Daxun Alloy - Hastelloy C2000 pipe made in China
As a leading supplier of Hastelloy C2000 pipes in China, Daxun provides high-performance alloy tubes to the world.
- Hastelloy C2000 types: Seamless tube, welded tube, forged tube
- Сертификация: ASTM, SGS, ISO,CE
- Срок поставки: 7-15 дней
- Обработка поверхности: Отжиг, полировка и т.д.
- MOQ : ≥300 кг
————Компания Daxun производит трубы из хастеллоя в Китае для удовлетворения разнообразных и ——требовательные потребности клиентов!
Characteristics & Properties of Hastelloy C2000
Hastelloy C2000 pipe is a nickel-based alloy pipe with excellent performance, which plays an important role in many industrial fields.It entered the market in late 1995 and has been highly recognized by the market for its versatility.
In terms of composition, it cleverly combines multiple key elements such as nickel, chromium, and molybdenum. Nickel gives the pipe good toughness and basic corrosion resistance; chromium enhances its corrosion resistance in oxidizing environments, enabling it to resist the erosion of various oxidizing media; molybdenum significantly improves the pipe’s resistance to pitting and crevice corrosion in reducing acids, greatly expanding its application range.
Hastelloy C2000 pipe has extremely excellent corrosion resistance. Whether facing harsh chemical media such as strong acids and alkalis, or in extreme environments such as high temperature and high pressure, it can maintain stable chemical properties and effectively resist corrosion. In the chemical industry, many chemical reaction processes will produce extremely corrosive substances, which ordinary pipes cannot withstand, but Hastelloy C2000 pipes can operate stably for a long time to ensure the normal operation of production equipment.
Its mechanical properties are also excellent. It has high strength and good toughness, and can withstand certain pressure and impact without deformation or rupture. This makes it an ideal choice for some occasions that require high mechanical properties of pipes, such as high-pressure pipeline systems and large reaction vessels.
In practical applications, Hastelloy C2000 pipes are widely used. In the petrochemical industry, it is often used in pipeline systems that transport various corrosive media to ensure the safety and stability of the petrochemical production process; in the field of marine engineering, due to its excellent seawater corrosion resistance, it is widely used in seawater desalination equipment, offshore platform pipelines and other facilities; in the power industry, it can be used to manufacture key components such as boiler feed water pipelines to ensure efficient power production.
However, due to the special material and properties of Hastelloy C2000 pipes, its processing difficulty is relatively large. During the welding process, it is necessary to strictly control the welding process parameters and use appropriate welding methods and materials to ensure the welding quality. Otherwise, welding defects are prone to occur, affecting the performance and service life of the pipe.
Hastelloy C2000 Parameters
- Химический состав
- Физические свойства
- Механические свойства
| Ni | Cr | Mo | W | Cu | Fe | C | Mn |
| 55% – 62% | 15% – 23%| | 6% – 16% | 2% – 4.5% | 1.3% – 1.9% | ≤3.0% | ≤0.01% – 0.25% | ≤0,5% |
| Si | P | S | Al | Ti | Nb | Co | |
| ≤0.08% – 0.080% | ≤0.02% | ≤0.08% | ≤0.3 – 0.5%≤0.2 – 0.5% | ≤3% | ≤2% |
| Недвижимость | Плотность | Температура плавления | Specific Heat Capacity | Теплопроводность | Электрическое сопротивление | Coefficient of Thermal Expansion | Модуль упругости | Твердость | Operating Temperature |
| Значение | 8.4 – 10.6 g/cm³ | 1280 – 1350°C | 0.102 – 0.46 J/(g·°C) | 7 – 13 W/m·K | 1.4 – 1.6 Ω·mm²/m | 12.4 – 20.0 μm/(m·°C) | 206 ГПа | 132 – 247 HB | -196°Cto650°C |
| Недвижимость | Прочность на разрыв | Предел текучести | Удлинение | Reduction of Area | Impact Toughness | Твердость |
| Значение | 752 – 1090MPa | 345 – 750MPa | 20% – 62% | ≥40% | ≥90J | 132 – 247HB |
Выберите Daxun, чтобы помочь вашему проекту взлететь.

