Ti 15333 Ti-15V-3O-3Sn-3Al Alloy Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:Ti 15333 – UNS R58153
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Titanium tube density The density of Ti 15333 titanium is approximately 4.76 g/cm3
  • Standards:ASTM B337

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

Ti 15333 Titanium Alloy Pipe Manufacturer

Ti-15-3-3-3, also known by its alloy designation Ti-15333, is a high-strength, metastable beta titanium alloy. Its chemical composition is approximately 15% Vanadium, 3% Chromium, 3% Aluminum, and 3% Tin, with the remainder being titanium. This unique composition gives it a distinct set of properties that differentiate it from the more common alpha-beta alloys like Ti-6Al-4V.

The primary advantage of Ti-15-3-3-3 lies in its excellent cold formability. In its solution-treated (annealed) condition, it is quite ductile and can be readily formed into complex shapes, including tubing, sheets, and wires, at room temperature. This is a significant benefit for manufacturing, as it reduces the need for high-temperature forming processes.

After forming, Ti-15-3-3-3 can be precipitation hardened (aged) to achieve very high tensile strength, often exceeding 1200 MPa (175 ksi). This combination of formability and high strength makes it a preferred material for demanding aerospace applications.

Key Characteristics of Ti-15-3-3-3 Tubing:

  • High Strength-to-Weight Ratio: Like all titanium alloys, it offers exceptional strength for its weight, which is critical in aerospace and high-performance motorsports.
  • Excellent Cold Formability: It can be easily manipulated into tubular and other structural components in its annealed state.
  • Good Weldability: The alloy can be welded using standard techniques, though post-weld heat treatment is often required to restore optimal mechanical properties.
  • Superior Corrosion Resistance: It exhibits excellent resistance to corrosion in many environments, including seawater and various chemical atmospheres.

Common Applications for Ti-15-3-3-3 Tubing:

Due to its specific property profile, Ti-15-3-3-3 tubing is predominantly used in high-performance sectors:

  • Aerospace: Used for structural components, airframe parts, and high-strength fasteners.
  • Sporting Goods: High-end bicycle frames, golf club heads, and other performance equipment where strength and lightness are paramount.
  • Medical Devices: Occasionally used for surgical implants and instruments that benefit from its combination of strength, biocompatibility, and formability.

Data

Element Content (%)
Titanium(Ti) 75
Vanadium(V) 15
Chromium(Cr) 3
Aluminum(Al) 3
Tin(Sn) 3
Iron(Fe) ≤ 0.25
Oxygen(O) ≤ 0.13
Carbon(C) ≤ 0.05
Nitrogen(N) ≤ 0.05
Hydrogen(H) ≤ 0.015

 

Property Value
Density (g/cm³) 4.8
Melting Point (°C) 1600-1650
Thermal Conductivity (W/m·K) 6.7-8.0
Specific Heat (J/kg·K) 510
Electrical Resistivity (μΩ·m) 1.30
Coefficient of Thermal Expansion (10^-6/K) 8.6-9.4

 

Property Value
Tensile Strength (MPa) 1100-1200
Yield Strength (MPa) 950-1050
Elongation (%) 10-15
Reduction of Area (%) 25-35
Hardness (HB) 350-400
Fatigue Strength (MPa) 550-650
Shear Strength (MPa) 670-770
Impact Toughness (J) 40-60

Choose Daxun to help your project take off.

Contact Daxun now

Advanced Production:Titanium seamless pipe

  • Titanium seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities. Hot rolled tube/hot extruded titanium seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm. Cold rolled titanium seamless tube: cold processed tubes are supplied after heat treatment, surface etching, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm.
  • (The above is agreed upon by the manufacturer and the customer based on the specific situation)
Contact Daxun now

Ti 15333 Titanium Tube Features

Ti 15333 Titanium Tube is the softest form of titanium and has the highest ductility. It has good cold forming characteristics and offers excellent corrosion resistance. It also has excellent welding properties and high impact toughness.

