Daxun is a 316/316L stainless steel angle steel supplier in China

As a leading stainless steel angle steel supplier and exporter in China, Daxun supplies stainless steel angle steel to all over the world.
  • Grade: S31600(316)-S31603(316L)
  • Equal Angle Steel/Unequal Angle Steel
  • Process: hot rolling and laser welding
  • Easy to weld and process
  • Length can be cut to size
  • Daxun specializes in custom stainless steel angles with fast delivery and competitive prices. Contact Daxun today.

Global leader in stainless steel angle fabrication services

304/304L and 316/316L Stainless Steel Angles
As China’s premier supplier of specialty metals, you can trust Daxun for all of your stainless steel angle needs. Our stainless steel angle selection includes 304/304L and 316/316L stainless steel angles. Our extensive product line offers durability and versatility, making it the perfect solution for your structural and fabrication needs.

Our stainless steel angles are available in 304/304L and 316/316L, all from fully certified factories. Our comprehensive product line is both durable and adaptable, ideal for structural and fabrication applications. As a leading stainless steel angle manufacturer, we offer a wide range of specialty angles and L-shaped angles. Daxun offers stainless steel angles in any length, up to 6 meters. The following stainless steel grades are also available: 304/304L and 316/316L. Stainless steel angles are most commonly used for supports or frames, but are also used in food equipment, building supports, structural supports, and medical equipment.

Can be welded and processed using simple procedures, 304/304L stainless steel angles are suitable for many environments, such as general industrial projects, chemical projects. While 316/316L angles are marine grade and have strong corrosion resistance in more demanding conditions.

The surface treatment we use on our stainless steel angles is hot rolling, annealing, and pickling. This surface treatment maximizes corrosion resistance and gives the angles a unique “stainless” appearance.

The two manufacturing methods are laser melting and hot rolling. Hot rolling produces stainless steel angles at a lower price. They usually have rounded or tapered edges. On the other hand, laser melted stainless steel angles have consistent sharp and square corners. They also have a sandblasted, smoother surface. Laser melted stainless steel angles have a smoother surface quality than hot rolled stainless steel angles.

Daxun Alloy manufactures laser melted and hot rolled stainless steel angles in metric and imperial sizes. We can ship them all over the world.

Ler mais

Dados

Padrão ASTM、EN、DIN、JIS,ASME, BS, GBetc,
Dimensões ∠20*20*3mm-∠200*200*24mm
Liga metálica 201, 310, 304, 304L, 316, 316L
Tipo Equal, Unequal
Comprimento 1.0-12.0m
Espessura 3mm-25mm
Opções personalizadas Sim
Tolerâncias ± ¼”, ± 1/16”
Acabamento Moinho, escova, espelho, polido
CHEMICAL COMPOSITION: ASTM A240, A666
Elemento Type 316 Type 316L
Carbono 0.08 max. 0.030 max.
Manganese 2.00 max. 2.00 max.
Sulfur 0.030 max. 0.030 max.
Phosphorus 0.045 max. 0.045 max.
Silicon 0.75 max. 0.75 max.
Chromium 16.0 – 18.0 16.0 – 18.0
Nickel 10.00 – 14.00 10.00 – 14.00
Molybdenum 2.00 – 3.00 2.00 – 3.00
Nitrogénio 0.10 max. 0.10 max.
Tipo Resistência ao escoamento 0.2% offset (KSI) Resistência à tração (KSI) % Elongation (2″ Gauge length)
316 30 min. 75 min. 40 min.
316L 25 min. 70 min. 40 min.
Densidade (lb./in^2) @ RT 0.29
Módulo de elasticidade em tensão (psi x 10^6) 28
Calor específico (BTU/o F/lb.) 32 a 212 oF 0.12
Condutividade térmica (BTU/hr/ft^2/ft) 212oF 9.4
932oF 12.4
Coeficiente médio de expansão térmica (pol. x 10^-6 por o F) 32 a 212oF 8.9
32 a 600oF 9
32 a 1.000oF 9.7
32 a 1.200oF 10.3
Resistividade eléctrica (micro ohms - cm) a 70oF 29.4
Gama de pontos de fusão (oF) 2500 – 2550
Grau UNS No Old British Euronorm Swedish SS Japanese JIS
BS En No Nome
316l S31603 316S11 – 1.4404 X2CrNiMo17-12-2 2348 SUS 316L

Escolha a Daxun e deixe os seus clientes satisfeitos.

