Daxun is a 304/304L stainless steel coil China supplier
As a leading stainless steel coil supplier and exporter in China, Daxun supplies stainless steel coils to all over the world.
- Coil grade: S30400-S30403
- Coil thickness: from 0.4 mm to 12.00 mm
- Coil width: 1000 mm, 1250 mm, 1500 mm and 2000 mm.
- Coil surface: 2B, BA, matte, polished, 8k mirror.
- If necessary, the stainless steel coil will come with a protective film to protect the metal surface from unnecessary damage.
Global leader in stainless steel Coil fabrication services
Daxun Metal offers a full range of premium SS 304/304L Stainless Steel Coil. Daxun strives to stay on the cutting edge of technology and practice so that we can always provide your business with the highest quality 304 Stainless Steel Coil. Daxun’s goal is to safely manufacture and sell the highest quality Stainless Steel Coil and supply it to customers around the world. Contact Daxun today and let us be your preferred 304/304L Stainless Steel Coil supplier!
304 Stainless Steel Coil is a low carbon, molybdenum-bearing austenitic stainless steel coil. Its chemical makeup contains at least 18% chromium and 8% nickel. These grades of stainless steel coils are employed because they are resistant to a wide range of chemical corrosives while also having strong mechanical qualities. 304 grade stainless steel is corrosion resistant, making it perfect for food processing equipment and surgical instruments. It has superior formability and welding properties when compared to other grades of stainless steel. Daxun is a well-known manufacturer, trader, and supplier of 304 stainless steel coils. Steel coils are manufactured with high precision and fulfill international quality standards.
Daxun is an ISO 9001:2008 certified firm that specializes in supplying and exporting ASTM A240 304 Stainless Steel Coils. 304 Stainless Steel Coil can be cut to your specifications and comes with a complete set of mill test results. Custom lengths and widths are available up to 2000 mm. Exporting is our specialty! We can obtain several hard-to-find grades and/or non-standard sizes to satisfy our customers’ specific needs. With our significant experience in processing steel coil goods, we can cut all ASTM SS 304 Steel Coils to the desired size.
Dados
- Parâmetro
- Elemento
- Propriedades mecânicas
- PROPRIEDADES FÍSICAS
- Todos os equivalentes
- 304 coil stock
| SS 304 / 304L Stainless Steel Coil Specification | ASTM A240 / ASME SA240 |
| SS 304 / 304L Stainless Steel Coil Manufacturing Process | Hot Rolled (HR) / Cold Rolled (CR) |
| SS 304 / 304L Stainless Steel Coil Grades | 202 / SS 304 / 304L / SS 304 / 304LL / SS 304 / 304LH / 309S / 310S / 316 / 316L / 316Ti / 317L / 321 / 321H / 347 / 347H / 904L etc. |
| UNS No. – UNS SSS 304 / 304L00, UNS SSS 304 / 304L03, UNS S31008, UNS S31620, UNS S31603, UNS S31603, UNS S31635, UNS S31703, UNS S32100, UNS S34700, UNS S34709, UNS S8904 | |
| EN No. – 1.4301, 1.4307, 1.4845, 1.4401, 1.4404, 1.4571, 1.4438, 1.4541, 1.4550, 1.4551, 1.4539 | |
| SS 304 / 304L Stainless Steel Coil Thickness | 0.6 MM TO 80 MM THICKNESS |
