CP Grade 3 Titanium Plate Manufacturer - Daxun Alloy

As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.

  • Plate Grade:R50550 / CP TI50A
  • Plate Production type:cold rolling, hot rolling, forging.
  • Features:High strength, Lightweight, High-temperature resistance
  • Surface:bright, polished, pickled, sandblasted, etc.
  • Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request

————Daxun produces titanium sheets in China to meet the diverse and ——müşterilerin zorlu ihtiyaçları!

Providing High-quality CP Grade 3 Titanium Plates to Serve Customers Worldwide

CP Grade 3 Titanium plate is a commercially pure titanium grade known for its excellent balance of strength and ductility. It offers higher mechanical properties compared to Grades 1 and 2, making it ideal for applications requiring moderate strength and good formability. This grade features outstanding corrosion resistance, especially in marine and chemical environments, along with low density and high toughness.

Key Characteristics:
  • Composition: CP Grade 3 is primarily titanium (typically ~99.1%), with small amounts of oxygen, iron, carbon, nitrogen, and hydrogen. The oxygen content is the main factor influencing its strength.
  • Mechanical Properties: It offers higher tensile and yield strength than Grades 1 and 2, making it suitable for applications requiring more robust performance while still maintaining good ductility.
  • Corrosion Resistance: Like all CP titanium grades, Grade 3 provides outstanding resistance to corrosion, especially in oxidizing environments such as those containing chlorides or seawater.
  • Fabrication: It can be welded, formed, and machined using conventional methods, which enhances its versatility in manufacturing.
  • Biocompatibility: The material is biocompatible, allowing its use in medical implants and other healthcare applications.
Common Applications:
  • Havacılık ve uzay: For components that need a mix of strength, light weight, and corrosion resistance.
  • Chemical Processing: Equipment exposed to corrosive environments.
  • Deniz Mühendisliği: Parts subject to seawater corrosion.
  • Medical Devices: Implants and surgical tools due to its biocompatibility.

 

CP Grade 3 vs. Other Titanium Grades

CP Grade 3 Titanium plate serves as a powerful middle-ground option in the titanium family. It delivers significantly higher strength than the softer, more formable Grades 1 and 2, making it suitable for components that face greater mechanical stress. Crucially, it achieves this strength boost while retaining excellent corrosion resistance and good weldability, a key advantage over the even stronger but less ductile CP Grade 4.

When compared to the popular alloy Grade 5 (Ti-6Al-4V), CP Grade 3 is less strong and not heat-treatable. However, it is far easier to form and fabricate, and it provides superior corrosion resistance in many reducing chemical environments. This makes CP Grade 3 the ideal choice when your project requires a step up in strength from the basic CP grades but cannot sacrifice the ease of manufacturing and outstanding durability needed for demanding aerospace, marine, and chemical processing applications.

Daha fazla bilgi edinin

Veri

Element Content (%)
Titanium (Ti) Balance (~99.1%)
Oxygen (O) 0.10 – 0.27
Demir (Fe) ≤ 0.30
Carbon © ≤ 0.08
Azot (N) ≤ 0.05
Hydrogen (H) ≤ 0.015
Mülkiyet Değer
Yoğunluk ~4.51 g/cm³
Erime Noktası ~1660–1670 °C
Elastisite Modülü ~103–107 GPa
Termal İletkenlik ~21.9 W/m·K (at 25°C)
Elektriksel Dirençlilik ~420 nΩ·m
Mülkiyet Değer
Çekme Dayanımı ~450–485 MPa
Akma Dayanımı ~380–415 MPa
Uzama ~20–30%
Sertlik (Brinell) ~200–240 HB

Projenizin yükselmesine yardımcı olmak için Daxun'u seçin.

Hızlı teslimat

At Daxun Alloys Co., Ltd., we specialize in the rapid supply of premium CP Grade 3 titanium plates to meet your urgent project needs. With our extensive inventory and efficient logistics network, we ensure prompt delivery without compromising on quality. Whether you require standard sizes or custom-cut solutions, our team is committed to providing reliable, on-time service to support your manufacturing and engineering schedules.

Özel Kesim

Daxun Alloy, titanyum plakaların boyut kaybını kontrol etmenize yardımcı olmak için müşterilere çeşitli boyutlarda özelleştirilmiş kesme çözümleri sunar, böylece işleme maliyetlerinizden ve zamandan tasarruf sağlar. Kesme yöntemlerimiz şunları içerir:

  • Su jeti ile kesim
  • Lazer kesim
  • Plazma kesim
  • Tel kesme
  • Bükme
  • Dilme
  • Testere

Paketleme

We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- Kutular ve kasalar
- Shrinkwrap
- Ahşap paletler
- Ahşap kutular

Teknik Destek

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.

