x
همین امروز استعلام خود را ارسال کنید
استعلام سریع

Daxun is an excellent manufacturer of grade 7 (Ti-0.15Pd) titanium rods and bars.

  • Titanium bar grade: Grade 7-Ti / UNS R52400
  • انواع میله‌های تیتانیوم: میله‌های نوردشده، میله‌های کشیده، میله‌های آهنگری‌شده
  • Titanium bar density: The density of grade 7 titanium is 4.51 g/cm³
  • استانداردهای اصلی: ASTM ASME GB GJB EN JIS DIN ISO ATP BS و غیره.
  • High corrosion resistance, excellent weldability, superior strength, lightweight, and outstanding performance in aggressive environments.

پیشرو جهانی در خدمات تولید میله‌های تیتانیوم خالص تجاری

Daxun, specializing in the production of alloy titanium rods for extreme environments—Grade 7 titanium alloy rods.

Grade 7 titanium bar (Ti Grade 7 / UNS R52400) is a palladium-enhanced, commercially pure (CP) titanium alloy specifically engineered for supreme corrosion resistance in aggressive environments. It consists of titanium (≥99%) with a critical addition of 0.12–0.25% palladium (Pd), which fundamentally alters its electrochemical behavior. This palladium modification dramatically improves resistance to reducing acids (e.g., sulfuric, hydrochloric, phosphoric), chloride solutions (including seawater and brines), and crevice/pitting corrosion—scenarios where standard CP grades like Grade 2 would rapidly degrade. While retaining the inherent advantages of titanium—low density (~4.5 g/cm³), high strength-to-weight ratio, excellent weldability, and biocompatibility—Grade 7 exhibits superior performance at elevated temperatures (up to ~400°C/750°F) and in highly oxidizing or acidic conditions. Its passive oxide layer, stabilized by palladium, provides unparalleled protection against chemical attack, making it one of the most corrosion-resistant metallic materials available.

Where is Grade 7 titanium bar used?

Grade 7 titanium bar is extensively used in chemical processing for critical components like valve stems, pump shafts, fasteners, and instrumentation components handling acids, chlorides, or organic solvents. In marine and offshore engineering, it serves in seawater desalination equipment, heat exchanger components, and subsea fastening systems exposed to high-salinity environments. The alloy also excels in pollution control systems (e.g., scrubber components), pharmaceutical manufacturing equipment, and medical implants (e.g., surgical instruments and orthopedic devices) due to its inertness and longevity. Despite its higher initial cost—driven by palladium content—Grade 7 delivers exceptional lifecycle value by minimizing downtime, maintenance, and replacement costs in corrosive service. Its reliability in preventing catastrophic failures ensures safety and efficiency in applications ranging from nuclear waste containment to aerospace fluid systems, justifying its selection as a premium solution for the most demanding corrosion challenges.

داکسون شرکت تولید میله‌های آلیاژ تیتانیوم مورد اعتماد شما است. داکسون تمام گریدهای آلیاژ تیتانیوم، از جمله سری تیتانیوم خالص تجاری (CP)، سری آلیاژ تیتانیوم، آلیاژ تیتانیوم نیکل و غیره را تولید می‌کند. این محصولات عملکرد قابل اعتمادی دارند و عملکرد بالایی را برای کاربردهای حیاتی شما فراهم می‌کنند. در صنایع و کاربردهای مختلف، می‌توانید برای مقاومت در برابر شرایط دمایی بالا و محیط‌های خورنده، روی میله‌های آلیاژ تیتانیوم داکسون حساب کنید. ده‌ها سال است که شرکت Daxun Metals متعهد به تولید راه‌حل‌های آلیاژ تیتانیوم با مهندسی پیشرفته برای پاسخگویی به سخت‌ترین چالش‌ها بوده است.