Contactar a Daxun agora

Resposta rápida

Fornecemos entrega atempada e rápida de produtos de aço inoxidável para clientes com necessidades urgentes. Por detrás da velocidade está o sistema de apoio, desde o fluxo de informação até à logística e ao fluxo de capital. Por exemplo, em termos de fluxo de informação, os dados das encomendas da Daxun são enviados para o sistema de logística em tempo real, e os dados estão perfeitamente ligados; em termos de logística, o centro de processamento está perto de auto-estradas, rios e mares, com uma programação razoável, resposta rápida, armazenamento e ligação de transporte, e carregamento eficiente, garantindo que a tarefa é concluída dentro do prazo.

Contactar a Daxun agora

Vantagens da Daxun

Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel uses the ERP system to achieve full traceability of each angle steel, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

Contactar a Daxun agora

Embalagem

A Daxun Alloy assegura a melhor qualidade de embalagem, uma vez que esta desempenha um papel importante no transporte internacional de mercadorias, onde as mercadorias passam por vários canais para chegar ao destino final, pelo que prestamos especial atenção à embalagem. Embalamos os nossos produtos de várias formas, consoante o produto. Embalamos os nossos produtos de várias formas, tais como:
- Caixas e caixotes
- Película retrátil
- Paletes de madeira
- Caixas de madeira

Contactar a Daxun agora

Qualidade, entrega, inspeção

  • Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    O nosso prazo de entrega está estritamente de acordo com o contrato.
  • Apoio a agências terceiras do cliente para se deslocarem à fábrica para inspeção
  • Apoio a amostras gratuitas aos clientes para testes
  • Apoio à inspeção de fábrica no local ou por vídeo
Contactar a Daxun agora

Informações para encomenda

As ordens de compra devem incluir quantidade, grau, tipo ou categoria, referência API5L, espessura, largura, comprimento e quaisquer anexos aplicáveis ou requisitos adicionais relacionados com a composição química, propriedades mecânicas, tratamento térmico, testes adicionais, processo de fabrico, revestimento de superfície ou acabamento final. Contacte Daxun agora, nós responderemos ao seu e-mail o mais rápido possível.

Contactar a Daxun agora

Apoio técnico

Se necessitar de qualquer assistência técnica adicional, o nosso metalúrgico residente e a nossa equipa experiente terão todo o prazer em ajudar. Além disso, a Daxun possui um laboratório de testes certificado - o primeiro na indústria de inventário de multi-metal e plástico. Isto, na nossa opinião, demonstra a nossa dedicação inabalável à qualidade e a nossa filosofia como um fornecedor de serviço completo.

SS 316-316L Stainless Steel angle Features

Alta resistência
Resistência à corrosão
Resistência ao calor
Resistência a baixas temperaturas
Proteção do ambiente
Desempenho da soldadura

Daxun Alloy Deixe a sua marca melhorar rapidamente

 

