x
Sorgunuzu Bugün Gönderin
Hızlı Alıntı

Stainless Steel Channel: 304 /304L for Building and Structural Use

As a leading stainless steel channel steel supplier and exporter in China, Daxun supplies stainless steel channel steel to all over the world.
  • Grade: S30400(304)-S30403(304L)
  • Delivery State: Hot Rolled, Laser Fused, Press Bending
  • Finish: Pickled ,Bright, Polishing, Mirror, Hairline
  • Standards:ASTM A276, ASTM A484M, DIN 1028, EN10056, GB4227
  • Full traceability with original mill test reports available.
  • building structure, construction structure, engineering structure

A global leader in stainless steel channel fabrication services

Daxun Alloys provides customers with high quality hot rolled and laser fused stainless steel channels. We stock material and can also offer custom made to order options. We offer a wide range of size options to fit your project needs and provide timely and affordable prices. We stock the following grades of material. Options include 304/304L, 316/316L, and 2205 Duplex. Stainless steel channels come in a variety of diameters; thickness, width, height, and length can all be customized or provided as standard. When determining which channel to use, you must check the height and width of your application. If you are not sure what size you need, contact us and we will help you find it.

China SS 304 and 316 Stainless Steel Channel Manufacturer. Stainless Steel Channel is a steel product with rounded edges that may be utilized for a number of applications. Hot rolled stainless steel channels are manufactured using rolling mills or laser welding lines. These channels are very resistant to corrosion and low temperatures. All of our channels have a dull rough mill finish, making them suitable for a wide range of fabrication applications that are subjected to harsh environmental conditions. Aside from that, channels can be employed in a wide range of applications, including building, roofing, walls, automobiles, and door frames. We are one of china’s largest stainless steel channel producers. Our primary goal is to supply high-quality products at competitive costs.

Daha fazla bilgi edinin

Veri

Standart ASTM、EN、DIN、JIS,ASME, BS, GB vb,
Boyutlar C5-C30
Alaşım 201, 310, 304, 304L, 316, 316L
Tip U Channel, C Channel,
Uzunluk 1.0-12.0m
Kalınlık 3mm-25mm
Özel Seçenekler Evet
Toleranslar ± ¼”, ± 1/16”
Bitirmek Değirmen, fırça, ayna, cilalı
Composition of 304/304L/304LN/304H 304 Stainless Steel channel
Sınıf 304 304L 304LN 304H
UNS Tanımlaması S30400 S30403 S30453 S30409
Karbon (C) Maks. 0.08 0.030* 0.03 0.04 - 0.10
Manganez (Mn) Maks. 2 2 2 2
Fosfor (P) Maks. 0.045 0.045 0.045 0.045
Sülfür (S) Maks. 0.03 0.03 0.03 0.03
Silikon (Si) Maks. 1 1 1 1
Krom (Cr) 18.0-20.0 18.0-20.0 18.0-20.0 18.0-20.0
Nikel (Ni) 8.0-11.0 8.0-11.0 8.0-11.0 8.0-11.0
Molibden (Mo) — — — —
Azot (N) — — 0.10-0.15 —
Demir (Fe) Bal. Bal. Bal. Bal.
Diğer Unsurlar — — — —
Tip Akma Dayanımı 0.2% ofset (KSI) Çekme Dayanımı (KSI) % Uzama (2″ Ölçü uzunluğu)
304 Ann 30 dakika. 75 dakika. 40 dakika.
304 ¼ Sert 75 dakika. 125 dakika. 12 dakika.
304 ½ Sert 110 dakika. 150 dakika. 7 dakika.
304L Ann 25 dakika. 70 dakika. 40 dakika.
304L ¼ Sert 75 dakika. 125 dakika. 12 dakika.
304L ½ Sert 110 dakika. 150 dakika. 6 dakika.
304 & 304L
Yoğunluk (lb./ in^2) @ RT 0.29
Gerilimdeki Elastisite Modülü (psi x 10^6) 28
Özgül Isı (BTU/o F/lb.) 32 ila 212 oF 0.12
Termal İletkenlik (BTU/hr/ft^2/ft) 212oF 9.4
932oF 12.4
Ortalama Termal Genleşme Katsayısı (in. x 10^-6 per o F) 32 ila 212oF 9.2
32 ila 600oF 9.9
32 ila 1,000oF 10.2
32 ila 1,200oF 10.4
Elektriksel Dirençlilik (mikro ohm - cm) 70oF'de 72
Erime Noktası Aralığı (oF) 2550 ila 2650
Oksidasyon Direnci - Sürekli Hizmet (oF) 1,650
Oksidasyon Direnci - Aralıklı Hizmet (oF) 1,500
STANDART WERKSTOFF NR. UNS JIS BS GOST  AFNOR EN
SS 304 1.4301 S30400 SUS 304 304S31 08Х18Н10 Z7CN18-09 X5CrNi18-10

