SS 416 stainless steel bars and round bars China supplier
As a leading stainless steel supplier and exporter in China, Daxun supplies stainless steel barsRod (Round Bar)to all over the world.
- Grade: AISI 416-Y1Cr13
- Manufacturing: hot rolled, cold drawn, forged
- Standards: ASTM, ASME, GB, DIN, JIS, ISO
- 416 stainless steel round bar is easy to process
- It is magnetic in both annealed and hardened conditions
- Different heating methods produce a variety of properties
The machinability of most free cutting steels, Stainless Steel 416 Bright Bar (SS 416 Bright Bar) can be enhanced by the addition of sulphur which results in the presence of manganese sulphides. Considering the national and international quality of raw materials, we also offer UNS S41600 Round Bar in customized sizes and thicknesses as per the specific needs of our valued clients at market leading prices.
416 Global leader in stainless rod and Round Bar fabrication services
Grade 416 stainless steel has the highest machinability of any stainless steel, accounting for nearly 85% of easily machinable carbon steels. For most other easily machinable steels, the addition of sulfur improves machinability by forming manganese sulfide inclusions; however, this sulfur addition reduces corrosion resistance, weldability, and formability to levels lower than those of the non-easy machinable equivalent steel, grade 410. Grade 416 stainless steel is sometimes used unhardened or hardened and severely tempered due to its inexpensive cost and simplicity of machining. Martensitic stainless steels are tailored for high hardness, with some compromises on other qualities. Fabrication procedures must accommodate poor weldability and, in most cases, allow for a final hardening and tempering heat treatment. Corrosion resistance is lower than that of normal austenitic grades, and its usable working temperature range is limited by loss of ductility at subzero temperatures and loss of strength at high temperatures owing to over-tempering.
Our network of service centers stock stainless steel bar products for fast, ready supply of bar in common sizes and alloys.We also produce custom-sized stainless steel rods and can arrange inventory schedules for quick turnaround in a timely manner if quantities are below factory minimums.Daxun Alloys stocks stainless steel round bars with diameters ranging from 1/16″ to 26″. Round bars are available in nearly every grade of stainless steel, including 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205, and Alloy 20. Heat treated stainless steel round bars are offered in 17-4PH, H900 temper (on request), H1025, H1150, Double H1150, and H1150M. Other heat-treated tempers can be manufactured upon request. We stock the following 400 series stainless steels: 410, 430, and 416. We also carry 303, 304, and 316/L precision and bearing quality stainless steel round bars. The majority of our inventory consists of our unique machined bar grades: stainless steel round bars that are melted to consistent standards to increase machinability and lower total cost per component. Our stainless steel bar processing machinery allows Daxun Alloys to produce to our customers’ exact specifications.
Данные
- Параметр
- Ingredients
- Механические свойства
- Все эквиваленты
| ASTM A479 416 Round Bar Specification | ASTM A479 / ASTM A479 /ASTM A182 / ASME SA479 / ASME SA479 / ASME SA182 |
| ASTM A479 416 Round Bar Manufacturing Process | Hot Rolled / Cold Rolled / Hot Forging / Rolling / Machining |
| ASTM A479 416 Round Bar Other Grades | 202 / 304 / 304L / 304H / 309S / 310S / 316 / 316L / 316Ti / 317L / 321 / 321H / 347 / 347H / 904L etc. |
| UNS No. – UNS S30400, UNS S30403, UNS S31008, UNS S31620, UNS S31603, UNS S31603, UNS S31635, UNS S31703, UNS S32100, UNS S34700, UNS S34709, UNS S8904 | |
| DIN / EN No. – 1.4301, 1.4307, 1.4845, 1.4401, 1.4404, 1.4571, 1.4438, 1.4541, 1.4550, 1.4551, 1.4539 | |
| AFNOR: Z2 CN 18.10, Z 6 CND 17-11, Z 2 CND 17-12,Z3 CrNi 22.05 AZ | |
| EURONORM: FeMi35Cr20Cu4Mo2, FeMi35Cr20Cu4Mo2, X1CrNiMo17 12 2, X3CrNiMo17 12 2, FeMi35Cr20Cu4Mo2, X2CrNiMoN 22.5.3 | |
| ASTM A479 416 Round Bar Dimension | Round Bars : Outside Diameter in the range of 4mm to 500mm |
| Bright Bars : Outside Diameter in the range of 4mm to 200mm | |
| Hex Bars : 18mm to 57mm (11/16″ to 2-3/4″) | |