Angle – Steel Data
    EQUAL AND UNEQUAL ANGLE
ANGLE is available in other sizes on request
    Description Width (W) Depth (D) Espessura Padrão Weight per Superfície
(mm) (mm) (T) (mm) Comprimento Metre Area per
(kg/m) Metre
(m²/m)
ANGLE 20 X 20 X 3.0mm 20 20 3 6.0 metres 0.98 0.0897
ANGLE 25 X 25 X 3.0mm 25 25 3 7.5 metres 1.12 0.0953
ANGLE 25 X 25 X 5.0mm 25 25 5 7.5 metres 1.65 0.0953
ANGLE 25 X 25 X 6.0mm 25 25 6 7.5 metres 2.08 0.0953
ANGLE 30 X 30 X 2.5mm 30 30 2.5 6.0 metres 1.06 0.117
ANGLE 30 X 30 X 3.0mm 30 30 3 7.5 metres 1.35 0.115
ANGLE 30 X 30 X 5.0mm 30 30 5 7.5 metres 2.01 0.115
ANGLE 30 X 30 X 6.0mm 30 30 6 7.5 metres 2.56 0.115
ANGLE 40 X 40 X 2.5mm 40 40 2.5 6.0 metres 1.43 0.157
ANGLE 40 X 40 X 3.0mm 40 40 3 7.5 metres 1.83 0.155
ANGLE 40 X 40 X 4.0mm 40 40 4 6.0 metres 2.2 0.155
ANGLE 40 X 40 X 5.0mm 40 40 5 9.0 metres 2.73 0.155
ANGLE 40 X 40 X 6.0mm 40 40 6 9.0 metres 3.5 0.155
ANGLE 45 X 45 X 3.0mm 45 45 3 9.0 metres 2.06 0.175
ANGLE 45 X 45 X 5.0mm 45 45 5 9.0 metres 3.1 0.175
ANGLE 45 X 45 X 6.0mm 45 45 6 9.0 metres 3.97 0.175
ANGLE 50 X 50 X 2.5mm 50 50 2.5 9.0 metres 1.81 0.197
ANGLE 50 X 50 X 3.0mm 50 50 3 7.5 metres 2.31 0.195
ANGLE 50 X 50 X 4.0mm 50 50 4 9.0 metres 2.79 0.195
ANGLE 50 X 50 X 5.0mm 50 50 5 9.0 metres 3.48 0.195
ANGLE 50 X 50 X 6.0mm 50 50 6 9.0 metres 4.46 0.195
ANGLE 50 X 50 X 8.0mm 50 50 8 9.0 metres 5.68 0.195
ANGLE 55 X 55 X 5.0mm 55 55 5 9.0 metres 3.84 0.215
ANGLE 55 X 55 X 6.0mm 55 55 6 9.0 metres 4.93 0.215
ANGLE 65 X 50 X 5.0mm 65 50 5 9.0 metres 4.02 0.225
ANGLE 65 X 50 X 6.0mm 65 50 6 9.0 metres 5.16 0.225
ANGLE 65 X 50 X 8.0mm 65 65 8 9.0 metres 6.59 0.225
ANGLE 65 X 65 X 4.0mm 65 65 4 9.0 metres 3.69 0.255
ANGLE 65 x 65 x 5.0mm 65 65 5 9.0 metres 4.56 0.255
ANGLE 65 X 65 X 6.0mm 65 65 6 9.0 metres 5.87 0.255
ANGLE 65 X 65 X 8.0mm 65 65 8 9.0 metres 7.51 0.255
ANGLE 65 X 65 X 10.0mm 65 65 10 9.0 metres 9.02 0.255
ANGLE 75 X 50 X 5.0mm 75 50 5 9.0 metres 4.4 0.244
ANGLE 75 X 50 X 6.0mm 75 50 6 9.0 metres 5.66 0.244
ANGLE 75 X 50 X 8.0mm 75 50 8 9.0 metres 7.23 0.244
ANGLE 75 X 75 X 4.0mm 75 75 4 9.0 metres 4.29 0.295
ANGLE 75 X 75 X 5.0mm 75 75 5 9.0 metres 5.27 0.292
ANGLE 75 X 75 X 6.0mm 75 75 6 9.0 metres 6.81 0.292
ANGLE 75 X 75 X 8.0mm 75 75 8 9.0 metres 8.73 0.292
ANGLE 75 X 75 X 10.0mm 75 75 10 9.0 metres 10.5 0.292
ANGLE 90 X 90 X 6.0mm 90 90   6.0 9.0 metres    8.22 0.352
ANGLE 90 X 90 X 8.0mm 90 90   8.0 9.0 metres    10.6 0.352
ANGLE 90 X 90 X 10.0mm 90 90   10.0 9.0 metres    12.7 0.352
ANGLE 100 X 75 X 6.0mm 100 75   6.0 9.0 metres    7.98 0.342
ANGLE 100 X 75 X 8.0mm 100 75   8.0 9.0 metres    10.3 0.342
ANGLE 100 X 75 X 10.0mm 100 75   10.0 9.0 metres    12.4 0.342
ANGLE 100 X 100 X 10.0mm 100 100   10.0 9.0 metres    14.2 0.392
ANGLE 100 X 100 X 12.0mm 100 100   12.0 9.0 metres    17.7 0.392
ANGLE 100 X 100 X 4.0mm 100 100   4.0 9.0 metres    5.78 0.395
ANGLE 100 X 100 X 6.0mm 100 100   6.0 9.0 metres    9.16 0.392
ANGLE 100 X 100 X 8.0mm 100 100   8.0 9.0 metres    11.8 0.392
ANGLE125 X 75 X 6.0mm 125 75   6.0 9.0 metres    9.16 0.392
ANGLE 125 X 75 X 8.0mm 125 75   8.0 9.0 metres    11.8 0.392
ANGLE 125 X 75 X 10.0mm 125 75   10.0 9.0 metres    14.2 0.392
ANGLE 125 X 75 X 12.0mm 125 75   12.0 9.0 metres    17.7 0.392
ANGLE 125 X 125 X 8.0mm 125 125   8.0 9.0 metres    14.9 0.491
ANGLE 125 X 125 X 10.0mm 125 125   10.0 9.0 metres    18 0.491
ANGLE 125 X 125 X 12.0mm 125 125   12.0 9.0 metres    22.5 0.491
ANGLE 125 X 125 X 16.0mm 125 125   16.0 9.0 metres    29.1 0.491
ANGLE 150 X 90 X 8.0mm 150 90   8.0 9.0 metres    14.3 0.471
 ANGLE 150 X 90 X 12.0mm 150 90   12.0 9.0 metres    21.6 0.471
ANGLE 150 X 90 X 16.0mm 150 90   16.0 9.0 metres    27.9 0.471
ANGLE 150 X 100 X 10.0mm 150 100   10.0 9.0 metres    18 0.491
ANGLE 150 X 100 X 12.0mm 150 100   12.0 9.0 metres    22.5 0.491
ANGLE 150 X 150 X 10.0mm 150 150   10.0 9.0 metres    21.9 0.59
ANGLE 150 X 150 X 12.0mm 150 150   12.0 9.0 metres    27.3 0.59
ANGLE 150 X 150 X 16.0mm 150 150   16.0 9.0 metres    35.4 0.59
ANGLE 150 X 150 X 19.0mm 150 150   19.0 9.0 metres    42.1 0.59
ANGLE 150 X 90 X 10.0mm 150 90   10.0 9.0 metres    17.3 0.471
ANGLE 200 x 200 x 13.0mm 200 200   13.0 9.0 metres    40 0.788
ANGLE 200 X 200 X 16.0mm 200 200   16.0 9.0 metres    48.7 0.788
ANGLE 200 X 200 X 20.0mm 200 200   20.0 9.0 metres    60.1 0.788
ANGLE 200 X 200 X 26.0mm 200 200   26.0 9.0 metres    76.8 0.788