Daxun'u seçin ve müşterilerinizi memnun edin.

Building and Structural Applications

Stainless steel channels are widely used in building and structural applications due to their high strength, corrosion resistance, and durability. These channels are ideal for construction projects, such as building frames, bridges, and other infrastructure. They can be utilized as beams, columns, or supports, and can be easily fabricated and finished to meet specific requirements.

In building applications, stainless steel channels are often used in conjunction with other materials, such as steel, aluminum, or wood. This versatility allows for the creation of complex structures, such as staircases, handrails, and door frames. Additionally, stainless steel channels can be used in decorative applications, such as architectural features, trim, and molding, adding an aesthetically pleasing appearance to any project.

 

Hızlı yanıt

Acil ihtiyaçları olan müşterilerimiz için paslanmaz çelik ürünlerinin zamanında ve hızlı teslimatını sağlıyoruz. Hızın arkasında bilgi akışından lojistik ve sermaye akışına kadar sistem desteği var. Örneğin, bilgi akışı açısından, Daxun'un sipariş verileri gerçek zamanlı olarak lojistik sistemine aktarılır ve veriler sorunsuz bir şekilde bağlanır; lojistik açısından, işleme merkezi otoyollara, nehirlere ve denizlere yakındır, makul zamanlama, hızlı yanıt, depolama ve nakliye bağlantısı ve verimli yükleme ile görevin zamanında tamamlanmasını sağlar Daxun'un paslanmaz çelik malzemeleri güvenilir kalitededir ve çeşitleri, özellikleri ve teslimat ağırlıkları kesinlikle standartlara uygundur.

Daxun Avantajları

Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel uses the ERP system to achieve full traceability of each channel steel type, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

Paketleme

Daxun Alloy, malların nihai varış noktasına ulaşmak için çeşitli kanallardan geçtiği uluslararası taşımacılıkta önemli bir rol oynadığı için en iyi ambalaj kalitesini sağlar, bu nedenle ambalajlamaya özel önem veririz. Ürünlerimizi ürüne bağlı olarak birçok şekilde paketliyoruz. Ürünlerimizi aşağıdaki gibi birçok şekilde paketliyoruz:
- Kutular ve kasalar
- Shrink ambalaj
- Ahşap paletler
- Ahşap kutular

Kalite, teslimat, denetim

Flattening tests to check material ductility

  1. Pitting and resistance tests for corrosion performance
  2. Mechanical tests to verify strength properties. The top and bottom flanges of our stainless steel channels, oriented at a 90-degree angle to the vertical web, play a crucial role in enhancing the channel’s strength and performance across various applications.
  3. Hardness tests ensuring consistent material quality
  4. Material positive identification for alloy composition
  5. Expansion tests to assess material behavior

 

Customer-Centric Services

  1. We welcome third-party inspections at our factory.
  2. Free samples are available for customer testing.
  3. On-site or video factory inspections are supported.

