x
همین امروز استعلام خود را ارسال کنید
استعلام سریع

Grade 7 Ti-0.15Pd Alloy Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:پایه هفتم – UNS R52400
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Titanium tube density The density of grade 7 titanium is approximately 4.51 g/cm3
  • Standards:ASTM B338、ASTM B861、ASTM B862

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

Grade 7 Titanium Alloy Pipe Manufacturer - Daxun Alloy

Provide High Quality Grade 7 Titanium Pipe to Customers Around The World
Grade 7 titanium pipe is a palladium-enhanced commercially pure titanium alloy (Ti-0.12Pd), engineered for ultimate corrosion resistance in the most aggressive environments. It combines the inherent formability and weldability of pure titanium with exceptional durability against reducing acids and chlorides. Its density (4.51 g/cm³) is approximately 60% that of steel, while offering unparalleled defense against chemical attack, pitting, and crevice corrosion. The alloy excels in harsh conditions—including hot reducing acids, chloride-rich solutions, and sour gas environments—maintaining integrity where other materials fail.

  • Palladium’s electrochemical role: Pd acts as a cathodic catalyst, promoting rapid repassivation of the titanium oxide layer when damaged. This self-healing mechanism prevents localized corrosion (pitting/crevice) in reducing acids like HCl, H₂SO₄, and wet chlorine environments where conventional titanium fails.
  • Synergy with titanium matrix: While retaining pure titanium’s inherent ductility and weldability, the Pd dopant creates a barrier against hydrogen embrittlement and stress corrosion cracking (SCC), enabling reliable performance in chemically aggressive media

Where is Grade 7 titanium pipe used?
In chemical processing plants, it’s the material of choice for reactor vessels, heat exchangers, and piping systems handling sulfuric acid, hydrochloric acid, and chlorinated organics due to its inertness. Marine and offshore industries rely on it for critical seawater systems, desalination equipment, and subsea components, leveraging its unmatched resistance to saltwater corrosion and biofouling. Oil and gas operations employ it in downhole tubing, Christmas tree components, and sour gas pipelines where high-pressure H₂S and CO₂ environments cause rapid degradation of standard alloys. Pharmaceutical and biotech facilities use it for ultra-pure water systems and chemical delivery lines, ensuring zero contamination. Additionally, nuclear waste treatment and pollution control systems utilize it for scrubbers and condensers exposed to corrosive flue gases and acidic effluents, combining longevity with absolute reliability.

Key Performance:

Strength-Ductility Balance:

  • Tensile Strength: 483 MPa (annealed state) – Matches Grade 2 but with superior corrosion resistance.
  • Elongation: ≥20% – Exceptional ductility for cold forming and high fatigue resistance.
  • Density: 4.51 g/cm³ – 60% lighter than steel, ideal for weight-sensitive applications.

Corrosion Resistance:

  • Palladium-enhanced performance: Resists pitting/crevice corrosion in seawater, chlorides, reducing acids (HCl, H₂SO₄), and sour gas (H₂S).
  • Outperforms Grade 2/9: Immune to corrosion in oxidizing media and aggressive chemical environments where stainless steel fails.
  • Galvanic compatibility: No risk of galvanic corrosion when paired with dissimilar metals.

Weldability & Processability:

  • Welding: Excellent TIG/laser weldability – no post-weld cracking due to Pd stabilization.
  • Forming: Superior cold workability vs. Grade 5; easily formed into tubes, sheets, and complex shapes.
  • Heat Treatment: Stress-relieved at 480–595°C to optimize corrosion resistance and ductility.