| SS 304 / 304L Stainless Steel Coil Width | 1250 MM / 1500 MM / 2000 MM / 04 Feet / 05 Feet and Custom Cut Width as Per Requirement |
| SS 304 / 304L Stainless Steel Coil Length | 2400 MM / 2420 MM / 6000 MM / 08 Feet / 10 Feet / Coil Cut and Custom Cut Length as Per Requirement |
| SS 304 / 304L Stainless Steel Coil Surface Finish | 2B, 2D, BA, MATT, MATT PVC, No.4, No.5, SB, HR, No.8, Mirror, Hairline, Brush, Textured, Oil base wet Polished, Both sides Polished available. |
| SS 304 / 304L Stainless Steel Coil Coating | PVC coating Normal / Laser, Film: 100 micrometer, Color: black/white. |
| SS 304 / 304L Stainless Steel Coil Other Testing | NACE MR0175, Ultrasoung TEST, IGC TEST, Intergranular Corrrosion Test as per ASTM A262 Practice E, Charpy Impact Test, Macro, Grain Size, Hardness, etc. |
| SS 304 / 304L Stainless Steel CoilValue Added Services | Gas Cutting / CNC Plasma Cutting / Profiling / Rolling / Bending / Sheet Metal Fabrication / Drill / Punch / Machining / Sand Blasting / Shot Blasting / Heat Treatment |
| SS 304 / 304L Stainless Steel Coil Packaging | Loose / Carrate / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps |
| SS 304 / 304L Stainless Steel Coil Shipment & Transportation | By Road – Truck / Train Partial Load, Full Load, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes |
| SS 304 / 304L Stainless Steel Coil Material Test Certificate | Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS, Bureau of Indian Standards BIS Approved ETC |
| Manufacturer | POSCO, Aperam, Jindal Stainless, DKC Korea, Thyssenkrup, Baosteel, TISCO,Arcelor Mittal, VDM,Nippon Metal, Outokumpu,Qingshan,Delong. |
| Shipping Port | Shanghai/Ningbo port/Tianjin/Qindao |
| Composition of 304/304L/304LN/304H tubing and pipe | ||||
| Grau | 304 | 304L | 304LN | 304H |
| Designação UNS | S30400 | S30403 | S30453 | S30409 |
| Carbono (C) Máx. | 0.08 | 0.030* | 0.03 | 0.04 - 0.10 |
| Manganês (Mn) Máx. | 2 | 2 | 2 | 2 |
| Fósforo (P) Máx. | 0.045 | 0.045 | 0.045 | 0.045 |
| Enxofre (S) Máx. | 0.03 | 0.03 | 0.03 | 0.03 |
| Silício (Si) Máx. | 1 | 1 | 1 | 1 |
| Crómio (Cr) | 18.0-20.0 | 18.0-20.0 | 18.0-20.0 | 18.0-20.0 |
| Níquel (Ni) | 8.0-11.0 | 8.0-11.0 | 8.0-11.0 | 8.0-11.0 |
| Molibdénio (Mo) | — | — | — | — |
| Azoto (N) | — | — | 0.10-0.15 | — |
| Ferro (Fe) | Bal. | Bal. | Bal. | Bal. |
| Outros elementos | — | — | — | — |
| Tipo | Resistência ao escoamento 0.2% offset (KSI) | Resistência à tração (KSI) | % Alongamento (comprimento do calibre de 2″) |
| 304 Anexos | 30 min. | 75 min. | 40 min. |
| 304 ¼ Duro | 75 min. | 125 min. | 12 min. |
| 304 ½ Duro | 110 min. | 150 min. | 7 min. |
| 304L Ann | 25 min. | 70 min. | 40 min. |
| 304L ¼ Duro | 75 min. | 125 min. | 12 min. |
| 304L ½ Duro | 110 min. | 150 min. | 6 min. |
| 304 & 304L | ||
| Densidade (lb./in^2) @ RT | 0.29 | |
| Módulo de elasticidade em tensão (psi x 10^6) | 28 | |
| Calor específico (BTU/o F/lb.) | 32 a 212 oF | 0.12 |
| Condutividade térmica (BTU/hr/ft^2/ft) | 212oF | 9.4 |
| 932oF | 12.4 | |
| Coeficiente médio de expansão térmica (pol. x 10^-6 por o F) | 32 a 212oF | 9.2 |
| 32 a 600oF | 9.9 | |