 

SS 316/316L Stainless Steel Angle Surface Type (3)

  • Applies to:curtain walls、entryways、canopies、handrails、window and door fittings、street furniture、cladding、masonry supports、fabrication projects,Can be used in a variety of applications, from decking, brackets, posts and frames to trim, tracks and siding

  • Applies to:curtain walls、entryways、canopies、handrails、window and door fittings、street furniture、cladding、masonry supports、fabrication projects,Can be used in a variety of applications, from decking, brackets, posts and frames to trim, tracks and siding

  • Applies to:curtain walls、entryways、canopies、handrails、window and door fittings、street furniture、cladding、masonry supports、fabrication projects,Can be used in a variety of applications, from decking, brackets, posts and frames to trim, tracks and siding

Informações disponíveis para consulta e descarregamento

Daxun is a trustworthy stainless steel Angle manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel angles have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

Produtos e projectos recentes de casos quentes

316L stainless steel Angle
stainless steel Angle
316L stainless steel Angle
stainless steel Angle
316L stainless steel Angle
stainless steel Angle
stainless steel Angle
316L stainless steel Angle
stainless steel Angle 316L
Introdução pormenorizada

Leading stainless steel angle Suppliers in China

A Daxun está envolvida em negócios internacionais há mais de dez anos. Em 2023, o volume de exportação ultrapassou os 100 milhões de dólares americanos, e o volume de exportação classificou-se entre os principais fabricantes chineses de aço inoxidável. A Daxun melhora continuamente as suas capacidades de serviço. Para servir o mercado global, estabeleceu três instalações de serviços de exportação na China, cooperando com empresas de engenharia, siderurgias e empresas de comércio internacional. A Daxun fornece serviços de cadeia de aço inoxidável e estabeleceu relações de cooperação de longo prazo com dezenas de siderúrgicas conhecidas em todo o mundo. O inventário inclui 50.000 toneladas de aço inoxidável convencional e 20.000 toneladas de aço duplex, ligas à base de níquel, aço resistente ao calor e outros metais. Os materiais de aço inoxidável da Daxun são de qualidade estável, e as variedades, especificações e pesos de entrega cumprem rigorosamente as normas.


316 Stainless Steel Angle

  • 316 Stainless Steel Angle is an austenitic chromium nickel angle shape containing molybdenum which provides superior corrosion resistance and increased strength at elevated temperatures when compared to 304 Stainless.
  • Because of the 4% molybdenum concentration, the 316 material is resistant to chloride ion stress corrosion. Stainless Steel 304 Unequal Angle Sizes vary depending on the application needs. Angles are used to hold components together using a grip. There are also angles with bolt holes for screws and bolts. The 316 Stainless Steel Unequal Angle is suitable for more corrosive applications than the 304 angles. The Stainless Steel Unequal Angle is just as frequent as the Equal Angle. They are utilized in a variety of applications, including brackets, trim, and reinforcements. Please contact us for more information about the angles and their costs.

