Stainless steel checkered plate

Stainless Steel Checkered Plate & Anti-skid Plate

  • Daxun is the world’s leading stainless steel checkered plate.
  • Supplier and stainless steel checkered plate manufacturer.
  • We produce high-quality stainless steel checkered plate.

Daxun stainless steel checkered plate

  • Daxun has a standing stainless steel checkered plate inventory of 30,000 tons.
  • It is divided into cold-rolled thin plates and hot-rolled medium and thick plates.
  • Daxun Alloy provides stainless steel checkered plates with various patterns.

Daxun stainless steel checkered plate introduction

Product Parameters: Stainless Steel Checkered Plate
نمره 201,304,304L,316,316L,317,321,309,310S,2205,2507,904L,409,410,420,430,436,444,441,17-4 etc.
عرض 10mm~2500mm
ضخامت 0.2mm~100mm Thickness tolerance
+/-0.03mm
استاندارد ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2
specification 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L
Mill Origin TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc.
Certification ISO, SGS, BV, TUV,CE etc

What is stainless steel checkered plate & stainless steel anti-slip plate?

Stainless steel checkered plate is a type of stainless steel sheet with raised patterns on its surface, which is processed by mechanical equipment to create designs such as diamond, lentil, or other embossed patterns. This type of plate began to be produced in small batches by large rolling mills in Europe in the early 1960s and has gradually developed and become popular since then.
Stainless steel checkered plate features a beautiful metallic texture, and its rapid rise is closely related to social development and changes in people’s aesthetic preferences. In addition to its aesthetic appeal, this plate also has excellent anti-slip performance, which is why it is often referred to as stainless steel anti-slip plate.
Stainless steel anti-slip plate is highly favored for its excellent slip resistance and corrosion resistance, and is widely used in various fields. In the construction industry, it is commonly used as flooring for factories and workshops and as stair treads, where its anti-slip properties ensure pedestrian safety. In shipbuilding, it is an ideal material for decks, providing good slip resistance to prevent crew members from slipping. Additionally, it is also widely used in places such as shopping malls, hospitals, and kitchens.
Stainless steel checkered plates come in various types based on different pattern designs. The most common types include diamond pattern, which offers excellent slip resistance and is widely used in industrial applications; lentil pattern, known for its decorative appearance and moderate anti-slip properties; and round pattern, which provides a unique aesthetic while maintaining good functionality. Other specialized patterns include finger-proof designs that minimize fingerprint visibility and custom patterns tailored for specific architectural or industrial requirements. Each type is designed to meet specific functional and aesthetic needs in different applications.

Checkered Plate Pattern Examples
Checkered Plate Pattern Examples

 

Beyond the standard functional patterns, stainless steel checkered plates also include decorative variants that cater primarily to aesthetic applications. These decorative plates feature intricate designs, artistic patterns, and even custom graphics that transform them into architectural elements. They are commonly used in interior design, wall cladding, elevator panels, and decorative partitions where visual appeal is as important as functionality. Some decorative variants combine different surface treatments like etching, PVD coating, or color printing with the embossed patterns to create stunning visual effects. These specialized decorative plates allow architects and designers to achieve both practical and artistic goals in their projects, making stainless steel checkered plate a versatile material that bridges the gap between industrial utility and architectural elegance.

بیشتر بخوانید

stainless steel checkered plate grades and characteristics

Each stainless steel plate material has its own different usage scenarios.

stainless steel checkered plate

201 stainless steel plate has low cost and is suitable for building decoration materials, equipment and machinery casings, etc.

Corrosion resistant,Suitable for building decoration, food and medicine, machinery and equipment, etc.

Corrosion resistant,Suitable for chemical equipment, food and medicine, mechanical equipment

Corrosion resistant,Suitable for chemical energy, marine engineering, mechanical equipment

Corrosion resistant,Suitable for chemical energy, marine engineering, mechanical equipment, etc.

Corrosion resistant,High temperature resistance,Suitable for chemical energy, marine engineering, mechanical equipment.