Application Advantages:

  • Chemical Processing: Reactors, piping, heat exchangers – handles hot reducing acids, chlorides, and sour gas.
  • Marine: Desalination plants, seawater cooling systems – lifetime immunity to saltwater corrosion.
  • Aerospace: Hydraulic fluid lines – lightweight durability in corrosive fuel/hydraulic environments.
  • Industrial: Pollution control scrubbers, geothermal systems – withstands high-temperature acidic vapors.
  • Medical: Implant components – biocompatible with enhanced corrosion resistance in bodily fluids.
بیشتر بخوانید

داده‌ها

عنصر نماد Composition Range (wt.%)
تیتانیوم تیتانیوم Balance (>99%)
Palladium Pd 0.12–0.25%
آهن آهن ≤0.30%
اکسیژن O ≤0.25%
کربن C ≤0.08%
نیتروژن N ≤0.03%
هیدروژن H ≤0.015%
عناصر دیگر Each ≤0.40% (single element)

Key Characteristics

  • Strength-to-Weight Ratio: Comparable to pure titanium (Grades 1–4) but lower than Ti-6Al-4V (Grade 5) or Ti-3Al-2.5V (Grade 9). Optimized for corrosion resistance over mechanical strength.
  • Corrosion Resistance: Unmatched in reducing acids (e.g., HCl, H₂SO₄), chlorides, and crevice corrosion environments. Outperforms all commercially pure grades (1–4) and Grade 5/9 in aggressive chemical media due to palladium (Pd) stabilization.
  • Biocompatibility: Fully non-toxic and MRI-compatible. Suitable for surgical instruments and chemical processing equipment, though not used for permanent implants (Grade 23 preferred).
  • Formability: Retains excellent cold formability, weldability, and machinability of pure titanium. Significantly easier to fabricate than Grade 5/9, enabling complex geometries without specialized tooling.
مالکیت Value (Imperial) Value (Metric)
تراکم 0.163 lb/in³ 4.51 g/cm³
نقطه ذوب 3,000–3,050°F 1,650–1,680°C
هدایت حرارتی 9.5 Btu/(hr·ft·°F) 16.4 W/(m·K)
Coefficient of Thermal Expansion 4.8 × 10⁻⁶/°F 8.6 × 10⁻⁶/K
مقاومت الکتریکی 1.78 × 10⁻⁶ Ω·cm 1.78 μΩ·m

 

مالکیت Value (Imperial) Value (Metric)
مقاومت کششی 50,000–65,000 psi 345–450 MPa
مقاومت تسلیم 30,000–45,000 psi 207–310 MPa
Elongation 20–30% 20–30%
سختی (برینل) 120–160 HB 120–160 HB
ماژول ارتجاعی 14.9–16.0 × 10⁶ psi 103–110 GPa

داکسون را انتخاب کنید تا به پروژه‌تان کمک کند اوج بگیرد.

همین حالا با داکسون تماس بگیرید

Advanced Production:Titanium seamless pipe

  • Titanium seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities. Hot rolled tube/hot extruded titanium seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm. Cold rolled titanium seamless tube: cold processed tubes are supplied after heat treatment, surface etching, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm.
  • (The above is agreed upon by the manufacturer and the customer based on the specific situation)
همین حالا با داکسون تماس بگیرید

Grade 7 Titanium Tube Features

Grade 7 Titanium Tube is the softest form of titanium and has the highest ductility. It has good cold forming characteristics and offers excellent corrosion resistance. It also has excellent welding properties and high impact toughness.

  • Highest Ductility
  • Excellent Corrosion Resistance
  • Good Cold Formability
همین حالا با داکسون تماس بگیرید

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

همین حالا با داکسون تماس بگیرید

گزارش‌های آزمون

The test reports we provide include: Factory test certificate for Grade 7 titanium welded pipe and Grade 7 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)

همین حالا با داکسون تماس بگیرید

Applications and standards

Titanium Grade 7 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
همین حالا با داکسون تماس بگیرید

کیفیت، تحویل، بازرسی

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 7 Titanium Welded Pipe and Grade 7 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • زمان تحویل ما دقیقاً مطابق قرارداد است.
  • از آژانس‌های ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
  • از نمونه‌های رایگان برای آزمایش مشتری پشتیبانی کنید.
  • حمایت از بازرسی کارخانه‌ای حضوری یا ویدیویی
همین حالا با داکسون تماس بگیرید