Characteristics

  • Cold Working: Good
  • Corrosion Resistance: Excellent
  • Heat Resistance: Good
  • Heat Treatment: Poor
  • Hot Working: Fair
  • Machinability: Good
  • Weldability: Very Good

 

Why should you buy stainless steel angles from Daxun?

Daxun’s objective is to supply you with the highest quality and most durable stainless steel angles and steel. We provide hundreds of stainless steel angles in various leg lengths, thicknesses, and material grades. Our 316/316L and 304/304L stainless steel angles are made at our well-equipped production facility using high-quality raw materials and cutting-edge technology, overseen by qualified workers. Some other significant benefits of partnering with us include:

  • When you purchase any steel products from us, you get the products directly from the manufacturer.
  •  Our employees are dedicated to providing the lowest prices and fastest shipping times so that you can start your project right away!
  •  We have a skilled, capable workforce for quality checks, packaging, and shipping.
  •  We follow multiple quality check levels, which helps ensure that the products are of the highest standards.
  •  We have a qualified and dedicated support team available 24×7 to help you out if any issues arise.

Suppliers from China Make Stainless Steel Angles to Size

  • Daxun is a leading supplier of stainless steel products in China. With high-quality products and customized services, we can meet all your stainless steel angle needs. Order online or by phone and get it delivered in as fast as 15 days.

304 and 316 Grade Stainless Steel Angles

  • This versatile right angle steel has a wide range of applications and is available in grades 304 /30L and 316 /316L. Grade 304 is the most versatile and commonly used grade of stainless steel angle steel and is suitable for most general applications. It is easy to weld and has good formability and corrosion resistance. Sometimes called 18/8 stainless steel because its composition includes 18% chromium and 8% nickel, grade 304 is well suited to most applications.
  • Grade 316 is more suitable for harsh environments, such as exposure to salt water and areas with high industrialization. Due to the higher nickel content and the addition of molybdenum to the metal, it has higher corrosion resistance than grade 304, especially to chlorides and chlorinated solutions. It also has good weldability, but is more difficult to process than grade 304.

There are two basic processes for manufacturing stainless steel angles:

  • laser melting and hot rolling. Hot rolled stainless steel angles are less expensive. They typically have rounded or tapered edges. On the other hand, laser melted stainless steel angles have consistent sharp and square corners. They also include sandblasting and a smoother finish. The surface of laser melted stainless steel angles is smoother than that of hot rolled stainless steel angles. ​​

Choose Your Size and Size

  • We offer a wide variety of stainless steel angles, so whatever your needs, we have you covered. Grade 304 stainless steel angles come in a variety of sizes with thicknesses from 3mm-16mm and lengths of 1m, 3m, or 6m.
  • Our grade 316 angles come in thicknesses from 3mm-16mm and lengths of 1m, 3m, or 6m. Angles are available in a variety of sizes.

Talk to Your Preferred Stainless Steel Angle Supplier

  • It couldn’t be easier to buy the stainless steel angles you need, as well as all of our other products, through our website. Alternatively, you can call our sales team in China at +8613382898899 to place your order and they will be happy to process your order. If you have any questions, you can even send an email to daxunalloy@gmail.com and our team will get back to you as soon as possible.
Como obter uma cotação OU compreender a informação de mercado o mais rapidamente possível?

Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email (Daxunalloy@gmail.com) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week

Podem dar-me algumas amostras?

As amostras podem ser fornecidas gratuitamente, mas o frete é suportado pelo cliente e será reembolsado após cooperação.

Para que países já exportou?

Exportámos para mais de 42 países, como o Canadá, Chile, Kuwait, Alemanha, Coreia do Sul, Arábia Saudita, Singapura, etc.

Qual é o vosso MOQ?

Our MOQ is 1 ton for 316L Stainless Steel Angle.

Como é que se controla a qualidade?

We have a complete organization from raw material purchasing to processing and shipment arranging. In the whole chain, the documentary people ad QC will look for and check it by precise requirements.The third party inspection is welcomed.

Qual é o prazo de entrega?

As encomendas de teste podem ser entregues no prazo de uma semana. Para as encomendas normais, são necessárias cerca de duas semanas.

Envie hoje o seu pedido de informação
Orçamento rápido