Super Austenitic 904l Stainless Steel Coil China Supplier
As a leading stainless steel coil supplier and exporter in China, Daxun supplies stainless steel coils to all over the world.
- Coil grade: 904L-N08904
- Stronger corrosion properties than Type 316L an 317L
- Good resistance to sulphuric, phosphoric and acetic acids
- High resistance to crevice and stress corrosion cracking
- Excellent formability and weldability
Global leader in stainless steel Coil fabrication services
Type 904L is a high alloy austenitic stainless steel that is renowned for its corrosion resistance. 904L alloy (UNS N08904) is a super austenitic stainless steel that may be used in a variety of process settings and has moderate to high corrosion resistance. The high chromium and nickel content, along with molybdenum and copper, ensures good to outstanding corrosion resistance. With a highly alloyed chemistry (25% nickel and 4.5% molybdenum), 904L offers better resistance to chloride stress corrosion cracking, pitting, and general corrosion than 316L and 317L molybdenum reinforced stainless steels. The 904L alloy was originally created to withstand dilute sulfuric acid conditions. It is also resistant to most organic acids and other inorganic acids, including hot phosphoric acid. 904L alloy is easily weldable and may be handled using typical shop fabrication procedures.
Dah Hsun is an ISO 9001:2008 certified firm that is a major supplier and exporter of ASTM A240 Stainless Steel Coils. Stainless steel coils can be cut to your requirements and include a full set of mill test results. Custom lengths and widths are available up to 2000mm. Exporting is our specialty! We can obtain several hard-to-find grades and/or non-standard sizes to satisfy our customers’ specific needs. We have vast experience processing steel coil goods and can divide all stainless steel coils to the desired sizes. Introducing our extensive line of Dah Hsun Stainless Steel goods – the pinnacle of dependability, durability, and performance. We are glad to provide a wide selection of grades and varieties to fulfill the diverse needs of industrial and architectural applications.
Our stainless steel coil goods, which range from the Austenitic series to the Ferritic series and other special categories, are well-known for their high performance and extensive requirements. The austenitic series includes 304/304L/304J1, 321 and 316/316L/317L/316Ti/310/309, which can fulfill varied thickness requirements and give a variety of surface treatments, including 2B, BA, NO.4, 8K, SB, HL, NO.1, and so on.
Our ferrite line, which includes 430, ultra-pure ferrite 443, and 436L/439/444/441, caters to customers looking for unique qualities and applications. These materials can accommodate thicknesses ranging from 0.4mm to 3.0mm and offer a variety of surface treatment options such as 2B, BA, NO.4, 8K, SB, HL, and so on.
By selecting our stainless steel coils, you are investing in a material that ensures long service life, great reliability, and exceptional performance. Don’t compromise on quality; choose our stainless steel solutions and see the impact they can make in your project. Contact Daxun today for additional information or to place an order for the stainless steel coil specs and quantities that you require.
Data
- Parameter
- Element
- Mechanical Properties
- PHYSICAL PROPERTIES
- All equivalent
- 904L coil stock
| 904L Stainless Steel Coil Specification | ASTM A240 / ASME SA240 |
| 904L Stainless Steel Coil Manufacturing Process | Hot Rolled (HR) / Cold Rolled (CR) |
