x
Send Your Inquiry Today
Quick Quote

Daxun is an excellent manufacturer of grade 23 (Ti-6Al-4V ELI)titanium rods and bars.

As China’s leading supplier of titanium and titanium alloy rods, Daxun provides high-performance titanium rods to the world.
  • Titanium bar grade: Grade 23-Ti6Al 4V ELI- USN R56401
  • Titanium bar types: rolled bars, drawn bars, forged titanium bars
  • Titanium bar density The density of grade 23 titanium is 4.43 g/cm3
  • Main standards: ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
  • High strength, high temperature resistance, corrosion resistance, light
  • weight, excellent comprehensive performance.

————Daxun produces titanium rods in China to meet the diverse and ——demanding needs of customers!

The global leader in commercially pure titanium rod manufacturing services

Daxun, specializing in the production of alloy titanium rods for extreme environments—Grade 23 titanium alloy rods.

Grade 23 titanium bar, also known as Ti-6Al-4V ELI, is a high-performance alloy known for its excellent strength-to-weight ratio, corrosion resistance, and biocompatibility. It is widely used in aerospace, medical, and high-tech industries due to its ability to withstand extreme conditions while remaining lightweight. Compared to other titanium grades, Grade 23 offers enhanced ductility and fracture toughness, making it ideal for critical applications such as aircraft components, surgical implants, and advanced engineering parts.

Daxun is your trusted titanium alloy rod production company. Daxun produces all grades of titanium alloys, including commercially pure titanium series CP, titanium alloy series, titanium nickel alloy, etc. They have reliable performance and provide high performance for your critical applications. In various industries and applications, you can rely on Daxun titanium alloy rods for high strength, high temperature and corrosive environments. For decades, Daxun Metals has been committed to producing highly engineered titanium alloy solutions to meet the most severe challenges.

Read More

Data

Specification Details
Material Titanium rod and bar Grade 23 (UNS R56400)
Standard ASTM B348, ASTM SB348, AMS 4921, AMS 4902
Dimensions EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN
Diameter Range 0.125″ – 14″ (3.175mm – 355.6mm), custom
Length Range Up to 240″ (6096mm), custom
Finish Cold (bright) drawn, centerless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centerless Ground & Black
Surface Finish Cold drawn, Centerless Ground, Polished, Or Rough Turned, Black, NO.4 Finish, BA Finish, Matt Finish, etc.
Condition Hardened & tempered, annealed
Tolerance Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm)
Form Titanium square bars, titanium ingots, titanium round bars, rectangular titanium bars, triangular titanium bars, forged titanium bars, titanium hexagonal bars, etc.
Physical Properties Density: 0.163 lb/in³ (4.51 g/cm³), Melting Point: 3,020°F (1,660°C), Elongation: 20-30%, Modulus of Elasticity: 16.5 x 10⁶ psi (114 GPa)
Chemical Composition Titanium (min): 99.2%, Oxygen (max): 0.25%, Carbon (max): 0.08%, Iron (max): 0.30%, Nitrogen (max): 0.03%, Hydrogen (max): 0.015%

 

Element Minimum (%) Maximum (%)
Titanium (Ti) 99.2 –
Aluminum (Al) 5.5 6.75
Vanadium (V) 3.5 4.5
Oxygen (O) – 0.25
Carbon © – 0.08
Iron (Fe) – 0.30
Nitrogen (N) – 0.03
Hydrogen (H) – 0.015
Property Value
Tensile Strength 130,000–170,000 psi (900–1,170 MPa)
Yield Strength (0.2% Offset) 115,000–150,000 psi (800–1,035 MPa)
Elongation 20–30%
Hardness (Brinell) 300–360 HB
Modulus of Elasticity 16.5 × 10⁶ psi (114 GPa)
Property Value
Density 0.163 lb/in³ (4.51 g/cm³)
Melting Point 3,020°F (1,660°C)
Thermal Conductivity 13.4 W/m·K (at 25°C)
Coefficient of Thermal Expansion 8.6 µm/m·°C (20–100°C)
Electrical Resistivity 4.1 × 10⁻⁷ Ω·m

Choose Daxun to help your project take off.

