Daxun is a 316/316L stainless steel angle steel supplier in China
As a leading stainless steel angle steel supplier and exporter in China, Daxun supplies stainless steel angle steel to all over the world.
- Grade: S31600(316)-S31603(316L)
- Equal Angle Steel/Unequal Angle Steel
- Process: hot rolling and laser welding
- Easy to weld and process
- Length can be cut to size
- Daxun specializes in custom stainless steel angles with fast delivery and competitive prices. Contact Daxun today.
Global leader in stainless steel angle fabrication services
304/304L and 316/316L Stainless Steel Angles
As China’s premier supplier of specialty metals, you can trust Daxun for all of your stainless steel angle needs. Our stainless steel angle selection includes 304/304L and 316/316L stainless steel angles. Our extensive product line offers durability and versatility, making it the perfect solution for your structural and fabrication needs.
Our stainless steel angles are available in 304/304L and 316/316L, all from fully certified factories. Our comprehensive product line is both durable and adaptable, ideal for structural and fabrication applications. As a leading stainless steel angle manufacturer, we offer a wide range of specialty angles and L-shaped angles. Daxun offers stainless steel angles in any length, up to 6 meters. The following stainless steel grades are also available: 304/304L and 316/316L. Stainless steel angles are most commonly used for supports or frames, but are also used in food equipment, building supports, structural supports, and medical equipment.
Can be welded and processed using simple procedures, 304/304L stainless steel angles are suitable for many environments, such as general industrial projects, chemical projects. While 316/316L angles are marine grade and have strong corrosion resistance in more demanding conditions.
The surface treatment we use on our stainless steel angles is hot rolling, annealing, and pickling. This surface treatment maximizes corrosion resistance and gives the angles a unique “stainless” appearance.
The two manufacturing methods are laser melting and hot rolling. Hot rolling produces stainless steel angles at a lower price. They usually have rounded or tapered edges. On the other hand, laser melted stainless steel angles have consistent sharp and square corners. They also have a sandblasted, smoother surface. Laser melted stainless steel angles have a smoother surface quality than hot rolled stainless steel angles.
Daxun Alloy manufactures laser melted and hot rolled stainless steel angles in metric and imperial sizes. We can ship them all over the world.
Данные
- Параметр
- Элемент
- Механические свойства
- ФИЗИЧЕСКИЕ СВОЙСТВА
- Все эквиваленты
| Стандарт | ASTM、EN、DIN、JIS,ASME, BS, GBetc, |
| Dimensions | ∠20*20*3mm-∠200*200*24mm |
| Сплав | 201, 310, 304, 304L, 316, 316L |
| Тип | Equal, Unequal |
| Длина | 1.0-12.0m |
| Толщина | 3mm-25mm |
| Custom Options | Yes |
| Допуски | ± ¼”, ± 1/16” |
| Finish | Mill, brush, mirror, polished |
| CHEMICAL COMPOSITION: ASTM A240, A666 | ||
| Элемент | Type 316 | Type 316L |
| Углерод | 0.08 max. | 0.030 max. |
| Марганцовка | 2.00 max. | 2.00 max. |
| Сера | 0.030 max. | 0.030 max. |
| Фосфор | 0.045 max. | 0.045 max. |
| Кремний | 0.75 max. | 0.75 max. |
| Хром | 16.0 – 18.0 | 16.0 – 18.0 |
| Никель | 10.00 – 14.00 | 10.00 – 14.00 |
| Molybdenum | 2.00 – 3.00 | 2.00 – 3.00 |
| Азот | 0.10 max. | 0.10 max. |
| Тип | Предел текучести 0,2% смещение (KSI) | Прочность на разрыв (KSI) | % Elongation (2″ Gauge length) |
| 316 | 30 min. | 75 мин. | 40 min. |
| 316L | 25 min. | 70 min. | 40 min. |
| Плотность (фунт/дюйм^2) @ RT | 0.29 | |
| Модуль упругости при растяжении (psi x 10^6) | 28 | |
| Удельная теплота (BTU/Ф/фунт) | От 32 до 212 oF | 0.12 |
| Теплопроводность (BTU/hr/ft^2/ft) | 212oF | 9.4 |
| 932oF | 12.4 | |
| Средний коэффициент теплового расширения (в дюймах x 10^-6 на o F) | От 32 до 212oF | 8.9 |
| От 32 до 600oF | 9 | |
| От 32 до 1,000oF | 9.7 | |
| 32 to 1,200oF | 10.3 | |
| Электрическое сопротивление (микро Ом - см) | при 70oF | 29.4 |
| Диапазон температуры плавления (oF) | 2500 – 2550 |
| Класс | UNS No | Старая Британия | Евронорм | Шведский эсэсовец | Японский JIS | ||
| BS | En | Нет | Имя | ||||
| 316l | S31603 | 316S11 | – | 1.4404 | X2CrNiMo17-12-2 | 2348 | SUS 316L |
Выберите Daxun и сделайте своих клиентов довольными.

