40 |
| H1025 | 155,000 | 145,000 | 12 | 45 | 331 | C35 | |
| H1075 | 145,000 | 125,000 | 13 | 45 | 311 | C32 | |
| H1150 | 135,000 | 105,000 | 16 | 50 | 277 | C28 | |
| H1150-M | 115,000 | 75,000 | 18 | 55 | 255 | C24 | |
| H1150-D | 125,000 | 105,000 | 16 | 50 | 255 min – 311 max | C24 – 33 |
| Heat Treated Condition | H900 |
| Density, lbs/in3 | 0.282 |
| Electrical Resistivity, microhm-cm | 77 |
| Specific Heat, BTU/lb/°F (32-212°F) | 0.1 |
| Thermal Conductivity, BTU/hr/ft2/in/°F | |
| 300°F | 124 |
| 500°F | 135 |
| 860°F | 156 |
| 900°F | 157 |
| Mean Coefficient of Thermal Expansion, in/in/°F | |
| -100 to 70°F | 5.8 x 10^-6 |
| 70 – 200°F | 6.0 x 10^-6 |
| 70 – 400°F | 6.0 x 10^-6 |
| 70 – 600°F | 6.3 x 10^-6 |
| 70 – 800°F | 6.5 x 10^-6 |
| 70 – 900°F | — |
| Modulus of Elasticity, ksi | 28.5 x 10^3 |
| Modulus of Rigidity, ksi | 11.2 x 10^3 |
| Poisson’s Ratio (all conditions) | 0.272 |
| Grade | UNS | Industry Specifications |
| 17-4 Duplex Stainless Steel | UNS 17-4PH | UNS: S17400 |
| • AMS: 5604 | ||
| • ASTM: A693 | ||
| • ASME: SA693 | ||
| • W. Nr./EN: 1.4548 | ||
| UNS 630 | UNS: S17400 | |
| • AMS: 5604 | ||
| • ASTM: A693 | ||
| • ASME: SA693 | ||
| • W. Nr./EN: 1.4548 |
| Stainless Steel 17-4PH/630 Bright Bar | SS 17-4PH/630 Bright Bar |
| 17-4PH/630 SS Bright Bar | |
| Stainless Steel 17-4PH/630 Bright Bar | |
| UNS S17-4PH/63000 SS Bright Bar | |
| WERKSTOFF NR. 1.4548 Bright Bar | |
| ASTM A276 17-4PH/630 Stainless Steel Bright Bar | |
| Stainless Steel 17-4PH/630 Hex Bar | SS 17-4PH/630 Hex Bar |
| 17-4PH/630 SS Hexagonal Bar | |
| 17-4PH/630 Stainless Steel Hex Bar | |
| UNS S17-4PH/63000 SS Hexagonal Bar | |
| ASTM A276 17-4PH/630 Stainless Steel Hex Bar | |
| Stainless Steel 17-4PH/630 Square Bar | SS 17-4PH/630 Square Bar |
| 17-4PH/630 SS Square Bars | |
| 17-4PH/630 Stainless Steel Square Bar | |
| UNS S17-4PH/63000 SS Square Bar | |
| WERKSTOFF NR. 1.4548 Square Bar | |
| ASTM A479 17-4PH/630 Stainless Steel Square Bars | |
| Stainless Steel 17-4PH/630 Rectangular Bar | SS 17-4PH/630 Rectangular Bar |
| 17-4PH/630 SS Rectangular Bars | |
| 17-4PH/630 Stainless Steel Rectangular Bar | |
| UNS S17-4PH/63000 SS Rectangular Bars | |
| WERKSTOFF NR. 1.4548 Rectangular Bar | |
| ASTM A276 17-4PH/630 Stainless Steel Rectangular Bar | |
| Stainless Steel 17-4PH/630 Flat Bars | SS 17-4PH/630 Flat Bar |
| 17-4PH/630 SS Flat Bars | |
| 17-4PH/630 Stainless Steel Flat Bars | |
| UNS S17-4PH/63000 SS Flat Bars | |
| WERKSTOFF NR. 1.4548 Flat Bars | |
| ASTM A276 17-4PH/630 Stainless Steel Flat Bars | |
| Stainless Steel 17-4PH/630 Polished Bar | SS 17-4PH/630 Polished Bar |
| 17-4PH/630 SS Polished Bars | |
| 17-4PH/630 Stainless Steel Polished Bar | |
| UNS S17-4PH/63000 SS Polished Bars | |
| WERKSTOFF NR. 1.4548 Polished Bar | |
| ASTM A476 17-4PH/630 Stainless Steel Polished Bar | |
| Stainless Steel 17-4PH/630 Threaded Bar | SS 17-4PH/630 Threaded Bar |
| 17-4PH/630 SS Threaded Bars | |
| 17-4PH/630 Stainless Steel Threaded Bar | |
| UNS S17-4PH/63000 SS Threaded Bar | |
| WERKSTOFF NR. 1.4548 Threaded Bar | |
| ASTM A276 17-4PH/630 Stainless Steel Threaded Bar |
Choose Daxun and make your customers satisfied.

