Grade 7 (Ti-0.15Pd) Titanium Alloy Plate Manufacturer - Daxun Alloy
As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.
- Plate Grade:7. Sınıf UNS R52400
- Plate Production type:cold rolling, hot rolling, forging.
- Standard:ASTM B 265,ASME SB265,AMS4911 etc
- Features:High strength, Lightweight, High-temperature resistance
- Surface:bright, polished, pickled, sandblasted, etc.
- Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request
————Daxun produces titanium sheets in China to meet the diverse and ——müşterilerin zorlu ihtiyaçları!
Providing High-quality Grade 7 Titanium Plate to Serve Customers Worldwide
Grade 7 titanium plate (Ti Grade 7 / UNS R52400) is a palladium-enhanced, commercially pure (CP) titanium alloy specifically engineered for supreme corrosion resistance in aggressive environments. It consists of titanium (≥99%) with a critical addition of 0.12–0.25% palladium (Pd), which fundamentally alters its electrochemical behavior. This palladium modification dramatically improves resistance to reducing acids (e.g., sulfuric, hydrochloric, phosphoric), chloride solutions (including seawater and brines), and crevice/pitting corrosion—scenarios where standard CP grades like Grade 2 would rapidly degrade. While retaining the inherent advantages of titanium—low density (~4.5 g/cm³), high strength-to-weight ratio, excellent weldability, and biocompatibility—Grade 7 exhibits superior performance at elevated temperatures (up to ~400°C/750°F) and in highly oxidizing or acidic conditions. Its passive oxide layer, stabilized by palladium, provides unparalleled protection against chemical attack, making it one of the most corrosion-resistant metallic materials available.
Where is Grade 7 titanium plate used?
Grade 7 titanium plate is extensively used in chemical processing for critical components like reactor vessels, heat exchangers, piping systems, and agitators handling acids, chlorides, or organic solvents. In marine and offshore engineering, it serves in seawater desalination plants, heat rejection systems, and subsea equipment exposed to high-salinity environments. The alloy also excels in pollution control systems (e.g., flue-gas desulfurization scrubbers), pharmaceutical manufacturing, and medical implants (e.g., orthopedic devices) due to its inertness and longevity. Despite its higher initial cost—driven by palladium content—Grade 7 delivers exceptional lifecycle value by minimizing downtime, maintenance, and replacement costs in corrosive service. Its reliability in preventing catastrophic failures ensures safety and efficiency in applications ranging from nuclear waste containment to aerospace fluid systems, justifying its selection as a premium solution for the most demanding corrosion challenges.
Veri
- Parametre
- Fiziksel Özellikler
- Mekanik Özellikler
| Element | Sembol | Composition Range (wt.%) |
|---|---|---|
| Titanyum | Ti | Balance (>99%) |
| Palladium | Pd | 0.12–0.25% |
| Demir | Fe | ≤0.30% |
| Oksijen | O | ≤0.25% |
| Karbon | C | ≤0,08% |
| Azot | N | ≤0,03% |
| Hidrojen | H | ≤0.015% |
| Diğer Unsurlar | Each | ≤0.40% (single element) |
Key Characteristics
- Strength-to-Weight Ratio: Comparable to pure titanium (Grades 1–4) but lower than Ti-6Al-4V (Grade 5) or Ti-3Al-2.5V (Grade 9). Optimized for corrosion resistance over mechanical strength.
- Corrosion Resistance: Unmatched in reducing acids (e.g., HCl, H₂SO₄), chlorides, and crevice corrosion environments. Outperforms all commercially pure grades (1–4) and Grade 5/9 in aggressive chemical media due to palladium (Pd) stabilization.
- Biocompatibility: Fully non-toxic and MRI-compatible. Suitable for surgical instruments and chemical processing equipment, though not used for permanent implants (Grade 23 preferred).
