Grade 9 (Ti-3Al-2.5V) Titanium Alloy Plate Manufacturer - Daxun Alloy

As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.

  • Plate Grade:Grade 9 UNS R56320
  • Plate Production type:cold rolling, hot rolling, forging.
  • Standard:ASTM B 265,ASME SB265,AMS491 etc
  • Features:High strength, Lightweight, High-temperature resistance
  • Surface:bright, polished, pickled, sandblasted, etc.
  • Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request

————Daxun produces titanium sheets in China to meet the diverse and ——demanding needs of customers!

Providing High-quality Grade 9 Titanium Plate to Serve Customers Worldwide

Grade 9 titanium plate is a high-performance near-alpha titanium alloy with a nominal composition of Ti-3Al-2.5V. It is based on pure titanium (Grades 1-4) reinforced with appropriate amounts of aluminum and vanadium, achieving an excellent balance of strength and toughness. Compared to pure titanium, Grade 9 boasts significantly higher strength and yield strength while maintaining good ductility and toughness. It is particularly renowned for its excellent weldability and cold formability. This material also offers lightweight, excellent corrosion resistance (especially in chloride environments), and good biocompatibility. It is both strong and durable, yet can withstand a variety of harsh operating conditions, making it an ideal choice for applications requiring high performance and reliability.

Where is Grade 9 titanium plate used?

In the aerospace industry, Grade 9 titanium plate is widely used in the manufacture of aircraft structures, fasteners, hydraulic systems, and engine components. Its combination of high strength and low density effectively reduces aircraft weight and improves fuel efficiency. In marine engineering and shipbuilding, its exceptional resistance to seawater corrosion makes it the material of choice for ship hull structures, desalination equipment, heat exchangers, and offshore platform components, ensuring long-term reliability in harsh marine environments. In the medical industry, Grade 9 titanium plate, due to its excellent biocompatibility and moderate strength, is widely used in the manufacture of orthopedic implants (such as plates and screws), dental implants, and surgical instruments. Furthermore, Grade 9 titanium plate demonstrates its unique value and adaptability in high-end sports equipment (such as bicycle frames and golf club heads), chemical equipment (corrosion-resistant reactors and heat exchangers), and precision mechanical components requiring lightweight and high strength.

Data

Element Composition Range (wt.%)
Ti Balance (>90%)
Al 2.50–3.50%
V 2.00–3.00%
Fe ≤0.25%
O ≤0.13%
C ≤0.08%
N ≤0.03%
H ≤0.015%
Andere ≤0.4% (single element)

Key Characteristics

  • Verhältnis Stärke/Gewicht: Higher than pure titanium (Grades 1–4) but lower than Ti-6Al-4V (Grade 5).
  • Korrosionsbeständigkeit: Excellent in marine, chemical, and chloride environments.
  • Biokompatibilität: Non-toxic and MRI-compatible, but less commonly used in implants than Grade 23.
  • Formability: Superior to Grade 5; suitable for complex forming, welding, and machining.

 Typische Anwendungen

  • Luft- und Raumfahrt: Hydraulic tubing, aircraft fittings, fasteners.
  • Marine: Heat exchangers, seawater components, propeller shafts.
  • Medical: Surgical instruments, non-implantable devices.
  • Industrial: Chemical processing equipment, pressure vessels.
Eigentum Value (Imperial) Value (Metric)
Density 0.160 lb/in³ 4.43 g/cm³
Melting Point 3,000–3,050°F 1,650–1,680°C
Thermal Conductivity 6.5 Btu/(hr·ft·°F) 11.2 W/(m·K)
Coefficient of Thermal Expansion 5.3 × 10⁻⁶/°F 9.5 × 10⁻⁶/K
Electrical Resistivity 120 µΩ·cm 120 nΩ·m

Room Temperature Properties (Annealed Condition)

Eigentum Value (Imperial) Value (Metric)
Zugfestigkeit 130–140 ksi 895–965 MPa
Yield Strength (0.2% offset) 120–125 ksi 825–860 MPa
Elongation 10–15% 10–15%
Reduction in Area 25–30% 25–30%
Härte (Brinell) 280–320 HB 290–330 HBW
Modulus of Elasticity 16.5 × 10⁶ psi 114 GPa

Leistung bei hohen Temperaturen

Temperature (°F) Tensile Strength (ksi) Yield Strength (ksi)
400°F (200°C) 115–125 105–110
600°F (315°C) 100–110 90–95
800°F (425°C) 85–95 75–80

Choose Daxun to help your project take off.

Common applications

Grade 9 titanium plates and sheets are primarily used for components that require an excellent balance of strength, ductility, and corrosion resistance, offering superior weldability and formability compared to other titanium alloys.

