x
Send Your Inquiry Today
Quick Quote

Super Austenitic 904L Stainless Steel Plate Supplier

As China’s leading stainless steel plate supplier and exporter, Daxun provides 904L stainless steel plates to the world.
  • Grade: AISI 904L-N08904
  • Features: Super corrosion resistance
  • Manufacturing: Cold-rolled plate, hot-rolled plate, forged plate
  • Standards: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Type: Cold-rolled thin plate, hot-rolled thick plate
  • Surface: 2B, NO.1, NO.4, HL, BA, 8K, etc.
  • Length: 2438mm3048mm6000mm can be customized
  • Origin: TISCO, Baosteel, Posco, Tsingshan, Delong, ATI,

Overview of 904L Stainless Steel

Alloy 904L is a superaustenitic stainless steel designed for moderate to high corrosion resistance in various process environments. This high alloy austenitic product is intended for use under severely corrosive conditions, making it a reliable choice for demanding applications. The high chromium and nickel content, along with the additions of molybdenum and copper, provide excellent corrosion resistance. With a highly alloyed chemistry that includes 25% nickel and 4.5% molybdenum, Alloy 904L is well-suited for applications requiring both high corrosion resistance and high strength. This unique composition allows it to withstand environments involving dilute sulfuric acid, hot phosphoric acid, and other inorganic acids, ensuring long-lasting performance in harsh conditions.

Dimensions and Sizes

Alloy 904L stainless steel plate is available in various dimensions and sizes to meet specific application requirements. The available thicknesses for Alloy 904L range from 3/16” through 2”, providing flexibility for different industrial needs. UNS N08904 Sheet can range up to 8mm in thickness, while 904L Plate is usually thicker than 8mm and can range up to 75mm in thickness. These dimensions can be customized to meet specific industry standards and specifications, ensuring that the material fits perfectly into any project. Additionally, 904L stainless steel plate can be easily welded and processed using standard shop fabrication practices, streamlining the manufacturing process and ensuring high-quality results.

Read More

Technical Data

Stainless Steel 904L Plate, Sheet and Strip ASTM B 168/ASME SB 168, ASTM B 906/ASME SB 906, ASME Code Cases 1827 and N-253, SAE/AMS 5540, BS 3072NA14 and 3073NA14, DIN 17750, ISO 6208, EN 10095, MIL-DTL-23228.
Standard Stainless Steel 904L Plate & Sheet Sizes 1000 x 2000 mm, 1220 x 2440 mm, 1500 x 3000 mm, 2000 x 2000 mm, 2000 x 4000 mm
Cold rolled 904L Steel Plate 0.5-6.4 mm
Hot rolled 904L Steel Plate 3.0–10.0 mm
SS 904L Plate Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard Stainless Steel 904L Sheet suppliers
Availability of Stainless Steel 904L Foil sizes Thickness : 8-100 microns (0.00031-0.004 in)
Width: Up to 500 mm (19.5 in)
Weight (in rolls) : Up to 50 kg (110 lb); e.g. approxi- mately 1400 m at 8 microns and ap- proximately 112 m at 100 microns.
Profiling To provide a full profiling service in China we use numerous profiling methods including:
Laser Plate Cutting
Plasma Plate Cutting
Oxy-propane Flame Cutting
Tolerances of width and thickness EN 10258 (formerly DIN 59381)
EN 10151 Stainless Steel 904L strip for springs
EN 10088 Stainless Steel 904L strip (general)
Stainless Steel 904L Plates standards and approvals EN ISO 18286
EN 10051
EN 10088-1
ISO 15510
EN ISO 9445
ASTM A 480
ASTM A 959
ASME IID
Plasma profiles As per customer’s drawings
Value added services for Stainless Steel 904L Plate Laser cutting, Waterjet cutting, Plasma cutting, Bending and mechanical processing, edge preparation, welding, sawing and shearing.
Value added services for Stainless Steel 904L Coil Cut-to-length
Slitting
Polishing
Blanking
SS 904L Plate Origin China Origin, European Origin, Japanese Origin
Packing of 904L Steel Sheet Bundles with waterproof cloth outside or plywood box
Test UT, SGS testing, TUV etc
Element % Present (in product form)
Carbon (C) 0.02
Silicon (Si) 0.7
Manganese (Mn) 2
Phosphorous (P) 0.03
Sulfur (S) 0.01
Chromium (Cr) 19.00 – 21.00
Nickel (Ni) 24.00 – 26.00
Nitrogen (N) 0.15
Molybdenum (Mo) 4.00 – 5.00
Copper (Cu) 1.20 – 2.00
Iron (Fe) Balance
Product Form
C H P L L TW/TS
Thickness (mm) Max. 8 13.5 75 160 2502) 60
Yield Strength Rp0.2聽N/mm2 2403) 2203) 2203) 2304) 2305) 2306)
Rp1.0聽N/mm2 2703) 2603) 2603) 2603) 2603) 2503)
Tensile Strength Rm聽N/mm2 530 – 7303) 530 – 7303) 520 – 7203) 530 – 7304) 530 – 7305) 520 – 7206)
Elongation min. in % Jmin聽(Longitudinal) – 100 100 100 – 120
Jmin聽(Transverse) – 60 60 – 60 90
Density at 20°C kg/m3 8
Thermal Conductivity W/m K at 20°C 12
Modulus of Elasticity kN/mm2 at 20°C 195
200°C 182
400°C 166
500°C 158
Specific Thermal Capacity at 20°C J/kg K 450
Electrical Resistivity at 20°C Ω mm2/m 1
UNS S904L 1.4539 UNS N08904
ASTM A240 ASTM A240 ASTM A240
ASTM A480 ASTM A480 ASTM A480
ASME SA240 ASME SA240 ASME SA240
AMS 5521 AMS 5521 AMS 5521

Choose Daxun and make your customers satisfied.

