What is High-temperature alloy

High-temperature alloy refers to a type of metal material based on iron, nickel and cobalt, which can work for a long time at high temperature above 600℃ and under certain stress. They have excellent high temperature strength, oxidation resistance, thermal corrosion resistance, good fatigue performance and fracture toughness, so they are also called “Superalloy”.

Performance characteristics of High-temperature alloy

  • Excellent high temperature performance: able to maintain high strength and good mechanical properties at high temperature.
  • Good oxidation resistance and corrosion resistance: excellent performance in high temperature oxidation and corrosion environment.
  • High reliability and long life: can maintain stable performance under extreme conditions and extend the service life of equipment.
  • Good fatigue performance and fracture toughness: excellent performance under cyclic load and impact load.

Common High-temperature Alloy Grades & Chemical Compositions

The following are the main features of several commonly used high-temperature  alloy grades:

GH4169

  • Main features:
    Precipitation-strengthened nickel-based high-temperature alloy, excellent high-temperature strength and oxidation resistance.
    Excellent performance in the temperature range of -253℃ to 700℃, and the yield strength below 650℃ ranks first among deformed high-temperature alloys.
    Good fatigue resistance, radiation resistance, corrosion resistance, as well as good processing and welding properties.
  • Application areas: aviation engines, nuclear energy, petroleum industry, used to manufacture turbine blades, combustion chambers, etc.

GH3030

  • Main features:
    Nickel-based high-temperature alloy, excellent high-temperature mechanical properties and corrosion resistance.
    Maintain good mechanical properties below 800℃, and high chromium content enhances the alloy’s oxidation resistance.
    Good thermal fatigue resistance and cold working performance, can be used to make various cold-rolled thin plates, pipes, wires and other deformed products.
  • Application areas: aerospace, petrochemical, nuclear energy and petrochemical equipment, used to manufacture high-temperature components such as turbine blades, combustion chambers, etc.

GH3039

  • Main features:
    Nickel-based high-temperature alloy, excellent high-temperature strength and oxidation resistance.
    The tensile strength is 650MPa at 850℃, and the oxidation weight gain is only 2-3mg/cm² after continuous use for more than 100 hours at 1000℃.
    Good cold formability and welding performance, suitable for aircraft engine combustion chamber and afterburner parts for long-term use below 850℃.
  • Application areas: aircraft engines, gas turbines, used for manufacturing turbine blades, guide blades, etc.

GH3044

  • Main features:
    Nickel-based high-temperature alloy, excellent high-temperature strength, oxidation resistance and hot corrosion resistance.
    The tensile strength at 1000℃ can reach 650MPa, and the creep rupture strength at 850℃ is 400MPa.
    The oxidation resistance in high-temperature oxidation environment is very good, and the thickness of the oxide film at 1000℃ is only about 10μm.
  • Application areas: aircraft engines, gas turbines, nuclear reactors, used to manufacture high-temperature components such as turbine disks, combustion chambers, etc.
Element / Alloy Designation GH4169 (Inconel 718) GH3030 GH3039 GH3044
ني: 50 – 55% 45 – 50% 48 – 53% >55%
كـ: 17 – 21% 20% 19 – 22% 18 – 21%
في: 5 – 10% 15% - -
مو: 2.8 – 3.3% - 2.8 – 3.3% 4 – 5%
ن.ب: 4.75 – 5.50% - - -
تي: 0.65 – 1.15% 2% 1.8 – 2.2% 0.3 – 0.5%
آل: 0.20 - 0.801 ت 3 ت 3 ت 3% 0.80% 0.2 – 0.5%
C : ≤0.08% ≤0.12% ≤0.08% -
P : ≤0.015% ≤0.02% ≤0.015% ≤0.02%
S : ≤0.01% ≤0.015% ≤0.01% ≤0.015%
Co: - 10% 12% 12 – 15%
من: ≤0.35% ≤0.7% ≤0.5% ≤0.5%
نعم: ≤0.35% ≤0.8% ≤0.5% ≤0.5%
Cu: ≤0.3% - - -
W : - - - 3 – 4%

GH4169

تم العثور على 4 منتجات.

GH3030

تم العثور على 4 منتجات.

GH3039

تم العثور على 4 منتجات.

GH3044

تم العثور على 4 منتجات.
هل لديك أي مخزون في المخزن؟

نعم، لدينا مواصفات ومخزون كامل ويمكننا تلبية احتياجاتك بسرعة.

هل يمكن تخصيصها حسب الطلب؟

نعم، يمكن تخصيصها حسب الطلب. يمكنك الاتصال بنا وإرسال المواصفات والكمية المخصصة لنا.

كيف تشحن البضائع؟

تشمل طرق النقل لدينا بشكل عام النقل البحري والنقل البري والنقل البحري. الوصول إليك بسرعة وأمان.

ما هو سعرك؟

نظرًا لأن إنتاجنا مرتفع، فإن التكلفة ستكون أقل بكثير، وبالتالي فإن السعر منخفض.

هل يمكنني الحصول على بعض العينات؟

يمكننا تقديم عينات من صفائح الفولاذ المقاوم للصدأ لك للتحقق من الجودة. العينة مجانية وما عليك سوى دفع أجرة الشحن.

كيف هي جودتك؟

نحن نولي أهمية كبيرة لجودة المنتج وقد اجتزنا العديد من اختبارات نظام الجودة.

أرسل استفسارك اليوم
اقتباس سريع