Daxun: A 304 Stainless Steel Angle Supplier in China
As a leading stainless steel angle steel supplier and exporter in China, Daxun supplies stainless steel angle steel to all over the world.
- Grade: S0400(304)-S0403(304L)
- Equal Angle Steel/Unequal Angle Steel
- Process: hot rolling and laser welding
- Easy to weld and process
- Length can be cut to size
- Daxun specializes in custom stainless steel angles with fast delivery and competitive prices. Contact Daxun today.
A global leader in stainless steel Angles fabrication services
Daxun is a leading special metal supplier in China, capable of meeting all your stainless steel angle steel needs. We offer a variety of products, including the popular 304/304L and 316/316L grades, which are renowned for their durability and versatility in various construction and manufacturing projects. We purchase angle steel from fully certified factories, so you can be confident in its quality.
We have a variety of standard and L-shaped angle steel for your selection, and can even cut them to custom lengths, up to 6 meters in length. These angle steels are very useful in many industries, from food processing equipment and construction supports to structural frames and medical equipment. They are usually used for frames and supports, but their versatility is enough to adapt to countless other applications.
The 304/304L grade is a real workhorse, offering excellent corrosion resistance and easy fabrication. It’s simple to weld using standard techniques, making it suitable for everything from general industrial work to demanding chemical projects. What’s more, 304 stainless steel can handle continuous temperatures up to 925°C. The low carbon content of 304L is a big plus, minimizing problems during welding and ensuring strong, reliable joints. If you need even better corrosion resistance, especially in harsh environments like marine settings, the 316/316L grade is the way to go.
Our stainless steel angles go through a special surface treatment process—hot rolling, annealing, and pickling. This not only maximizes their resistance to corrosion but also gives them that classic “stainless” look. The lower carbon content in 304L makes it even better suited for corrosive environments.
We use two main manufacturing methods: hot rolling and laser melting. Hot rolling is a cost-effective option, typically resulting in angles with slightly rounded or tapered edges. Laser melting, on the other hand, produces angles with sharp, precise corners and a smoother, sandblasted finish. This method gives you a superior surface quality compared to hot rolling. If you’re doing heavy welding, you might need to do some post-weld annealing to keep the material in top condition.
Daxun makes both laser-melted and hot-rolled stainless steel angles in both metric and imperial sizes, and we ship them all over the world. So, no matter where you are or what you need, Daxun is your reliable partner for stainless steel angle solutions.