| 904L Stainless Steel Coil Grades | 201 / 304 / 304L/ 904L / 309S / 420 / 316 / 316L / 316Ti / 317L / 321 / 321H / 347 / 347H / 904L etc. |
| UNS No. – UNS S904L, UNS S31008, UNS S31600, UNS S31603, UNS S31603, UNS S31600, UNS S31703, UNS S32100, UNS S34700, UNS S34709, UNS S8904 | |
| EN No. 1.4845, 1.4401, 1.4404, 1.4571, 1.4438, 1.4541, 1.4550, 1.4551, 1.4539 | |
| 904L Stainless Steel Coil Thickness | 0.6 MM TO 16 MM THICKNESS |
| 904L Stainless Steel Coil Width | 1250 MM / 1500 MM / 2000 MM / 04 Feet / 05 Feet and Custom Cut Width as Per Requirement |
| 904L Stainless Steel Coil Length | 2400 MM / 2420 MM / 6000 MM / 08 Feet / 10 Feet / Coil Cut and Custom Cut Length as Per Requirement |
| 904L Stainless Steel Coil Surface Finish | 2B, 2D, BA, MATT, MATT PVC, No.4, No.5, SB, HR, No.8, Mirror, Hairline, Brush, Textured, Oil base wet Polished, Both sides Polished available. |
| 904L Stainless Steel Coil Coating | PVC coating Normal / Laser, Film: 100 micrometer, Color: black/white. |
| 904L Stainless Steel Coil Other Testing | NACE MR0175, Ultrasoung TEST, IGC TEST, Intergranular Corrrosion Test as per ASTM A262 Practice E, Charpy Impact Test, Macro, Grain Size, Hardness, etc. |
| 904L Stainless Steel CoilValue Added Services | Gas Cutting / CNC Plasma Cutting / Profiling / Rolling / Bending / coil Metal Fabrication / Drill / Punch / Machining / Sand Blasting / Shot Blasting / Heat Treatment |
| 904L Stainless Steel Coil Packaging | Loose / Carrate / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps |
| 904L Stainless Steel Coil Shipment & Transportation | By Road – Truck / Train Partial Load, Full Load, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes |
| 904L Stainless Steel Coil Material Test Certificate | Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS, Bureau of Indian Standards BIS Approved ETC |
| Manufacturer | POSCO, Aperam, Jindal Stainless, DKC Korea, Thyssenkrup, Baosteel, TISCO,Arcelor Mittal, VDM,Nippon Metal, Outokumpu,Qingshan,Delong. |
| Shipping Port | Shanghai/Ningbo port/Tianjin/Qindao |
| Element | % Present (in product form) |
| Carbon (C) | 0.02 |
| Silicon (Si) | 0.7 |
| Manganese (Mn) | 2 |
| Phosphorous (P) | 0.03 |
| Sulfur (S) | 0.01 |
| Chromium (Cr) | 19.00 – 21.00 |
| Nickel (Ni) | 24.00 – 26.00 |
| Nitrogen (N) | 0.15 |
| Molybdenum (Mo) | 4.00 – 5.00 |
| Copper (Cu) | 1.20 – 2.00 |
| Iron (Fe) | Balance |
| Yield Strength | Ultimate Tensile | Elongation | Hardness | ||
| 0.2% Offset | Strength | in 2 in. | |||
| psi (min.) | (MPa) | psi (min.) | (MPa) | % (min.) | (max.) |
| 31,000 | 220 | 71,000 | 490 | 36 | 70-90 Rockwell B |
| Reference data on some physical properties | ||
| Density at 20°C kg/m3 | 8 | |
| Thermal Conductivity W/m K at | 20°C | 12 |
| Modulus of Elasticity kN/mm2 at | 20°C | 195 |
| 200°C | 182 | |
| 400°C | 166 | |
| 500°C | 158 | |
| Specific Thermal Capacity at 20°C J/kg K | 450 | |
| Electrical Resistivity at 20°C Ω mm2/m | 1 | |
| STANDARD | WERKSTOFF NR. | UNS | JIS | AFNOR | BS | GOST | EN |
| SS 904L | 1.4539 | N08904 | SUS 904l | Z2 NCDU 25-20 | 904S13 | – | X1NiCrMoCu25-20-5 |
| • 904L Stainless Steel HR coil | • Baosteel Stainless Steel 904L coil |
| • 904L Stainless Steel Chequered coil | • Stainless Steel Cladding 904L coil |
| • 904L Stainless Steel Golden Laser Pattern coil | • Black SS 904L coil 4mm Thick |
| • Super thin-Mirror surface BA ss 904L coil | • Bright-pickled Stainless Steel 904L coil |
| • Super Austenitic SS 904L coil | • Cold rolled, heat treated 904L coil |
| • ASTM A240 904L coil | • 3mm Cold Rolled AISI SS 904L coil |
| • JMSS cold rolled ss 904L coil | • Mill Supply SS 904L coil |
| • Cold Rolled No.1 Finish SS 904L coil | • Grade Prime SS 904L coil |