Corrosion resistant,High temperature resistance,Suitable for boiler equipment, heat-resistant equipment, mechanical equipment.

high strength,Suitable for refining industry, petrochemical and marine industry.

16 Products Found.

Performance of stainless steel plate

مقاومت در برابر خوردگی

The chemical compositions on stainless steel sheets protect them from rust. Their corrosion resistance feature increases with necessarily polished finishes, perfect for kitchen appliances.

Low-Cost

Since SS sheets have a lower melting point, they don’t need special tools. They are also durable and lasting materials, making industries save on working and maintenance costs.

Valuable Metal

The smarter option material SS sheets have far lesser drawbacks than other alloys. They provide excellent value, cost-effectiveness, and durability. SS is an easy-to-clean metal material.

Workability

Stainless steel sheet materials are excellent options for various applications, like fabrications. They are simple to work with and ideal for massive industrial and intricate usage.

Huge Stock Choiceable Material

With choiceable material from the very start comes our high quality stainless steel products.Daxun have stainless steel inventories for common grades and common sizes to ensure fast response to our customers’ demand.

Stainless Steel Sheet Finishes Options

  • Brushed Finish: This finish looks like straight hair, known as a hairline finish.
  • Sandblasted: The sandblasted surface results in a bead-blasted sheet finish with an even matte surface.
  • Mirror Finish: It is also called a mirror-polished sheet. This finish is processed with high-gloss and non-directional polished.
  • Etched Finish: This finish is achieved by using electrochemical techniques. It is a lasting etched pattern with high accuracy.
  • Embossed Finish: This finish comes with unique and stunning designs, forming concave-convex textures.

Strict Quality Control

Daxun cuts and finishes high quality stainless steel to your exact size specifications. Stainless steel sheets are fully certified. As a proud member of BSSA and ISO 9001 certified, all our stainless steel sheets are sourced from reliable factories and must pass our stringent quality control procedures before delivery to our warehouse.We will carry out strict quality control for every production from the very start till the end, to ensure the goods to be received will be a great satisfaction to you.

Stainless steel plate processing and customization

We have laser cutting machines, water jet cutting machines, CNC bending machines, CNC shearing machines. We can provide customized processing services for stainless steel plate cutting and bending. You just need to provide us with the drawings and we can customize it according to the size of your stainless steel plate.

Packaging of Stainless Plates

Packing method

At Daxun, we choose different packaging for different stainless steel products, including: kraft paper, wooden boxes, woven bags, wooden pallets, based on the highest industry standards to ensure that the goods arrive in your hands in good condition.

Material Test Certification

All our stainless steel materials are certified by different industry standards such as ISO9001:2008, ISO14001:2014, AAA Certification, CQGC Certifications, and more. Our company also have certifications from ISO9001:2015 quality management system.

Actual Weight & Good Quality

At Daxun, we have testing laboratory and equipment to ensure that our stainless steel materials are in actual weight and good quality before shipment. Our strict quality control team also performs strict and 100% inspection on all production stages.

Excellent After-Sales Services

Our support and services are not only limited from the beginning of our transactions. Even if you have received your orders, TuoLian will continue to provide excellent after-sales services. We will continue providing assistance and warranty to your orders.

Stainless Steel plate application cases in different industries

تزئینات ساختمان

Stainless steel plates are widely used in the construction field and can be used for exterior wall decoration, interior decoration, roofing materials, building structures, etc. Stainless steel plates have beautiful appearance and high strength, and can meet the design needs of different buildings.

Mechanical equipment

Stainless steel plates have the advantages of corrosion resistance, no rust, no discoloration, easy removal of attached food, and good high and low temperature mechanical properties. They are widely used in food machinery, such as sanitation systems, fluid pipe troughs, food storage tanks, thermal Exchangers, vacuum vessels, etc.

هوافضا

Stainless steel plates have good strength, toughness and corrosion resistance and are widely used in aircraft structural parts. For example, the wing structure, fuselage supports, seats and other parts are all made of stainless steel.