Contact Daxun now

DAXUN® Grade 23 Titanium Rod Features

DAXUN® Ti Grade 5 is a titanium alloy bar (6al-4v) featuring:

  • Good hot formability and weldability;
  • Tensile strength can reach 1000MPa;
  • Dimensional work at high temperature
  • Insensitive to seawater or seawater;
  • Not affected by various corrosive media;
  • High strength and good toughness;
  • Resist crack initiation and crack propagation.
Contact Daxun now

Daxun Factory Advantages

Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

Contact Daxun now

Grade 23 Titanium Rod Production Method

Daxun produces high-quality titanium bars with high performance, and can also manufacture according to customer’s agreement:

  • Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.
Contact Daxun now

Grade 23 Rods Applications and Standards

Grade 23 Titanium Rods are widely used in the following industries under extreme corrosive conditions:

  • Aerospace, shipbuilding, oil and gas industry, marine engineering, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, military industry, pharmaceutical and food processing equipment, etc.
  • Specifications: AMS 4928,AMS 4967,AMS 4965 ,AMS 6931 ,ASTM B 348
  • Standards: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
Contact Daxun now

Quality, delivery, inspection

Daxun performs several quality assurance tests, these tests include mechanical tests like area tensile, chemical analysis, material positive identification – PMI test, micro and macro testing, intergranular corrosion (IGC) test, ultrasonic flaw detection test, pitting and resistance test, hardness test, material positive identification, expansion test etc. All these tests ensure that the Grade 2 Titanium Rod and Grade 2 Titanium Round Bar material is suitable for the required application. During the production process, we measure the diameter, thickness and surface of the product.

  • Our delivery time is strictly in accordance with the contract.
  • Support customer third-party agencies to go to the factory for inspection
  • Support free samples for customer testing
  • Support on-site or video factory inspection
Contact Daxun now

Packaging

Daxun Alloy ensures the best quality of packaging as it plays an important role in international freight where goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
• Boxes and crates
• Shrink wrap
• Wooden pallets
• Wooden boxes

Contact Daxun now

Technical Support

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Daxun Grade 23 Titanium Rods help your brand improve quickly

NOMINAL SIZE h5 h6 h7 h8 h9 H10 H11 h12
DIAMETER mm
~ to 3 +0.004/0 +0.006/0 +0.01/0 +0.014/0 +0.025/0 +0.04/0 +0.06/0 +0.1/0
over 3 to 6 +0.005/0 +0.008/0 +0.012/0 +0.018/0 +0.03/0 +0.048/0 +0.075/0 +0.12/0
over 6 to 10 +0.006/0 +0.009/0 +0.015/0 +0.022/0 +0.036/0 +0.058/0 +0.09/0 +0.15/0
over 10 to 18 +0.008/0 +0.011/0 +0.018/0 +0.027/0 +0.043/0 +0.07/0 +0.11/0 +0.18/0
over 18 to 30 +0.009/0 +0.013/0 +0.021/0 +0.033/0 +0.052/0 +0.084/0 +0.13/0 +0.21/0
over 30 to 50 +0.011/0 +0.016/0 +0.025/0 +0.039/0 +0.062/0 +0.1/0 +0.16/0 +0.25/0
over 50 to 80 +0.013/0 +0.019/0 +0.03/0 +0.046/0 +0.074/0 +0.12/0 +0.19/0 +0.3/0
over 80 to 120 +0.015/0 +0.022/0 +0.035/0 +0.054/0 +0.087/0 +0.14/0 +0.22/0 +0.35/0
over 120 to 180 +0.018/0 +0.025/0 +0.04/0 +0.063/0 +0.1/0 +0.16/0 +0.25/0 +0.4/0
over 180 to 250 +0.02/0 +0.029/0 +0.046/0 +0.072/0 +0.115/0 +0.185/0 +0.29/0 +0.46/0

Titanium rod

Recent hot case projects and products

Grade 23 Titanium rod and bar
Titanium rod and bar
Titanium rod and bar
Titanium rod and bar
Titanium rod and bar
Titanium rod and bar
Ti6AL-4V ELI Titanium Alloy Bar, Titanium Bar Grade 23/UNS R56401

Daxun has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 23 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.