دادهها
- پارامتر
- عنصر
- خواص مکانیکی
- خواص فیزیکی
- همه معادل
| استاندارد | ASTM、EN、DIN、JIS,ASME, BS, GBetc, |
| ابعاد | ∠20*20*3mm-∠200*200*24mm |
| آلیاژ | 201, 310, 304, 304L, 316, 316L |
| نوع | Equal, Unequal |
| طول | 1.0-12.0m |
| ضخامت | 3mm-25mm |
| Custom Options | بله |
| Tolerances | ± ۱/۴ اینچ، ± ۱/۱۶ اینچ” |
| پایان | Mill, brush, mirror, polished |
| Composition of 304/304L/304LN/304H tubing and pipe | ||||
| نمره | 304 | ۳۰۴ال | ۳۰۴ الان | ۳۰۴H |
| تعیینکنندهٔ سازمان ملل متحد | S30400 | اس۳۰۴۰۳ | S30453 | اس۳۰۴۰۹ |
| کربن (C) بیشینه. | 0.08 | 0.030* | 0.03 | 0.04 – 0.10 |
| منگنز (Mn) حداکثر. | 2 | 2 | 2 | 2 |
| فسفر (P) حداکثر. | 0.045 | 0.045 | 0.045 | 0.045 |
| گوگرد (S) حداکثر. | 0.03 | 0.03 | 0.03 | 0.03 |
| سیلیکون (Si) حداکثر. | 1 | 1 | 1 | 1 |
| کروم (Cr) | ۱۸.۰–۲۰.۰ | ۱۸.۰–۲۰.۰ | ۱۸.۰–۲۰.۰ | ۱۸.۰–۲۰.۰ |
| نیکل (Ni) | ۸.۰–۱۱.۰ | ۸.۰–۱۱.۰ | ۸.۰–۱۱.۰ | ۸.۰–۱۱.۰ |
| مولیبدن (Mo) | — | — | — | — |
| نیتروژن (N) | — | — | 0.10–0.15 | — |
| آهن (Fe) | تراز. | تراز. | تراز. | تراز. |
| عناصر دیگر | — | — | — | — |
| نوع | نرخ بازده ۰.۲۱TP3T جابجایی (KSI) | مقاومت کششی (کیاسآی) | % کشش (طول گیج ۲ اینچ) |
| ۳۰۴ آن | ۳۰ دقیقه. | ۷۵ دقیقه. | ۴۰ دقیقه. |
| ۳۰۴ یکچهارم سخت | ۷۵ دقیقه. | ۱۲۵ دقیقه. | ۱۲ دقیقه. |
| ۳۰۴ ½ سخت | ۱۱۰ دقیقه. | ۱۵۰ دقیقه. | ۷ دقیقه. |
| ۳۰۴L آن | ۲۵ دقیقه. | ۷۰ دقیقه. | ۴۰ دقیقه. |
| ۳۰۴L ¼ سخت | ۷۵ دقیقه. | ۱۲۵ دقیقه. | ۱۲ دقیقه. |
| 304L ½ سخت | ۱۱۰ دقیقه. | ۱۵۰ دقیقه. | ۶ دقیقه. |
| ۳۰۴ و ۳۰۴L | ||
| تراکم (پوند بر اینچ مربع) در دمای اتاق | 0.29 | |
| ماژول ارتجاعی در کشش (پوند بر اینچ مربع × ۱۰^۶) | 28 | |
| گرمای ویژه (بیتییو بر درجه فارنهایت بر پوند) | ۳۲ تا ۲۱۲ درجه فارنهایت | 0.12 |
| هدایت حرارتی (بیتییو بر ساعت بر فوت مربع بر فوت) | ۲۱۲ درجه فارنهایت | 9.4 |
| ۹۳۲ درجه فارنهایت | 12.4 | |
| ضریب متوسط انبساط حرارتی (اینچ در × ۱۰⁻⁶ به ازای هر درجه فارنهایت) | ۳۲ تا ۲۱۲ درجه فارنهایت | 9.2 |
| ۳۲ تا ۶۰۰ درجه فارنهایت | 9.9 | |
| ۳۲ تا ۱۰۰۰ درجه فارنهایت | 10.2 | |
| ۳۲ تا ۱۲۰۰ درجه فارنهایت | 10.4 | |
| مقاومت الکتریکی (میکرو اهم بر سانتیمتر) | در دمای ۷۰ درجه فارنهایت | 72 |
| دامنه نقطه ذوب (درجه فارنهایت) | ۲۵۵۰ تا ۲۶۵۰ | |
| مقاومت در برابر اکسیداسیون – سرویس مداوم (درجه فارنهایت) | 1,650 | |
| مقاومت در برابر اکسیداسیون – سرویس متناوب (درجه فارنهایت) | 1,500 |
| STANDARD | WERKSTOFF NR. | بدون سرویس | جیآیاس | بیاس | گست | آفنور | انگلیسی |
| استیل ۳۰۰۴ | 1.4301 | S30400 | استیل ضد زنگ ۳۰۰۴ | ۳۰۴S۳۱ | ۰۸Х۱۸ن۱۰ | Z7CN18‐09 | X5CrNi18-10 |
داکسون را انتخاب کنید و مشتریان خود را راضی کنید.

پاسخ سریع
We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule. Daxun’s stainless steel materials are of reliable quality, and their varieties, specifications and delivery weights strictly comply with the standards.
مزایای داکسون
Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel uses the ERP system to achieve full traceability of each angle steel, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.