Quick response-17-4 Stainless Steel Rod
Daxun provides customers with timely and fast delivery of 17-4 stainless steel bar products. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to ports and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Daxun Advantages
- Varieties: We offer a wide range of sizes and grades, including 300 series, 400, 600 series, and more.
- Flexibility: Whether you need hot-rolled or cold-drawn bars, our stainless steel bar lengths are designed to meet your specific project requirements.
- Quality Standards: 17-4 Stainless Steel Rod meet strict ASTM, ISO9001, GB, NSF/ANSI standards to ensure reliability and performance.
- Custom Orders: Looking for special sizes of stainless steel bars? We offer a variety of stainless steel bar customization options with competitive prices and convenient online ordering.
17-4 Stainless Steel Rod packaging
We pay attention to every process to ensure quality, the 17-4 round steel packaging we usually adopt is to pack the stainless steel round bars with environmentally friendly plastic bags, and then put them into fumigation-free wooden boxes or wooden pallets. Customized packaging, such as OEM, can also be negotiated. We provide almost everything to meet your round bar packaging requirements. We attach great importance to packaging. The round bars are packed in wooden corrugated boxes, and the outside is wrapped with plastic packaging and bubble film.
Quality, delivery, inspection
- Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
- During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
Our delivery time is strictly in accordance with the contract. - Support customer third-party agencies to go to the factory for inspection
- Support free samples to customers for testing
- Support on-site or video factory inspection
17-4PH/630 Stainless Steel Rod Features
Daxun Alloy Let your brand improve rapidly
- Gallery
- Delivery State
- Age Hardening
| Delivery State Choice | Surface Condition |
| Forged | Black |
| Polished | |
| Hot Rolled | Black |
| Polished | |
| Bright | |
| Pickled | |
| Cold Drawn | Polished |
| Bright | |
| Note: | |
| 1. If you require different deliver state than the above listed, kindly confirm with us. | |
| 2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here. | |
| Material in the solution annealed condition may be age hardened as follows:-*Denotes Double Overaged | ||||||||||||
| Condition | H900 (H480) | H925 (H495) | H1025 (H550) | H1075 (H580) | H1100 (H595) | H1150 (H620) | H1150M (H620M)* | Plus | H1150D (H620D)* | Plus | ||
| Heat to | ±15oF | 900oF | 925 oF | 1025oF | 1075oF | 1100oF | 1150oF | 1400oF | 1150oF | 1150oF | 1150oF | |
| ±9oC | 480oC | 495oC | 550oC | 580oC | 595oC | 620oC | 760oC | 620oC | 620oC | 620oC | ||
| Hold for Hours | 1 | 4 | 4 | 4 | 4 | 4 | 2 | 4 | 4 | 4 | ||
| Cool to Below | Air | Air | Air | Air | Air | Air | Air | Air | Air | Air | ||
| 90oF (32oC) | ||||||||||||
Types of 17-4PH/630 Stainless Steel Rods (6)
Information available for reference and download
Stainless Steel Rod Production
Daxun is a trustworthy stainless steel rod and bar manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless rod are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 17-4 Stainless Steel Rod have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
Recent hot case projects and products
Related Products (12)
We can provide 17-4 Stainless Steel Rod samples for you to check the quality. Sample is free and you just pay the freight.
We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.
Our MOQ is 1 ton for 17-4 Stainless Steel Rod.
Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.