بسته‌بندی

داکسون آلیاژ بهترین کیفیت بسته‌بندی را تضمین می‌کند، زیرا بسته‌بندی نقش مهمی در حمل‌ونقل بین‌المللی دارد که کالاها از مسیرهای مختلف عبور می‌کنند تا به مقصد نهایی برسند؛ بنابراین ما توجه ویژه‌ای به بسته‌بندی داریم. ما کالاهای خود را بسته به محصول به روش‌های مختلف بسته‌بندی می‌کنیم. روش‌های بسته‌بندی محصولات ما عبارتند از:
• جعبه‌ها و صندوق‌ها
• سلفون منقبض‌شونده
• پالت‌های چوبی
• جعبه‌های چوبی

همین حالا با داکسون تماس بگیرید

پشتیبانی فنی

اگر به هرگونه پشتیبانی فنی اضافی نیاز دارید، متالورژیست مقیم ما و کارکنان آگاه ما با کمال میل آماده کمک‌رسانی هستند. علاوه بر این، داکسون دارای آزمایشگاه آزمون معتبر است—نخستین در صنعت موجودی چندفلزی و پلاستیکی. به نظر ما، این امر تعهد تزلزل‌ناپذیر ما به کیفیت و فلسفه ما به‌عنوان یک تأمین‌کننده تمام‌خدمت را نشان می‌دهد.

Daxun Grade 7 Titanium TUBE Let your brand improve rapidly

Grade 7 titanium tube form (4)

پروژه‌ها و محصولات داغ اخیر

Grade 7 Titanium pipe and tube
Grade 7 Titanium pipe and tube
Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
کدام گرید تیتانیوم بهترین است؟

رتبه آلیاژ تیتانیومی که نیاز دارید به پروژه‌ای که روی آن کار می‌کنید بستگی دارد، زیرا هر رتبه مزایای متفاوتی دارد.

تمام گریدهای آلیاژ تیتانیوم فوق‌العاده قوی و مقاوم در برابر خوردگی هستند، به این معنی که در سخت‌ترین شرایط نیز به خوبی کار خواهند کرد.

درجهٔ بالاتر آلیاژ تیتانیوم (۵–۱۲) آلیاژهایی هستند که برای مزایای خاص طراحی شده‌اند. برای مثال، آلیاژ تیتانیوم درجهٔ ۱۲ مقاومت حرارتی عالی دارد و آن را به گزینه‌ای ایده‌آل برای مبدل‌های حرارتی پوسته و لوله‌ای، لوله‌کشی هیدرولیک و تجهیزات صنعت شیمی تبدیل می‌کند.

درجه‌های ۱ تا ۴ آلیاژهای تیتانیوم خالص هستند و اگر به ماده‌ای جوش‌پذیر و چکش‌خوار برای سیستم‌های لوله‌کشی و تیوب‌ها نیاز داشته باشید، انتخابی ایده‌آل‌اند. درجه‌های پایین‌تر را در صنایع دریایی و صنعتی خواهید یافت.

اگر در حال شروع یک پروژه هستید و مطمئن نیستید کدام گرید آلیاژ تیتانیوم برای شما مناسب‌تر است، همین امروز با ما تماس بگیرید؛ ما با کمال میل به شما کمک خواهیم کرد.

کلاس‌های بالاتر تیتانیوم چه تفاوتی با کلاس‌های پایین‌تر دارند؟

در داکسون، ما طیف گسترده‌ای از گریدهای آلیاژ تیتانیوم از گرید ۱ تا گرید ۱۲ را ارائه می‌دهیم.

گریدهای ۱ تا ۴ تیتانیوم خالص هستند، در حالی که گریدهای بالاتر آلیاژ هستند.

کلاس‌های آلیاژ به‌خاطر نسبت بالای استحکام به وزن‌شان محبوب هستند.