| 32 a 1.000oF | 10.2 | |
| 32 a 1.200oF | 10.4 | |
| Resistividade eléctrica (micro ohms - cm) | a 70oF | 72 |
| Gama de pontos de fusão (oF) | 2550 a 2650 | |
| Resistência à oxidação - Serviço contínuo (oF) | 1,650 | |
| Resistência à oxidação - Serviço intermitente (oF) | 1,500 |
| PADRÃO | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | PT |
| SS 304 | 1.4301 | S30400 | SUS 304 | 304S31 | 08Х18Н10 | Z7CN18-09 | X5CrNi18-10 |
| • 304 Stainless Steel HR Coil | • Baosteel Stainless Steel 304 Coil |
| • 304 Stainless Steel Chequered Coil | • Stainless Steel Cladding 304 Coil |
| • 304 Stainless Steel Golden Laser Pattern Coil | • Black SS 304 Coil 4mm Thick |
| • Super thin-Mirror surface BA ss 304 Coil | • Bright-pickled Stainless Steel 304 Coil |
| • Super Austenitic SS 304 Coil | • Cold rolled, heat treated 304 Coil |
| • ASTM A240 304 Coil | • 3mm Cold Rolled AISI SS 304 Coil |
| • JMSS cold rolled ss 304 Coil | • Mill Supply SS 304 Coil |
| • Cold Rolled No.1 Finish SS 304 Coil | • Grade Prime SS 304 Coil |
| • SEW 400 Stainless Steel 304 Coil | • Carpenter Custom 450 Stainless Steel 304 Coil |
| • Hot Rolled Stainless Steel 304 Coil | • Cut to Size Stainless Steel 304 Coil |
| • Sales Promotion SS 304 Coil | • Non Magnetic Polishing Stainless Steel 304 Coil |
| • Cr Stainless Steel 304 Coil | • ASME SA240 304 Coil |
| • SS 304 Mill Test Certificate Coil | • Grade 304 SS Finish coil |
| • ASTM A240 304 Coil | • 304 Stainless Steel Blank Coil |
| • Cold rolled, bright annealed 304 Coil | • 304 Stainless Steel Perforated Coil |
| • Ground Stainless Steel 304 Coil | • Embossed ss 304 Coil |
| • Hot Selling AISI SS 304 Coil | • Cheap cold rolled ss 304 Coil with best price |
| • SS 304 Rose Golden Coil | • Brush finish ss 304 Coil price list |
| • Surface coated Stainless Steel 304 Coil | • SS URANUS B6 304 Coil |
| • Satin finish Stainless Steel 304 Coil | • 2B SUS SS 304 Coil |
| • AISI stainless steel 304 armor Coil | • Food Grade Stainless Steel 304 Coil |
| • Satin finish Stainless Steel 304 Coil | • No. 4 PVC Coated SS 304 Coil |
| • Mirror Finish SS 304 Coil | • SS 304 Coil Blasted Tin-Gold Rose |
| • SS 304 Coil Gold Brush Finish | • 2mm ASTM SS 304 Coil |
| • 304 Stainless Steel CR Coil | • Stainless Steel Corrugated 304 Coil |
| • 304 Stainless Steel 2B Coil | • ASTM B625 304 Coil |
| • 304 Stainless Steel B. Q. Profile Coil | • Brushed or dull polished Stainless Steel 304 Coil |
| • Best selling 4’x8′ mirror finished ss 304 Coil | • Cold rolled, heat treated, pickled 304 Coil |
| • Decorative hairline inox cold rolled ss 304 Coil | • 10K Mirror Finish Surface SS 304 Coil |
| • Hair Line Finish SS 304 Coil | • Gold Etched SS 304 Coil |
| • Laser cutting ss 304 Coil | • 18 Gauge SS 304 Coil |
| • Tisco Supplier 3mm Thickness Stainless Steel 304 Coil | • Patterned Stainless Steel 304 Coil |
| • Decorative Stainless Steel 304 Coil | • #4 Finish Stainless Steel 304 Coil |
| • Scotch Brite SS 304 Coil | • Patterned Stainless Steel 304 Coil |
| • Dimensional SS Grade 304 coil | • Passenger Elevator Cabin SS 304 Coil |
Escolha a Daxun e deixe os seus clientes satisfeitos.