  • Softest Titanium
  • Highest Ductility
  • Excellent Corrosion Resistance
  • Good Cold Formability
Contact Daxun now

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

Contact Daxun now

Test Reports

The test reports we provide include: Factory test certificate for Ti 15333 titanium welded pipe and Ti 15333 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)

Contact Daxun now

Applications and standards

Titanium 15333 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
Contact Daxun now

Quality, delivery, inspection

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Ti 15333 Titanium Welded Pipe and Ti 15333 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • Our delivery time is strictly in accordance with the contract.
  • Support customer third-party agencies to go to the factory for inspection
  • Support free samples for customer testing
  • Support on-site or video factory inspection
Contact Daxun now

Packaging

Daxun Alloy ensures the best quality of packaging as it plays an important role in international freight where goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
• Boxes and crates
• Shrink wrap
• Wooden pallets
• Wooden boxes

Contact Daxun now

Technical Support

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Daxun Ti 15333 Titanium TUBE Let your brand improve rapidly

Ti 15333 titanium tube form (4)

  • Titanium seamless tubes are made by piercing and drawing solid titanium bars, and the hollow part of the tube is made by piercing or hot extrusion. Titanium seamless tubes are ideal for very large diameter to wall thickness ratios and have very good external dimensional tolerances.

  • Titanium welded pipe is a tubular product made of strip titanium that is roll formed and fusion welded along the longitudinal seam. The welding process used by Daxun Alloy does not use any filler metal during the welding process.

  • Titanium square tubes are drawn from round tubes or round tube billets and can be formed into right angles or rounded corners. They can also be cold extruded, which is efficient and low cost. The only disadvantage is that the tolerance will gradually increase.

  • Tubular products are welded and then re-drawn to final size. Welding and drawing is ideal for producing thick walled, large diameter tubes that cannot be welded directly to size but still offer cost savings over seamless tubes. All Daxun welded and drawn tubes are bright annealed.

Recent hot case projects and products

Ti 15333 Titanium pipe and tube
Ti 15333 Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
What is Ti-15-3-3-3 titanium alloy, and how is it different from Ti-6Al-4V?

Ti-15-3-3-3 (or Ti-15333) is a beta-rich titanium alloy known for its exceptional cold formability. Unlike the more common Ti-6Al-4V (an alpha-beta alloy), Ti-15-3-3-3 can be easily formed into complex shapes, like tubing, at room temperature. After forming, it can be heat-treated to achieve very high strength, making it ideal for applications that require both intricate manufacturing and high performance.

Can Ti-15-3-3-3 tubing be welded?

Yes, Ti-15-3-3-3 has good weldability. However, to achieve the best mechanical properties in the welded joint, a post-weld heat treatment (solution treating and aging) is typically recommended. This process restores the high strength that the alloy is known for.

What sizes and specifications of Ti-15-3-3-3 tubing does Daxun Alloys Co., Ltd. offer?

At Daxun Alloys Co., Ltd., we supply Ti-15-3-3-3 tubing in a wide range of outer diameters, wall thicknesses, and lengths to meet your specific project requirements. We offer tubing in both the annealed (easily formable) and aged (high-strength) conditions. Please contact us with your detailed specifications for a custom quote.

Does the grade of titanium affect the cost?

While the grade of titanium does increase the cost slightly, the total cost is primarily determined by the shape and form of titanium you require.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

Unfortunately, it is difficult to come up with a price online without knowing much about your project and what the titanium will be used for.

Fortunately, our team of experts are always here to help and advise you on your titanium needs. By sending an email to daxunalloy@gmail.com, we will be able to get back to you with some advice and an accurate quote.

Make sure to include as much information as possible about the grade, shape and quantity of titanium you require to get a better understanding of your needs.

How to get a quote OR understand the market information ASAP?

Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email (Daxunalloy@gmail.com) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week

Can I get some samples?

We can provide titanium tube samples for you to check the quality. Sample is free and you just pay the freight.

Which countries have you already exported?

We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.

What is your MOQ?

Our MOQ is 1 ton for titanium tube.

How long is your delivery time?

Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.

Send Your Inquiry Today
Quick Quote