Быстрый ответ
Мы обеспечиваем своевременную и быструю доставку продукции из нержавеющей стали для клиентов со срочными потребностями. За скоростью стоит системная поддержка - от информационных потоков до логистики и движения капитала. Например, с точки зрения информационного потока, данные о заказах Daxun поступают в логистическую систему в режиме реального времени, и данные беспрепятственно соединяются; с точки зрения логистики, центр обработки находится вблизи автомагистралей, рек и морей, с разумным планированием, быстрым реагированием, хранением и транспортировкой, эффективной погрузкой, что обеспечивает выполнение задачи в срок. Материалы из нержавеющей стали Daxun имеют надежное качество, а их сорта, технические характеристики и вес поставки строго соответствуют стандартам.
Преимущества Daxun
Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel uses the ERP system to achieve full traceability of each angle steel, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.


Упаковка
Daxun Alloy обеспечивает наилучшее качество упаковки, поскольку она играет важную роль в международных перевозках, где товары проходят через различные каналы, чтобы достичь конечного пункта назначения, поэтому мы уделяем особое внимание упаковке. Мы упаковываем наши товары различными способами в зависимости от продукта. Мы упаковываем наши товары различными способами, такими как:
- Коробки и ящики
- Термоусадочная пленка
- Деревянные поддоны
- Деревянные ящики
Качество, доставка, проверка
- Daxun также проводит несколько тестов для обеспечения качества. Эти тесты включают в себя испытание на сплющивание, испытание на точечную коррозию и стойкость, механическое испытание, испытание на твердость, положительную идентификацию материала, испытание на расширение и т.д. Все эти испытания гарантируют, что материал подходит для требуемого применения.
- В процессе производства мы измеряем диаметр, толщину и поверхность изделия. Наш стандартный срок поставки составляет 7-15 дней, за исключением некоторых изделий специального размера, срок поставки увеличивается до 20 дней.
Сроки доставки строго соответствуют договору. - Поддержка сторонних агентств клиентов для посещения завода для проверки
- Поддержка бесплатных образцов для клиентов для тестирования
- Поддержка инспекции на месте или видеоинспекции на заводе


Информация для заказа
Заказы на поставку должны включать количество, сорт, тип или категорию, ссылку на API5L, толщину, ширину, длину, а также любые применимые приложения или дополнительные требования, связанные с химическим составом, механическими свойствами, термообработкой, дополнительными испытаниями, процессом производства, покрытием поверхности или конечной отделкой. Свяжитесь с Daxun сейчас, мы ответим на ваше письмо как можно скорее.
Техническая поддержка
Если вам потребуется дополнительная техническая помощь, наш постоянный металлург и компетентный персонал будут рады помочь. Кроме того, Daxun может похвастаться сертифицированной испытательной лабораторией - впервые в отрасли производства инвентаря из нескольких металлов и пластика. Это, по нашему мнению, демонстрирует нашу неизменную приверженность качеству и философию поставщика полного цикла.