Передовое производство: Труба из сплава хастеллоя
Hastelloy C2000 alloy is an all-around nickel-chromium-molybdenum-tungsten alloy with good resistance to pitting, crevice corrosion and stress corrosion cracking. It has excellent resistance to oxidative aqueous media, including wet chlorine, nitric acid or mixed acids of oxidizing acids containing chloride ions. At the same time, Hastelloy C2000 alloy also has ideal resistance to reducing and oxidizing environments encountered in the process. Relying on this versatile performance, it can be used in some troublesome environments or in factories for a variety of production purposes.
Hastelloy C-2000 Pipe Features
Hastelloy C2000 alloy has an exceptional resistance to various chemical environments, including strong oxidizing substances, such as ferric chloride, cupric chloride, chlorine, thermally contaminated solutions (organic and inorganic), formic acid, acetic acid, acetic anhydride, seawater and salt solutions, etc. Hastelloy C2000 alloy has the ability to resist the formation of grain boundary precipitation in the heat affected zone of welding, so that it can also be used in many chemical processes in the welding state.


Качество, доставка, проверка
Daxun conducts a series of quality assurance tests on Hastelloy C2000 pipes. These tests include flattening test, flaring test, ultrasonic flaw detection, crevice corrosion resistance test, mechanical property test, hardness test, material positive identification, and expansion test, etc. All these tests are designed to ensure that the Hastelloy C2000 pipes meet the requirements of the intended applications. During the production process, we meticulously measure the outer diameter, wall thickness, and surface quality of the products. Our standard delivery time is 5 – 7 days, and for special sizes, it is 15 – 20 days.
- Сроки доставки строго соответствуют договору.
- Поддержка сторонних агентств клиентов для посещения завода для проверки
- Поддержка бесплатных образцов для тестирования клиентов
- Поддержка инспекции на месте или видеоинспекции на заводе
Упаковка
Daxun Alloy обеспечивает наилучшее качество упаковки, поскольку она играет важную роль в международных перевозках, где товары проходят через различные каналы, чтобы достичь конечного пункта назначения, поэтому мы уделяем особое внимание упаковке. Мы упаковываем наши товары различными способами в зависимости от продукта. Мы упаковываем наши товары различными способами, такими как:
- Коробки и ящики
- Термоусадочная пленка
- Деревянные поддоны
- Деревянные ящики


Техническая поддержка
Если вам нужна дополнительная техническая помощь, наш постоянный металлург и компетентный персонал будут рады помочь. [Свяжитесь с нами сейчас]Кроме того, Daxun может похвастаться сертифицированной испытательной лабораторией - впервые в отрасли производства инвентаря из нескольких металлов и пластика. Это, по нашему мнению, свидетельствует о нашей неизменной приверженности качеству и философии поставщика полного спектра услуг.
Daxun является надежным производителем труб из нержавеющей стали
Будучи профессиональным производителем, компания Daxun гарантирует высокое качество всех выпускаемых нами изделий. Поэтому мы гарантируем, что все титановые трубы сертифицированы по ISO9001, SGS, CE, OQC и другим международным стандартам качества. Мы также проводим строгий контроль качества, чтобы гарантировать, что трубы из нержавеющей стали имеют меньше дефектов. В Daxun вы можете быть уверены, что все продукты долговечны, высококачественны и превосходны по своим характеристикам.
Сопутствующие товары (8)
Пожалуйста, заполните форму на странице “Контакты” или позвоните нашему менеджеру по продажам по телефону “+86 13382898899”, мы свяжемся с вами в кратчайшие сроки. Наш WhatsApp работает в режиме онлайн, а электронная почта (Daxunalloy@gmail.com) будет проверена в течение 6 часов. На каждый запрос или сообщение мы ответим незамедлительно. Кроме того, каждую неделю мы делимся с нашими клиентами информацией о рынке
Мы можем предоставить вам образцы листов из нержавеющей стали для проверки качества. Образец бесплатен, и вы просто оплачиваете перевозку.
Мы экспортировали продукцию в более чем 42 страны, такие как Канада, Чили, Кувейт, Германия, Южная Корея, Саудовская Аравия, Сингапур и др.
Минимальный объем заказа для нашей продукции из хастеллоя составляет 300 кг.
Пробные заказы могут быть доставлены в течение недели. Для обычных заказов требуется примерно две недели.