بیشتر بخوانید

داده‌ها

مشخصات جزئیات
مواد Titanium rod and bar Grade 7 (UNS R52400)
استاندارد ASTM B348, ASTM SB348, AMS 4921, AMS 4902
ابعاد EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN
محدوده قطر 0.125″ – 14″ (3.175mm – 355.6mm), custom
محدوده طول Up to 240″ (6096mm), custom
پایان Cold (bright) drawn, centerless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centerless Ground & Black
پایان‌کاری سطح کشیده شده سرد، بدون مرکز تراشیده شده، صیقلی، یا تراش‌خورده خام، مشکی، پرداخت شماره ۴، پرداخت BA، پرداخت مات، و غیره.
وضعیت سخت‌شده و تمپرشده، آنیل‌شده
بردباری Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm)
فرم میله‌های مربعی تیتانیوم، شمش‌های تیتانیوم، میله‌های گرد تیتانیوم، میله‌های مستطیلی تیتانیوم، میله‌های مثلثی تیتانیوم، میله‌های کوبیده‌شده تیتانیوم، میله‌های شش‌ضلعی تیتانیوم و غیره.
عنصر نماد Composition Range (wt.%)
تیتانیوم تیتانیوم Balance (>99%)
Palladium Pd 0.12–0.25%
آهن آهن ≤0.30%
اکسیژن O ≤0.25%
کربن C ≤0.08%
نیتروژن N ≤0.03%
هیدروژن H ≤0.015%
عناصر دیگر Each ≤0.40% (single element)

 

مالکیت Value (Imperial) Value (Metric)
مقاومت کششی 50,000–65,000 psi 345–450 MPa
مقاومت تسلیم 30,000–45,000 psi 207–310 MPa
Elongation 20–30% 20–30%
سختی (برینل) 120–160 HB 120–160 HB
ماژول ارتجاعی 14.9–16.0 × 10⁶ psi 103–110 GPa
مالکیت Value (Imperial) Value (Metric)
تراکم 0.163 lb/in³ 4.51 g/cm³
نقطه ذوب 3,000–3,050°F 1,650–1,680°C
هدایت حرارتی 9.5 Btu/(hr·ft·°F) 16.4 W/(m·K)
Coefficient of Thermal Expansion 4.8 × 10⁻⁶/°F 8.6 × 10⁻⁶/K
مقاومت الکتریکی 1.78 × 10⁻⁶ Ω·cm 1.78 μΩ·m

 

داکسون را انتخاب کنید تا به پروژه‌تان کمک کند اوج بگیرد.

همین حالا با داکسون تماس بگیرید

مزایای کارخانه داکسون

مفهوم “مدیریت تعالی عملکرد” شرکت داکسون مدل مدیریتی “PDCA + Lean” را ترویج می‌کند. کارت ویزیت شرکت عبارت “داکسون = کیفیت قابل اعتماد” را نشان می‌دهد. داکسون از سیستم ERP برای دستیابی به قابلیت ردیابی کامل تنوع، مشخصات و منشأ هر میله تیتانیوم استفاده می‌کند و از مبارزه با جعل در صنعت حمایت و تشویق می‌کند. داکسون برای پردازش و سفارشی‌سازی به فناوری متکی است و دقت بالا و کیفیت بالا معیارهای صنعت محسوب می‌شوند؛ از نظر خدمات، مدیریت چرخه عمر محصول را ترویج می‌دهد، پیش از فروش راه‌حل‌های حرفه‌ای انتخاب و پردازش مواد را ارائه می‌کند، در حین فروش نظارت دقیقی دارد و پس از فروش ضمانت‌های خدمات بی‌دغدغه ارائه می‌دهد.

همین حالا با داکسون تماس بگیرید

Grade 7 Titanium Rod Production Method

داکسون میله‌های تیتانیومی با کیفیت بالا و عملکرد عالی تولید می‌کند و همچنین می‌تواند طبق توافق مشتری تولید نماید:

  • شمش‌های تیتانیوم نیاز به انجام عملیات حرارتی و ماشین‌کاری، آزمون فراصوتی غوطه‌وری، آزمون خواص مکانیکی، بازرسی ریزساختاری و درشت‌ساختاری و سایر فرآیندها دارند. فرآیند تولید: میله‌های تیتانیوم نورد گرم – بازده بالا، عملکرد پایدار؛ میله‌های تیتانیوم آهنگری‌شده – ابعاد انعطاف‌پذیر، آهنگری چندمرحله‌ای، بهبود عملکرد کلی میله‌های تیتانیوم؛ میله‌های تیتانیوم کشش سرد – معمولاً میله‌های تیتانیوم کوچک‌جثه و با دقت بالا؛ تمامی میله‌های تیتانیوم فوق با سطح براق تحویل داده می‌شوند.
همین حالا با داکسون تماس بگیرید

گزارش‌های آزمون

The test reports we provide include: Grade 2 Titanium Rod and Grade 5 Titanium Round Bar Factory Test Certificate, EN 10204 3.1, Chemical Report, Mechanical Report, PMI Test Report, Visual Inspection Report, Third Party Inspection Report, Destructive Test Report, Non-destructive Testing Report. (Daxun will provide according to customer requirements)