| Square Bars : 18mm to 57mm (11/16″ to 2-3/4″) | |
| Flat Bars : 1/2″to 10″in thickness range of 2mm to 150mm, Custom Size Stainless Steel Flats available | |
| ASTM A479 416 Round Bar Length | 2 meters to 7.5 meters ( 8 feet to 24 feet), or Custom Length as per Requirement |
| ASTM A479 416 Round Bar Forms and Shape | Round, Square, Hex (A/F), Rectangle, Billet, Ingot, HRAP, Bright, Shaft, Forging Etc. |
| ASTM A479 416 Round Bar Finish | Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish |
| ASTM A479 416 Round Bar Dimension Standard | ASTM A 484 / ISO h11 / ISO K12 Tolerances F8 / h8, h9, h10, h11, h12, k12, k13, A-484, EN-10060, DIN-1013 etc. |
| ASTM A479 416 Round Bar Heat Treatment | Condition A in which the bars are Annealed |
| Condition H in which the bars are Hardened and Tempered at a relative Temperature | |
| Condition T in which the bars are Hardened and Tempered at a relatively High Temperature | |
| Condition S in which the bars are Strain Hardened or relatively Light Cold Worked | |
| Condition B in which the bars are Relatively severe Cold worked. | |
| Solution Annealed, Aging and Double Aging | |
| ASTM A479 416 Round Bar Surface Finish | Centreless Ground & Belt Polished, up to Ra value = 0.2 um (12 RMS), and Grit Polished of up to 180 to 600 |
| ASTM A479 416 Round Bar Chamfering | Available in 30°, 45° & 60° through fully automatic, both-end chamfering machine |
| ASTM A479 416 Round Bar Other Testing | NACE MR0175, IGC TEST, Intergranular Corrrosion Test as per ASTM A262 Practice E, Charpy Impact Test, Macro, Grain Size, Hardness, Magnetic Particle Inspection (MPI), 100% tested thru Digital Ultrasonic Flaw Detector, as per ASTM A-388, EN 10308 (class 1to4),API 6A/ISO 10423:2003-PSL3,SEP 1920:1984 ( class A,B,C), MIL STD 2154 etc. |
| ASTM A479 416 Round Bar Value Added Services | Rolling, Drill, Punch, CNC Machining, Sand Blasting, Shot Blasting, Heat Treatment, Anti-rust Paint, Polishing |
| ASTM A479 416 Round Bar Packaging | Loose / Carrate / Wooden Pallet / Wooden Box / Plastic Cloth Wraps |
| ASTM A479 416 Round Bar Shipment & Transportation | По дороге - грузовик / поезд с частичной загрузкой, полная загрузка, По морю - обычное судно типа Break-bulk / FCL (полный контейнерный груз) / LCL (меньший контейнерный груз) / 20 футовый контейнер / 40 футовый контейнер / 45 футовый контейнер / контейнер High Cube / контейнер Open Top, По воздуху - гражданские пассажирские и грузовые самолеты Freighter |
| ASTM A479 416 Round Bar Material Test Certificate | Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS, Bureau of CHINA Standards BIS Approved ETC |
| ASTM A479 416 Round Bar Documentation | Commercial Invoice which includes HS Code / Packing List including net weight and gross weight, number of boxes, Marks and Numbers / Certificate of Origin legalized/attested by Chamber of Commerce or Embassy / Fumigation Certificates / Raw Material Test Reports / Material Traceability Records / Quality Assurance Plan (QAP) / Heat Treatment Charts / Test Certificates certifying NACE MR0103, NACE MR0175 / Material Test Certificates (MTC) as per EN 10204 3.1 and EN 10204 3.2 / Guarantee Letter / NABL approved Laboratory Test Reports / Welding Procedure Specification/Procedure Qualification Record, WPS/PQR / Form A for the purposes of the Generalized System of Preferences (GSP) |
| Chemical Composition Limits | ||||||||
| Weight% | C | P | Si | Mn | S | Cr | Fe | Se |
| Alloy 416 Type 1 | 0.15 max | 0.060 max | 1 max | 1.25 max | 0.40 max | 11.50-13.50 | bal | 0.18-0.35 |
| Alloy 416 Type 2 | 0.15 max | 0.060 max | 1 max | 2.50 max | 0.40 max | 11.50-13.50 | bal | - |
| Материал | Tempering Temp °F (°C) | 0.2 % Yield Strength (Mpa) | Tensile Strength (Mpa) | % Elongation in 2″ | % Reduction of Area | Hardness Brinell |
| SS 416 | 300 (149) | 1034 | 1344 | 10 | 40 | 390 |
| SS 416 | 500 (260) | 979 | 1276 | 13 | 45 | 375 |
| SS 416 | 700 (371) | 1007 | 1310 | 13 | 48 | 390 |
| SS 416 | 900 (482) | 896 | 1158 | 14 | 50 | 341 |
| SS 416 | 1000 (538) | 793 | 1000 | 15 | 50 | 300 |
| SS 416 | 1100 (593) | 689 | 862 | 17 | 53 | 262 |
| SS 416 | 1200 (650) | 586 | 758 | 18 | 55 | 225 |
| СТАНДАРТ | ВЕРКСТОФФ НР. | UNS | JIS | BS | AFNOR | EN |
| SS 416 | 1.4005 | S41600 | SUS 416 | 416S21 | - | X12CrS13 |
Выберите Daxun и сделайте своих клиентов довольными.