304 Stainless Steel Angle Packaging
داکسون آلیاژ بهترین کیفیت بستهبندی را تضمین میکند، زیرا بستهبندی نقش مهمی در حملونقل بینالمللی دارد که کالاها از مسیرهای مختلف عبور میکنند تا به مقصد نهایی برسند؛ بنابراین ما توجه ویژهای به بستهبندی داریم. ما کالاهای خود را بسته به محصول به روشهای مختلف بستهبندی میکنیم. روشهای بستهبندی محصولات ما عبارتند از:
• جعبهها و صندوقها
• سلفون منقبضشونده
• پالتهای چوبی
• جعبههای چوبی
کیفیت، تحویل، بازرسی
- Daxun puts its products through a bunch of quality checks, including flattening, pitting and resistance, mechanical, and hardness tests, plus material identification and expansion tests, just to name a few. All this testing makes sure the material is right for your project.
- During production, we carefully measure the diameter, thickness, and surface of every product. We usually ship within 7-15 days. If you order a special size, it might take a little longer—up to 20 days.
Our delivery time is strictly by the contract. - از آژانسهای ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
- از ارائه نمونههای رایگان به مشتریان برای آزمایش پشتیبانی کنید.
- حمایت از بازرسی کارخانهای حضوری یا ویدیویی


304 Stainless Steel Angle Ordering Information
When you place an order, please let us know the quantity, grade, type, API5L reference, thickness, width, length, and any other specific needs you have, like chemical makeup, strength, heat treatment, extra testing, how it’s made, surface coating, or finish. Get in touch with Daxun today, and we’ll get back to you ASAP.
پشتیبانی فنی
If you need any extra technical help, our in-house metallurgist and knowledgeable team are happy to assist. Plus, Daxun has its own certified testing lab—the first of its kind in the multi-metal and plastic supply industry. We think this really shows how committed we are to quality and our goal of being a full-service supplier.

SS 304-304L Stainless Steel angle Features
داکسون آلیاژ به برند شما کمک میکند تا بهسرعت پیشرفت کند.
- جدول مشخصات
| Angle – Steel Data | |||||||||||||
| EQUAL AND UNEQUAL ANGLE | |||||||||||||
| ANGLE is available in other sizes on request | |||||||||||||
| Description | Width (W) | Depth (D) | ضخامت | استاندارد | Weight per | سطح | |||||||
| (mm) | (mm) | (T) (mm) | طول | Metre | Area per | ||||||||
| (کیلوگرم بر متر) | Metre | ||||||||||||
| (m²/m) | |||||||||||||
| ANGLE 20 X 20 X 3.0mm | 20 | 20 | 3 | 6.0 metres | 0.98 | 0.0897 | |||||||
| ANGLE 25 X 25 X 3.0mm | 25 | 25 | 3 | 7.5 metres | 1.12 | 0.0953 | |||||||
| ANGLE 25 X 25 X 5.0mm | 25 | 25 | 5 | 7.5 metres | 1.65 | 0.0953 | |||||||
| ANGLE 25 X 25 X 6.0mm | 25 | 25 | 6 | 7.5 metres | 2.08 | 0.0953 | |||||||
| ANGLE 30 X 30 X 2.5mm | 30 | 30 | 2.5 | 6.0 metres | 1.06 | 0.117 | |||||||
| ANGLE 30 X 30 X 3.0mm | 30 | 30 | 3 | 7.5 metres | 1.35 | 0.115 | |||||||
| ANGLE 30 X 30 X 5.0mm | 30 | 30 | 5 | 7.5 metres | 2.01 | 0.115 | |||||||
| ANGLE 30 X 30 X 6.0mm | 30 | 30 | 6 | 7.5 metres | 2.56 | 0.115 | |||||||
| ANGLE 40 X 40 X 2.5mm | 40 | 40 | 2.5 | 6.0 metres | 1.43 | 0.157 | |||||||
| ANGLE 40 X 40 X 3.0mm | 40 | 40 | 3 | 7.5 metres | 1.83 | 0.155 | |||||||
