CP Grade 3 Titanium Plate Manufacturer - Daxun Alloy
As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.
- Plate Grade:R50550 / CP TI50A
- Plate Production type:cold rolling, hot rolling, forging.
- Features:High strength, Lightweight, High-temperature resistance
- Surface:bright, polished, pickled, sandblasted, etc.
- Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request
————Daxun produces titanium sheets in China to meet the diverse and ——требовательные потребности клиентов!
Providing High-quality CP Grade 3 Titanium Plates to Serve Customers Worldwide
CP Grade 3 Titanium plate is a commercially pure titanium grade known for its excellent balance of strength and ductility. It offers higher mechanical properties compared to Grades 1 and 2, making it ideal for applications requiring moderate strength and good formability. This grade features outstanding corrosion resistance, especially in marine and chemical environments, along with low density and high toughness.
Key Characteristics:
- Composition: CP Grade 3 is primarily titanium (typically ~99.1%), with small amounts of oxygen, iron, carbon, nitrogen, and hydrogen. The oxygen content is the main factor influencing its strength.
- Mechanical Properties: It offers higher tensile and yield strength than Grades 1 and 2, making it suitable for applications requiring more robust performance while still maintaining good ductility.
- Corrosion Resistance: Like all CP titanium grades, Grade 3 provides outstanding resistance to corrosion, especially in oxidizing environments such as those containing chlorides or seawater.
- Fabrication: It can be welded, formed, and machined using conventional methods, which enhances its versatility in manufacturing.
- Biocompatibility: The material is biocompatible, allowing its use in medical implants and other healthcare applications.
Common Applications:
- Аэрокосмическая промышленность: For components that need a mix of strength, light weight, and corrosion resistance.
- Chemical Processing: Equipment exposed to corrosive environments.
- Marine Engineering: Parts subject to seawater corrosion.
- Медицинские приборы: Implants and surgical tools due to its biocompatibility.
CP Grade 3 vs. Other Titanium Grades
CP Grade 3 Titanium plate serves as a powerful middle-ground option in the titanium family. It delivers significantly higher strength than the softer, more formable Grades 1 and 2, making it suitable for components that face greater mechanical stress. Crucially, it achieves this strength boost while retaining excellent corrosion resistance and good weldability, a key advantage over the even stronger but less ductile CP Grade 4.
When compared to the popular alloy Grade 5 (Ti-6Al-4V), CP Grade 3 is less strong and not heat-treatable. However, it is far easier to form and fabricate, and it provides superior corrosion resistance in many reducing chemical environments. This makes CP Grade 3 the ideal choice when your project requires a step up in strength from the basic CP grades but cannot sacrifice the ease of manufacturing and outstanding durability needed for demanding aerospace, marine, and chemical processing applications.
Данные
- Параметр
- Физические свойства
- Механические свойства
| Элемент | Содержание (%) |
|---|---|
| Titanium (Ti) | Balance (~99.1%) |
| Oxygen (O) | 0.10 – 0.27 |
| Железо (Fe) | ≤ 0.30 |
| Carbon © | ≤ 0.08 |
| Азот (N) | ≤ 0.05 |
| Hydrogen (H) | ≤ 0.015 |
| Недвижимость | Значение |
|---|---|
| Плотность | ~4.51 g/cm³ |
| Температура плавления | ~1660–1670 °C |
| Modulus of Elasticity | ~103–107 GPa |
| Теплопроводность | ~21.9 W/m·K (at 25°C) |
| Электрическое сопротивление | ~420 nΩ·m |
| Недвижимость | Значение |
|---|---|
| Прочность на разрыв | ~450–485 MPa |
| Предел текучести | ~380–415 MPa |
| Удлинение | ~20–30% |
| Твердость (Бринелль) | ~200–240 HB |
Выберите Daxun, чтобы помочь вашему проекту взлететь.

Быстрая доставка
At Daxun Alloys Co., Ltd., we specialize in the rapid supply of premium CP Grade 3 titanium plates to meet your urgent project needs. With our extensive inventory and efficient logistics network, we ensure prompt delivery without compromising on quality. Whether you require standard sizes or custom-cut solutions, our team is committed to providing reliable, on-time service to support your manufacturing and engineering schedules.
Custom Cutting
Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:
- Water jet cutting
- Laser cutting
- Plasma cutting
- Wire cutting
- Bending
- Slitting
- Sawing


Упаковка
We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- Коробки и ящики
• Shrinkwrap
- Деревянные поддоны
- Деревянные ящики
Техническая поддержка
If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.