همین حالا با داکسون تماس بگیرید

Grade 7 Rods Applications and Standards

Grade 7 Titanium Rods are widely used in the following industries under extreme corrosive conditions:

  • صنایع هوافضا، کشتی‌سازی، نفت و گاز، مهندسی دریایی، کارخانه‌های شیمیایی، ماشین‌آلات صنعتی، صنعت برق، صنعت کاغذ و خمیر کاغذ، صنایع فرآوری مواد غذایی، پالایشگاه‌ها، صنعت نظامی، تجهیزات دارویی و فرآوری مواد غذایی و غیره.
  • مشخصات: AMS 4928,AMS 4967,AMS 4965 ,AMS 6931 ,ASTM B 348
  • استانداردها: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
همین حالا با داکسون تماس بگیرید

کیفیت، تحویل، بازرسی

داکسون چندین آزمون تضمین کیفیت را انجام می‌دهد که این آزمون‌ها شامل آزمون‌های مکانیکی مانند کشش سطحی، آنالیز شیمیایی، شناسایی مثبت مواد – آزمون PMI، آزمون‌های میکرو و ماکرو، آزمون خوردگی بین‌دانه‌ای (IGC)، آزمون تشخیص عیوب با فراصوت، آزمون فرورفتگی و مقاومت، آزمون سختی، شناسایی مثبت مواد، آزمون انبساط و غیره می‌شود. تمام این آزمون‌ها تضمین می‌کنند که مواد میله‌ تیتانیوم گرید ۲ و شمش گرد تیتانیوم گرید ۲ برای کاربرد مورد نظر مناسب هستند. در طول فرآیند تولید، قطر، ضخامت و سطح محصول را اندازه‌گیری می‌کنیم.

  • زمان تحویل ما دقیقاً مطابق قرارداد است.
  • از آژانس‌های ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
  • از نمونه‌های رایگان برای آزمایش مشتری پشتیبانی کنید.
  • حمایت از بازرسی کارخانه‌ای حضوری یا ویدیویی
همین حالا با داکسون تماس بگیرید

بسته‌بندی

داکسون آلیاژ بهترین کیفیت بسته‌بندی را تضمین می‌کند، زیرا بسته‌بندی نقش مهمی در حمل‌ونقل بین‌المللی دارد که کالاها از مسیرهای مختلف عبور می‌کنند تا به مقصد نهایی برسند؛ بنابراین ما توجه ویژه‌ای به بسته‌بندی داریم. ما کالاهای خود را بسته به محصول به روش‌های مختلف بسته‌بندی می‌کنیم. روش‌های بسته‌بندی محصولات ما عبارتند از:
• جعبه‌ها و صندوق‌ها
• سلفون منقبض‌شونده
• پالت‌های چوبی
• جعبه‌های چوبی

همین حالا با داکسون تماس بگیرید

پشتیبانی فنی

اگر به هرگونه پشتیبانی فنی اضافی نیاز دارید، متالورژیست مقیم ما و کارکنان آگاه ما با کمال میل آماده کمک‌رسانی هستند. علاوه بر این، داکسون دارای آزمایشگاه آزمون معتبر است—نخستین در صنعت موجودی چندفلزی و پلاستیکی. به نظر ما، این امر تعهد تزلزل‌ناپذیر ما به کیفیت و فلسفه ما به‌عنوان یک تأمین‌کننده تمام‌خدمت را نشان می‌دهد.

