x
Senden Sie Ihre Anfrage noch heute
Schnelles Angebot

Daxun is a 321 stainless steel sheet supplier from China

As China’s leading stainless steel plate supplier and exporter, Daxun provides 321 stainless steel plates to the world.
  • Grade: AISI 321/S32100
  • Manufacturing: cold-rolled plate, hot-rolled plate, forged plate
  • Standard: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Type: cold-rolled thin plate, hot-rolled thick plate
  • Surface: 2B, NO.1, NO.4, HL, BA, 8K, etc.
  • Length: 2438mm3048mm6000mm can be customized
  • Origin: TISCO, Baosteel, Pohang, Tsingshan, Delong

Global leader in stainless steel sheet fabrication services

Daxun 321 Stainless Steel Plate (UNS S32100) is a titanium-stabilized austenitic stainless steel with excellent resistance to intergranular corrosion. This grade is designed for high temperature applications up to 1500°F (815°C), where the addition of titanium stabilizes the material against the formation of chromium carbides. Since titanium has a greater affinity for carbon than chromium, titanium carbides occur within the grains rather than at the grain boundaries. While its annealed corrosion resistance is comparable to 304 and 304L, it has stronger creep and stress rupture properties. These properties make it suitable for pressure vessel and boiler applications. 321 Stainless Steel is non-magnetic and heat resistant, allowing long-term use at high temperatures.

Daxun Alloys stocks 321 Alloy stainless steel plate in thicknesses ranging from 3/16″ to 4″. You can also order the high carbon version 321H Alloy (UNS S32109) in the same thickness range.The alloy can be used in most dilute organic acids at moderate temperatures, pure phosphoric acid at lower temperatures, and dilute solutions up to 10% at elevated temperatures. Alloy 321 resists polythionic acid stress corrosion cracking in hydrocarbon service. It can also be used in alkaline solutions without chlorides or fluorides at moderate temperatures. Alloy 321 does not perform well in chloride solutions (even at low concentrations) or in sulfuric acid environments.

Weiterlesen

Technical Data

Product Parameters:   321(UNS S32100) Stainless Steel Sheet/Plate
Breite 10mm~2500mm
Dicke 0.2mm~100mm Thickness tolerance +/-0.03mm
Standard ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2
Oberfläche 2B,BA,8K,NO.1,NO.4,NO.3,hairline,checkered,gold ,black ,rose gold,etc
Spezifikation 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L
 Mühlenursprung TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc.
Zertifizierung ISO, SGS, BV, TUV,CE etc
Element % Present (in product form)
C, H, P L TW TS
Carbon (C) ≤0.08 ≤0.08 ≤0.08 ≤0.08
Silicon (Si) ≤1.00 ≤1.00 ≤1.00 ≤1.00
Manganese (Mn) ≤2.00 ≤2.00 ≤2.00 ≤2.00
Phosphorous (P) ≤0.045 ≤0.045 ≤0.0453) ≤0.040
Sulfur (S) ≤0.0151) ≤0.0301) ≤0.0153) ≤0.0151)
Chromium (Cr) 17.00 – 19.00 17.00 – 19.00 17.00 – 19.00 17.00 – 19.00
Nickel (Ni) 9.00 – 12.00 9.00 – 12.002) 9.00 – 12.00 9.00 – 12.002)
Titanium (Ti) 5xC to 0.70 5xC to 0.70 5xC to 0.70 5xC to 0.70
Iron (Fe) Balance Balance Balance Balance
Density (lb./ in^2) @ RT 0.29
Modulus of Elasticity in Tension (psi x 10^6) 28.0
Specific Heat (BTU/o F/lb.) 32 to 212 oF 0.12
Thermal Conductivity (BTU/hr/ft^2/ft) 212oF 9.3
932oF 12.8
Mean Coefficient of Thermal Expansion (in. x 10^-6 per o F) 32 to 212oF 9.2
32 to 600oF 9.5
32 to 1,000oF 10.3
32 to 1,200oF 10.7
Electrical Resistivity (micro ohms – cm) at 70oF 28.4
Melting Point Range (oF) 2500 – 2550
uct Form Max Thickness (mm) Yield Strength Zugfestigkeit Elongation min. in % Impact Energy (ISO-V) ≥ 10mm thick
0.2% Rp0.2 N/mm2 1% Rp1.0 N/mm2 Rm N/mm2 A1) %min (longitudinal) A1) %min (transverse) Jmin (longitudinal) Jmin (transverse)
C 8 2203) 2203) 520-7203) – 40 – –
H 13.5 2003) 2403) 520-7203) – 40 100 60
P 75 2003) 2403) 500-7003) – 40 100 60
L 160 1904) 2254) 500-7004) 40 – 100 –
L 2502) 1907) 2257) 500-7007) – 30 – 60
TW 60 1805) 2155) 460-6805) 35 30 100 60
TS 60 1805) 2155) 460-6805) 35 30 100 60

Choose Daxun and make your customers satisfied.

Contact Daxun now

Fast delivery

Daxun provides customers with timely and fast delivery of stainless steel plate products. Behind the speed is the system support from production capacity, information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to ports and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.