Daxun CP Grade 3 Titanium sheet Let your brand improve rapidly
- Other Titanium Plate Grades
| Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of Plate, Bar and Tube. | |
| Products/Processing Standard | Grade/Size |
| Titanium Plate, Sheet, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136 | GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Thickness:( 0.0197”-6”)Max Width: 12 feet,Max Length: 50 feet) |
| AMS-T-9046 | |
| Titanium and Titanium alloy sheet, plate | |
| Commercially pure titanium (CP) | |
| Code designation | Yield strength |
| minimum, ksi 1 / | |
| CP-1 Gr1 | 70 |
| CP-2 Gr2 | 55 |
| CP-3 Gr3 | 40 |
| CP-4 Gr4 | 25 |
| Alpha titanium alloys(A) | |
| Code designation | Composition |
| A-1 | 5A1-2.5Sn |
| A-2 | 5A1-2.5Sn(ELI) 2 / |
| A-3 | 6A1-2Cb-1Ta-0.8Mo |
| A-4 | 8A1-1Mo-1V |
| Alpha-beta titanium alloys(AB) | |
| Code designation | Composition |
| AB-1 Gr5 | 6A1-4V |
| AB-2 Gr5 | 6A1-4V(ELI) |
| AB-3 | 6A1-6V-2Sn |
| AB-4 | 6A1-2Sn-4Zr-2Mo |
| AB-5 | 3A1-2.5V |
| AB-6 | 8Mn |
| Beta titanium alloys(B) | |
| Code designation | Composition |
| B-1 | 13V-11Cr-3A1 |
| B-2 | 11.5Mo-6Zr-4.5Sn |
| B-3 | 3A1-8V-6Cr-4Mo-4Zr |
| B-4 | 8Mo-8V-2Fe-3A1 |
| Processing: | |
| Горячая прокатка | Холодная прокатка |
| Available Grades: | |
| CP Класс 1 | Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2) |
| CP Класс 2 | Grade 6Al-4V ELI (Formerly Grade 23) |
| Grade 7 | Grade 6Al-6V-2Sn (6-62) |
| Grade 19 | Grade 8Al-1Mo-1V (8-1-1) |
| Grade 5 (6Al-4V) | Grade 9 (3Al-2.5V) |
| Grade 6 (5Al-2.5Sn) | CP 3 класс |
| Application | |
| Химическая промышленность | Desalination Of Sea Water |
| Petrochemical Industry | Аэрокосмическая промышленность |
| Machining Field, Automobile Field | Mobile Phone Component Field. |
Последние проекты и продукты для горячих случаев






Сопутствующие товары (7)
The primary difference is strength. CP Grade 3 offers significantly higher tensile and yield strength than Grade 2, making it suitable for components that must withstand greater mechanical stress. It still maintains excellent corrosion resistance and good weldability.
How to choose:
- Choose Grade 2 if your project demands excellent formability and cost-effectiveness with moderate strength.
- Choose CP Grade 3 if your parts need to endure medium to high mechanical loads without sacrificing corrosion resistance or weldability.
Yes, we provide professional custom cutting services. To minimize your material waste and machining time, we can cut the titanium plates to your exact specifications based on your drawings or dimensions. Please provide your detailed requirements when requesting a quote, and our team will offer the best solution.
Absolutely. All our CP Grade 3 titanium plates comply with international standards such as ASTM B265 / ASME SB265. With every shipment, we can provide a certified Material Test Report (MTR) detailing the chemical composition and mechanical properties, ensuring full traceability and quality assurance.
CP Grade 3 titanium has excellent weldability. We recommend using TIG (Gas Tungsten Arc Welding) or MIG (Gas Metal Arc Welding). The most critical step is to provide proper shielding with an inert gas (typically argon) to protect the weld pool from atmospheric contamination. With correct protection, the weld’s performance will be as strong as the base material.
Пожалуйста, заполните форму на странице “Контакты” или позвоните нашему менеджеру по продажам по телефону “+86 13382898899”, мы свяжемся с вами в кратчайшие сроки. Наш WhatsApp работает в режиме онлайн, а электронная почта (Daxunalloy@gmail.com) будет проверена в течение 6 часов. На каждый запрос или сообщение мы ответим незамедлительно. Кроме того, каждую неделю мы делимся с нашими клиентами информацией о рынке
We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.
Мы экспортировали продукцию в более чем 42 страны, такие как Канада, Чили, Кувейт, Германия, Южная Корея, Саудовская Аравия, Сингапур и др.
Пробные заказы могут быть доставлены в течение недели. Для обычных заказов требуется примерно две недели.