Daxun is a 316/316L stainless steel angle steel supplier in China

As a leading stainless steel angle steel supplier and exporter in China, Daxun supplies stainless steel angle steel to all over the world.
  • Grade: S31600(316)-S31603(316L)
  • Equal Angle Steel/Unequal Angle Steel
  • Process: hot rolling and laser welding
  • Easy to weld and process
  • Length can be cut to size
  • Daxun specializes in custom stainless steel angles with fast delivery and competitive prices. Contact Daxun today.

Global leader in stainless steel angle fabrication services

304/304L and 316/316L Stainless Steel Angles
As China’s premier supplier of specialty metals, you can trust Daxun for all of your stainless steel angle needs. Our stainless steel angle selection includes 304/304L and 316/316L stainless steel angles. Our extensive product line offers durability and versatility, making it the perfect solution for your structural and fabrication needs.

Our stainless steel angles are available in 304/304L and 316/316L, all from fully certified factories. Our comprehensive product line is both durable and adaptable, ideal for structural and fabrication applications. As a leading stainless steel angle manufacturer, we offer a wide range of specialty angles and L-shaped angles. Daxun offers stainless steel angles in any length, up to 6 meters. The following stainless steel grades are also available: 304/304L and 316/316L. Stainless steel angles are most commonly used for supports or frames, but are also used in food equipment, building supports, structural supports, and medical equipment.

Can be welded and processed using simple procedures, 304/304L stainless steel angles are suitable for many environments, such as general industrial projects, chemical projects. While 316/316L angles are marine grade and have strong corrosion resistance in more demanding conditions.

The surface treatment we use on our stainless steel angles is hot rolling, annealing, and pickling. This surface treatment maximizes corrosion resistance and gives the angles a unique “stainless” appearance.

The two manufacturing methods are laser melting and hot rolling. Hot rolling produces stainless steel angles at a lower price. They usually have rounded or tapered edges. On the other hand, laser melted stainless steel angles have consistent sharp and square corners. They also have a sandblasted, smoother surface. Laser melted stainless steel angles have a smoother surface quality than hot rolled stainless steel angles.

Daxun Alloy manufactures laser melted and hot rolled stainless steel angles in metric and imperial sizes. We can ship them all over the world.

قراءة المزيد

البيانات

قياسي ASTM、EN、DIN、JIS,ASME, BS, GBetc,
الأبعاد ∠20*20*3mm-∠200*200*24mm
Alloy 201, 310, 304, 304L, 316, 316L
النوع Equal, Unequal
Length 1.0-12.0m
السُمك 3mm-25mm
Custom Options Yes
التفاوتات المسموح بها ± ¼”, ± 1/16”
الإنهاء Mill, brush, mirror, polished
التركيب الكيميائي: ASTM A240، A666
العنصر النوع 316 النوع 316L
الكربون 0.08 كحد أقصى. 0.030 كحد أقصى.
المنجنيز 2.00 كحد أقصى. 2.00 كحد أقصى.
الكبريت 0.030 كحد أقصى. 0.030 كحد أقصى.
الفوسفور 0.045 كحد أقصى. 0.045 كحد أقصى.
السيليكون 0.75 كحد أقصى. 0.75 كحد أقصى.
الكروم 16.0 - 18.0 16.0 - 18.0
نيكل 10.00 - 14.00 10.00 - 14.00
الموليبدينوم 2.00 - 3.00 2.00 - 3.00
النيتروجين 0.10 كحد أقصى. 0.10 كحد أقصى.
النوع إزاحة قوة الخضوع 0.2% (KSI) قوة الشد (KSI) % استطالة % (2″ طول المقياس)
316 30 دقيقة. 75 دقيقة. 40 دقيقة.
316L 25 دقيقة. 70 دقيقة. 40 دقيقة.
الكثافة (رطل./ بوصة^2) عند RT 0.29
معامل المرونة في الشد (رطل لكل بوصة مربعة × 10^6) 28
الحرارة النوعية (BTU/o F/رطل) 32 إلى 212 درجة فهرنهايت 0.12
الموصلية الحرارية (BTU/ساعة/قدم^2/قدم) 212 درجة فهرنهايت 9.4
932 درجة فهرنهايت 12.4
متوسط معامل التمدد الحراري (بوصة × 10^6 لكل درجة فهرنهايت) 32 إلى 212 درجة فهرنهايت 8.9
32 إلى 600 درجة فهرنهايت 9
32 إلى 1,000 درجة فهرنهايت 9.7
32 إلى 1,200 درجة فهرنهايت 10.3
المقاومة الكهربائية (ميكرو أوم - سم) عند 70 درجة فهرنهايت 29.4
نطاق درجة الانصهار (درجة فهرنهايت) 2500 - 2550
الصف رقم الأمم المتحدة بريطاني قديم يورونورم قوات الأمن الخاصة السويدية JIS اليابانية
ب إن لا يوجد الاسم
316l S31603 316S11 – 1.4404 X2CrNiMo17-12-2 2348 SUS 316L