Quick response 304 Stainless Steel coil
Fornecemos entrega atempada e rápida de produtos de aço inoxidável para clientes com necessidades urgentes. Por detrás da velocidade está o sistema de apoio, desde o fluxo de informação até à logística e ao fluxo de capital. Por exemplo, em termos de fluxo de informação, os dados das encomendas da Daxun são enviados para o sistema de logística em tempo real, e os dados estão perfeitamente ligados; em termos de logística, o centro de processamento está perto de auto-estradas, rios e mares, com uma programação razoável, resposta rápida, armazenamento e ligação de transporte, e carregamento eficiente, garantindo que a tarefa é concluída dentro do prazo.
Vantagens da Daxun
Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel achieves full traceability of each 304 Stainless Steel coil from the ERP system, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strict monitoring during sales, and provides worry-free service guarantees after sales.


Stainless Steel coil packaging
A Daxun Alloy assegura a melhor qualidade de embalagem, uma vez que esta desempenha um papel importante no transporte internacional de mercadorias, onde as mercadorias passam por vários canais para chegar ao destino final, pelo que prestamos especial atenção à embalagem. Embalamos os nossos produtos de várias formas, consoante o produto. Embalamos os nossos produtos de várias formas, tais como:
- Caixas e caixotes
- Película retrátil
- Paletes de madeira
- Caixas de madeira
Qualidade, entrega, inspeção
- Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
- During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
O nosso prazo de entrega está estritamente de acordo com o contrato. - Apoio a agências terceiras do cliente para se deslocarem à fábrica para inspeção
- Apoio a amostras gratuitas aos clientes para testes
- Apoio à inspeção de fábrica no local ou por vídeo

304 Stainless Steel coil Ordering Information
As ordens de compra devem incluir quantidade, grau, tipo ou categoria, referência API5L, espessura, largura, comprimento e quaisquer anexos aplicáveis ou requisitos adicionais relacionados com a composição química, propriedades mecânicas, tratamento térmico, testes adicionais, processo de fabrico, revestimento de superfície ou acabamento final. Contacte Daxun agora, nós responderemos ao seu e-mail o mais rápido possível.
Apoio técnico
Se necessitar de qualquer assistência técnica adicional, o nosso metalúrgico residente e a nossa equipa experiente terão todo o prazer em ajudar. Além disso, a Daxun possui um laboratório de testes certificado - o primeiro na indústria de inventário de multi-metal e plástico. Isto, na nossa opinião, demonstra a nossa dedicação inabalável à qualidade e a nossa filosofia como um fornecedor de serviço completo.
SS 304 Stainless Steel Coil Features
Daxun Alloy Deixe a sua marca melhorar rapidamente
- Galeria
- Product Series
- Main Equipment
| Grau | Tipo | Espessura | Superfície |
| Austenítico | 304/304H/304L/304J1 | 0,25-150mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0,4-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0,3-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Ferrite | 430 | 0,4-3,0 mm | 2B/BA/NO.4/8K/SB/HL |
| Ferrite ultra-puro | 443 | 0,4-2,0 mm | 2B |
| 436L/439/444/441 | 0,5-3,0 mm | 2B、2D | |
| 409L | 0,4-2,5 mm | 2B、2D | |
| Aço superaustenítico | N08904 | 0,6-50mm | SWE / JPN / CHN |
| S31254 | 0,5-50mm | SWE / JPN / CHN | |
| N08926 | 0,5-50mm | SWE / JPN / CHN | |
| N08367 | 0,5-50mm | SWE / JPN / CHN | |
| Liga à base de níquel | N08031 | 1.0-50mm | EUA / JPN / GER |
| N08810/N08800 | 0,8-50mm | EUA / JPN / CHN | |
| N08028 | 1,0-20mm | EUA / GER / JPN | |
| N08020 | 1,0-20mm | EUA / GER / JPN | |
| N08825 | 0,8-40mm | US / GER / SWE / JPN / CHN | |
| N10276 | 0,5-50mm | EUA / GER / JPN | |