Daxun offers flexible inspection options to ensure your confidence. Our transparent processes demonstrate our commitment to quality. We encourage customers to verify our high standards firsthand. Free samples allow you to test our products in your specific applications. Choose Daxun for reliable, high-quality stainless steel and exceptional service. Your satisfaction is our priority at every step of the process.

 

Sipariş Bilgileri

When placing your order, please include these key details:

  1. Quantity required
  2. Grade of stainless steel
  3. Type or category of product
  4. API5L reference (if applicable)
  5. Thickness specifications
  6. Width measurements
  7. Length requirements
  8. Channel 304

Service detail

Daxun ensures a prompt response to all inquiries. Contact us now for expert assistance with your order. Our team is ready to guide you through the process. We’ll help tailor your order to meet your exact project needs. Expect a swift reply to your email inquiry. Choose Daxun for efficient ordering and superior stainless steel products.

Fabrication and Finishing

Stainless steel channels can be fabricated and finished using a variety of methods, including cutting, drilling, welding, and polishing. These processes allow for customization to meet specific project requirements, ensuring high-quality finishes and increased strength and durability.

Cutting techniques, such as sawing or laser cutting, can be used to achieve precise lengths and shapes. Drilling and tapping create holes and threads for fasteners, facilitating easy assembly and installation. Welding is a common method for joining stainless steel channels, with techniques like shielded metal arc welding (SMAW), gas metal arc welding (GMAW), and gas tungsten arc welding (GTAW) providing strong and reliable connections.

 

Daxun ile şimdi iletişime geçin

Teknik Destek

Herhangi bir ek teknik yardıma ihtiyacınız olursa, yerleşik metalürji uzmanımız ve bilgili personelimiz size yardımcı olmaktan memnuniyet duyacaktır. Ayrıca Daxun, çoklu metal ve plastik envanter endüstrisinde bir ilk olan sertifikalı bir test laboratuvarına sahiptir. Bu, bize göre, kaliteye olan sarsılmaz bağlılığımızı ve tam hizmet tedarikçisi olarak felsefemizi göstermektedir.

SS 304-304L Stainless Steel channel Features

Yüksek mukavemetli
Korozyon direnci
Isı direnci
Düşük sıcaklık direnci
Çevre koruma
Kaynak performansı

Daxun Alloy Markanızın hızla gelişmesine izin verin

Channel steel cross-sectional dimensions, cross-sectional area and theoretical weight table
model size Sectional area Theoretical weight
h b d t r r 1
(mm) (cm2) (kg/m)
5 50 37 4.5 7 7 3.5 6.925 5.44
6.3 63 40 4.8 7.5 7.5 3.8 8.446 6.63
6.5 65 40 4.3 7.5 7.5 3.8 8.292 6.51
8 80 43 5 8 8 4 10.24 8.04
10 100 48 5.3 8.5 8.5 4.25 12.74 10
12 120 53 5.5 9 9 4.5 15.36 12.1
12.6 126 53 5.5 9 9 4.5 15.69 12.3
14a 140 58 6 9.5 9.5 4.8 18.51 14.5
14b 60 8 21.31 16.7
16a 160 63 6.5 10 10 5 21.95 17.2
16b 65 8.5 25.15 19.8
18a 180 68 7 10.5 10.5 5.2 25.69 20.2
18b 70 9 29.29 23
20a 200 73 7 11 11 5.5 28.83 22.6
20b 75 9 32.83 25.8
22a 220 77 7 11.5 11.5 5.8 31.83 25
22b 79 9 36.23 28.5
24a 240 78 7 12 12 6 34.21 26.9
24b 80 9 39.01 30.6
24c 82 11 43.81 34.4
25a 250 78 7 12 12 6 34.91 27.4
25b 80 9 39.91 31.3
25c 82 11 44.91 35.3
27a 270 82 7.5 12.5 12.5 6.2 39.27 30.8
27b 84 9.5 44.67 35.1
27c 86 11.5 50.07 39.3
28a 280 82 7.5 12.5 12.5 6.2 40.02 31.4
28b 84 9.5 45.62 35.8
28c 86 11.5 51.22 40.2
30a 300 85 7.5 13.5 13.5 6.8 43.89 34.5
30b 87 9.5 49.89 39.2
30c 89 11.5 55.89 43.9
32a 320 88 8 14 14 7 48.5 38.1
32b 90 10 54.9 43.1
32c 92 12 61.3 48.1
36a 360 96 9 16 16 8 60.89 47.8
36b 98 11 68.09 53.5
36c 100 13 75.29 59.1
40a 400 100 10.5 18 18 9 75.04 58.9
40b 102 12.5 83.04 65.2
40c 104 14.5 91.04 71.5