اختر Daxun واجعل عملاءك راضين.

اتصل بـ Daxun الآن

استجابة سريعة

نحن نقدم تسليم منتجات الفولاذ المقاوم للصدأ في الوقت المناسب وبسرعة للعملاء ذوي الاحتياجات العاجلة. ويقف وراء السرعة دعم النظام من تدفق المعلومات إلى التدفق اللوجستي وتدفق رأس المال. على سبيل المثال، فيما يتعلق بتدفق المعلومات، يتم دفع بيانات طلبات Daxun إلى نظام الخدمات اللوجستية في الوقت الفعلي، ويتم توصيل البيانات بسلاسة؛ وفيما يتعلق بالخدمات اللوجستية، فإن مركز المعالجة قريب من الطرق السريعة والأنهار والبحار، مع جدولة معقولة، واستجابة سريعة، وربط التخزين والنقل، والتحميل الفعال، مما يضمن إنجاز المهمة في الموعد المحدد، ومواد الفولاذ المقاوم للصدأ من Daxun ذات جودة موثوقة، وتتوافق أصنافها ومواصفاتها وأوزان التسليم بدقة مع المعايير.

اتصل بـ Daxun الآن

مزايا داكسون

Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel uses the ERP system to achieve full traceability of each angle steel, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

اتصل بـ Daxun الآن

التعبئة والتغليف

تضمن شركة Daxun Alloy أفضل جودة للتغليف لأنها تلعب دورًا مهمًا في الشحن الدولي حيث تمر البضائع عبر قنوات مختلفة للوصول إلى الوجهة النهائية، لذلك نولي اهتمامًا خاصًا بالتغليف. نقوم بتغليف بضائعنا بعدة طرق حسب المنتج. نقوم بتغليف منتجاتنا بعدة طرق مثل:
- الصناديق والصناديق
- الغلاف المنكمش
- منصات خشبية
- صناديق خشبية

اتصل بـ Daxun الآن

الجودة والتسليم والتفتيش

  • تجري Daxun أيضًا العديد من اختبارات ضمان الجودة. وتتضمن هذه الاختبارات اختبار التسطيح، واختبار الحفر والمقاومة، والاختبار الميكانيكي، واختبار الصلابة، والتحديد الإيجابي للمادة، واختبار التمدد، وما إلى ذلك. تضمن جميع هذه الاختبارات أن المادة مناسبة للتطبيق المطلوب.
  • أثناء عملية الإنتاج، نقوم بقياس قطر المنتج وسماكته وسطحه. وقت التسليم القياسي لدينا هو 7-15 يومًا، باستثناء بعض المنتجات ذات الأحجام الخاصة، سيزيد وقت التسليم إلى 20 يومًا.
    وقت التسليم لدينا يتوافق تمامًا مع العقد.
  • دعم الوكالات الخارجية للعملاء للذهاب إلى المصنع للفحص
  • دعم العينات المجانية للعملاء لاختبارها
  • دعم الفحص الموقعي أو فحص المصنع بالفيديو
اتصل بـ Daxun الآن

معلومات الطلب

يجب أن تتضمن طلبات الشراء الكمية والدرجة والنوع أو الفئة ومرجع API5L والسماكة والعرض والطول وأي مرفقات قابلة للتطبيق أو متطلبات إضافية تتعلق بالتركيب الكيميائي أو الخواص الميكانيكية أو المعالجة الحرارية أو الاختبارات الإضافية أو عملية التصنيع أو طلاء السطح أو التشطيب النهائي. اتصل ب Daxun الآن، وسوف نقوم بالرد على بريدك الإلكتروني في أقرب وقت ممكن.