| ANGLE 40 X 40 X 4.0mm | 40 | 40 | 4 | 6.0 metres | 2.2 | 0.155 | |||||||
| ANGLE 40 X 40 X 5.0mm | 40 | 40 | 5 | 9.0 metres | 2.73 | 0.155 | |||||||
| ANGLE 40 X 40 X 6.0mm | 40 | 40 | 6 | 9.0 metres | 3.5 | 0.155 | |||||||
| ANGLE 45 X 45 X 3.0mm | 45 | 45 | 3 | 9.0 metres | 2.06 | 0.175 | |||||||
| ANGLE 45 X 45 X 5.0mm | 45 | 45 | 5 | 9.0 metres | 3.1 | 0.175 | |||||||
| ANGLE 45 X 45 X 6.0mm | 45 | 45 | 6 | 9.0 metres | 3.97 | 0.175 | |||||||
| ANGLE 50 X 50 X 2.5mm | 50 | 50 | 2.5 | 9.0 metres | 1.81 | 0.197 | |||||||
| ANGLE 50 X 50 X 3.0mm | 50 | 50 | 3 | 7.5 metres | 2.31 | 0.195 | |||||||
| ANGLE 50 X 50 X 4.0mm | 50 | 50 | 4 | 9.0 metres | 2.79 | 0.195 | |||||||
| ANGLE 50 X 50 X 5.0mm | 50 | 50 | 5 | 9.0 metres | 3.48 | 0.195 | |||||||
| ANGLE 50 X 50 X 6.0mm | 50 | 50 | 6 | 9.0 metres | 4.46 | 0.195 | |||||||
| ANGLE 50 X 50 X 8.0mm | 50 | 50 | 8 | 9.0 metres | 5.68 | 0.195 | |||||||
| ANGLE 55 X 55 X 5.0mm | 55 | 55 | 5 | 9.0 metres | 3.84 | 0.215 | |||||||
| ANGLE 55 X 55 X 6.0mm | 55 | 55 | 6 | 9.0 metres | 4.93 | 0.215 | |||||||
| ANGLE 65 X 50 X 5.0mm | 65 | 50 | 5 | 9.0 metres | 4.02 | 0.225 | |||||||
| ANGLE 65 X 50 X 6.0mm | 65 | 50 | 6 | 9.0 metres | 5.16 | 0.225 | |||||||
| ANGLE 65 X 50 X 8.0mm | 65 | 65 | 8 | 9.0 metres | 6.59 | 0.225 | |||||||
| ANGLE 65 X 65 X 4.0mm | 65 | 65 | 4 | 9.0 metres | 3.69 | 0.255 | |||||||
| ANGLE 65 x 65 x 5.0mm | 65 | 65 | 5 | 9.0 metres | 4.56 | 0.255 | |||||||
| ANGLE 65 X 65 X 6.0mm | 65 | 65 | 6 | 9.0 metres | 5.87 | 0.255 | |||||||
| ANGLE 65 X 65 X 8.0mm | 65 | 65 | 8 | 9.0 metres | 7.51 | 0.255 | |||||||
| ANGLE 65 X 65 X 10.0mm | 65 | 65 | 10 | 9.0 metres | 9.02 | 0.255 | |||||||
| ANGLE 75 X 50 X 5.0mm | 75 | 50 | 5 | 9.0 metres | 4.4 | 0.244 | |||||||
| ANGLE 75 X 50 X 6.0mm | 75 | 50 | 6 | 9.0 metres | 5.66 | 0.244 | |||||||
| ANGLE 75 X 50 X 8.0mm | 75 | 50 | 8 | 9.0 metres | 7.23 | 0.244 | |||||||
| ANGLE 75 X 75 X 4.0mm | 75 | 75 | 4 | 9.0 metres | 4.29 | 0.295 | |||||||
| ANGLE 75 X 75 X 5.0mm | 75 | 75 | 5 | 9.0 metres | 5.27 | 0.292 | |||||||
| ANGLE 75 X 75 X 6.0mm | 75 | 75 | 6 | 9.0 metres | 6.81 | 0.292 | |||||||
| ANGLE 75 X 75 X 8.0mm | 75 | 75 | 8 | 9.0 metres | 8.73 | 0.292 | |||||||
| ANGLE 75 X 75 X 10.0mm | 75 | 75 | 10 | 9.0 metres | 10.5 | 0.292 | |||||||
| ANGLE 90 X 90 X 6.0mm | 90 | 90 | 6.0 | 9.0 metres | 8.22 | 0.352 | |||||||
| ANGLE 90 X 90 X 8.0mm | 90 | 90 | 8.0 | 9.0 metres | 10.6 | 0.352 | |||||||
| ANGLE 90 X 90 X 10.0mm | 90 | 90 | 10.0 | 9.0 metres | 12.7 | 0.352 | |||||||
| ANGLE 100 X 75 X 6.0mm | 100 | 75 | 6.0 | 9.0 metres | 7.98 | 0.342 | |||||||
| ANGLE 100 X 75 X 8.0mm | 100 | 75 | 8.0 | 9.0 metres | 10.3 | 0.342 | |||||||
| ANGLE 100 X 75 X 10.0mm | 100 | 75 | 10.0 | 9.0 metres | 12.4 | 0.342 | |||||||
| ANGLE 100 X 100 X 10.0mm | 100 | 100 | 10.0 | 9.0 metres | 14.2 | 0.392 | |||||||
| ANGLE 100 X 100 X 12.0mm | 100 | 100 | 12.0 | 9.0 metres | 17.7 | 0.392 | |||||||
| ANGLE 100 X 100 X 4.0mm | 100 | 100 | 4.0 | 9.0 metres | 5.78 | 0.395 | |||||||