| N06022 | 1.0-50mm | EUA / GER / JPN | |
| N06625 | 0,8-20mm | EUA / GER / CHN | |
| N04400 | 1,0-20mm | EUA / GER / JPN | |
| N06600 | 1.0-50mm | US / GER / JPN / CHN | |
| N02201 | 0,5-20mm | EUA / JPN | |
| Titânio | TA1/Gr1 | 0,5-50mm | JPN / CHN |
| TA2/Gr2 | 0,5-50mm | JPN / CHN | |
| Material de soldadura | ERNiCrMo-13 | 1.2、2.4mm | ALEMANHA |
| ERNiCrMo-3 | 2,4 mm | ALEMANHA | |
| ERNiCrMo-4 | 2,4 mm | EUA |
| Subsidiary | Main Equipments | Qty | Annual Capacity |
| Daxun Stainless steel co.(JiangSu) | Slitting Machine | 1 | Decorative Sheet:60,000 tons |
| Cutting Machine | 1 | ||
| No.4 And Hairline Sheet To Sheet Polishing Machine | 1 | ||
| No.4/Hairline Coil To Coil Polishing Machines | 1 | ||
| 8K/Super Mirror Sheet To Sheet Polishing Machines | 2 | ||
| 8K/Super Mirror Coil To Coil Polishing Machines | 3 | ||
| PVD Color Coating Machines | 4 | ||
| Liquid Chemical Coating Machines | 2 | ||
| Anti Finger Printing Machines | 2 | ||
| Auto Pick and Place machines | 16 | ||
| 304 Stainless Steel coil Washing Machine | 1 | ||
| Daxun Stainless steel co.(Shanghai) | Cold Rolling Machine | 3 | 2B Coils:100,000 tons |
| Annealing & Pickling Line | 2 | Decorative Sheet;30,000 tons | |
| Slitting Machine | 1 | ||
| Cut to Length Machine | 1 | ||
| No.4/HL Polishing Machine(Sheet to Sheet) | 3 | ||
| 8K Polishing Machine(Sheet to Sheet) | 13 | ||
| PVD Titanium Coating Machine | 4 | ||
| Liquid Chemical Coating Machines | 1 | ||
| Daxun Stainless steel co.(Shandong) | Cold Rolling Machine | 3 | 2B & BA Coil:220,000 tons |
| Annealing & Pickling Line(2B & BA) | 2 | Decorative Sheet:60,000 tons | |
| Tension Levering & Skin Pass | 1 | ||
| Slitting Machine | 1 | ||
| Cut to Length Machine | 1 | ||
| No.4/HL Polishing Machine(Sheet to Sheet) | 1 | ||
| 8K Polishing Machine(Sheet to Sheet) | 11 | ||
| Automatic Copper Coating Machine | 1 | ||
| Digital Printing Machine | 1 | ||
| PVD Titanium Coating Machine | 3 | ||
| Liquid Chemical Coating Machines | 1 | ||
| Anti-finger Machine | 1 | ||
| Daxun Stainless steel co.(Sichuan) | Slitting Machine | 1 | 2B & BA Coil:180,000 tons |
| Cutting Machine | 1 | Decorative Sheet:50,000 tons | |
| No.4 And Hairline Sheet To Sheet Polishing Machine | 1 | ||
| No.4/Hairline Coil To Coil Polishing Machines | 1 | ||
| 8K/Super Mirror Sheet To Sheet Polishing Machines | 1 | ||
| 8K/Super Mirror Coil To Coil Polishing Machines | 1 | ||
| PVD Color Coating Machines | 1 | ||
| Liquid Chemical Coating Machines | 1 | ||
| Anti Finger Printing Machines | 1 |
SS304 Surface Types of Stainless Steel Coils (6)
Informações disponíveis para consulta e descarregamento
Daxun is a trustworthy stainless steel coil manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the 304 Stainless Steel coil have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
Produtos e projectos recentes de casos quentes
Produtos relacionados (11)
Leading stainless steel coil Suppliers in China
Daxun has been engaged in international business for more than ten years. In 2023, its export revenue exceeded US$100 million, and its export volume ranked among the top Chinese stainless steel manufacturers. Daxun continues to improve its service skills. In order to serve the global market, we have established three export service facilities in China and cooperated with engineering enterprises, steel mills and international trading companies. Daxun provides stainless steel chain services and has established long-term cooperative relationships with dozens of well-known steel mills around the world. Its inventory includes 50,000 tons of conventional stainless steel coils and 20,000 tons of duplex steel, nickel-based alloys, heat-resistant steel and other metals. Daxun’s stainless steel materials are of consistent quality. Types, specifications and delivery weights strictly comply with standards.