رایج‌ترین گرید آلیاژ تیتانیومی که می‌یابیم، گرید ۵ است. اگرچه همچنان غنی از تیتانیوم است، این گرید یکی از قابل‌اعتمادترین‌هاست زیرا می‌تواند دماهای تا ۶۰۰ درجه فارنهایت را تحمل کند و در شرایط شدید دوام بیاورد.

در صنایعی مانند صنایع هوافضا و دریایی، به دلیل مقاومت در برابر سایش و خوردگی، گریدهای بالاتر ترجیح داده می‌شوند.

برعکس، گریدهای پایین‌تر عمدتاً به دلیل استحکام کمتر برای جوشکاری استفاده می‌شوند.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

آیا درجه تیتانیوم بر هزینه تأثیر دارد؟

اگرچه درجه تیتانیوم کمی هزینه را افزایش می‌دهد، اما هزینه کل عمدتاً به شکل و فرم تیتانیومی که نیاز دارید بستگی دارد.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

متأسفانه بدون اطلاع کافی از پروژه شما و کاربرد تیتانیوم، تعیین قیمت به‌صورت آنلاین دشوار است.

خوشبختانه تیم کارشناسان ما همیشه در خدمت شماست تا در زمینه نیازهای تیتانیومی‌تان به شما کمک و مشاوره دهد. با ارسال ایمیل به daxunalloy@gmail.com، ما قادر خواهیم بود با ارائه مشاوره و برآورد دقیق هزینه به شما پاسخ دهیم.

حتماً تا حد امکان اطلاعاتی دربارهٔ گرید، شکل و مقدار تیتانیومی که نیاز دارید ارائه دهید تا نیازهایتان بهتر درک شود.

از کجا می‌توانم دربارهٔ گریدهای تیتانیوم بیشتر بیاموزم؟

تیم DAXUN باتجربه، آگاه و خوش‌برخورد است. با سال‌ها تجربه در این صنعت، آن‌ها همه چیز را درباره تیتانیوم، از کاربردها و مزایا گرفته تا گریدهای مختلف آن، می‌دانند.

برای دریافت به‌روزرسانی‌های منظم درباره تیتانیوم، کاربردها و مصارف آن در صنایع مختلف، حتماً وبلاگ ما را بررسی کنید. کارشناسان ما راهنماهای ساده‌ای نوشته‌اند که همیشه می‌توانید هنگام پرسش به آن‌ها مراجعه کنید.

اگر همچنان با مشکل مواجه هستید، با ما تماس بگیرید؛ خوشحال می‌شویم به شما کمک کنیم.

با ارسال ایمیل به daxunalloy@gmail.com، پاسخ سریعی دریافت خواهید کرد. لطفاً در سؤال خود تا حد امکان جزئیات بیشتری درج کنید تا بتوانیم راه‌حل مناسبی پیشنهاد دهیم.

چگونه سریعاً یک برآورد قیمت دریافت کنیم یا اطلاعات بازار را بفهمیم؟

لطفاً فرم صفحه “تماس با ما” را پر کنید یا با مدیر فروش ما به شماره +86 13382898899 تماس بگیرید. ما در اسرع وقت با شما تماس خواهیم گرفت. واتس‌اپ ما آنلاین است و ایمیل (Daxunalloy@gmail.com) ظرف ۶ ساعت بررسی می‌شود. به هر پرسش یا پیام به‌سرعت پاسخ داده خواهد شد. علاوه بر این، ما هر هفته اطلاعات بازار را با مشتریان خود به اشتراک می‌گذاریم.

می‌توانم چند نمونه بگیرم؟

We can provide titanium samples for you to check the quality. Sample is free and you just pay the freight.

تا کنون به کدام کشورها صادرات داشته‌اید؟

ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشته‌ایم.

حداقل مقدار سفارش شما چیست؟

Our MOQ is 1 ton for titanium tube.

زمان تحویل شما چقدر است؟

سفارش‌های آزمایشی را می‌توان ظرف یک هفته تحویل داد. برای سفارش‌های معمولی تقریباً دو هفته زمان لازم است.

همین امروز استعلام خود را ارسال کنید
استعلام سریع