Petrochemical

The manufacturing and maintenance of petroleum refining equipment also uses 321-316L and other brands of medium-thick plates and cold-rolled stainless steel sheets for petrochemical containers (usually 0.3-0.6mm, 1219-1520mm, SUS316, surface condition is NO.2B/2D)

military armor

Main application parts: wing skin, wing stringers, upper and lower edge strips of wing spar, web, fuselage stringers, seat rails, keel beam, side frames, fuselage skin, lower fuselage wall panels, Main floor stringers, etc.

Ship field

Stainless steel plates are widely used in the shipbuilding industry. The stainless steel plates supplied by Daxun are used in the shipbuilding and petroleum industries. They have high strength, good toughness, and are resistant to seawater corrosion, fatigue, and wear resistance.

مهندسی دریایی

SS316L is the primary austenitic stainless steel grade used in offshore installations, where it enhances strength at high temperatures and protects structures from severe acidic environments.There are also duplex stainless steels, which offer an excellent combination of mechanical properties and resistance to stress corrosion cracking, making them ideal for offshore applications. UNS S32205 steel is the most commonly used duplex stainless steel grade for offshore installations.

Electric power field

The application of stainless steel in electricity is mainly for the processing and manufacturing of large turbine units in power stations. Stainless steel’s excellent corrosion resistance and high strength make it the preferred material for power generation components.

about-feature3
Let us be your trustworthy stainless steel plate supplier

Our stainless steel panels are fully certified and traceable. We provide the highest quality stainless steel plates to leading industries such as building decoration, industrial equipment, chemical energy, shipbuilding and petrochemicals.

Our stainless steel plate stock sizes

Thickness (mm) Width (mm) Length (mm) Comment
0.5 1000/1219/1500 2000/2438/3000 AAA
0.8 1000/1219/1500 2000/2438/3000 AAA
1.0 1000/1219/1500 2000/2438/3000 AAA
1.5 1000/1219/1500 2000/2438/3000 AAA
2.5 1000/1219/1500 2000/2438/3000 AAA
3.0 1000/1219/1500 2000/2438/3000 AAA
5.0 1500/1800/2000 3000/6000/8000 AAA
6-8.0 1500/1800/2000 3000/6000/8000 AAA
1.0-20.0 1500/1800/2000 3000/6000/8000 AAA
20.0-50.0 1500/1800/2000 3000/6000/8000 AAA
50.0+ 1500/1800/2000 3000/6000/8000 AAA
Tolerances
                                       رتبه تحمل
اندازه گروه ۱ گروه ۲ گروه ۳ وضعیت تحویل وضعیت سطح
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39 نورد سرد دو بی
دو بعدی
کارشناسی هنر
خط موی سر
شمارهٔ ۳
شمارهٔ ۴
۶ کیلومتر
کیوکیو
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9 وضعیت تحویل شمارهٔ یک
شمارهٔ ۳
شمارهٔ ۴
۶ کیلومتر
کیوکیو
شور شده
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
توجه:
۱. در صورتی که به وضعیت تحویل متفاوتی از موارد فوق نیاز دارید، لطفاً با ما هماهنگ فرمایید.
۲. در صورت هرگونه پرسش یا سفارش، لطفاً ما را از هرگونه نیاز اضافی که در اینجا ذکر نشده است، مطلع سازید.
Finish Designation Method and degree of finish
شمارهٔ یک After hot rolling, heat treatment, pickling or other equivalent treatment is applied.
No.2D Annealing and pickling are performed after cold rolling; material is soft with surface of silver-white luster; used for general applications and deep drawing.
No.2B After 2D finish, skin pass rolling is performed to obtain a more suitable luster; the surface becomes very exquisite; used for general applications.
شمارهٔ ۳ Intermediate 100-120 grit finish; used for applications in which surface polishing is performed after shaping.
شمارهٔ ۴ General 150-180 grit finish; used for restaurants and kitchen equipment and tools.
#240 240 grit finish; used when a finer finish than No. 4 is required; typically for restaurants and kitchen equipment and tools.
#320 320 grit finish polished product.
HL This finish is performed by continuous linear polishing using an abrasive of appropriate grain size; mainly used for architectural applications.
کارشناسی هنر Achieved by performing bright annealing after cold rolling and then skin pass rolling to obtain even greater reflectance; provides excellent corrosion resistance; used for household appliances, kitchen equipment, and automobiles.
کیوکیو Through multiple grinding, it achieves very high brightness and smoothness, like a mirror.
  • “Thank you Daxun for the extremely durable, world-class quality stainless steel plate. I also appreciate the professional customization service. I am happy to work with you for my stainless steel plate needs. Looking forward to working with you next time!”