Daxun CP Grade 3 Titanium sheet Let your brand improve rapidly

Aşağıda listelenen ürünler dışında, mevcut diğer metal ürünler burada listelenmemiştir. DAXUN'un üretip tedarik edebileceği diğer metal ürünler arasında ağırlıklı olarak Levha, Çubuk ve Boru şeklinde olan Tantal, Niyobyum, Zirkonyum, Hafniyum, Nikel, Bakır vb. bulunmaktadır.
Ürünler/İşleme Standardı Sınıf / Boyut
Titanyum Levha, Levha, Rulo- ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7, GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3 (Kalınlık: ( 0.0197”-6”) Maksimum Genişlik: 12 fit, Maksimum Uzunluk: 50 fit)
AMS-T-9046
Titanyum ve Titanyum alaşımlı levha, plaka
Ticari olarak saf titanyum (CP)
Kod tanımı Akma dayanımı
minimum, ksi 1 /
CP-1 Gr1 70
CP-2 Gr2 55
CP-3 Gr3 40
CP-4 Gr4 25
Alfa titanyum alaşımları(A)
Kod tanımı Kompozisyon
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0,8Mo
A-4 8A1-1Mo-1V
Alfa-beta titanyum alaşımları (AB)
Kod tanımı Kompozisyon
AB-1 Gr5 6A1-4V
AB-2 Gr5 6A1-4V (ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
Beta titanyum alaşımları (B)
Kod tanımı Kompozisyon
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
İşleniyor:
Sıcak Haddeleme Soğuk Haddeleme
Mevcut Sınıflar:
CP Sınıf 1 Sınıf 6Al-2Sn-4Zr-2Mo (6-2-4-2)
CP Sınıf 2 Sınıf 6Al-4V ELI (Eski Sınıf 23)
7. Sınıf Sınıf 6Al-6V-2Sn (6-62)
19. Sınıf Sınıf 8Al-1Mo-1V (8-1-1)
5. Sınıf (6Al-4V) 9. Sınıf (3Al-2,5V)
Sınıf 6 (5Al-2,5Sn) CP Sınıf 3
Uygulama
Kimya Endüstrisi Deniz Suyunun Tuzdan Arındırılması
Petrokimya Endüstrisi Havacılık ve Uzay
Talaşlı İmalat Alanı, Otomobil Alanı Cep Telefonu Bileşen Alanı.

Güncel sıcak vaka projeleri ve ürünleri

CP Grade 3 Titanium Titanium Plate and sheet
Naval vessels
Titanyum Plaka ve Levha
Aviation and Aerospace
Titanyum Plaka ve Levha
Military armor
Titanyum Plaka ve Levha
Guidance components
Titanyum Plaka ve Levha
Yeni enerji endüstrisi
Titanyum Plaka ve Levha
Gemi Makineleri Mühendisliği
What is the main difference between CP Grade 3 and the more common Grade 2 titanium? How do I choose?

The primary difference is strength. CP Grade 3 offers significantly higher tensile and yield strength than Grade 2, making it suitable for components that must withstand greater mechanical stress. It still maintains excellent corrosion resistance and good weldability.

How to choose:

  • Choose Grade 2 if your project demands excellent formability and cost-effectiveness with moderate strength.
  • Choose CP Grade 3 if your parts need to endure medium to high mechanical loads without sacrificing corrosion resistance or weldability.
Do you offer cutting services for CP Grade 3 titanium plates? Can I get custom sizes?

Yes, we provide professional custom cutting services. To minimize your material waste and machining time, we can cut the titanium plates to your exact specifications based on your drawings or dimensions. Please provide your detailed requirements when requesting a quote, and our team will offer the best solution.

Are your CP Grade 3 titanium plates certified to international standards? Can you provide a Material Test Report (MTR)?

Absolutely. All our CP Grade 3 titanium plates comply with international standards such as ASTM B265 / ASME SB265. With every shipment, we can provide a certified Material Test Report (MTR) detailing the chemical composition and mechanical properties, ensuring full traceability and quality assurance.

How is the weldability of CP Grade 3 titanium? Does it require special procedures?

CP Grade 3 titanium has excellent weldability. We recommend using TIG (Gas Tungsten Arc Welding) or MIG (Gas Metal Arc Welding). The most critical step is to provide proper shielding with an inert gas (typically argon) to protect the weld pool from atmospheric contamination. With correct protection, the weld’s performance will be as strong as the base material.

Fiyat teklifi nasıl alınır veya piyasa bilgileri en kısa sürede nasıl anlaşılır?

Lütfen “Bize Ulaşın” sayfasındaki formu doldurun veya “+86 13382898899” adresinden satış müdürümüzü arayın, en kısa sürede sizinle iletişime geçeceğiz. WhatsApp'ımız çevrimiçidir ve e-posta (Daxunalloy@gmail.com) 6 saat içinde kontrol edilecektir. Her soruya veya mesaja derhal yanıt verilecektir. Ayrıca, her hafta müşterilerimizle pazar bilgilerini paylaşıyoruz

Biraz örnek alabilir miyim?

We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.

Şimdiye kadar hangi ülkelere ihracat yaptınız?

Kanada, Şili, Kuveyt, Almanya, Güney Kore, Suudi Arabistan, Singapur gibi 42'den fazla ülkeye ihracat yaptık.

Teslimat süreniz ne kadar?

Deneme siparişleri bir hafta içinde teslim edilebilir. Normal siparişler için bu süre yaklaşık iki haftadır.

Sorgunuzu Bugün Gönderin
Hızlı Alıntı