اتصل بـ Daxun الآن

الدعم الفني

إذا كنت بحاجة إلى أي مساعدة فنية إضافية، فسيكون من دواعي سرور أخصائي المعادن المقيم لدينا وموظفينا المطلعين تقديم المساعدة. بالإضافة إلى ذلك، تفتخر Daxun بوجود مختبر اختبار معتمد - وهو الأول من نوعه في صناعة مخزون المعادن المتعددة والبلاستيك. وهذا، في رأينا، يدل على تفانينا الثابت للجودة وفلسفتنا كمورد متكامل الخدمات.

SS 316-316L Stainless Steel angle Features

قوة عالية
مقاومة التآكل
مقاومة الحرارة
مقاومة درجات الحرارة المنخفضة
حماية البيئة
أداء اللحام

سبائك داكسون دع علامتك التجارية تتحسن بسرعة

 

Angle – Steel Data
    EQUAL AND UNEQUAL ANGLE
ANGLE is available in other sizes on request
    Description Width (W) Depth (D) السُمك قياسي Weight per السطح
(mm) (mm) (T) (mm) Length Metre Area per
(kg/m) Metre
(m²/m)
ANGLE 20 X 20 X 3.0mm 20 20 3 6.0 metres 0.98 0.0897
ANGLE 25 X 25 X 3.0mm 25 25 3 7.5 metres 1.12 0.0953
ANGLE 25 X 25 X 5.0mm 25 25 5 7.5 metres 1.65 0.0953
ANGLE 25 X 25 X 6.0mm 25 25 6 7.5 metres 2.08 0.0953
ANGLE 30 X 30 X 2.5mm 30 30 2.5 6.0 metres 1.06 0.117
ANGLE 30 X 30 X 3.0mm 30 30 3 7.5 metres 1.35 0.115
ANGLE 30 X 30 X 5.0mm 30 30 5 7.5 metres 2.01 0.115
ANGLE 30 X 30 X 6.0mm 30 30 6 7.5 metres 2.56 0.115
ANGLE 40 X 40 X 2.5mm 40 40 2.5 6.0 metres 1.43 0.157
ANGLE 40 X 40 X 3.0mm 40 40 3 7.5 metres 1.83 0.155
ANGLE 40 X 40 X 4.0mm 40 40 4 6.0 metres 2.2 0.155
ANGLE 40 X 40 X 5.0mm 40 40 5 9.0 metres 2.73 0.155
ANGLE 40 X 40 X 6.0mm 40 40 6 9.0 metres 3.5 0.155
ANGLE 45 X 45 X 3.0mm 45 45 3 9.0 metres 2.06 0.175
ANGLE 45 X 45 X 5.0mm 45 45 5 9.0 metres 3.1 0.175
ANGLE 45 X 45 X 6.0mm 45 45 6 9.0 metres 3.97 0.175
ANGLE 50 X 50 X 2.5mm 50 50 2.5 9.0 metres 1.81 0.197
ANGLE 50 X 50 X 3.0mm 50 50 3 7.5 metres 2.31 0.195
ANGLE 50 X 50 X 4.0mm 50 50 4 9.0 metres 2.79 0.195
ANGLE 50 X 50 X 5.0mm 50 50 5 9.0 metres 3.48 0.195
ANGLE 50 X 50 X 6.0mm 50 50 6 9.0 metres 4.46 0.195
ANGLE 50 X 50 X 8.0mm 50 50 8 9.0 metres 5.68 0.195
ANGLE 55 X 55 X 5.0mm 55 55 5 9.0 metres 3.84 0.215
ANGLE 55 X 55 X 6.0mm 55 55 6 9.0 metres 4.93 0.215
ANGLE 65 X 50 X 5.0mm 65 50 5 9.0 metres 4.02 0.225
ANGLE 65 X 50 X 6.0mm 65 50 6 9.0 metres 5.16 0.225
ANGLE 65 X 50 X 8.0mm 65 65 8 9.0 metres 6.59 0.225
ANGLE 65 X 65 X 4.0mm 65 65 4 9.0 metres 3.69 0.255
ANGLE 65 x 65 x 5.0mm 65 65 5 9.0 metres 4.56 0.255
ANGLE 65 X 65 X 6.0mm 65 65 6 9.0 metres 5.87 0.255
ANGLE 65 X 65 X 8.0mm 65 65 8 9.0 metres 7.51 0.255
ANGLE 65 X 65 X 10.0mm 65 65 10 9.0 metres 9.02 0.255
ANGLE 75 X 50 X 5.0mm 75 50 5 9.0 metres 4.4 0.244