    Testimonials from customers located in the Middle East
  • “Daxun has always been a trustworthy company when it comes to stainless steel plates. All the stainless steel plates I purchased are of very high quality. I ordered stainless steel plates at a very low price at Daxun. The staff was also happy to answer my questions .” Asked questions and was impressed with my needs! “

    Testimonials from customers located in Europe and the United States
  • “We were very impressed with the quality and superiority of Daxun stainless steel plates. There are a variety of sizes available that fit our needs perfectly. Additionally, we really appreciate the affordable price and service.”

    Testimonials from customers located in Russia

داکسون آلیاژ

Regarding stainless steel plates, we can handle any type of inquiry. Please feel free to ask us. We will make recommendations based on each client’s needs.

Stainless Steel Sheets from Well-Known Suppliers in China.

Buy stainless steel sheets (also known as steel sheets) with various finishes from well-known suppliers in China. You only need to look once for a stainless steel sheet supplier, because Daxun offers free cutting and fast delivery, as fast as 1-2 days.

All stainless steel sheets have a variety of different finishes.

Our stainless steel sheets come in a variety of different beautiful finishes: brushed, 2B smooth, 8K mirror and round polished, etc.

Each of our stainless steel sheet metal products comes with a film covering the final surface. After installation or fabrication, it can be easily torn off to protect the surface of the material from wear and marks. The back part is not filmed.

The most commonly used type of stainless steel is 300 series stainless steel sheet. It has good formability, good corrosion resistance and easy welding.

We can provide you with any size of stainless steel sheet you need.

Our stainless steel sheets are available in three coatings and a wide range of sizes to meet your specific needs. In addition, since we provide free unlimited cutting services, we can easily meet any unique size you may need.

We can meet any size requirement, ranging from 0.3mm to 30mm in thickness, and from 50mm x 50mm to 2500mm x 1250mm in size. In addition, we offer free unlimited cutting with every transaction, using first-class cutting machines to precisely meet your needs.

Buy stainless steel plates by phone or online.

Ordering stainless steel plates has never been easier. Just follow the simple step-by-step instructions on our website. You can also contact our sales team by email at daxunalloy@gmail.com or phone +8613382898899. They will be happy to accept your purchase and answer any questions you may have.

We have three shipping methods for you to choose from, including ship, land and air. Daxun hopes to deliver the goods to you quickly and safely every time.

Important Safety Note:

The edges of the metal plates we sell are not polished, ground or finished, so they may be sharp like any other stainless steel plates. We advise customers to handle, install and use these products with care.

Do you have any stock in stock?

Yes, we have complete specifications and inventory and can quickly meet your needs.

Can it be customized?

Yes, it can be customized. You can contact us and send us the customized specifications and quantity.

How do you ship the goods?

Our transportation methods generally include sea transportation, land transportation, and sea transportation. Reach you quickly and safely.

What's your price like?

Because our output is high, the cost will be much lower, so the price is low.

می‌توانم چند نمونه بگیرم؟

ما می‌توانیم نمونه‌های ورق فولاد ضدزنگ را برای بررسی کیفیت در اختیار شما قرار دهیم. نمونه رایگان است و شما فقط هزینه حمل را پرداخت می‌کنید.

کیفیت شما چگونه است؟

We attach great importance to product quality and have passed various quality system tests.

همین امروز استعلام خود را ارسال کنید