Referans ve indirme için mevcut bilgiler

Daxun is a trustworthy stainless steel channel manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel is certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel channels have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

Güncel sıcak vaka projeleri ve ürünleri

304 Stainless steel channel
Paslanmaz çelik kanal
Paslanmaz çelik kanal
304L Stainless steel channel
304L Stainless steel channel
Paslanmaz çelik kanal
Paslanmaz çelik kanal
304 Stainless steel channel
Stainless steel channel 316
Detaylı Giriş

Leading stainless steel channel Suppliers in China

Daxun has been engaged in international business for more than ten years. In 2023, the export volume exceeded 100 million US dollars, and the export volume ranked among the top Chinese stainless steel manufacturers. Daxun continuously improves its service skills. To serve the global market, it has established three export service facilities in China, cooperating with engineering companies, steel mills, and international trading companies. Daxun provides stainless steel chain services and has established long-term cooperative relations with dozens of well-known steel mills around the world. The inventory includes 50,000 tons of conventional stainless steel and 20,000 tons of duplex steel, nickel-based alloys, heat-resistant steel and other metals. Daxun’s stainless steel materials are of stable quality, and the varieties, specifications, and delivery weights strictly meet the standards.


Our range of stainless steel channels can cater to all your requirements.

Our stock range of stainless channel includes both hot rolled and laser fused stainless steel channels, ensuring we have the size and grade you want for immediate dispatch. Grades include: 316 and 304. We also stock specialist products, non-standard sizes and offer a quick turnaround finish service for commercial customers.

All of our stainless steel channels can be cut to size.

Whether you are looking for a large stock, or one of our domestic customers with smaller requirements, we are here to help. C-Channel, with its shorter legs and thinner body, is particularly suitable for corrosive environments, making it ideal for use around chemicals and salt water. Our friendly and experienced team can help you determine the size, grade and finish that will suit you best. So for more information, help and advice please email us at: daxunalloy@gmail.com

Standards

  • ASTM A276, ASTM A484M, DIN 1028, EN10056, GB4227

Özellikler

Our stainless steel offers a range of impressive characteristics:

  1. Superior Corrosion Resistance Alloy composition determines the level of protection.
  2. Excellent Heat Resistance Withstands high temperatures without compromising integrity.
  3. Versatile Workability Performs well in both cold and hot working conditions. Some channels are available with tapered legs, influencing the overall design and potential applications.
  4. Outstanding Toughness Resists fracture and maintains strength under stress.
  5. Comprehensive Performance Balances multiple properties for diverse applications.
  6. Wide Application Range Suitable for various industries and environments.

Daxun’s stainless steel products combine these features for optimal performance. Our alloys offer tailored solutions to meet specific project needs. The corrosion resistance varies based on the chosen alloy composition. This versatility makes our products ideal for challenging environments. Choose Daxun for stainless steel that excels in diverse applications. Experience the perfect blend of durability, workability, and resistance.

The hot rolled stainless steel channel meets the specifications listed below: 

  • ASTM A276
  • ASTM A484
  • ASTM A479
  • ASME SA479

produce laser-welded stainless-steel channels by manufacturing: 

  • ASTM A1069/A1069M/11

Tolerances in terms of dimensions, as well as grades according to: 

  • ASTM A276
  • ASTM A484
  • ASTM A479/A479

Talk to Your Preferred Stainless Steel Channel Supplier

  • It couldn’t be easier to buy the stainless steel channels you need, as well as all of our other products, through our website. Alternatively, you can call our sales team in China at +8613382898899 to place your order and they will be happy to process your order. If you have any questions, you can even send an email to daxunalloy@gmail.com and our team will get back to you as soon as possible.