Quick response-416 Stainless Steel Rod
We provide customers with timely and fast delivery of 416 stainless steel bar products. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to ports and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Преимущества Daxun
- Varieties: We offer a wide range of sizes and grades, including 300 series, 400, 600 series, and more.
- Flexibility: Whether you need hot-rolled or cold-drawn bars, our stainless steel bar lengths are designed to meet your specific project requirements.
- Quality Standards: Our 416 Stainless Steel Rod meet strict ASTM, ISO9001, GB, NSF/ANSI standards to ensure reliability and performance.
- Custom Orders: Looking for special sizes of stainless steel bars? We offer a variety of stainless steel bar customization options with competitive prices and convenient online ordering.

416 Stainless Steel Rod packaging
We pay attention to every process to ensure quality. The 416 round steel packaging we usually adopt is to pack the stainless steel round bars with environmentally friendly plastic bags and then put them into fumigation-free wooden boxes or wooden pallets. Customized packaging such as OEM can also be negotiated. We provide almost everything to meet your round bar packaging requirements. We attach great importance to packaging. The round bars are packed in wooden corrugated boxes, wrapped with plastic packaging and bubble film on the outside.
Качество, доставка, проверка
- Daxun также проводит несколько тестов для обеспечения качества. Эти тесты включают в себя испытание на сплющивание, испытание на точечную коррозию и стойкость, механическое испытание, испытание на твердость, положительную идентификацию материала, испытание на расширение и т.д. Все эти испытания гарантируют, что материал подходит для требуемого применения.
- В процессе производства мы измеряем диаметр, толщину и поверхность изделия. Наш стандартный срок поставки составляет 7-15 дней, за исключением некоторых изделий специального размера, срок поставки увеличивается до 20 дней.
Сроки доставки строго соответствуют договору. - Поддержка сторонних агентств клиентов для посещения завода для проверки
- Поддержка бесплатных образцов для клиентов для тестирования
- Поддержка инспекции на месте или видеоинспекции на заводе
Техническая поддержка
Если вам потребуется дополнительная техническая помощь, наш постоянный металлург и компетентный персонал будут рады помочь. Кроме того, Daxun может похвастаться сертифицированной испытательной лабораторией - впервые в отрасли производства инвентаря из нескольких металлов и пластика. Это, по нашему мнению, демонстрирует нашу неизменную приверженность качеству и философию поставщика полного цикла.
416 Stainless Steel Rod Ordering Information
Purchase orders for 416 round bars shall include quantity, PSL grade, type or category, API5L reference, diameter, surface finish, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish, or end treatment. Bars are solution bright annealed.
SS 416 Stainless Steel Rod Features
Сплав Daxun Пусть ваш бренд быстро улучшается
- Галерея
- Состояние доставки
- Age Hardening
| Выбор государства доставки | Состояние поверхности |
| Кованые | Black |
| Полированный | |
| Горячекатаный | Black |
| Полированный | |
| Яркий | |
| Маринованные | |
| Холодная вытяжка | Полированный |
| Яркий | |
| Примечание: | |
| 1. Если вам требуется другое состояние доставки, чем перечисленные выше, пожалуйста, подтвердите с нами. | |
| 2. В случае запроса или заказа, пожалуйста, сообщите нам о любых дополнительных требованиях, не указанных здесь. | |
| Material in the solution annealed condition may be age hardened as follows:-*Denotes Double Overaged | ||||||||||||
| Condition | H900 (H480) | H925 (H495) | H1025 (H550) | H1075 (H580) | H1100 (H595) | H1150 (H620) | H1150M (H620M)* | Plus | H1150D (H620D)* | Plus | ||
| Heat to | ±15oF | 900oF | 925 oF | 1025oF | 1075oF | 1100oF | 1150oF | 1400oF | 1150oF | 1150oF | 1150oF | |
| ±9oC | 480oC | 495oC | 550oC | 580oC | 595oC | 620oC | 760oC | 620oC | 620oC | 620oC | ||
| Hold for Hours | 1 | 4 | 4 | 4 | 4 | 4 | 2 | 4 | 4 | 4 | ||
| Cool to Below | Air | Air | Air | Air | Air | Air | Air | Air | Air | Air | ||
| 90oF (32oC) | ||||||||||||
Types of SS 416 Stainless Steel Rods (6)
Информация доступна для ознакомления и скачивания
Stainless Steel Rod Production
Daxun is a trustworthy stainless steel rod and bar manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless rod are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 416 Stainless Steel Rod have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
Последние проекты и продукты для горячих случаев
Сопутствующие товары (12)
We can provide 416 Stainless Steel Rod samples for you to check the quality. Sample is free and you just pay the freight.
Мы экспортировали продукцию в более чем 42 страны, такие как Канада, Чили, Кувейт, Германия, Южная Корея, Саудовская Аравия, Сингапур и др.
Our MOQ is 1 ton for 416 Stainless Steel Rod.
Пробные заказы могут быть доставлены в течение недели. Для обычных заказов требуется примерно две недели.