| • SEW 400 Stainless Steel 904L coil | • Carpenter Custom 450 Stainless Steel 904L coil |
| • Hot Rolled Stainless Steel 904L coil | • Cut to Size Stainless Steel 904L coil |
| • Sales Promotion SS 904L coil | • Non Magnetic Polishing Stainless Steel 904L coil |
| • Cr Stainless Steel 904L coil | • ASME SA240 904L coil |
| • SS 904L Mill Test Certificate coil | • Grade 904L Stainless Steel Finish coil |
| • ASTM A240 904L coil | • 904L Stainless Steel Blank coil |
| • Cold rolled, bright annealed 904L coil | • 904L Stainless Steel Perforated coil |
| • Ground Stainless Steel 904L coil | • Embossed ss 904L coil |
| • Hot Selling AISI SS 904L coil | • Cheap cold rolled ss 904L coil with best price |
| • SS 904L Rose Golden coil | • Brush finish ss 904L coil price list |
| • Surface coated Stainless Steel 904L coil | • SS URANUS B6 904L coil |
| • Satin finish Stainless Steel 904L coil | • 2B SUS SS 904L coil |
| • AISI stainless steel 904L armor coil | • Food Grade Stainless Steel 904L coil |
| • Satin finish Stainless Steel 904L coil | • No. 4 PVC Coated SS 904L coil |
| • Mirror Finish SS 904L coil | • SS 904L coil Blasted Tin-Gold Rose |
| • SS 904L coil Gold Brush Finish | • 2mm ASTM SS 904L coil |
| • 904L Stainless Steel CR coil | • Stainless Steel Corrugated 904L coil |
| • 904L Stainless Steel 2B coil | • ASTM A240 904L coil |
| • 904L Stainless Steel B. Q. Profile coil | • Brushed or dull polished Stainless Steel 904L coil |
| • Best selling 4’x8′ mirror finished ss 904L coil | • Cold rolled, heat treated, pickled 904L coil |
| • Decorative hairline inox cold rolled ss 904L coil | • 10K Mirror Finish Surface SS 904L coil |
| • Hair Line Finish SS 904L coil | • Gold Etched SS 904L coil |
| • Laser cutting ss 904L coil | • 18 Gauge SS 904L coil |
| • Tisco Supplier 3mm Thickness Stainless Steel 904L coil | • Patterned Stainless Steel 904L coil |
| • Decorative Stainless Steel 904L coil | • Patterned Stainless Steel 904L coil |
| • Scotch Brite SS 904L coil | • Passenger Elevator Cabin SS 904L coil |
Choose Daxun and make your customers satisfied.
Quick response 904L Stainless Steel coil
We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule.Daxun’s stainless steel materials are of reliable quality, and their varieties, specifications and delivery weights strictly comply with the standards.
Daxun Advantages
Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel achieves full traceability of each steel plate from the ERP system, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strict monitoring during sales, and provides worry-free service guarantees after sales.


904L Stainless Steel coil Packaging
Daxun Alloy ensures the best quality of packaging as it plays an important role in international freight where goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
• Boxes and crates
• Shrink wrap
• Wooden pallets
• Wooden boxes
Quality, delivery, inspection
- Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
- During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
Our delivery time is strictly in accordance with the contract. - Support customer third-party agencies to go to the factory for inspection
- Support free samples to customers for testing
- Support on-site or video factory inspection

904L Stainless Steel coil Ordering Information
Purchase orders should include quantity, grade, type or category, API5L reference, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact Daxun now, we will reply to your email as soon as possible.
Technical Support
If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.