SPECIFICATIONS

AMS 4928 – Bars, Forgings, and Forging Stock (Annealed)
AMS 4965 – Bars, Forgings (Solution treated and aged)
AMS 4967 – Bars, Forgings (Annealed, Heat Treatable)


HEAT TREATMENT

When high hardness, tensile strength, and fatigue strength are required, annealing can be performed at 1,700-1,900°F (927 – 1,038°C).
DAXUN 6-4™ Grade 23 alloy can be heat treated in a variety of ways:

  1. Anneal: 1,275 – 1,400°F (691 – 760°C), ½ to 2 hours, air or furnace cool
  2. Stress Relief Anneal: 1,000 – 1,200°F (538 – 649°C), 1 to 8 hours, air or furnace cool
  3. Solution Heat Treat: 1,675 – 1,750°F (913 – 954°C), 1 hour, water quench
  4. Aging: 975 – 1,025°F (524 – 552°C), 4 to 8 hours – air cool

In the solution treated and aged condition, rapid quenching of small sections yields optimum properties. Larger section sizes and/or delayed quenching may result in less than optimum properties.


HARDNESS

Typical hardness in the annealed condition is Rockwell C 30-34, and about Rockwell C 35-39 in the solution and aged condition.


Forgeability / Formability

Ti-6Al-4V ELI (Grade 23) alloy bar is forged at 1,750°F (954°C) with a final forging temperature of 1,450°F (788°C). A minimum of 35% reduction is recommended for optimum properties.

Grade 23 alloy bar is difficult to form at room temperature, even in the annealed condition. Therefore, severe forming operations such as bending or stretching can be performed on annealed material at temperatures up to 1,200°F (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000 – 1,200°F (538 – 649°C).


Machinability

Ti-6Al-4V ELI (Grade 23) alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids.


Weldability

Grade 23 titanium rod is readily weldable in the annealed condition or in the solution and partially aged condition, with aging being accomplished during post weld heat treatment. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. Spot, seam, and flash welding may be performed without the aid of a protective atmosphere.


Special Considerations

Grade 23 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics.


Size Range

Grade 23 Titanium Bar Dimensions
Ø 0.7 – 30 mm (drawn, ground)
Ø 16 – 400 mm (hot rolled, peeled)
Tolerances: h11–h5 (ISO 286-2)
Tighter or different tolerances available on request
Lengths up to 9,000 mm long, depending on diameter
For larger diameters, other bar lengths and tolerances can be agreed upon request


Availability Grade 23 Titanium Rods

Processing options include:

  • Drawing, straightening
  • Drawing, straightening, polishing
  • Drawing, grinding, polishing
  • Drawing, straightening, grinding, polishing
  • Drawing, annealing, straightening
  • Drawing, annealing, polishing
  • Drawing, annealing, grinding, polishing
  • Drawing, annealing, straightening, grinding, polishing

We produce bars according to your requirements.
Excellent surface and straightness, perfect roundness and tightest diameter tolerances (according to ISO 286-2 up to h5). Available in straightened, ground, polished conditions.