ANGLE 75 X 50 X 6.0mm 75 50 6 9.0 metres 5.66 0.244
ANGLE 75 X 50 X 8.0mm 75 50 8 9.0 metres 7.23 0.244
ANGLE 75 X 75 X 4.0mm 75 75 4 9.0 metres 4.29 0.295
ANGLE 75 X 75 X 5.0mm 75 75 5 9.0 metres 5.27 0.292
ANGLE 75 X 75 X 6.0mm 75 75 6 9.0 metres 6.81 0.292
ANGLE 75 X 75 X 8.0mm 75 75 8 9.0 metres 8.73 0.292
ANGLE 75 X 75 X 10.0mm 75 75 10 9.0 metres 10.5 0.292
ANGLE 90 X 90 X 6.0mm 90 90   6.0 9.0 metres    8.22 0.352
ANGLE 90 X 90 X 8.0mm 90 90   8.0 9.0 metres    10.6 0.352
ANGLE 90 X 90 X 10.0mm 90 90   10.0 9.0 metres    12.7 0.352
ANGLE 100 X 75 X 6.0mm 100 75   6.0 9.0 metres    7.98 0.342
ANGLE 100 X 75 X 8.0mm 100 75   8.0 9.0 metres    10.3 0.342
ANGLE 100 X 75 X 10.0mm 100 75   10.0 9.0 metres    12.4 0.342
ANGLE 100 X 100 X 10.0mm 100 100   10.0 9.0 metres    14.2 0.392
ANGLE 100 X 100 X 12.0mm 100 100   12.0 9.0 metres    17.7 0.392
ANGLE 100 X 100 X 4.0mm 100 100   4.0 9.0 metres    5.78 0.395
ANGLE 100 X 100 X 6.0mm 100 100   6.0 9.0 metres    9.16 0.392
ANGLE 100 X 100 X 8.0mm 100 100   8.0 9.0 metres    11.8 0.392
ANGLE125 X 75 X 6.0mm 125 75   6.0 9.0 metres    9.16 0.392
ANGLE 125 X 75 X 8.0mm 125 75   8.0 9.0 metres    11.8 0.392
ANGLE 125 X 75 X 10.0mm 125 75   10.0 9.0 metres    14.2 0.392
ANGLE 125 X 75 X 12.0mm 125 75   12.0 9.0 metres    17.7 0.392
ANGLE 125 X 125 X 8.0mm 125 125   8.0 9.0 metres    14.9 0.491
ANGLE 125 X 125 X 10.0mm 125 125   10.0 9.0 metres    18 0.491
ANGLE 125 X 125 X 12.0mm 125 125   12.0 9.0 metres    22.5 0.491
ANGLE 125 X 125 X 16.0mm 125 125   16.0 9.0 metres    29.1 0.491
ANGLE 150 X 90 X 8.0mm 150 90   8.0 9.0 metres    14.3 0.471
 ANGLE 150 X 90 X 12.0mm 150 90   12.0 9.0 metres    21.6 0.471
ANGLE 150 X 90 X 16.0mm 150 90   16.0 9.0 metres    27.9 0.471
ANGLE 150 X 100 X 10.0mm 150 100   10.0 9.0 metres    18 0.491
ANGLE 150 X 100 X 12.0mm 150 100   12.0 9.0 metres    22.5 0.491
ANGLE 150 X 150 X 10.0mm 150 150   10.0 9.0 metres    21.9 0.59
ANGLE 150 X 150 X 12.0mm 150 150   12.0 9.0 metres    27.3 0.59
ANGLE 150 X 150 X 16.0mm 150 150   16.0 9.0 metres    35.4 0.59
ANGLE 150 X 150 X 19.0mm 150 150   19.0 9.0 metres    42.1 0.59
ANGLE 150 X 90 X 10.0mm 150 90   10.0 9.0 metres    17.3 0.471
ANGLE 200 x 200 x 13.0mm 200 200   13.0 9.0 metres    40 0.788
ANGLE 200 X 200 X 16.0mm 200 200   16.0 9.0 metres    48.7 0.788
ANGLE 200 X 200 X 20.0mm 200 200   20.0 9.0 metres    60.1 0.788
ANGLE 200 X 200 X 26.0mm 200 200   26.0 9.0 metres    76.8 0.788