Daxun Grade 7 Titanium Rods help your brand improve quickly

اندازه اسمی سرتیتر سربرگ h7 hatred h9 H10 H11 سرتیتر ۱۲
قطر میلی‌متر
تا ۳ +0.004/0 +0.006/0 +0.01/0 +0.014/0 +0.025/0 +0.04/0 +0.06/0 +0.1/0
بیش از ۳ تا ۶ +0.005/0 +0.008/0 +0.012/0 +0.018/0 +0.03/0 +0.048/0 +0.075/0 +0.12/0
بیش از ۶ تا ۱۰ +0.006/0 +0.009/0 +0.015/0 +0.022/0 +0.036/0 +0.058/0 +0.09/0 +0.15/0
بیش از ۱۰ تا ۱۸ +0.008/0 +0.011/0 +0.018/0 +0.027/0 +0.043/0 +0.07/0 +0.11/0 +0.18/0
بیش از ۱۸ تا ۳۰ ساله +0.009/0 +0.013/0 +0.021/0 +0.033/0 +0.052/0 +0.084/0 +0.13/0 +0.21/0
بیش از ۳۰ تا ۵۰ +0.011/0 +0.016/0 +0.025/0 +0.039/0 +0.062/0 +0.1/0 +0.16/0 +0.25/0
بیش از ۵۰ تا ۸۰ +0.013/0 +0.019/0 +0.03/0 +0.046/0 +0.074/0 +0.12/0 +0.19/0 +0.3/0
بیش از ۸۰ تا ۱۲۰ +0.015/0 +0.022/0 +0.035/0 +0.054/0 +0.087/0 +0.14/0 +0.22/0 +0.35/0
بیش از ۱۲۰ تا ۱۸۰ +0.018/0 +0.025/0 +0.04/0 +0.063/0 +0.1/0 +0.16/0 +0.25/0 +0.4/0
بیش از ۱۸۰ تا ۲۵۰ +0.02/0 +0.029/0 +0.046/0 +0.072/0 +0.115/0 +0.185/0 +0.29/0 +0.46/0

میل تیتانیوم

پروژه‌ها و محصولات داغ اخیر

میل و شمش تیتانیوم
میل و شمش تیتانیوم
میل و شمش تیتانیوم
میل و شمش تیتانیوم
Titanium Alloy Bar, Titanium Bar Grade 7/UNS 52400

Daxun has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 7 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.


مشخصات

ASTM B348 – Titanium and Titanium Alloy Bars and Billets
ASTM SB348 – Specification for Titanium and Titanium Alloy Bars and Billets
AMS 4921 – Titanium Alloy Bars, Wire, and Forgings
AMS 4902 – Titanium Alloy Bars and Billets


عملیات حرارتی

When enhanced corrosion resistance and mechanical properties are required, annealing can be performed at 1,200-1,400°F (649-760°C).
DAXUN Grade 7 alloy can be heat treated in a variety of ways:

  1. Anneal: 1,200-1,400°F (649-760°C), 1 to 2 hours, air cool
  2. Stress Relief Anneal: 900-1,100°F (482-593°C), 1 to 4 hours, air cool

سختی

Typical hardness in the annealed condition is Rockwell B 70-80, providing excellent machinability while maintaining superior corrosion resistance.


Forgeability / Formability

Grade 7 titanium alloy bar is forged at 1,650-1,750°F (899-954°C) with a final forging temperature of 1,450°F (788°C). A minimum of 30% reduction is recommended for optimum properties.

Grade 7 alloy bar exhibits good formability in the annealed condition. For severe forming operations such as bending or stretching, these can be performed at temperatures up to 1,200°F (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000-1,200°F (538-649°C).


قابلیت ماشین‌کاری

Grade 7 titanium alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids. The palladium content does not significantly affect machinability compared to other CP titanium grades.


قابلیت جوشکاری

Grade 7 titanium rod is readily weldable in the annealed condition. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. The palladium addition enhances weld integrity in corrosive environments.


ملاحظات ویژه

Grade 7 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics. The palladium content provides additional protection against corrosion in contaminated conditions.


Size Range

Grade 7 Titanium Bar Dimensions
Ø 0.7 – 30 mm (drawn, ground)
Ø ۱۶ – ۴۰۰ میلی‌متر (نورد گرم، پوست‌کنده)
Tolerances: h11–h5 (ISO 286-2)
تoleranceهای دقیق‌تر یا متفاوت بنا به درخواست موجود است.
طول تا ۹۰۰۰ میلی‌متر، بسته به قطر
برای قطرهای بزرگتر، سایر طول‌ها و تلرانس‌های میله‌ فولادی در صورت درخواست قابل توافق است.


Availability Grade 7 Titanium Rods

Processing options include:

  • کشیدن، صاف کردن
  • کشش، صاف‌کاری، پولیش‌کاری
  • کشیدن، آسیاب کردن، صیقل دادن
  • کشش، صاف‌کاری، سنگ‌زنی، صیقل‌کاری
  • کشش، آنیل، صاف‌کاری
  • کشش، آنیل، صیقل‌کاری
  • کشش، آنیل، سنگ‌زنی، صیقل‌کاری
  • کشش، آنیل، راست‌کاری، سنگ‌زنی، صیقل‌کاری

ما میله‌ها را طبق نیازهای شما تولید می‌کنیم.
سطح و صافی عالی، کروییت کامل و تلرانس‌های قطر بسیار تنگ (طبق ISO 286-2 تا h5). قابل عرضه در شرایط راست‌شده، سنگ‌زده و صیقلی.