304 STAINLESS STEEL Cost
- This grade of stainless steel’s relatively low cost is resulting in more frequent use among engineers and architects. Because it’s light in weight, you can pack in more per pound.
What are the applications that 304 stainless steel coils can be used?
304 stainless steel coils can be used for a variety of applications, including:
- 1. Food and beverage processing.
304 stainless steel coils are used in the food sector to construct equipment such as water heaters, boilers and tanks.2. Healthcare Equipment - 2.Hospitals employ 304 stainless steel coils to manufacture a wide range of medical equipment, such as operating tables, bedpans, and baby incubators.
- 3. Industrial Machinery
Industrial machinery manufacturers use 304 stainless steel coils for items like valves and pumps in their products. - 4. Construction Equipment
Building contractors utilize 304 stainless steel coils to create weatherproofing materials that protect structures from rain and snow while they are being built or renovated.
Features of 304 stainless steel coils
304 stainless steel coils have the following features:
- 1. 304 stainless steel coils have high strength, hardness, wear resistance, corrosion resistance, and thermal conductivity.
- 2. 304 stainless steel coils have great temperature resistance (up to 870 degrees).
- 3. 304 stainless steel coils have good anti-oxidation properties and may be used in a variety of applications;
- 4. 304 stainless steel coils are widely utilized in a variety of industries, including food, chemical industry, and metallurgy.
- 5. Although 304 stainless steel coils are less expensive than other grades, their price will climb swiftly as demand develops.
PROCESSING:
Types 304 and 304L cannot be hardened by thermal treatment. Annealing: Heat to 1850o F to 2050 o F and cool at sufficiently high rates through 1500oF to 800oF to avoid precipitation of chromium carbides. Stress Relief Annealing: Cold worked parts should be stress relieved at 750oF for ½ to 2 hours.
FORMING:
Annealed Types 304 and 304L can be fabricated by roll forming, deep drawing, bending and most other fabrication techniques. Due to the high work hardening rate of these materials, intermediate anneals maybe required to successfully fabricate the part.
WELDING:
Types 304 and 304L are weldable by most fusion or resistance welding techniques. If filler metal is required, Type 308 is normally used. Type 304L should be used in heavier sections to reduce the occurrence of carbide precipitation in the heat affected region adjacent to the weld pool
CORROSION:
Types 304 and 304L provides corrosion resistance in a wide range of moderately oxidizing and reducing conditions, fresh water and non-marine applications.
What are the commonly used surfaces of stainless steel coils?
The surface finish of 201 stainless steel coil might vary depending on the cold rolling processing methods used and the surface treatment used after rolling. Surface treatments for stainless steel coils include NO.1, 2B, 4, HL, 6, 8, BA, TR hard, heavy rolling bright 2H, polished bright, and other surface treatments:
- NO.1: The surface obtained after hot rolling, heat treatment and pickling of stainless steel strip. It is used to remove the black oxide scale formed by pickling or similar processes during hot rolling and heat treatment. It ranks first in surface treatment. The No. 1 surface is silvery white and matte. It is generally used in heat-resistant and corrosion-resistant industries that do not require high surface gloss, such as the alcohol industry, chemical industry, large containers, etc.
- 2B: Unlike the 2D surface, the 2B surface is smoothed by a light roller, and the surface is brighter. The surface roughness Ra value measured by the equipment ranges from 0.1 to 0.5μm, which is a typical value for most processing types. This stainless steel strip surface has the strongest adaptability and is suitable for industries such as chemical, papermaking, petroleum, medical, and a wide range of fields such as building curtain walls.