Contact Daxun now

321 stainless steel plate features

Ausgezeichnete Korrosionsbeständigkeit
Good high temperature resistance
Good mechanical properties
Excellent toughness at sub-zero temperatures
Ausgezeichnete Oxidationsbeständigkeit
Easy to weld and form
Improved creep/rupture properties

Contact Daxun now

SS 321 Plate Surface Treatment

1D: The surface is matte with discontinuous particle shape.
2D: White with a silvery tone.
2B: Silver gray with better gloss and flatness than 2D surface.
Ba: Close to mirror surface with excellent gloss and reflectivity.
No.3: Good gloss and rough surface.
No.4: The surface has fine lines and good gloss.
HL: Silver gray with golden hair.
8K: Mirror surface.

Contact Daxun now

Quality, delivery, inspection

  • Daxun strictly controls product quality. Before placing an order, we will send you the product warranty, or if you need samples for testing, we can also send samples for free.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    Our delivery time is strictly in accordance with the contract.
  • Support customer third-party agencies to go to the factory for inspection
  • Support free samples to customers for testing
  • Support on-site or video factory inspection
Contact Daxun now

Technical Support

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Contact Daxun now

Advanced machining

Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel uses the ERP system to achieve full traceability of the variety, specification, and origin of each stainless steel plate, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

321 plate stainless steel Features

High strength
Corrosion resistance
Heat resistance
Low temperature resistance
Environmental protection
Welding performance

Daxun Let your brand improve rapidly

Tolerance for 2B Sheet
Size Tolerance Rank
Group 1 Group 2 Group 3
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
Tolerance for No.1 Hot Rolled Plate
Size Tolerance Rank
Group 1 Group 2 Group 3
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
16 15.2~ 15.5 15.5~ 15.7 15.7~ 16.1
18 17.2~ 17.5 17.5~ 17.7 17.7~ 18.1
20 19.2~ 19.5 19.5~ 19.7 19.7~ 20.1
30 29.2~ 29.5 29.5~ 29.7 29.7-30.1
40 39.2~ 39.5 39.5~ 39.7 39.7~ 40.1
50 49.2~ 49.5 49.5~ 49.7 49.7~ 50.1
60 59.2~ 59.5 59.5~ 59.7 59.7~ 60.1
Delivery State Choice Surface Condition
Cold Rolled 2B
2D
BA
Hairline
No.3
No.4
6K
8K
Note:
1. If you require different deliver state than the above listed, kindly confirm with us.
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here.
Delivery State
Delivery State Choice Surface Condition
Hot Rolled No.1
No.3
No.4
6K
8K
Pickled
Note:
1. If you require different deliver state than the above listed, kindly confirm with us.
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here.
Klasse Typ Dicke Oberfläche
Austenitisch 304/304H/304L/304J1 0.25-150mm 2B/BA/NO.4/8K/SB/HL/NO.1
321 0.4-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
316/316L/317L/316Ti 0.3-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
Ferrite 430 0.4-3.0mm 2B/BA/NO.4/8K/SB/HL
Ultra Pure Ferrite 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B、2D
409L 0.4-2.5mm 2B、2D
Klasse Typ Dicke Original
Heat-resistant Steel 309S 0.5-40mm CHN
310S Edelstahlplatte 0.5-40mm CHN
Duplex Steel 2101 1.5-50mm CHN
2304 3.0-50mm CHN
2205 0.5-60mm CHN
2507 1.0-60mm SWE / JPN / CHN
Super Austenitic Steel N08904 0.6-50mm SWE / JPN / CHN
S31254 0.5-50mm SWE / JPN / CHN
N08926 0.5-50mm SWE / JPN / CHN
N08367 0.5-50mm SWE / JPN / CHN
Nickel Base Alloy N08031 1.0-50mm US / JPN / GER
N08810/N08800 0.8-50mm US / JPN / CHN
N08028 1.0-20mm US / GER / JPN
N08020 1.0-20mm US / GER / JPN
N08825 0.8-40mm US / GER / SWE / JPN / CHN
N10276 0.5-50mm US / GER / JPN
N06022 1.0-50mm US / GER / JPN
N06625 0.8-20mm US / GER / CHN
N04400 1.0-20mm US / GER / JPN
N06600 1.0-50mm US / GER / JPN / CHN
N02201 0.5-20mm US / JPN
Titan TA1/Gr1 0.5-50mm JPN / CHN
TA2/Gr2 0.5-50mm JPN / CHN
Welding Material ERNiCrMo-13 1.2、2.4mm GER
ERNiCrMo-3 2.4mm GER
ERNiCrMo-4 2.4mm US

The surface and shape of 321 stainless steel plate (7)

Daxun is a trustworthy stainless steel plate manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel plates are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the stainless steel plates have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

Recent hot case projects and products

321 plate stainless steel
astm a240 plate stainless steel
321 flat stainless steel plate
321 stainless steel sheet suppliers
321 2b stainless steel sheet
321 stainless steel sheet
Kann ich ein paar Muster bekommen?

Wir können Ihnen Muster aus Edelstahlblech zur Qualitätsprüfung zur Verfügung stellen. Das Muster ist kostenlos, Sie zahlen lediglich die Versandkosten.

Which countries have you already exported?

We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.

What is your MOQ?

Our MOQ is 1 ton for stainless steel sheet.

How long is your delivery time?

Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.

Senden Sie Ihre Anfrage noch heute