x
همین امروز استعلام خود را ارسال کنید
استعلام سریع

Grade 9 (Ti-3Al-2.5V) Titanium Alloy Plate Manufacturer - Daxun Alloy

As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.

  • Plate Grade:Grade 9 UNS R56320
  • Plate Production type:cold rolling, hot rolling, forging.
  • Standard:ASTM B 265,ASME SB265,AMS491 etc
  • Features:High strength, Lightweight, High-temperature resistance
  • Surface:bright, polished, pickled, sandblasted, etc.
  • Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request

————Daxun produces titanium sheets in China to meet the diverse and ——نیازهای سخت‌گیرانه مشتریان!

Providing High-quality Grade 9 Titanium Plate to Serve Customers Worldwide

Grade 9 titanium plate is a high-performance near-alpha titanium alloy with a nominal composition of Ti-3Al-2.5V. It is based on pure titanium (Grades 1-4) reinforced with appropriate amounts of aluminum and vanadium, achieving an excellent balance of strength and toughness. Compared to pure titanium, Grade 9 boasts significantly higher strength and yield strength while maintaining good ductility and toughness. It is particularly renowned for its excellent weldability and cold formability. This material also offers lightweight, excellent corrosion resistance (especially in chloride environments), and good biocompatibility. It is both strong and durable, yet can withstand a variety of harsh operating conditions, making it an ideal choice for applications requiring high performance and reliability.

Where is Grade 9 titanium plate used?

In the aerospace industry, Grade 9 titanium plate is widely used in the manufacture of aircraft structures, fasteners, hydraulic systems, and engine components. Its combination of high strength and low density effectively reduces aircraft weight and improves fuel efficiency. In marine engineering and shipbuilding, its exceptional resistance to seawater corrosion makes it the material of choice for ship hull structures, desalination equipment, heat exchangers, and offshore platform components, ensuring long-term reliability in harsh marine environments. In the medical industry, Grade 9 titanium plate, due to its excellent biocompatibility and moderate strength, is widely used in the manufacture of orthopedic implants (such as plates and screws), dental implants, and surgical instruments. Furthermore, Grade 9 titanium plate demonstrates its unique value and adaptability in high-end sports equipment (such as bicycle frames and golf club heads), chemical equipment (corrosion-resistant reactors and heat exchangers), and precision mechanical components requiring lightweight and high strength.

داده‌ها

عنصر Composition Range (wt.%)
تیتانیوم Balance (>90%)
آل 2.50–3.50%
V 2.00–3.00%
آهن ≤0.25%
O ≤0.13%
C ≤0.08%
N ≤0.03%
H ≤0.015%
سایر ≤0.4% (single element)

Key Characteristics

  • نسبت قدرت به وزن: Higher than pure titanium (Grades 1–4) but lower than Ti-6Al-4V (Grade 5).
  • مقاومت در برابر خوردگی: Excellent in marine, chemical, and chloride environments.
  • سازگاری زیستی: Non-toxic and MRI-compatible, but less commonly used in implants than Grade 23.
  • Formability: Superior to Grade 5; suitable for complex forming, welding, and machining.

 کاربردهای معمول

  • هوافضا: Hydraulic tubing, aircraft fittings, fasteners.
  • Marine: Heat exchangers, seawater components, propeller shafts.
  • Medical: Surgical instruments, non-implantable devices.
  • Industrial: Chemical processing equipment, pressure vessels.
مالکیت Value (Imperial) Value (Metric)
تراکم 0.160 lb/in³ 4.43 g/cm³
نقطه ذوب 3,000–3,050°F 1,650–1,680°C
هدایت حرارتی 6.5 Btu/(hr·ft·°F) 11.2 W/(m·K)
Coefficient of Thermal Expansion 5.3 × 10⁻⁶/°F 9.5 × 10⁻⁶/K
مقاومت الکتریکی 120 µΩ·cm 120 nΩ·m

Room Temperature Properties (Annealed Condition)

مالکیت Value (Imperial) Value (Metric)
مقاومت کششی 130–140 ksi 895–965 MPa
Yield Strength (0.2% offset) 120–125 ksi 825–860 MPa
Elongation 10–15% 10–15%
Reduction in Area 25–30% 25–30%
سختی (برینل) 280–320 HB 290–330 HBW
ماژول ارتجاعی 16.5 × 10⁶ psi 114 GPa

عملکرد در دمای بالا

Temperature (°F) Tensile Strength (ksi) Yield Strength (ksi)
400°F (200°C) 115–125 105–110
600°F (315°C) 100–110 90–95
800°F (425°C) 85–95 75–80

داکسون را انتخاب کنید تا به پروژه‌تان کمک کند اوج بگیرد.