SS 316-316L Stainless Steel angle Features
Сплав Daxun Пусть ваш бренд быстро улучшается
- Specification Table
| Angle – Steel Data | |||||||||||||
| EQUAL AND UNEQUAL ANGLE | |||||||||||||
| ANGLE is available in other sizes on request | |||||||||||||
| Description | Width (W) | Depth (D) | Толщина | Стандарт | Weight per | Поверхность | |||||||
| (mm) | (mm) | (T) (mm) | Длина | Metre | Area per | ||||||||
| (kg/m) | Metre | ||||||||||||
| (m²/m) | |||||||||||||
| ANGLE 20 X 20 X 3.0mm | 20 | 20 | 3 | 6.0 metres | 0.98 | 0.0897 | |||||||
| ANGLE 25 X 25 X 3.0mm | 25 | 25 | 3 | 7.5 metres | 1.12 | 0.0953 | |||||||
| ANGLE 25 X 25 X 5.0mm | 25 | 25 | 5 | 7.5 metres | 1.65 | 0.0953 | |||||||
| ANGLE 25 X 25 X 6.0mm | 25 | 25 | 6 | 7.5 metres | 2.08 | 0.0953 | |||||||
| ANGLE 30 X 30 X 2.5mm | 30 | 30 | 2.5 | 6.0 metres | 1.06 | 0.117 | |||||||
| ANGLE 30 X 30 X 3.0mm | 30 | 30 | 3 | 7.5 metres | 1.35 | 0.115 | |||||||
| ANGLE 30 X 30 X 5.0mm | 30 | 30 | 5 | 7.5 metres | 2.01 | 0.115 | |||||||
| ANGLE 30 X 30 X 6.0mm | 30 | 30 | 6 | 7.5 metres | 2.56 | 0.115 | |||||||
| ANGLE 40 X 40 X 2.5mm | 40 | 40 | 2.5 | 6.0 metres | 1.43 | 0.157 | |||||||
| ANGLE 40 X 40 X 3.0mm | 40 | 40 | 3 | 7.5 metres | 1.83 | 0.155 | |||||||
| ANGLE 40 X 40 X 4.0mm | 40 | 40 | 4 | 6.0 metres | 2.2 | 0.155 | |||||||
| ANGLE 40 X 40 X 5.0mm | 40 | 40 | 5 | 9.0 metres | 2.73 | 0.155 | |||||||
| ANGLE 40 X 40 X 6.0mm | 40 | 40 | 6 | 9.0 metres | 3.5 | 0.155 | |||||||
| ANGLE 45 X 45 X 3.0mm | 45 | 45 | 3 | 9.0 metres | 2.06 | 0.175 | |||||||
| ANGLE 45 X 45 X 5.0mm | 45 | 45 | 5 | 9.0 metres | 3.1 | 0.175 | |||||||
| ANGLE 45 X 45 X 6.0mm | 45 | 45 | 6 | 9.0 metres | 3.97 | 0.175 | |||||||
| ANGLE 50 X 50 X 2.5mm | 50 | 50 | 2.5 | 9.0 metres | 1.81 | 0.197 | |||||||
| ANGLE 50 X 50 X 3.0mm | 50 | 50 | 3 | 7.5 metres | 2.31 | 0.195 | |||||||
| ANGLE 50 X 50 X 4.0mm | 50 | 50 | 4 | 9.0 metres | 2.79 | 0.195 | |||||||
| ANGLE 50 X 50 X 5.0mm | 50 | 50 | 5 | 9.0 metres | 3.48 | 0.195 | |||||||
| ANGLE 50 X 50 X 6.0mm | 50 | 50 | 6 | 9.0 metres | 4.46 | 0.195 | |||||||
| ANGLE 50 X 50 X 8.0mm | 50 | 50 | 8 | 9.0 metres | 5.68 | 0.195 | |||||||
| ANGLE 55 X 55 X 5.0mm | 55 | 55 | 5 | 9.0 metres | 3.84 | 0.215 | |||||||
| ANGLE 55 X 55 X 6.0mm | 55 | 55 | 6 | 9.0 metres | 4.93 | 0.215 | |||||||
| ANGLE 65 X 50 X 5.0mm | 65 | 50 | 5 | 9.0 metres | 4.02 | 0.225 | |||||||
| ANGLE 65 X 50 X 6.0mm | 65 | 50 | 6 | 9.0 metres | 5.16 | 0.225 | |||||||
| ANGLE 65 X 50 X 8.0mm | 65 | 65 | 8 | 9.0 metres | 6.59 | 0.225 | |||||||
| ANGLE 65 X 65 X 4.0mm | 65 | 65 | 4 | 9.0 metres | 3.69 | 0.255 | |||||||
| ANGLE 65 x 65 x 5.0mm | 65 | 65 | 5 | 9.0 metres | 4.56 | 0.255 | |||||||
| ANGLE 65 X 65 X 6.0mm | 65 | 65 | 6 | 9.0 metres | 5.87 | 0.255 | |||||||
| ANGLE 65 X 65 X 8.0mm | 65 | 65 | 8 | 9.0 metres | 7.51 | 0.255 | |||||||