| ANGLE 100 X 100 X 6.0mm | 100 | 100 | 6.0 | 9.0 metres | 9.16 | 0.392 | |||||||
| ANGLE 100 X 100 X 8.0mm | 100 | 100 | 8.0 | 9.0 metres | 11.8 | 0.392 | |||||||
| ANGLE125 X 75 X 6.0mm | 125 | 75 | 6.0 | 9.0 metres | 9.16 | 0.392 | |||||||
| ANGLE 125 X 75 X 8.0mm | 125 | 75 | 8.0 | 9.0 metres | 11.8 | 0.392 | |||||||
| ANGLE 125 X 75 X 10.0mm | 125 | 75 | 10.0 | 9.0 metres | 14.2 | 0.392 | |||||||
| ANGLE 125 X 75 X 12.0mm | 125 | 75 | 12.0 | 9.0 metres | 17.7 | 0.392 | |||||||
| ANGLE 125 X 125 X 8.0mm | 125 | 125 | 8.0 | 9.0 metres | 14.9 | 0.491 | |||||||
| ANGLE 125 X 125 X 10.0mm | 125 | 125 | 10.0 | 9.0 metres | 18 | 0.491 | |||||||
| ANGLE 125 X 125 X 12.0mm | 125 | 125 | 12.0 | 9.0 metres | 22.5 | 0.491 | |||||||
| ANGLE 125 X 125 X 16.0mm | 125 | 125 | 16.0 | 9.0 metres | 29.1 | 0.491 | |||||||
| ANGLE 150 X 90 X 8.0mm | 150 | 90 | 8.0 | 9.0 metres | 14.3 | 0.471 | |||||||
| ANGLE 150 X 90 X 12.0mm | 150 | 90 | 12.0 | 9.0 metres | 21.6 | 0.471 | |||||||
| ANGLE 150 X 90 X 16.0mm | 150 | 90 | 16.0 | 9.0 metres | 27.9 | 0.471 | |||||||
| ANGLE 150 X 100 X 10.0mm | 150 | 100 | 10.0 | 9.0 metres | 18 | 0.491 | |||||||
| ANGLE 150 X 100 X 12.0mm | 150 | 100 | 12.0 | 9.0 metres | 22.5 | 0.491 | |||||||
| ANGLE 150 X 150 X 10.0mm | 150 | 150 | 10.0 | 9.0 metres | 21.9 | 0.59 | |||||||
| ANGLE 150 X 150 X 12.0mm | 150 | 150 | 12.0 | 9.0 metres | 27.3 | 0.59 | |||||||
| ANGLE 150 X 150 X 16.0mm | 150 | 150 | 16.0 | 9.0 metres | 35.4 | 0.59 | |||||||
| ANGLE 150 X 150 X 19.0mm | 150 | 150 | 19.0 | 9.0 metres | 42.1 | 0.59 | |||||||
| ANGLE 150 X 90 X 10.0mm | 150 | 90 | 10.0 | 9.0 metres | 17.3 | 0.471 | |||||||
| ANGLE 200 x 200 x 13.0mm | 200 | 200 | 13.0 | 9.0 metres | 40 | 0.788 | |||||||
| ANGLE 200 X 200 X 16.0mm | 200 | 200 | 16.0 | 9.0 metres | 48.7 | 0.788 | |||||||
| ANGLE 200 X 200 X 20.0mm | 200 | 200 | 20.0 | 9.0 metres | 60.1 | 0.788 | |||||||
| ANGLE 200 X 200 X 26.0mm | 200 | 200 | 26.0 | 9.0 metres | 76.8 | 0.788 | |||||||
SS 304 /304L Stainless Steel Angle Surface Type (3)
اطلاعات موجود برای مرجع و دانلود
Daxun is a trustworthy stainless steel Angle manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel angles have fewer defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
پروژهها و محصولات داغ اخیر
محصولات مرتبط (8)
Leading stainless steel angle Suppliers in China
Daxun has been engaged in international business for more than ten years. In 2023, the export volume exceeded 100 million US dollars, and the export volume ranked among the top Chinese stainless steel manufacturers. Daxun continuously improves its service skills. To serve the global market, it has established three export service facilities in China, cooperating with engineering companies, steel mills, and international trading companies. Daxun provides stainless steel chain services and has established long-term cooperative relations with dozens of well-known steel mills around the world. The inventory includes 50,000 tons of conventional stainless steel and 20,000 tons of duplex steel, nickel-based alloys, heat-resistant steel and other metals. Daxun’s stainless steel materials are of stable quality, and the varieties, specifications, and delivery weights strictly meet the standards.