Sawing

  • Band saws (up to Ø510 mm)
  • Bench band saws (up to 6,000 x 3,000 x 400 mm)
  • High-performance sawing machines for precise sawing

Titanium Bar End Machining

  • Single or double sided
  • Chamfer 90° (45°)
  • Point 60° (30°)
  • Flat end
  • Centered

Delivery Form

  • ASTM American Society for Testing and Materials Standards
  • AMS American Aerospace Materials Standards
  • NACE American Association of Corrosion Engineers International Standards
  • ASME American Society of Mechanical Engineers Standards
  • GB Chinese National Standards
  • GJB Chinese National Military Standards
  • ISO International Standards
  • DIN German Standards
  • EN European Standards
  • API American Petroleum Institute Standards

Detection Method

Non-destructive testing > 100% testing
Testing methods:

  • Eddy current testing / eddy current crack testing
  • Defect-free surface (level 4)
  • Flat bottom hole diameter 0.7 mm and 0.4 mm
  • Blind area can be cut off according to fixed length > Test to the end of the bar
  • Full diameter ultrasonic testing

Our Titanium Bar Material Services

As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.

We will be happy to provide you with a consultation and explain everything you need to know about obtaining Grade 23 titanium bar material, including which standards require greater attention for the components to be manufactured.

If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee prices and quantities for a specified period.

Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about Grade 23 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.


Ordering Information

Purchase orders should include quantity, grade, type or category, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact Daxun now, we will reply to your email as soon as possible.

Which grade of titanium is the best?

The grade of titanium alloy you need depends on the project you are working on, as each grade has different benefits.

All grades of titanium alloy are extremely strong and corrosion resistant, which means they will continue to work well in the harshest conditions.

The higher grades of titanium alloy (5-12) are alloys designed for specific benefits. For example, grade 12 titanium alloy has excellent heat resistance, making it a perfect choice for shell and tube heat exchangers, hydraulic piping, and chemical industry equipment.

Grades 1-4 are pure titanium alloys, and they are a perfect choice if you need a weldable, ductile material for piping systems and tubing. You will find lower grades used in the marine and industrial industries.

If you are starting a project and are unsure which grade of titanium alloy is best for you, contact us today; we are more than happy to help you.

How are higher grades of titanium different to the lower grades?

At DAXUN, we offer a wide range of titanium alloy grades from grade 1 to grade 12.

Grades 1-4 are pure titanium, while higher grades are alloys.

Alloy grades are popular for their high strength-to-weight ratio.

The most commonly used titanium alloy grade we find is grade 5. While still high in titanium, this grade is one of the most reliable because it can withstand temperatures up to 600°F and withstand extreme conditions.

Higher grades are favored by industries such as aerospace and marine industries for their wear and corrosion resistance.

Conversely, lower grades are primarily used for welding due to their lower strength.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

Does the grade of titanium affect the cost?

While the grade of titanium does increase the cost slightly, the total cost is primarily determined by the shape and form of titanium you require.

At DAXUN, we offer a wide range of titanium products, including plates, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

Unfortunately, it is difficult to come up with a price online without knowing much about your project and what the titanium will be used for.

Fortunately, our team of experts are always here to help and advise you on your titanium needs. By sending an email to daxunalloy@gmail.com, we will be able to get back to you with some advice and an accurate quote.

Make sure to include as much information as possible about the grade, shape and quantity of titanium you require to get a better understanding of your needs.

Where can I learn more about grades of titanium?

The team at DAXUN is experienced, knowledgeable, and friendly. With years of experience in the industry, they know all about titanium, including its uses, benefits, and grades.

For regular updates on titanium, its uses, and its applications across industries, be sure to check out our blog. Our experts have written easy-to-follow guides that you can always refer to when you have questions.

If you’re still having trouble, feel free to contact us; we’ll be happy to help.

By sending an email to daxunalloy@gmail.com, you’ll receive a quick response. Make sure to include as much detail as possible in your question so we can recommend a suitable solution.

How to get a quote OR understand the market information ASAP?

Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email (Daxunalloy@gmail.com) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week

Can I get some samples?

We can provide titanium rod samples for you to check the quality. Sample is free and you just pay the freight.

Which countries have you already exported?

We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.

What is your MOQ?

Our MOQ is 300 Kg for titanium rod.

How long is your delivery time?

Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.

Send Your Inquiry Today
Quick Quote