| ANGLE 65 X 65 X 10.0mm | 65 | 65 | 10 | 9.0 metres | 9.02 | 0.255 | |||||||
| ANGLE 75 X 50 X 5.0mm | 75 | 50 | 5 | 9.0 metres | 4.4 | 0.244 | |||||||
| ANGLE 75 X 50 X 6.0mm | 75 | 50 | 6 | 9.0 metres | 5.66 | 0.244 | |||||||
| ANGLE 75 X 50 X 8.0mm | 75 | 50 | 8 | 9.0 metres | 7.23 | 0.244 | |||||||
| ANGLE 75 X 75 X 4.0mm | 75 | 75 | 4 | 9.0 metres | 4.29 | 0.295 | |||||||
| ANGLE 75 X 75 X 5.0mm | 75 | 75 | 5 | 9.0 metres | 5.27 | 0.292 | |||||||
| ANGLE 75 X 75 X 6.0mm | 75 | 75 | 6 | 9.0 metres | 6.81 | 0.292 | |||||||
| ANGLE 75 X 75 X 8.0mm | 75 | 75 | 8 | 9.0 metres | 8.73 | 0.292 | |||||||
| ANGLE 75 X 75 X 10.0mm | 75 | 75 | 10 | 9.0 metres | 10.5 | 0.292 | |||||||
| ANGLE 90 X 90 X 6.0mm | 90 | 90 | 6.0 | 9.0 metres | 8.22 | 0.352 | |||||||
| ANGLE 90 X 90 X 8.0mm | 90 | 90 | 8.0 | 9.0 metres | 10.6 | 0.352 | |||||||
| ANGLE 90 X 90 X 10.0mm | 90 | 90 | 10.0 | 9.0 metres | 12.7 | 0.352 | |||||||
| ANGLE 100 X 75 X 6.0mm | 100 | 75 | 6.0 | 9.0 metres | 7.98 | 0.342 | |||||||
| ANGLE 100 X 75 X 8.0mm | 100 | 75 | 8.0 | 9.0 metres | 10.3 | 0.342 | |||||||
| ANGLE 100 X 75 X 10.0mm | 100 | 75 | 10.0 | 9.0 metres | 12.4 | 0.342 | |||||||
| ANGLE 100 X 100 X 10.0mm | 100 | 100 | 10.0 | 9.0 metres | 14.2 | 0.392 | |||||||
| ANGLE 100 X 100 X 12.0mm | 100 | 100 | 12.0 | 9.0 metres | 17.7 | 0.392 | |||||||
| ANGLE 100 X 100 X 4.0mm | 100 | 100 | 4.0 | 9.0 metres | 5.78 | 0.395 | |||||||
| ANGLE 100 X 100 X 6.0mm | 100 | 100 | 6.0 | 9.0 metres | 9.16 | 0.392 | |||||||
| ANGLE 100 X 100 X 8.0mm | 100 | 100 | 8.0 | 9.0 metres | 11.8 | 0.392 | |||||||
| ANGLE125 X 75 X 6.0mm | 125 | 75 | 6.0 | 9.0 metres | 9.16 | 0.392 | |||||||
| ANGLE 125 X 75 X 8.0mm | 125 | 75 | 8.0 | 9.0 metres | 11.8 | 0.392 | |||||||
| ANGLE 125 X 75 X 10.0mm | 125 | 75 | 10.0 | 9.0 metres | 14.2 | 0.392 | |||||||
| ANGLE 125 X 75 X 12.0mm | 125 | 75 | 12.0 | 9.0 metres | 17.7 | 0.392 | |||||||
| ANGLE 125 X 125 X 8.0mm | 125 | 125 | 8.0 | 9.0 metres | 14.9 | 0.491 | |||||||
| ANGLE 125 X 125 X 10.0mm | 125 | 125 | 10.0 | 9.0 metres | 18 | 0.491 | |||||||
| ANGLE 125 X 125 X 12.0mm | 125 | 125 | 12.0 | 9.0 metres | 22.5 | 0.491 | |||||||
| ANGLE 125 X 125 X 16.0mm | 125 | 125 | 16.0 | 9.0 metres | 29.1 | 0.491 | |||||||
| ANGLE 150 X 90 X 8.0mm | 150 | 90 | 8.0 | 9.0 metres | 14.3 | 0.471 | |||||||
| ANGLE 150 X 90 X 12.0mm | 150 | 90 | 12.0 | 9.0 metres | 21.6 | 0.471 | |||||||
| ANGLE 150 X 90 X 16.0mm | 150 | 90 | 16.0 | 9.0 metres | 27.9 | 0.471 | |||||||
| ANGLE 150 X 100 X 10.0mm | 150 | 100 | 10.0 | 9.0 metres | 18 | 0.491 | |||||||
| ANGLE 150 X 100 X 12.0mm | 150 | 100 | 12.0 | 9.0 metres | 22.5 | 0.491 | |||||||
| ANGLE 150 X 150 X 10.0mm | 150 | 150 | 10.0 | 9.0 metres | 21.9 | 0.59 | |||||||
| ANGLE 150 X 150 X 12.0mm | 150 | 150 | 12.0 | 9.0 metres | 27.3 | 0.59 | |||||||