304 stainless steel angle
- 304 stainless steel angle bar is a structural shape composed of AISI 304, or simply 304 stainless steel. This alloy is a versatile and commonly used stainless steel composed of chromium (18-20%), nickel (8-10.5%), and a trace of carbon (up to 0.08%). The inclusion of these elements provides 304 stainless steel with exceptional corrosion resistance, durability, and mechanical qualities, making it appropriate for a wide range of applications.
- Angle bars are L-shaped cross-sections having two legs at 90-degree angles. They are normally available in two leg lengths: equal (both sides are the same length) and uneven (one side is longer than the other). Angle bar dimensions may vary according to the application and production norms.
- Because of its chromium and nickel composition and ease of production, it has good corrosion resistance and is suitable for a wide range of applications. Its surface treatment makes everything from kitchen utensils to building facades look smooth and lovely. Other benefits include minimal maintenance costs and durability, making this stainless steel an affordable option for designs ranging from utilitarian to elaborate or extravagant.
Large inventory
-
Because we keep so much stock in so many different sizes, we’re sure to have the right product for you. Our angles are easy to cut, machine, and shape, and the low-carbon material handles both hot and cold temperatures really well. Like all stainless steel, it’s easy to keep clean and looking good, with a nice, high-quality finish.
MEETING CUSTOMER REQUIREMENTS
-
We can supply angles in standard lengths or cut them to the exact size you need. We do all our cutting ourselves, either at our main warehouse or through our three service centers across China. Because we keep so much stock on hand, we can be your one-stop shop for all your stainless steel needs.
Stainless Steel Angle Applications
Stainless steel angles, especially those made from 304 stainless steel, are used in tons of different applications across many industries, including:
- هوافضا
- Architectural
- ساختمانسازی
- شیمیایی
- فرآوری مواد غذایی
- Oil & Gas
- And more
Stainless Angle Benefits
There are lots of advantages to using 304 stainless steel angles. These benefits make them really useful for many different jobs. Here are some of the key advantages:
- Good corrosion resistance
- Easily machined
- غیرمغناطیسی
- Good strength-to-weight ratio
- Damage resistant
- Excellent long-term value
زاویه فولاد ضد زنگ ۳۰۴
-
304 stainless steel is the most popular type of stainless steel used today. It’s not magnetic and can’t be heat-treated, so it has to be shaped by cold working. It’s very resistant to corrosion and easy to machine. Because it’s strong but lightweight and resistant to damage, it’s perfect for lots of different uses, including machinery, food processing equipment, furniture, and many other things.
