x
همین امروز استعلام خود را ارسال کنید
استعلام سریع

Ti 15333 Ti-15V-3O-3Sn-3Al Alloy Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:Ti 15333 – UNS R58153
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Titanium tube density The density of Ti 15333 titanium is approximately 4.76 g/cm3
  • Standards:ASTM B337

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

Ti 15333 Titanium Alloy Pipe Manufacturer

Ti-15-3-3-3, also known by its alloy designation Ti-15333, is a high-strength, metastable beta titanium alloy. Its chemical composition is approximately 15% Vanadium, 3% Chromium, 3% Aluminum, and 3% Tin, with the remainder being titanium. This unique composition gives it a distinct set of properties that differentiate it from the more common alpha-beta alloys like Ti-6Al-4V.

The primary advantage of Ti-15-3-3-3 lies in its excellent cold formability. In its solution-treated (annealed) condition, it is quite ductile and can be readily formed into complex shapes, including tubing, sheets, and wires, at room temperature. This is a significant benefit for manufacturing, as it reduces the need for high-temperature forming processes.

After forming, Ti-15-3-3-3 can be precipitation hardened (aged) to achieve very high tensile strength, often exceeding 1200 MPa (175 ksi). This combination of formability and high strength makes it a preferred material for demanding aerospace applications.

Key Characteristics of Ti-15-3-3-3 Tubing:

  • High Strength-to-Weight Ratio: Like all titanium alloys, it offers exceptional strength for its weight, which is critical in aerospace and high-performance motorsports.
  • Excellent Cold Formability: It can be easily manipulated into tubular and other structural components in its annealed state.
  • Good Weldability: The alloy can be welded using standard techniques, though post-weld heat treatment is often required to restore optimal mechanical properties.
  • Superior Corrosion Resistance: It exhibits excellent resistance to corrosion in many environments, including seawater and various chemical atmospheres.

Common Applications for Ti-15-3-3-3 Tubing:

Due to its specific property profile, Ti-15-3-3-3 tubing is predominantly used in high-performance sectors:

  • Aerospace: Used for structural components, airframe parts, and high-strength fasteners.
  • Sporting Goods: High-end bicycle frames, golf club heads, and other performance equipment where strength and lightness are paramount.
  • Medical Devices: Occasionally used for surgical implants and instruments that benefit from its combination of strength, biocompatibility, and formability.

داده‌ها

عنصر Content (%)
Titanium(Ti) 75
Vanadium(V) 15
Chromium(Cr) 3
Aluminum(Al) 3
Tin(Sn) 3
Iron(Fe) ≤ 0.25
Oxygen(O) ≤ 0.13
Carbon(C) ≤ 0.05
Nitrogen(N) ≤ 0.05
Hydrogen(H) ≤ 0.015

 

مالکیت ارزش
Density (g/cm³) 4.8
Melting Point (°C) 1600-1650
هدایت حرارتی (وات بر متر بر کلوین) 6.7-8.0
Specific Heat (J/kg·K) 510
Electrical Resistivity (μΩ·m) 1.30
Coefficient of Thermal Expansion (10^-6/K) 8.6-9.4

 

مالکیت ارزش
مقاومت کششی (مگاپاسکال) 1100-1200
Yield Strength (MPa) 950-1050
افزایش طول (%) 10-15
Reduction of Area (%) 25-35
Hardness (HB) 350-400
Fatigue Strength (MPa) 550-650
Shear Strength (MPa) 670-770
Impact Toughness (J) 40-60

داکسون را انتخاب کنید تا به پروژه‌تان کمک کند اوج بگیرد.

همین حالا با داکسون تماس بگیرید

Advanced Production:Titanium seamless pipe

  • Titanium seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities. Hot rolled tube/hot extruded titanium seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm. Cold rolled titanium seamless tube: cold processed tubes are supplied after heat treatment, surface etching, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm.
  • (The above is agreed upon by the manufacturer and the customer based on the specific situation)
همین حالا با داکسون تماس بگیرید

Ti 15333 Titanium Tube Features

Ti 15333 Titanium Tube is the softest form of titanium and has the highest ductility. It has good cold forming characteristics and offers excellent corrosion resistance. It also has excellent welding properties and high impact toughness.

  • Softest Titanium
  • Highest Ductility
  • Excellent Corrosion Resistance
  • Good Cold Formability
همین حالا با داکسون تماس بگیرید

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

همین حالا با داکسون تماس بگیرید

گزارش‌های آزمون

The test reports we provide include: Factory test certificate for Ti 15333 titanium welded pipe and Ti 15333 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)

همین حالا با داکسون تماس بگیرید

Applications and standards

Titanium 15333 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
همین حالا با داکسون تماس بگیرید

کیفیت، تحویل، بازرسی

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Ti 15333 Titanium Welded Pipe and Ti 15333 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • زمان تحویل ما دقیقاً مطابق قرارداد است.
  • از آژانس‌های ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
  • از نمونه‌های رایگان برای آزمایش مشتری پشتیبانی کنید.
  • حمایت از بازرسی کارخانه‌ای حضوری یا ویدیویی
همین حالا با داکسون تماس بگیرید