- TR hard surface: TR stainless steel is also called hard steel. Its characteristic steel grades include 304 and 301, which are used for items that require high strength and hardness, such as railway vehicles, conveyor belts, springs and washers. The idea is to use the work hardening characteristics of austenitic stainless steel to improve the strength and hardness of 304 Stainless Steel coil through cold working methods such as rolling. In order to replace the gentle flatness of the 2B base surface, the hard material is gently rolled by a few percent to tens of percent, and no annealing is performed after rolling. Therefore, the TR hard surface of the hard material is the rolled surface after the cold rolling process.
- Re-rolled bright 2H: After the rolling operation, the stainless steel strip will be bright annealed. A continuous annealing line can be used to quickly cool the strip. The stainless steel strip travels along the line at a speed of 60-80m/min. After this process, the surface finish will be 2H re-rolled bright.
- No. 4: The No. 4 surface has a good polishing effect and is brighter than No. 3. It can also be obtained by polishing the cold-rolled 304 Stainless Steel coilwith a 2D or 2B surface, and then polishing the processed surface with a sanding belt with a particle size of 150-180#. The tool measures the surface roughness (Ra) between 0.2 and 1.5μm. The No. 4 surface is widely used in restaurants and cooking equipment, medical equipment, architectural decoration, containers and other applications.
- HL: The HL surface is often called a hairline finish. The Japanese JIS standard specifies a continuous hairline abrasive surface obtained by polishing with a 150-240# abrasive belt. The restrictions under the Chinese GB3280 standard are unclear. HL surface finish is commonly used for architectural decoration, such as elevators, escalators, and exterior walls.
- No. 6: The No. 6 surface is further polished on the basis of No. 4 with a Tampico brush or a W63 grit abrasive material specified in the GB2477 standard. The surface has good metallic luster, softness, weak reflection, and no imaging. Due to its good performance, it is very suitable for curtain walls, tassel decoration, and cooking supplies.
- BA: BA is a surface that is brightly heat treated after cold rolling. Bright heat treatment is annealing in a protective atmosphere to ensure that the surface is not oxidized and retain the gloss of the cold-rolled surface, and then it is polished with a high-precision smooth roller to improve the surface brightness. The instrument evaluates the surface roughness to be 0.05-0.1μm, indicating that the surface is close to a mirror surface. BA surfaces can be used in a variety of applications, including food utensils, household appliances, medical equipment, automotive parts, and decorations.
- No. 8: Mirror surface, maximum reflectivity, no abrasive particles. The stainless steel deep processing industry also refers to 8K board. BA material is often used as raw material for mirror processing. It only needs to be polished. The surface is beautiful after mirror processing and is often used in building entrances and interior decoration.
What is the standard sea packaging stainless steel coil?
- Standard export sea packaging:
Waterproof Paper Winding+PVC Film+Strap Banding+Wooden Pallet or Wooden Case; - Customized packaging as your request (Logo or other contents accepted to be printed on the packaging);
- Other special packaging will be designed as customer’s request;
Eye to wall and eye to sky are both available; - By International Express: DHL/UPS/FEDEX/EMS and our own express line;
- By air, sea or land;
- Shipping Port: Shanghai, Ningbo, Qingdao, Tianjin or as your request.
Contact your stainless steel coil suppliers
- You can easily order stainless steel coils in any size and quantity online.
Alternatively, our friendly sales team will be happy to take your order. Simply call +86 13382898899 or email Daxunhejin@gmail and we will get back to you as soon as possible.
Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email (Daxunalloy@gmail.com) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week
As amostras podem ser fornecidas gratuitamente, mas o frete é suportado pelo cliente e será reembolsado após cooperação.
Exportámos para mais de 42 países, como o Canadá, Chile, Kuwait, Alemanha, Coreia do Sul, Arábia Saudita, Singapura, etc.
Our MOQ is 1 ton for 304 Stainless Steel coil
We have a complete organization from raw material purchasing to processing and shipment arranging. In the whole chain, the documentary people ad QC will look for and check it by precise requirements.The third party inspection is welcomed.
As encomendas de teste podem ser entregues no prazo de uma semana. Para as encomendas normais, são necessárias cerca de duas semanas.