Common applications

Grade 9 titanium plates and sheets are primarily used for components that require an excellent balance of strength, ductility, and corrosion resistance, offering superior weldability and formability compared to other titanium alloys.

  1. Applications include aerospace components such as airframe structures, pressure vessels, and engine components that require moderate strength but exceptional corrosion resistance.
  2. Industrial applications include chemical processing equipment, heat exchangers, and marine components due to their outstanding resistance to corrosive environments.
  3. Oil and gas industry components, including downhole drilling equipment and subsea systems, where both strength and corrosion resistance are critical.
  4. Medical implants and surgical instruments, particularly where biocompatibility and moderate strength are required.
  5. Performance automotive components, including exhaust systems, suspension parts, and high-performance vehicle frames that benefit from titanium’s strength-to-weight ratio.

تحویل سریع

Daxun provides customers with timely and fast delivery of grade 9 titanium plate products. Behind the speed is the system support from professional production capacity, and information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected.

titanium plate

Custom Cutting

Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:

  • Water jet cutting
  • Laser cutting
  • Plasma cutting
  • Wire cutting
  • Bending
  • برش شیاری
  • ارّه‌کاری

بسته‌بندی

We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
• جعبه‌ها و صندوق‌ها
• Shrinkwrap
• پالت‌های چوبی
• جعبه‌های چوبی

پشتیبانی فنی

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.

Daxun Grade 9 Titanium sheet Let your brand improve rapidly

به جز محصولات فهرست‌شده در زیر، سایر محصولات فلزی موجود در اینجا ذکر نشده‌اند. سایر محصولات فلزی که DAXUN می‌تواند تولید و عرضه کند شامل تانتال، نیوبیوم، زیرکونیوم، هافنیوم، نیکل، مس و غیره هستند که عمدتاً به شکل ورق، شمش و لوله عرضه می‌شوند.
محصولات/استاندارد فرآوری رتبه/اندازه
Titanium Plate, Sheet, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7, GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3 (ضخامت: (0.0197”-6”)حداکثر عرض: ۱۲ فوت، حداکثر طول: ۵۰ فوت)
AMS-T-9046
Titanium and Titanium alloy sheet, plate
تیتانیوم خالص تجاری (CP)
نشانه‌گذاری کد مقاومت تسلیم
حداقل، ksi ۱ /
CP-1 Gr1 70
CP-2 Gr2 55
CP-3 Gr3 40
CP-4 Gr4 25
آلیاژهای تیتانیوم آلفا (الف)
نشانه‌گذاری کد ترکیب
الف-۱ ۵A۱-۲.۵Sn
الف-۲ ۵A۱-۲.۵Sn(ELI) ۲ /
الف-۳ ۶A۱-۲Cb-۱Ta-۰.۸Mo
الف-۴ ۸A۱-۱Mo-۱V
آلیاژهای تیتانیوم آلفا-بتا (AB)
نشانه‌گذاری کد ترکیب
AB-1 Gr5 ۶A۱-۴V
AB-2 Gr5 ۶A۱-۴V(ELI)
AB-3 ۶A۱-۶V-۲Sn
AB-4 ۶آی۱-۲اس‌ان-۴زیر-۲موی
AB-5 ۳A۱-۲.۵V
AB-6 ۸ منگنز
آلیاژهای تیتانیوم بتا (B)
نشانه‌گذاری کد ترکیب
بی-یک ۱۳V-۱۱Cr-۳A1
بی-۲ ۱۱.۵ مولی‌بروم-۶ زِیرکونیم-۴.۵ قلع
بی-۳ ۳A۱-۸V-۶Cr-۴Mo-۴Zr
بی-۴ ۸ منگنز-۸ تیتانیوم-۲ آهن-۳ آلومینیوم
پردازش:
نورد گرم نورد سرد
مراحل در دسترس:
رتبه ۱ CP Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2)
رتبهٔ ۲ CP Grade 6Al-4V ELI (پیش‌تر Grade 23)
پایه هفتم Grade 6Al-6V-2Sn (6-62)
کلاس نوزدهم پایه ۸، ال-۱ مو-۱ وی (۸-۱-۱)
کلاس پنجم (۶آلومینیوم-۴ونادیوم) کلاس ۹ (۳ آل-۲.۵ ولت)
کلاس ۶ (۵آلومینیوم-۲.۵ قلع) CP درجه ۳
کاربرد
صنعت شیمیایی شیرین‌سازی آب دریا
صنعت پتروشیمی هوافضا
حوزه ماشین‌کاری، حوزه خودروسازی میدان قطعه تلفن همراه.