Warranty and Returns

At Daxun Alloy, we stand behind the quality of our stainless steel channels and offer a comprehensive warranty and return policy. Our warranty covers defects in materials and workmanship for a period of [timeframe]. If a product is found to be defective, we will replace it free of charge.

We also offer a return policy for products that do not meet customer expectations. If a customer is not satisfied with a product, they can return it within [timeframe] for a full refund or exchange. This policy ensures that our customers can purchase with confidence, knowing that their satisfaction is our top priority.

Our warranty and return policy is designed to provide customers with peace of mind and confidence in their purchase. We are committed to providing high-quality products and excellent customer service. If you have any questions or concerns about our warranty and return policy, please do not hesitate to contact us.

Get in Touch with Daxun Alloy

We’re ready to assist you with your stainless steel needs. Here’s how to reach us:

  1. Fill out our “Contact Us” form on our website
  2. Call our sales manager directly: +86 13382898899
  3. Send us an email: Daxunalloy@gmail.com (checked every 6 hours)
  4. Connect with us on WhatsApp for instant messaging

Our commitment to you:

  • Prompt responses to all inquiries and messages
  • Email replies within 18 hours
  • Weekly market information updates for our customer

Daxun values clear communication and rapid service. We’re here to answer your questions and provide expert guidance. Our team ensures you stay informed with regular market insights. Experience Daxun’s dedication to customer satisfaction. Reach out today and discover how we can support your stainless steel requirements.

Biraz örnek alabilir miyim?

Numuneler ücretsiz olarak temin edilebilir, ancak navlun müşteri tarafından karşılanır ve işbirliğinden sonra iade edilir.

Şimdiye kadar hangi ülkelere ihracat yaptınız?

Daxun Alloy proudly exports to over 42 countries worldwide, showcasing our global reach and reliability. Our diverse client base spans across continents, including North America, South America, Europe, the Middle East, and Asia. Notable destinations for our high-quality stainless steel products include Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, and Singapore, among many others.

MOQ'unuz nedir?

Our MOQ is 1 ton for 304 Stainless Steel channel.

Kaliteyi nasıl kontrol ediyorsunuz?

At Daxun Alloy, we maintain rigorous quality control throughout our entire production chain. Our comprehensive process begins with careful raw material purchasing and extends through processing to final shipment arrangements. At each stage, our dedicated team of documentarians and quality control specialists meticulously inspect and verify products against precise requirements. We employ state-of-the-art testing methods to ensure consistent high quality. Our commitment to transparency means we welcome third-party inspections, providing additional assurance to our clients. This integrated approach to quality management ensures that every product leaving our facility meets the exacting standards our customers expect from Daxun Alloy. By combining internal expertise with openness to external verification, we guarantee the superior quality of our stainless steel products in every shipment.

Teslimat süreniz ne kadar?

Deneme siparişleri bir hafta içinde teslim edilebilir. Normal siparişler için bu süre yaklaşık iki haftadır.

Sonuç

Stainless steel channels are a versatile and reliable material used in a wide range of applications, including building and structural, fabrication and finishing, and treatment applications. They offer several benefits, including high strength, corrosion resistance, and durability.

At Daxun Alloy, we are committed to providing high-quality stainless steel channels and excellent customer service. Our products are designed to meet specific requirements and are fabricated and finished using state-of-the-art techniques.

We hope this information has been helpful in understanding the benefits and applications of stainless steel channels. If you have any further questions or would like to learn more about our products, please do not hesitate to contact us. Choose Daxun Alloy for your stainless steel needs and experience the perfect blend of durability, workability, and resistance.

Sorgunuzu Bugün Gönderin
Hızlı Alıntı