بسته‌بندی

داکسون آلیاژ بهترین کیفیت بسته‌بندی را تضمین می‌کند، زیرا بسته‌بندی نقش مهمی در حمل‌ونقل بین‌المللی دارد که کالاها از مسیرهای مختلف عبور می‌کنند تا به مقصد نهایی برسند؛ بنابراین ما توجه ویژه‌ای به بسته‌بندی داریم. ما کالاهای خود را بسته به محصول به روش‌های مختلف بسته‌بندی می‌کنیم. روش‌های بسته‌بندی محصولات ما عبارتند از:
• جعبه‌ها و صندوق‌ها
• سلفون منقبض‌شونده
• پالت‌های چوبی
• جعبه‌های چوبی

همین حالا با داکسون تماس بگیرید

پشتیبانی فنی

اگر به هرگونه پشتیبانی فنی اضافی نیاز دارید، متالورژیست مقیم ما و کارکنان آگاه ما با کمال میل آماده کمک‌رسانی هستند. علاوه بر این، داکسون دارای آزمایشگاه آزمون معتبر است—نخستین در صنعت موجودی چندفلزی و پلاستیکی. به نظر ما، این امر تعهد تزلزل‌ناپذیر ما به کیفیت و فلسفه ما به‌عنوان یک تأمین‌کننده تمام‌خدمت را نشان می‌دهد.

Daxun Ti 15333 Titanium TUBE Let your brand improve rapidly

Ti 15333 titanium tube form (4)

پروژه‌ها و محصولات داغ اخیر

Ti 15333 Titanium pipe and tube
Ti 15333 Titanium pipe and tube
Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
What is Ti-15-3-3-3 titanium alloy, and how is it different from Ti-6Al-4V?

Ti-15-3-3-3 (or Ti-15333) is a beta-rich titanium alloy known for its exceptional cold formability. Unlike the more common Ti-6Al-4V (an alpha-beta alloy), Ti-15-3-3-3 can be easily formed into complex shapes, like tubing, at room temperature. After forming, it can be heat-treated to achieve very high strength, making it ideal for applications that require both intricate manufacturing and high performance.

Can Ti-15-3-3-3 tubing be welded?

Yes, Ti-15-3-3-3 has good weldability. However, to achieve the best mechanical properties in the welded joint, a post-weld heat treatment (solution treating and aging) is typically recommended. This process restores the high strength that the alloy is known for.

What sizes and specifications of Ti-15-3-3-3 tubing does Daxun Alloys Co., Ltd. offer?

At Daxun Alloys Co., Ltd., we supply Ti-15-3-3-3 tubing in a wide range of outer diameters, wall thicknesses, and lengths to meet your specific project requirements. We offer tubing in both the annealed (easily formable) and aged (high-strength) conditions. Please contact us with your detailed specifications for a custom quote.

آیا درجه تیتانیوم بر هزینه تأثیر دارد؟

اگرچه درجه تیتانیوم کمی هزینه را افزایش می‌دهد، اما هزینه کل عمدتاً به شکل و فرم تیتانیومی که نیاز دارید بستگی دارد.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

متأسفانه بدون اطلاع کافی از پروژه شما و کاربرد تیتانیوم، تعیین قیمت به‌صورت آنلاین دشوار است.

خوشبختانه تیم کارشناسان ما همیشه در خدمت شماست تا در زمینه نیازهای تیتانیومی‌تان به شما کمک و مشاوره دهد. با ارسال ایمیل به daxunalloy@gmail.com، ما قادر خواهیم بود با ارائه مشاوره و برآورد دقیق هزینه به شما پاسخ دهیم.

حتماً تا حد امکان اطلاعاتی دربارهٔ گرید، شکل و مقدار تیتانیومی که نیاز دارید ارائه دهید تا نیازهایتان بهتر درک شود.

چگونه سریعاً یک برآورد قیمت دریافت کنیم یا اطلاعات بازار را بفهمیم؟

لطفاً فرم صفحه “تماس با ما” را پر کنید یا با مدیر فروش ما به شماره +86 13382898899 تماس بگیرید. ما در اسرع وقت با شما تماس خواهیم گرفت. واتس‌اپ ما آنلاین است و ایمیل (Daxunalloy@gmail.com) ظرف ۶ ساعت بررسی می‌شود. به هر پرسش یا پیام به‌سرعت پاسخ داده خواهد شد. علاوه بر این، ما هر هفته اطلاعات بازار را با مشتریان خود به اشتراک می‌گذاریم.

می‌توانم چند نمونه بگیرم؟

We can provide titanium tube samples for you to check the quality. Sample is free and you just pay the freight.

تا کنون به کدام کشورها صادرات داشته‌اید؟

ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشته‌ایم.

حداقل مقدار سفارش شما چیست؟

Our MOQ is 1 ton for titanium tube.

زمان تحویل شما چقدر است؟

سفارش‌های آزمایشی را می‌توان ظرف یک هفته تحویل داد. برای سفارش‌های معمولی تقریباً دو هفته زمان لازم است.

همین امروز استعلام خود را ارسال کنید
استعلام سریع