  1. Applications include aerospace components such as airframe structures, pressure vessels, and engine components that require moderate strength but exceptional corrosion resistance.
  2. Industrial applications include chemical processing equipment, heat exchangers, and marine components due to their outstanding resistance to corrosive environments.
  3. Oil and gas industry components, including downhole drilling equipment and subsea systems, where both strength and corrosion resistance are critical.
  4. Medical implants and surgical instruments, particularly where biocompatibility and moderate strength are required.
  5. Performance automotive components, including exhaust systems, suspension parts, and high-performance vehicle frames that benefit from titanium’s strength-to-weight ratio.

Fast delivery

Daxun provides customers with timely and fast delivery of grade 9 titanium plate products. Behind the speed is the system support from professional production capacity, and information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected.

titanium plate

Custom Cutting

Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:

  • Water jet cutting
  • Laser cutting
  • Plasma cutting
  • Wire cutting
  • Bending
  • Slitting
  • Sawing

Verpackung

We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
• Boxes and crates
• Shrinkwrap
• Wooden pallets
• Wooden boxes

Technical Support

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.

Daxun Grade 9 Titanium sheet Let your brand improve rapidly

Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of Plate, Bar and Tube.
Products/Processing Standard Grade/Size
Titanium Plate, Sheet, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Thickness:( 0.0197”-6”)Max Width: 12 feet,Max Length: 50 feet)
AMS-T-9046
Titanium and Titanium alloy sheet, plate
Commercially pure titanium (CP)
Code designation Yield strength
minimum, ksi 1 /
CP-1 Gr1 70
CP-2 Gr2 55
CP-3 Gr3 40
CP-4 Gr4 25
Alpha titanium alloys(A)
Code designation Zusammensetzung
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0.8Mo
A-4 8A1-1Mo-1V
Alpha-beta titanium alloys(AB)
Code designation Zusammensetzung
AB-1 Gr5 6A1-4V
AB-2 Gr5 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
Beta titanium alloys(B)
Code designation Zusammensetzung
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
Processing:
Warmwalzen Kaltwalzen
Available Grades:
CP Grade 1 Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2)
CP Grade 2 Grade 6Al-4V ELI (Formerly Grade 23)
Grade 7 Grade 6Al-6V-2Sn (6-62)
Grade 19 Grade 8Al-1Mo-1V (8-1-1)
Grade 5 (6Al-4V) Grade 9 (3Al-2.5V)
Grade 6 (5Al-2.5Sn) CP Grade 3
Anwendung
Chemische Industrie Desalination Of Sea Water
Petrochemical Industry Luft- und Raumfahrt
Machining Field, Automobile Field Mobile Phone Component Field.

Recent hot case projects and products

Grade 9 Titanium Plate and sheet
Naval vessels
Grade 9 Titanium Plate and sheet
Aviation and Aerospace
Titanium Plate and sheet
Military armor
Titanium Plate and sheet
Guidance components
Titanium Plate and sheet
New energy industry
Titanium Plate and sheet
Schiffstechnik
What makes Grade 9 titanium different from other titanium alloys?

Grade 9 titanium (Ti-3Al-2.5V) offers an optimal balance between strength, ductility, and corrosion resistance. It contains 3% aluminum and 2.5% vanadium, which gives it approximately 20-30% higher strength than pure titanium (Grade 1-4) while maintaining excellent formability and weldability that surpasses many other titanium alloys.

What are the main advantages of using Grade 9 titanium plates in industrial applications?

Grade 9 titanium plates provide exceptional corrosion resistance, high strength-to-weight ratio, excellent weldability, and good formability. These properties make them ideal for applications requiring durability in harsh environments while reducing overall weight, which can lead to improved fuel efficiency in transportation applications.

What are the recommended machining practices for Grade 9 titanium plates?

Machining Grade 9 titanium requires slower speeds, lower feed rates, and ample coolant compared to steel or aluminum. Using sharp, high-quality carbide tools with rigid setups is essential. The material has a tendency to work-harden, so maintaining positive cutting action and avoiding dwell times is important for successful machining.

How does Grade 9 titanium perform in marine environments compared to other alloys?

Grade 9 titanium excels in marine environments, offering outstanding resistance to seawater corrosion, crevice corrosion, and stress corrosion cracking. Unlike many stainless steels that may require regular maintenance or replacement in marine applications, Grade 9 titanium can provide decades of service with minimal degradation, making it cost-effective despite higher initial material costs.

Is Grade 9 titanium suitable for welding and fabrication processes?

Yes, Grade 9 titanium is highly suitable for welding and fabrication. It can be welded using TIG, MIG, plasma arc, and electron beam welding processes. The alloy requires proper shielding from atmospheric contamination during welding, but generally offers excellent weldability without the need for post-weld heat treatment in most applications.

How to get a quote OR understand the market information ASAP?

Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email (Daxunalloy@gmail.com) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week

Kann ich ein paar Muster bekommen?

We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.

Which countries have you already exported?

We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.

What is your MOQ?

Our MOQ is 1 ton for titanium sheet.

How long is your delivery time?

Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.

Senden Sie Ihre Anfrage noch heute
Schnelles Angebot