Why should you buy stainless steel angles from Daxun?
Daxun’s goal is to give you the highest quality and most durable stainless steel angles and steel. We offer loads of stainless steel angles in all kinds of sizes (leg lengths and thicknesses) and material grades. We make our 316/316L and 304/304L stainless steel angles in our state-of-the-art factory, using top-quality raw materials and the latest technology, all overseen by experienced workers.
Here are some of the big advantages of working with us:
- When you purchase any steel products from us, you get the products directly from the manufacturer.
- Our employees are dedicated to providing the lowest prices and fastest shipping times so that you can start your project right away!
- We have a skilled, capable workforce for quality checks, packaging, and shipping.
- We follow multiple quality check levels, which helps ensure that the products are of the highest standards.
- We have a qualified and dedicated support team available 24×7 to help you out if any issues arise.
Suppliers from China Make Stainless Steel Angles to Size
-
Daxun is a leading supplier of stainless steel products in China. With high-quality products and customized services, we can meet all your stainless steel angle needs. Order online or by phone and get it delivered in as fast as 15 days.
304 and 316 Grade Stainless Steel Angles
- This handy right-angle steel is super versatile and comes in 304/304L and 316/316L grades. 304 is the most popular and widely used, perfect for most general applications. It’s easy to weld, and shape, and resists corrosion well. Sometimes called 18/8 stainless steel because it’s made of 18% chromium and 8% nickel, 304 works great for most jobs.
- If you need something for tougher conditions, like saltwater or highly industrialized areas, 316 is a better choice. With more nickel and added molybdenum, it’s even more resistant to corrosion than 304, especially against chlorides and chlorinated solutions. It’s still weldable, but a bit harder to work with than 304.
There are two basic processes for manufacturing stainless steel angles:
- We use two main ways to make our angles: laser melting and hot rolling. Hot-rolled angles are less expensive, but they usually have rounded or tapered edges. Laser-melted angles have sharp, consistent, square corners and a smoother, sandblasted finish—they just look and feel nicer.
Choose Your Size and Size
- We offer a huge range of stainless steel angles, so we’ve got something for everyone. Our 304 stainless steel angles come in various sizes, with thicknesses from 3mm to 16mm and lengths of 1m, 3m, or 6m.
- Our grade 316 angles come in thicknesses from 3mm-16mm and lengths of 1m, 3m, or 6m. Angles are available in a variety of sizes.
Talk to Your Preferred Stainless Steel Angle Supplier
-
It’s super easy to buy our stainless steel angles and other products! You can order right on our website. Or, if you prefer, call our sales team in China at +8613382898899. They’ll be happy to help you place your order. If you have any questions, just send an email to daxunalloy@gmail.com and we’ll get back to you as soon as possible.
لطفاً فرم صفحه “تماس با ما” را پر کنید یا با مدیر فروش ما به شماره +86 13382898899 تماس بگیرید؛ ما در اسرع وقت با شما تماس خواهیم گرفت. واتساپ ما آنلاین است و ایمیل (Daxunalloy@gmail.com) ظرف ۶ ساعت بررسی میشود. به هر پرسش یا پیام بهسرعت پاسخ داده خواهد شد. علاوه بر این، ما هر هفته اطلاعات بازار را با مشتریان خود به اشتراک میگذاریم.
نمونهها میتوانند بهصورت رایگان ارائه شوند، اما هزینه حمل بر عهده مشتری است و پس از همکاری بازپرداخت خواهد شد.
ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشتهایم.
我们的 316L 不锈钢角钢最小起订量为 1 吨。
我们从原材料采购到加工、出货安排都有一套完整的组织机构,整个链条都有跟单人员和质检人员按照严格的要求进行查找和检查,也欢迎第三方检验。
试订单一周内即可发货,常规订单大约需要两周时间。