 

SS 316/316L Stainless Steel Angle Surface Type (3)

  • Applies to:curtain walls、entryways、canopies、handrails、window and door fittings、street furniture、cladding、masonry supports、fabrication projects,Can be used in a variety of applications, from decking, brackets, posts and frames to trim, tracks and siding

  • Applies to:curtain walls、entryways、canopies、handrails、window and door fittings、street furniture、cladding、masonry supports、fabrication projects,Can be used in a variety of applications, from decking, brackets, posts and frames to trim, tracks and siding

  • Applies to:curtain walls、entryways、canopies、handrails、window and door fittings、street furniture、cladding、masonry supports、fabrication projects,Can be used in a variety of applications, from decking, brackets, posts and frames to trim, tracks and siding

المعلومات المتاحة للرجوع إليها وتنزيلها

Daxun is a trustworthy stainless steel Angle manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel angles have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

أحدث مشاريع ومنتجات الحالة الساخنة

مقدمة مفصلة

Leading stainless steel angle Suppliers in China

Daxun has been engaged in international business for more than ten years. In 2023, the export volume exceeded 100 million US dollars, and the export volume ranked among the top Chinese stainless steel manufacturers. Daxun continuously improves its service skills. To serve the global market, it has established three export service facilities in China, cooperating with engineering companies, steel mills, and international trading companies. Daxun provides stainless steel chain services and has established long-term cooperative relations with dozens of well-known steel mills around the world. The inventory includes 50,000 tons of conventional stainless steel and 20,000 tons of duplex steel, nickel-based alloys, heat-resistant steel and other metals. Daxun’s stainless steel materials are of stable quality, and the varieties, specifications, and delivery weights strictly meet the standards.


316 Stainless Steel Angle

  • 316 Stainless Steel Angle is an austenitic chromium nickel angle shape containing molybdenum which provides superior corrosion resistance and increased strength at elevated temperatures when compared to 304 Stainless.
  • Because of the 4% molybdenum concentration, the 316 material is resistant to chloride ion stress corrosion. Stainless Steel 304 Unequal Angle Sizes vary depending on the application needs. Angles are used to hold components together using a grip. There are also angles with bolt holes for screws and bolts. The 316 Stainless Steel Unequal Angle is suitable for more corrosive applications than the 304 angles. The Stainless Steel Unequal Angle is just as frequent as the Equal Angle. They are utilized in a variety of applications, including brackets, trim, and reinforcements. Please contact us for more information about the angles and their costs.

Characteristics

  • Cold Working: Good
  • Corrosion Resistance: Excellent
  • Heat Resistance: Good
  • Heat Treatment: Poor
  • Hot Working: Fair
  • Machinability: Good
  • Weldability: Very Good

 

Why should you buy stainless steel angles from Daxun?

Daxun’s objective is to supply you with the highest quality and most durable stainless steel angles and steel. We provide hundreds of stainless steel angles in various leg lengths, thicknesses, and material grades. Our 316/316L and 304/304L stainless steel angles are made at our well-equipped production facility using high-quality raw materials and cutting-edge technology, overseen by qualified workers. Some other significant benefits of partnering with us include:

  • When you purchase any steel products from us, you get the products directly from the manufacturer.
  •  Our employees are dedicated to providing the lowest prices and fastest shipping times so that you can start your project right away!
  •  We have a skilled, capable workforce for quality checks, packaging, and shipping.
  •  We follow multiple quality check levels, which helps ensure that the products are of the highest standards.
  •  We have a qualified and dedicated support team available 24×7 to help you out if any issues arise.