ارّه‌کاری

  • اره‌های نواری (تا Ø۵۱۰ میلی‌متر)
  • Bench band saws (up to 6,000 x 3,000 x 400 mm)
  • ماشین‌آلات برش با کارایی بالا برای برش دقیق

Titanium Bar End Machining

  • یک‌رو یا دو‌رو
  • فاصلهٔ لبه‌زاویهٔ ۹۰° (۴۵°)
  • نقطه ۶۰° (۳۰°)
  • انتهای صاف
  • متمرکز

Delivery Form

  • ASTM American Society for Testing and Materials Standards
  • AMS American Aerospace Materials Standards
  • NACE American Association of Corrosion Engineers International Standards
  • ASME American Society of Mechanical Engineers Standards
  • GB Chinese National Standards
  • GJB Chinese National Military Standards
  • ISO International Standards
  • DIN German Standards
  • انگلیسی استانداردهای اروپایی
  • API American Petroleum Institute Standards

Detection Method

آزمایش غیرمخرب > آزمایش 100%
Testing methods:

  • Eddy current testing / eddy current crack testing
  • سطح بدون نقص (سطح ۴)
  • قطر سوراخ کف‌مسطح ۰٫۷ میلی‌متر و ۰٫۴ میلی‌متر
  • Blind area can be cut off according to fixed length > Test to the end of the bar
  • آزمایش فراصوتی با قطر کامل

خدمات مواد میله‌ای تیتانیوم ما

As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.

We will be happy to provide you with a consultation and explain everything you need to know about obtaining Grade 7 titanium bar material, including which standards require greater attention for the components to be manufactured.

اگر تعهد تأمین بلندمدت دارید، می‌توانید یک قرارداد چارچوبی با داکسون منعقد کنید. ما قیمت‌ها و مقادیر را برای مدت زمان مشخصی تضمین می‌کنیم.

Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about Grade 7 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.


اطلاعات سفارش

Purchase orders should include quantity, grade, type or category, API5L reference, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact داکسون now, we will reply to your email as soon as possible.

کدام گرید تیتانیوم بهترین است؟

رتبه آلیاژ تیتانیومی که نیاز دارید به پروژه‌ای که روی آن کار می‌کنید بستگی دارد، زیرا هر رتبه مزایای متفاوتی دارد.

تمام گریدهای آلیاژ تیتانیوم فوق‌العاده قوی و مقاوم در برابر خوردگی هستند، به این معنی که در سخت‌ترین شرایط نیز به خوبی کار خواهند کرد.

درجهٔ بالاتر آلیاژ تیتانیوم (۵–۱۲) آلیاژهایی هستند که برای مزایای خاص طراحی شده‌اند. برای مثال، آلیاژ تیتانیوم درجهٔ ۱۲ مقاومت حرارتی عالی دارد و آن را به گزینه‌ای ایده‌آل برای مبدل‌های حرارتی پوسته و لوله‌ای، لوله‌کشی هیدرولیک و تجهیزات صنعت شیمی تبدیل می‌کند.

درجه‌های ۱ تا ۴ آلیاژهای تیتانیوم خالص هستند و اگر به ماده‌ای جوش‌پذیر و چکش‌خوار برای سیستم‌های لوله‌کشی و تیوب‌ها نیاز داشته باشید، انتخابی ایده‌آل‌اند. درجه‌های پایین‌تر را در صنایع دریایی و صنعتی خواهید یافت.

اگر در حال شروع یک پروژه هستید و مطمئن نیستید کدام گرید آلیاژ تیتانیوم برای شما مناسب‌تر است، همین امروز با ما تماس بگیرید؛ ما با کمال میل به شما کمک خواهیم کرد.

کلاس‌های بالاتر تیتانیوم چه تفاوتی با کلاس‌های پایین‌تر دارند؟

در داکسون، ما طیف گسترده‌ای از گریدهای آلیاژ تیتانیوم از گرید ۱ تا گرید ۱۲ را ارائه می‌دهیم.

گریدهای ۱ تا ۴ تیتانیوم خالص هستند، در حالی که گریدهای بالاتر آلیاژ هستند.

کلاس‌های آلیاژ به‌خاطر نسبت بالای استحکام به وزن‌شان محبوب هستند.