| ANGLE 150 X 150 X 16.0mm | 150 | 150 | 16.0 | 9.0 metres | 35.4 | 0.59 | |||||||
| ANGLE 150 X 150 X 19.0mm | 150 | 150 | 19.0 | 9.0 metres | 42.1 | 0.59 | |||||||
| ANGLE 150 X 90 X 10.0mm | 150 | 90 | 10.0 | 9.0 metres | 17.3 | 0.471 | |||||||
| ANGLE 200 x 200 x 13.0mm | 200 | 200 | 13.0 | 9.0 metres | 40 | 0.788 | |||||||
| ANGLE 200 X 200 X 16.0mm | 200 | 200 | 16.0 | 9.0 metres | 48.7 | 0.788 | |||||||
| ANGLE 200 X 200 X 20.0mm | 200 | 200 | 20.0 | 9.0 metres | 60.1 | 0.788 | |||||||
| ANGLE 200 X 200 X 26.0mm | 200 | 200 | 26.0 | 9.0 metres | 76.8 | 0.788 | |||||||
SS 316/316L Stainless Steel Angle Surface Type (3)
Информация доступна для ознакомления и скачивания
Daxun is a trustworthy stainless steel Angle manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel angles have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
Последние проекты и продукты для горячих случаев
Сопутствующие товары (8)
Leading stainless steel angle Suppliers in China
Daxun has been engaged in international business for more than ten years. In 2023, the export volume exceeded 100 million US dollars, and the export volume ranked among the top Chinese stainless steel manufacturers. Daxun continuously improves its service skills. To serve the global market, it has established three export service facilities in China, cooperating with engineering companies, steel mills, and international trading companies. Daxun provides stainless steel chain services and has established long-term cooperative relations with dozens of well-known steel mills around the world. The inventory includes 50,000 tons of conventional stainless steel and 20,000 tons of duplex steel, nickel-based alloys, heat-resistant steel and other metals. Daxun’s stainless steel materials are of stable quality, and the varieties, specifications, and delivery weights strictly meet the standards.
316 Stainless Steel Angle
- 316 Stainless Steel Angle is an austenitic chromium nickel angle shape containing molybdenum which provides superior corrosion resistance and increased strength at elevated temperatures when compared to 304 Stainless.
- Because of the 4% molybdenum concentration, the 316 material is resistant to chloride ion stress corrosion. Stainless Steel 304 Unequal Angle Sizes vary depending on the application needs. Angles are used to hold components together using a grip. There are also angles with bolt holes for screws and bolts. The 316 Stainless Steel Unequal Angle is suitable for more corrosive applications than the 304 angles. The Stainless Steel Unequal Angle is just as frequent as the Equal Angle. They are utilized in a variety of applications, including brackets, trim, and reinforcements. Please contact us for more information about the angles and their costs.