Suppliers from China Make Stainless Steel Angles to Size

  • Daxun is a leading supplier of stainless steel products in China. With high-quality products and customized services, we can meet all your stainless steel angle needs. Order online or by phone and get it delivered in as fast as 15 days.

304 and 316 Grade Stainless Steel Angles

  • This versatile right angle steel has a wide range of applications and is available in grades 304 /30L and 316 /316L. Grade 304 is the most versatile and commonly used grade of stainless steel angle steel and is suitable for most general applications. It is easy to weld and has good formability and corrosion resistance. Sometimes called 18/8 stainless steel because its composition includes 18% chromium and 8% nickel, grade 304 is well suited to most applications.
  • Grade 316 is more suitable for harsh environments, such as exposure to salt water and areas with high industrialization. Due to the higher nickel content and the addition of molybdenum to the metal, it has higher corrosion resistance than grade 304, especially to chlorides and chlorinated solutions. It also has good weldability, but is more difficult to process than grade 304.

There are two basic processes for manufacturing stainless steel angles:

  • laser melting and hot rolling. Hot rolled stainless steel angles are less expensive. They typically have rounded or tapered edges. On the other hand, laser melted stainless steel angles have consistent sharp and square corners. They also include sandblasting and a smoother finish. The surface of laser melted stainless steel angles is smoother than that of hot rolled stainless steel angles. ​​

Choose Your Size and Size

  • We offer a wide variety of stainless steel angles, so whatever your needs, we have you covered. Grade 304 stainless steel angles come in a variety of sizes with thicknesses from 3mm-16mm and lengths of 1m, 3m, or 6m.
  • Our grade 316 angles come in thicknesses from 3mm-16mm and lengths of 1m, 3m, or 6m. Angles are available in a variety of sizes.

Talk to Your Preferred Stainless Steel Angle Supplier

  • It couldn’t be easier to buy the stainless steel angles you need, as well as all of our other products, through our website. Alternatively, you can call our sales team in China at +8613382898899 to place your order and they will be happy to process your order. If you have any questions, you can even send an email to daxunalloy@gmail.com and our team will get back to you as soon as possible.
كيف تحصل على عرض أسعار أو تفهم معلومات السوق في أسرع وقت ممكن؟

يُرجى ملء النموذج الموجود في صفحة “اتصل بنا”، أو الاتصال بمدير المبيعات لدينا على “+86 13382898899”، وسوف نتصل بك في أقرب وقت ممكن. واتسابنا على الإنترنت، وسيتم التحقق من البريد الإلكتروني (Daxunalloy@gmail.com) في غضون 6 ساعات. سيتم الرد على كل استفسار أو رسالة على الفور. بالإضافة إلى ذلك، نشارك معلومات السوق مع عملائنا كل أسبوع

هل يمكنني الحصول على بعض العينات؟

يمكن تقديم العينات مجانًا، ولكن يتحمل العميل أجرة الشحن، وسيتم ردها بعد التعاون.

ما هي الدول التي قمت بتصديرها بالفعل؟

لقد قمنا بالتصدير إلى أكثر من 42 دولة، مثل كندا، وتشيلي، والكويت، وألمانيا، وكوريا الجنوبية، والمملكة العربية السعودية، وسنغافورة، وغيرها.

ما هو موك الخاص بك؟

Our MOQ is 1 ton for 316L Stainless Steel Angle.

كيف تتحكم في الجودة؟

لدينا منظمة كاملة من شراء المواد الخام إلى المعالجة وترتيب الشحن. في السلسلة بأكملها، سيبحث الأشخاص المختصون بمراقبة الجودة عن المستندات ويتحققون منها حسب المتطلبات الدقيقة، ونرحب بالتفتيش من طرف ثالث.

ما هي مدة التوصيل؟

يمكن تسليم الطلبات التجريبية في غضون أسبوع. بالنسبة للطلبات العادية، يستغرق الأمر أسبوعين تقريباً.