پروژه‌ها و محصولات داغ اخیر

Grade 9 Titanium Plate and sheet
Naval vessels
Grade 9 Titanium Plate and sheet
Aviation and Aerospace
Titanium Plate and sheet
Military armor
Titanium Plate and sheet
Guidance components
Titanium Plate and sheet
صنعت انرژی نو
Titanium Plate and sheet
مهندسی دریایی
What makes Grade 9 titanium different from other titanium alloys?

Grade 9 titanium (Ti-3Al-2.5V) offers an optimal balance between strength, ductility, and corrosion resistance. It contains 3% aluminum and 2.5% vanadium, which gives it approximately 20-30% higher strength than pure titanium (Grade 1-4) while maintaining excellent formability and weldability that surpasses many other titanium alloys.

What are the main advantages of using Grade 9 titanium plates in industrial applications?

Grade 9 titanium plates provide exceptional corrosion resistance, high strength-to-weight ratio, excellent weldability, and good formability. These properties make them ideal for applications requiring durability in harsh environments while reducing overall weight, which can lead to improved fuel efficiency in transportation applications.

What are the recommended machining practices for Grade 9 titanium plates?

Machining Grade 9 titanium requires slower speeds, lower feed rates, and ample coolant compared to steel or aluminum. Using sharp, high-quality carbide tools with rigid setups is essential. The material has a tendency to work-harden, so maintaining positive cutting action and avoiding dwell times is important for successful machining.

How does Grade 9 titanium perform in marine environments compared to other alloys?

Grade 9 titanium excels in marine environments, offering outstanding resistance to seawater corrosion, crevice corrosion, and stress corrosion cracking. Unlike many stainless steels that may require regular maintenance or replacement in marine applications, Grade 9 titanium can provide decades of service with minimal degradation, making it cost-effective despite higher initial material costs.

Is Grade 9 titanium suitable for welding and fabrication processes?

Yes, Grade 9 titanium is highly suitable for welding and fabrication. It can be welded using TIG, MIG, plasma arc, and electron beam welding processes. The alloy requires proper shielding from atmospheric contamination during welding, but generally offers excellent weldability without the need for post-weld heat treatment in most applications.

چگونه سریعاً یک برآورد قیمت دریافت کنیم یا اطلاعات بازار را بفهمیم؟

لطفاً فرم صفحه “تماس با ما” را پر کنید یا با مدیر فروش ما به شماره +86 13382898899 تماس بگیرید. ما در اسرع وقت با شما تماس خواهیم گرفت. واتس‌اپ ما آنلاین است و ایمیل (Daxunalloy@gmail.com) ظرف ۶ ساعت بررسی می‌شود. به هر پرسش یا پیام به‌سرعت پاسخ داده خواهد شد. علاوه بر این، ما هر هفته اطلاعات بازار را با مشتریان خود به اشتراک می‌گذاریم.

می‌توانم چند نمونه بگیرم؟

We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.

تا کنون به کدام کشورها صادرات داشته‌اید؟

ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشته‌ایم.

حداقل مقدار سفارش شما چیست؟

Our MOQ is 1 ton for titanium sheet.

زمان تحویل شما چقدر است؟

سفارش‌های آزمایشی را می‌توان ظرف یک هفته تحویل داد. برای سفارش‌های معمولی تقریباً دو هفته زمان لازم است.

همین امروز استعلام خود را ارسال کنید
استعلام سریع