Characteristics
- Cold Working: Good
- Corrosion Resistance: Excellent
- Heat Resistance: Good
- Heat Treatment: Poor
- Hot Working: Fair
- Machinability: Good
- Weldability: Very Good
Why should you buy stainless steel angles from Daxun?
Daxun’s objective is to supply you with the highest quality and most durable stainless steel angles and steel. We provide hundreds of stainless steel angles in various leg lengths, thicknesses, and material grades. Our 316/316L and 304/304L stainless steel angles are made at our well-equipped production facility using high-quality raw materials and cutting-edge technology, overseen by qualified workers. Some other significant benefits of partnering with us include:
- When you purchase any steel products from us, you get the products directly from the manufacturer.
- Our employees are dedicated to providing the lowest prices and fastest shipping times so that you can start your project right away!
- We have a skilled, capable workforce for quality checks, packaging, and shipping.
- We follow multiple quality check levels, which helps ensure that the products are of the highest standards.
- We have a qualified and dedicated support team available 24×7 to help you out if any issues arise.
Suppliers from China Make Stainless Steel Angles to Size
- Daxun is a leading supplier of stainless steel products in China. With high-quality products and customized services, we can meet all your stainless steel angle needs. Order online or by phone and get it delivered in as fast as 15 days.
304 and 316 Grade Stainless Steel Angles
- This versatile right angle steel has a wide range of applications and is available in grades 304 /30L and 316 /316L. Grade 304 is the most versatile and commonly used grade of stainless steel angle steel and is suitable for most general applications. It is easy to weld and has good formability and corrosion resistance. Sometimes called 18/8 stainless steel because its composition includes 18% chromium and 8% nickel, grade 304 is well suited to most applications.
- Grade 316 is more suitable for harsh environments, such as exposure to salt water and areas with high industrialization. Due to the higher nickel content and the addition of molybdenum to the metal, it has higher corrosion resistance than grade 304, especially to chlorides and chlorinated solutions. It also has good weldability, but is more difficult to process than grade 304.
There are two basic processes for manufacturing stainless steel angles:
- laser melting and hot rolling. Hot rolled stainless steel angles are less expensive. They typically have rounded or tapered edges. On the other hand, laser melted stainless steel angles have consistent sharp and square corners. They also include sandblasting and a smoother finish. The surface of laser melted stainless steel angles is smoother than that of hot rolled stainless steel angles.
Choose Your Size and Size
- We offer a wide variety of stainless steel angles, so whatever your needs, we have you covered. Grade 304 stainless steel angles come in a variety of sizes with thicknesses from 3mm-16mm and lengths of 1m, 3m, or 6m.
- Our grade 316 angles come in thicknesses from 3mm-16mm and lengths of 1m, 3m, or 6m. Angles are available in a variety of sizes.
Talk to Your Preferred Stainless Steel Angle Supplier
- It couldn’t be easier to buy the stainless steel angles you need, as well as all of our other products, through our website. Alternatively, you can call our sales team in China at +8613382898899 to place your order and they will be happy to process your order. If you have any questions, you can even send an email to daxunalloy@gmail.com and our team will get back to you as soon as possible.
Пожалуйста, заполните форму на странице “Контакты” или позвоните нашему менеджеру по продажам по телефону “+86 13382898899”, мы свяжемся с вами в кратчайшие сроки. Наш WhatsApp работает в режиме онлайн, а электронная почта (Daxunalloy@gmail.com) будет проверена в течение 6 часов. На каждый запрос или сообщение мы ответим незамедлительно. Кроме того, каждую неделю мы делимся с нашими клиентами информацией о рынке
Образцы могут быть предоставлены бесплатно, но расходы на перевозку несет заказчик, и они будут возмещены после сотрудничества.
Мы экспортировали продукцию в более чем 42 страны, такие как Канада, Чили, Кувейт, Германия, Южная Корея, Саудовская Аравия, Сингапур и др.
Our MOQ is 1 ton for 316L Stainless Steel Angle.
У нас есть полная организация от закупки сырья до обработки и организации отгрузки. Во всей цепи, документальные люди ad QC будут искать и проверять его по точным требованиям. Инспекция третьей стороны приветствуется.
Пробные заказы могут быть доставлены в течение недели. Для обычных заказов требуется примерно две недели.