Daxun Alloy - Hastelloy G30 pipe made in China
As a leading supplier of Hastelloy G30 pipes in China, Daxun provides high-performance alloy tubes to the world.
- Hastelloy G30 types: Seamless tube, welded tube, forged tube
- Certification : ASTM,SGS,ISO,CE
- Delivery Time : 7-15 days
- Surface finish: Annealed, polished etc.
- MOQ : ≥300kg
————Daxun produces hastelloy pipe in China to meet the diverse and ——نیازهای سختگیرانه مشتریان!
Characteristics & Properties of Hastelloy G30
Hastelloy G30 pipe is a high-performance nickel-based alloy tube with unique chemical composition and excellent comprehensive performance. It is based on nickel as the main matrix and is rich in various alloy elements such as chromium, molybdenum, and tungsten. With this precise composition design, it has excellent corrosion resistance. It can show excellent corrosion resistance in strong oxidizing acids such as phosphoric acid and nitric acid, as well as reducing acid environments such as hydrofluoric acid and sulfuric acid, and effectively cope with complex and harsh chemical environments. In addition, it can maintain stable mechanical properties under high temperature conditions, with a high melting point and moderate thermal expansion coefficient, so that it can function normally in high-temperature working scenarios.
The application field of Hastelloy G30 pipe is very wide, covering many industries such as chemical, petroleum and natural gas. In the chemical industry, it is often used in chemical reaction vessels, piping systems, etc. to ensure long-term stable operation in highly corrosive media; in the oil and gas industry, it can be used in sulfuric acid treatment units and oil and gas extraction-related equipment in refineries and petrochemical plants; it can also be used in marine engineering, nuclear pipelines, food processing equipment and other fields. With its own high-performance advantages, it can meet the stringent requirements of different industries for corrosion-resistant and high-temperature resistant materials.
Hastelloy G30 Parameters
- ترکیب شیمیایی
- Physical properties
- خواص مکانیکی
| نی | کروم | آهن | مو | Co | C |
| 30% – 35% | 20% – 24% | 28% – 32% | 6% – 8% | ≤1% | ≤0.1% |
| امان | سی | آل | تیتانیوم | P | S |
| ≤1% | ≤1% | ≤0.5% | ≤0.5% | ≤0.04% | ≤0.03% |
| مالکیت | تراکم | نقطه ذوب | ظرفیت گرمایی ویژه | هدایت حرارتی | مقاومت الکتریکی | Coefficient of Thermal Expansion | Elastic Modulus | Hardness |
| ارزش | 8.2 g/cm³ | 1350 – 1390°C | 0.44 J/(g·°C) | 18 W/m·K | 1.1 Ω·mm²/m | 13.7 μm/(m·°C) | ۲۰۰ گیگاپاسکال | 160 HB |
| مالکیت | مقاومت کششی | مقاومت تسلیم | Elongation | کاهش مساحت | Impact Toughness |
| ارزش | 690MPa | 310MPa | 40% | ≥50% | ≥80J |
داکسون را انتخاب کنید تا به پروژهتان کمک کند اوج بگیرد.

Advanced Production:Hastelloy alloy pipe
Hastelloy G30 alloy is an all-around nickel-chromium-molybdenum-tungsten alloy with good resistance to pitting, crevice corrosion and stress corrosion cracking. It has excellent resistance to oxidative aqueous media, including wet chlorine, nitric acid or mixed acids of oxidizing acids containing chloride ions. At the same time, Hastelloy G30 alloy also has ideal resistance to reducing and oxidizing environments encountered in the process. Relying on this versatile performance, it can be used in some troublesome environments or in factories for a variety of production purposes.
Hastelloy G30 Pipe Features
Hastelloy G30 alloy has an exceptional resistance to various chemical environments, including strong oxidizing substances, such as ferric chloride, cupric chloride, chlorine, thermally contaminated solutions (organic and inorganic), formic acid, acetic acid, acetic anhydride, seawater and salt solutions, etc. Hastelloy G30 alloy has the ability to resist the formation of grain boundary precipitation in the heat affected zone of welding, so that it can also be used in many chemical processes in the welding state.


کیفیت، تحویل، بازرسی
Daxun conducts a series of quality assurance tests on Hastelloy G30 pipes. These tests include flattening test, flaring test, ultrasonic flaw detection, crevice corrosion resistance test, mechanical property test, hardness test, material positive identification, and expansion test, etc. All these tests are designed to ensure that the Hastelloy G30 pipes meet the requirements of the intended applications. During the production process, we meticulously measure the outer diameter, wall thickness, and surface quality of the products. Our standard delivery time is 5 – 7 days, and for special sizes, it is 15 – 20 days.
- زمان تحویل ما دقیقاً مطابق قرارداد است.
- از آژانسهای ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
- از نمونههای رایگان برای آزمایش مشتری پشتیبانی کنید.
- حمایت از بازرسی کارخانهای حضوری یا ویدیویی
بستهبندی
داکسون آلیاژ بهترین کیفیت بستهبندی را تضمین میکند، زیرا بستهبندی نقش مهمی در حملونقل بینالمللی دارد که کالاها از مسیرهای مختلف عبور میکنند تا به مقصد نهایی برسند؛ بنابراین ما توجه ویژهای به بستهبندی داریم. ما کالاهای خود را بسته به محصول به روشهای مختلف بستهبندی میکنیم. روشهای بستهبندی محصولات ما عبارتند از:
• جعبهها و صندوقها
• سلفون منقبضشونده
• پالتهای چوبی
• جعبههای چوبی


پشتیبانی فنی
If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. [همین حالا با ما تماس بگیرید]Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.
Daxun is a trustworthy stainless steel tube manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel tubes have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
محصولات مرتبط (8)
لطفاً فرم صفحه “تماس با ما” را پر کنید یا با مدیر فروش ما به شماره +86 13382898899 تماس بگیرید. ما در اسرع وقت با شما تماس خواهیم گرفت. واتساپ ما آنلاین است و ایمیل (Daxunalloy@gmail.com) ظرف ۶ ساعت بررسی میشود. به هر پرسش یا پیام بهسرعت پاسخ داده خواهد شد. علاوه بر این، ما هر هفته اطلاعات بازار را با مشتریان خود به اشتراک میگذاریم.
ما میتوانیم نمونههای ورق فولاد ضدزنگ را برای بررسی کیفیت در اختیار شما قرار دهیم. نمونه رایگان است و شما فقط هزینه حمل را پرداخت میکنید.
ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشتهایم.
The minimum order quantity for our Hastelloy products is 300kg
سفارشهای آزمایشی را میتوان ظرف یک هفته تحویل داد. برای سفارشهای معمولی تقریباً دو هفته زمان لازم است.