904L Stainless Steel Coil Features
Daxun Alloy Let your brand improve rapidly
- Gallery
- Product Series
- Main Equipment
| Grade | Type | Thickness | Surface |
| Austenitic | 304/304H/304L/304J1 | 0.25-150mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0.4-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0.3-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Ferrite | 430 | 0.4-3.0mm | 2B/BA/NO.4/8K/SB/HL |
| Ultra Pure Ferrite | 443 | 0.4-2.0mm | 2B |
| 436L/439/444/441 | 0.5-3.0mm | 2B、2D | |
| 409L | 0.4-2.5mm | 2B、2D | |
| Super Austenitic Steel | N08904 | 0.6-50mm | SWE / JPN / CHN |
| S31254 | 0.5-50mm | SWE / JPN / CHN | |
| N08926 | 0.5-50mm | SWE / JPN / CHN | |
| N08367 | 0.5-50mm | SWE / JPN / CHN | |
| Nickel Base Alloy | N08031 | 1.0-50mm | US / JPN / GER |
| N08810/N08800 | 0.8-50mm | US / JPN / CHN | |
| N08028 | 1.0-20mm | US / GER / JPN | |
| N08020 | 1.0-20mm | US / GER / JPN | |
| N08825 | 0.8-40mm | US / GER / SWE / JPN / CHN | |
| N10276 | 0.5-50mm | US / GER / JPN | |
| N06022 | 1.0-50mm | US / GER / JPN | |
| N06625 | 0.8-20mm | US / GER / CHN | |
| N04400 | 1.0-20mm | US / GER / JPN | |
| N06600 | 1.0-50mm | US / GER / JPN / CHN | |
| N02201 | 0.5-20mm | US / JPN | |
| Titanium | TA1/Gr1 | 0.5-50mm | JPN / CHN |
| TA2/Gr2 | 0.5-50mm | JPN / CHN | |
| Welding Material | ERNiCrMo-13 | 1.2、2.4mm | GER |
| ERNiCrMo-3 | 2.4mm | GER | |
| ERNiCrMo-4 | 2.4mm | US |
| Subsidiary | Main Equipments | Qty | Annual Capacity |
| Daxun Stainless steel co.(JiangSu) | Slitting Machine | 1 | Decorative coil:60,000 tons |
| Cutting Machine | 1 | ||
| No.4 And Hairline coil To coil Polishing Machine | 1 | ||
| No.4/Hairline Coil To Coil Polishing Machines | 1 | ||
| 8K/Super Mirror coil To coil Polishing Machines | 2 | ||
| 8K/Super Mirror Coil To Coil Polishing Machines | 3 | ||
| PVD Color Coating Machines | 4 | ||
| Liquid Chemical Coating Machines | 2 | ||
| Anti Finger Printing Machines | 2 | ||
| Auto Pick and Place machines | 16 | ||
| Plate Washing Machine | 1 | ||
| Daxun Stainless steel co.(Shanghai) | Cold Rolling Machine | 3 | 2B Coils:100,000 tons |
| Annealing & Pickling Line | 2 | Decorative Sheet;30,000 tons | |
| Slitting Machine | 1 | ||
| Cut to Length Machine | 1 | ||
| No.4/HL Polishing Machine(Sheet to Sheet) | 3 | ||
| 8K Polishing Machine(Sheet to Sheet) | 13 | ||
| PVD Titanium Coating Machine | 4 | ||
| Liquid Chemical Coating Machines | 1 | ||
| Daxun Stainless steel co.(Shandong) | Cold Rolling Machine | 3 | 2B & BA Coil:220,000 tons |
| Annealing & Pickling Line(2B & BA) | 2 | Decorative Sheet:60,000 tons | |
| Tension Levering & Skin Pass | 1 | ||
| Slitting Machine | 1 | ||
| Cut to Length Machine | 1 | ||
| No.4/HL Polishing Machine(Sheet to Sheet) | 1 | ||
| 8K Polishing Machine(Sheet to Sheet) | 11 | ||
| Automatic Copper Coating Machine | 1 | ||
| Digital Printing Machine | 1 | ||
| PVD Titanium Coating Machine | 3 | ||
| Liquid Chemical Coating Machines | 1 | ||
| Anti-finger Machine | 1 | ||
| Daxun Stainless steel co.(Sichuan) | Slitting Machine | 1 | 2B & BA Coil:180,000 tons |
| Cutting Machine | 1 | Decorative Sheet:50,000 tons | |
| No.4 And Hairline Sheet To Sheet Polishing Machine | 1 | ||
| No.4/Hairline Coil To Coil Polishing Machines | 1 | ||
| 8K/Super Mirror Sheet To Sheet Polishing Machines | 1 | ||
| 8K/Super Mirror Coil To Coil Polishing Machines | 1 | ||
| PVD Color Coating Machines | 1 | ||
| Liquid Chemical Coating Machines | 1 | ||
| Anti Finger Printing Machines | 1 |
SS 904L Surface Types of Stainless Steel Coils (6)
Information available for reference and download
Daxun is a trustworthy stainless steel coil manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel plates have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
Recent hot case projects and products
Related Products (10)
Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email ([email protected]) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week
Samples can be provided free of charge, but the freight is borne by the customer, and will be refunded after cooperation.
We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.
Our MOQ is 1 ton for stainless steel sheet.
We have a complete organization from raw material purchasing to processing and shipment arranging. In the whole chain, the documentary people ad QC will look for and check it by precise requirements.The third party inspection is welcomed.
Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.