رایج‌ترین گرید آلیاژ تیتانیومی که می‌یابیم، گرید ۵ است. اگرچه همچنان غنی از تیتانیوم است، این گرید یکی از قابل‌اعتمادترین‌هاست زیرا می‌تواند دماهای تا ۶۰۰ درجه فارنهایت را تحمل کند و در شرایط شدید دوام بیاورد.

در صنایعی مانند صنایع هوافضا و دریایی، به دلیل مقاومت در برابر سایش و خوردگی، گریدهای بالاتر ترجیح داده می‌شوند.

برعکس، گریدهای پایین‌تر عمدتاً به دلیل استحکام کمتر برای جوشکاری استفاده می‌شوند.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

آیا درجه تیتانیوم بر هزینه تأثیر دارد؟

اگرچه درجه تیتانیوم کمی هزینه را افزایش می‌دهد، اما هزینه کل عمدتاً به شکل و فرم تیتانیومی که نیاز دارید بستگی دارد.

در DAXUN، ما طیف گسترده‌ای از محصولات تیتانیومی از جمله صفحات، لوله‌ها، کویل‌ها و میله‌ها را ارائه می‌دهیم. طول، عرض و تعداد هر قلم مورد نیاز شما بر مبلغ پرداختی شما در زمان تسویه حساب تأثیر خواهد گذاشت.

متأسفانه بدون اطلاع کافی از پروژه شما و کاربرد تیتانیوم، تعیین قیمت به‌صورت آنلاین دشوار است.

خوشبختانه تیم کارشناسان ما همیشه در خدمت شماست تا در زمینه نیازهای تیتانیومی‌تان به شما کمک و مشاوره دهد. با ارسال ایمیل به daxunalloy@gmail.com، ما قادر خواهیم بود با ارائه مشاوره و برآورد دقیق هزینه به شما پاسخ دهیم.

حتماً تا حد امکان اطلاعاتی دربارهٔ گرید، شکل و مقدار تیتانیومی که نیاز دارید ارائه دهید تا نیازهایتان بهتر درک شود.

از کجا می‌توانم دربارهٔ گریدهای تیتانیوم بیشتر بیاموزم؟

تیم DAXUN باتجربه، آگاه و خوش‌برخورد است. با سال‌ها تجربه در این صنعت، آن‌ها همه چیز را درباره تیتانیوم، از کاربردها و مزایا گرفته تا گریدهای مختلف آن، می‌دانند.

برای دریافت به‌روزرسانی‌های منظم درباره تیتانیوم، کاربردها و مصارف آن در صنایع مختلف، حتماً وبلاگ ما را بررسی کنید. کارشناسان ما راهنماهای ساده‌ای نوشته‌اند که همیشه می‌توانید هنگام پرسش به آن‌ها مراجعه کنید.

اگر همچنان با مشکل مواجه هستید، با ما تماس بگیرید؛ خوشحال می‌شویم به شما کمک کنیم.

با ارسال ایمیل به daxunalloy@gmail.com، پاسخ سریعی دریافت خواهید کرد. لطفاً در سؤال خود تا حد امکان جزئیات بیشتری درج کنید تا بتوانیم راه‌حل مناسبی پیشنهاد دهیم.

چگونه سریعاً یک برآورد قیمت دریافت کنیم یا اطلاعات بازار را بفهمیم؟

لطفاً فرم صفحه “تماس با ما” را پر کنید یا با مدیر فروش ما به شماره +86 13382898899 تماس بگیرید. ما در اسرع وقت با شما تماس خواهیم گرفت. واتس‌اپ ما آنلاین است و ایمیل (Daxunalloy@gmail.com) ظرف ۶ ساعت بررسی می‌شود. به هر پرسش یا پیام به‌سرعت پاسخ داده خواهد شد. علاوه بر این، ما هر هفته اطلاعات بازار را با مشتریان خود به اشتراک می‌گذاریم.

می‌توانم چند نمونه بگیرم؟

ما می‌توانیم نمونه‌های میله‌ای تیتانیوم را برای بررسی کیفیت در اختیار شما قرار دهیم. نمونه رایگان است و شما فقط هزینه حمل را پرداخت می‌کنید.

تا کنون به کدام کشورها صادرات داشته‌اید؟

ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشته‌ایم.

حداقل مقدار سفارش شما چیست؟

Our MOQ is 300 Kg for titanium rod.

زمان تحویل شما چقدر است؟

سفارش‌های آزمایشی را می‌توان ظرف یک هفته تحویل داد. برای سفارش‌های معمولی تقریباً دو هفته زمان لازم است.

همین امروز استعلام خود را ارسال کنید
استعلام سریع