- Formability: Retains excellent cold formability, weldability, and machinability of pure titanium. Significantly easier to fabricate than Grade 5/9, enabling complex geometries without specialized tooling.
| Mülkiyet | Value (Imperial) | Value (Metric) |
|---|---|---|
| Yoğunluk | 0.163 lb/in³ | 4.51 g/cm³ |
| Erime Noktası | 3,000–3,050°F | 1,650–1,680°C |
| Termal İletkenlik | 9.5 Btu/(hr·ft·°F) | 16.4 W/(m·K) |
| Coefficient of Thermal Expansion | 4.8 × 10⁻⁶/°F | 8.6 × 10⁻⁶/K |
| Elektriksel Dirençlilik | 1.78 × 10⁻⁶ Ω·cm | 1.78 μΩ·m |
| Mülkiyet | Value (Imperial) | Value (Metric) |
|---|---|---|
| Çekme Dayanımı | 50,000–65,000 psi | 345–450 MPa |
| Akma Dayanımı | 30,000–45,000 psi | 207–310 MPa |
| Uzama | 20–30% | 20–30% |
| Sertlik (Brinell) | 120–160 HB | 120–160 HB |
| Elastisite Modülü | 14.9–16.0 × 10⁶ psi | 103–110 GPa |
Projenizin yükselmesine yardımcı olmak için Daxun'u seçin.

Common applications
Grade 7 titanium plates and sheets are primarily utilized in applications requiring exceptional corrosion resistance, particularly in aggressive chemical environments, combined with moderate strength and excellent weldability.
- Applications include chemical processing equipment such as heat exchangers, reactor vessels, and piping systems that handle chlorides, acids, and other corrosive substances.
- Industrial applications include marine components, offshore oil and gas equipment, and desalination plants where exposure to saltwater and harsh chemicals is common.
- Pharmaceutical and food processing equipment that demands high purity standards and resistance to corrosive cleaning agents.
- Laboratory equipment and analytical instruments that require superior chemical resistance for accurate testing and processing.
- Pollution control systems, including scrubbers and ductwork in power plants and industrial facilities that handle corrosive exhaust gases.
Hızlı teslimat
Daxun provides customers with timely and fast delivery of grade 7 titanium plate products. Behind the speed is the system support from professional production capacity, and information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected.


Özel Kesim
Daxun Alloy, titanyum plakaların boyut kaybını kontrol etmenize yardımcı olmak için müşterilere çeşitli boyutlarda özelleştirilmiş kesme çözümleri sunar, böylece işleme maliyetlerinizden ve zamandan tasarruf sağlar. Kesme yöntemlerimiz şunları içerir:
- Su jeti ile kesim
- Lazer kesim
- Plazma kesim
- Tel kesme
- Bükme
- Dilme
- Testere
Paketleme
We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- Kutular ve kasalar
- Shrinkwrap
- Ahşap paletler
- Ahşap kutular


Teknik Destek
If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.
Daxun Grade 7 Titanium sheet Let your brand improve rapidly
- Other Titanium Plate Grades
| Aşağıda listelenen ürünler dışında, mevcut diğer metal ürünler burada listelenmemiştir. DAXUN'un üretip tedarik edebileceği diğer metal ürünler arasında ağırlıklı olarak Levha, Çubuk ve Boru şeklinde olan Tantal, Niyobyum, Zirkonyum, Hafniyum, Nikel, Bakır vb. bulunmaktadır. | |
| Ürünler/İşleme Standardı | Sınıf / Boyut |
| Titanyum Levha, Levha, Rulo- ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136 | GR1, GR2, GR3, GR4, GR5, GR7, GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3 (Kalınlık: ( 0.0197”-6”) Maksimum Genişlik: 12 fit, Maksimum Uzunluk: 50 fit) |
| AMS-T-9046 | |
| Titanyum ve Titanyum alaşımlı levha, plaka | |
| Ticari olarak saf titanyum (CP) | |