Fast delivery

We provide timely and fast delivery of 904L stainless steel plate products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.

904L plate features

Type 904L is a high alloy austenitic stainless steel that is known for its corrosion properties.

  • Non-magnetic
  • Stronger corrosion properties than Type 316L an 317L
  • Good resistance to sulphuric, phosphoric and acetic acids
  • High resistance to crevice and stress corrosion cracking
  • Excellent formability and weldability

Stainless Steel 904L Applications

Application of using Type 904L stainless steel:

  • Cooling equipment for seawater
  • Chemical processing of sulphuric, phosphoric and acetic acids
  • Heat exchangers
  • Condenser tubes
  • Gas washing
  • Control and instrumentation
  • Oil and gas industry
  • Pharmaceutical production
  • Wiring in electrostatic precipitators

Quality, delivery, inspection

  • Daxun Alloy is committed to quality assurance. The company conducts various tests to ensure material suitability. These tests include flattening, pitting, and resistance tests. Mechanical, hardness, and expansion tests are also performed. Material positive identification is another key quality assurance measure. All these tests guarantee that the materials meet application requirements. Customers can trust Daxun Alloy for high-quality, suitable products.

  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    Our delivery time is strictly in accordance with the contract.
  • Support customer third-party agencies to go to the factory for inspection
  • Support free samples to customers for testing
  • Support on-site or video factory inspection

Technical Services

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Advanced machining

Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel uses the ERP system to achieve full traceability of the variety, specification, and origin of each stainless steel plate, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

904L plate stainless steel Features

High strength
Corrosion resistance
Heat resistance
Low temperature resistance
Environmental protection
Welding performance

Daxun Let your brand improve rapidly

Tolerance for 2B Sheet
Size Tolerance Rank
Group 1 Group 2 Group 3
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
Tolerance for No.1 Hot Rolled Plate
Size Tolerance Rank
Group 1 Group 2 Group 3
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
16 15.2~ 15.5 15.5~ 15.7 15.7~ 16.1
18 17.2~ 17.5 17.5~ 17.7 17.7~ 18.1
20 19.2~ 19.5 19.5~ 19.7 19.7~ 20.1
30 29.2~ 29.5 29.5~ 29.7 29.7-30.1
40 39.2~ 39.5 39.5~ 39.7 39.7~ 40.1
50 49.2~ 49.5 49.5~ 49.7 49.7~ 50.1
60 59.2~ 59.5 59.5~ 59.7 59.7~ 60.1
Delivery State Choice Surface Condition
Cold Rolled 2B
2D
BA
Hairline
No.3
No.4
6K
8K
Note:
1. If you require different deliver state than the above listed, kindly confirm with us.
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here.
Delivery State
Delivery State Choice Surface Condition
Hot Rolled No.1
No.3
No.4
6K
8K
Pickled
Note:
1. If you require different deliver state than the above listed, kindly confirm with us.
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here.
Grade Type Thickness Surface
Austenitic 304/304H/304L/304J1 0.25-150mm 2B/BA/NO.4/8K/SB/HL/NO.1
321 0.4-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
316/316L/317L/316Ti 0.3-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
Ferrite 430 0.4-3.0mm 2B/BA/NO.4/8K/SB/HL
Ultra Pure Ferrite 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B、2D
409L 0.4-2.5mm 2B、2D
Grade Type Thickness Original
Heat-resistant Steel 309S 0.5-40mm CHN
310S 0.5-40mm CHN
Duplex Steel 2101 1.5-50mm CHN
2304 3.0-50mm CHN
2205 0.5-60mm CHN
2507 1.0-60mm SWE / JPN / CHN
Super Austenitic Steel N08904 0.6-50mm SWE / JPN / CHN
S31254 0.5-50mm SWE / JPN / CHN
N08926 0.5-50mm SWE / JPN / CHN
N08367 0.5-50mm SWE / JPN / CHN
Nickel Base Alloy N08031 1.0-50mm US / JPN / GER
N08810/N08800 0.8-50mm US / JPN / CHN
N08028 1.0-20mm US / GER / JPN
N08020 1.0-20mm US / GER / JPN
N08825 0.8-40mm US / GER / SWE / JPN / CHN
N10276 0.5-50mm US / GER / JPN
N06022 1.0-50mm US / GER / JPN
N06625 0.8-20mm US / GER / CHN
N04400 1.0-20mm US / GER / JPN
N06600 1.0-50mm US / GER / JPN / CHN
N02201 0.5-20mm US / JPN
Titanium TA1/Gr1 0.5-50mm JPN / CHN
TA2/Gr2 0.5-50mm JPN / CHN
Welding Material ERNiCrMo-13 1.2、2.4mm GER
ERNiCrMo-3 2.4mm GER
ERNiCrMo-4 2.4mm US

The surface and shape of 904L stainless steel plate (7)

Daxun is a trustworthy stainless steel plate manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel plates are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the stainless steel plates have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

Recent hot case projects and products

904L plate stainless steel
904L plate stainless steel
904L plate stainless steel
904L plate stainless steel
904L plate stainless steel
904L plate stainless steel
Can I get some samples?

We can provide stainless steel sheet samples for you to check the quality. Sample is free and you just pay the freight.

Which countries have you already exported?

We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.

What is your MOQ?

Our MOQ is 1 ton for stainless steel sheet.

How long is your delivery time?

Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.

Send Your Inquiry Today
Quick Quote