| Kod tanımı | Akma dayanımı |
| minimum, ksi 1 / | |
| CP-1 Gr1 | 70 |
| CP-2 Gr2 | 55 |
| CP-3 Gr3 | 40 |
| CP-4 Gr4 | 25 |
| Alfa titanyum alaşımları(A) | |
| Kod tanımı | Kompozisyon |
| A-1 | 5A1-2.5Sn |
| A-2 | 5A1-2.5Sn(ELI) 2 / |
| A-3 | 6A1-2Cb-1Ta-0,8Mo |
| A-4 | 8A1-1Mo-1V |
| Alfa-beta titanyum alaşımları (AB) | |
| Kod tanımı | Kompozisyon |
| AB-1 Gr5 | 6A1-4V |
| AB-2 Gr5 | 6A1-4V (ELI) |
| AB-3 | 6A1-6V-2Sn |
| AB-4 | 6A1-2Sn-4Zr-2Mo |
| AB-5 | 3A1-2.5V |
| AB-6 | 8Mn |
| Beta titanyum alaşımları (B) | |
| Kod tanımı | Kompozisyon |
| B-1 | 13V-11Cr-3A1 |
| B-2 | 11.5Mo-6Zr-4.5Sn |
| B-3 | 3A1-8V-6Cr-4Mo-4Zr |
| B-4 | 8Mo-8V-2Fe-3A1 |
| İşleniyor: | |
| Sıcak Haddeleme | Soğuk Haddeleme |
| Mevcut Sınıflar: | |
| CP Sınıf 1 | Sınıf 6Al-2Sn-4Zr-2Mo (6-2-4-2) |
| CP Sınıf 2 | Sınıf 6Al-4V ELI (Eski Sınıf 23) |
| 7. Sınıf | Sınıf 6Al-6V-2Sn (6-62) |
| 19. Sınıf | Sınıf 8Al-1Mo-1V (8-1-1) |
| 5. Sınıf (6Al-4V) | 9. Sınıf (3Al-2,5V) |
| Sınıf 6 (5Al-2,5Sn) | CP Sınıf 3 |
| Uygulama | |
| Kimya Endüstrisi | Deniz Suyunun Tuzdan Arındırılması |
| Petrokimya Endüstrisi | Havacılık ve Uzay |
| Talaşlı İmalat Alanı, Otomobil Alanı | Cep Telefonu Bileşen Alanı. |
Güncel sıcak vaka projeleri ve ürünleri
İlgili Ürünler (7)
Grade 7 titanium plate is a commercially pure titanium alloy with the addition of 0.12-0.25% palladium, which significantly enhances its corrosion resistance. This combination maintains the excellent formability and weldability of pure titanium while providing superior resistance to reducing acids and other highly corrosive environments.
Grade 7 titanium plates offer good strength with a minimum yield strength of 275 MPa and minimum tensile strength of 485 MPa. They maintain excellent ductility with approximately 20% elongation, allowing for good formability during fabrication processes.
Yes, Grade 7 titanium plates can be welded using standard titanium welding procedures including TIG, MIG, and plasma arc welding. However, proper shielding with inert gas is essential to prevent contamination during welding. The palladium addition does not significantly affect weldability compared to other commercially pure titanium grades.
We offer Grade 7 titanium plates in various surface finishes including hot-rolled, pickled, sandblasted, and polished finishes. Custom surface treatments can also be provided based on specific application requirements.
Our Grade 7 titanium plates undergo strict quality control including chemical composition analysis, mechanical property testing, and ultrasonic inspection. We provide full material traceability and certification with each order, ensuring compliance with applicable standards such as ASTM B265 and AMS 4902.
Standard lead times for Grade 7 titanium plates typically range from 2-4 weeks depending on size, thickness, and quantity requirements. We also maintain a stock of commonly used dimensions for immediate delivery and can accommodate urgent requests when possible.
Lütfen “Bize Ulaşın” sayfasındaki formu doldurun veya “+86 13382898899” adresinden satış müdürümüzü arayın, en kısa sürede sizinle iletişime geçeceğiz. WhatsApp'ımız çevrimiçidir ve e-posta (Daxunalloy@gmail.com) 6 saat içinde kontrol edilecektir. Her soruya veya mesaja derhal yanıt verilecektir. Ayrıca, her hafta müşterilerimizle pazar bilgilerini paylaşıyoruz
We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.
Kanada, Şili, Kuveyt, Almanya, Güney Kore, Suudi Arabistan, Singapur gibi 42'den fazla ülkeye ihracat yaptık.