Grade 23 Ti 6Al-4V ELI Titanium Alloy Plate Manufacturer - Daxun Alloy
As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.
- Plate Grade:Grade 23 UNS R56401
- Plate Production type:cold rolling, hot rolling, forging.
- Standard:ASTM B 265,ASME SB265,AMS4911 etc
- Features:High strength, Lightweight, High-temperature resistance
- Surface:bright, polished, pickled, sandblasted, etc.
- Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request
————Daxun produces titanium sheets in China to meet the diverse and ——müşterilerin zorlu ihtiyaçları!
Provide High Quality Grade 23 Titanium Plates to Customers Around The World
Grade 23 titanium plate is a commercial grade of Ti-6Al-4V ELI (Extra Low Interstitial). It is an improved alloy that further reduces the content of interstitial elements such as oxygen, iron, and nitrogen (such as oxygen content ≤ 0.13%) based on the classic Ti-6Al-4V (Grade 5). It is characterized by high strength, light weight, strong corrosion resistance, and is very friendly to the human body (high biocompatibility). This material is both strong and durable and can be used in various harsh environments, such as strong acids, strong alkalis, and seawater. It is not easily damaged. Its density is much smaller than that of steel, but its strength is close to that of steel, so it is often used to manufacture products that require both lightness and high durability.
Where is Grade 23 titanium plate used?
In the medical field, it is used to make artificial joints, bone fixation plates and dental implants because it is harmless to the human body and can be used for a long time without being easily damaged. It is also used to make key parts on aircraft and spacecraft, such as landing gear and engine parts, which can reduce weight and ensure strength. Chemical plants use it to make corrosion-resistant pipes and reactors, which can also be used for a long time in strong acid and alkali environments. In shipbuilding and marine engineering, it is used to make ship parts and seawater treatment equipment, and is not afraid of seawater corrosion. In addition, this material is also used in some parts of high-end sports equipment and nuclear power plants because it is both light and durable and can adapt to various extreme environments.
Veri
- Parametre
| Element | Ti | Al | V | O | Fe | C | N | H | Other elements |
| Composition Range (wt.%) | >89% | 5.50 – 6.5% | 3.50 – 4.50% | ≤ 0.13% | ≤ 0.25% | ≤ 0.08% | ≤ 0.05% | ≤ 0.0125% | ≤ 0.4% |
Key Notes:
ELI (Extra Low Interstitial): Grade 23 has stricter limits on oxygen, nitrogen, hydrogen, and carbon compared to standard Grade 5 (Ti-6Al-4V) to enhance ductility and biocompatibility.
Primary alloying elements: Aluminum (Al) and vanadium (V) contribute to strength and phase stability.
Impurity control: Low iron, carbon, nitrogen, and hydrogen ensure superior corrosion resistance and fatigue performance.
Key performance:
High strength + high toughness: tensile strength can reach 895-930 MPa (annealed state), elongation ≥10%, better than ordinary Grade 5, suitable for scenes with dynamic loads.
Excellent corrosion resistance: acid resistance (such as hydrochloric acid, sulfuric acid), alkali resistance, seawater resistance, outstanding performance in medical implants and chemical equipment.
Biocompatibility: non-magnetic, non-toxic, excellent compatibility with human tissue, is the preferred material for orthopedic implants.
Processability: can be formed by forging, rolling, machining, welding performance is better than ordinary titanium alloy.
Projenizin yükselmesine yardımcı olmak için Daxun'u seçin.

Key Features
Grade 23 titanium alloy plate is the most commercially available of all titanium alloys. It combines high strength and toughness. Grade 23 can be cold drawn and extruded, but this process is generally limited to smaller industrial facilities and is more commonly applied to commercially pure grades.
Ti-6Al-4V ELI Grade 23 titanium alloy has good comprehensive properties:
- Yüksek mukavemetli
- Creep resistance
- Fatigue resistance
- Heat treatable
- Good ductility
- Good plasticity
- Good weldability
- Suitable for service temperatures -196°C-450°C
Common applications
Ti-6AL-4V ELI titanium plates and sheets are primarily used for components that demand superior corrosion resistance, high strength at elevated temperatures (400-450°C), as well as good ductility and lateral strength.
1. Applications include jet engine compressor blades, disks, and rings, fuselage components like wings and doors, turbine disks, bulkheads, military aircraft parts, engine nozzles, landing gear doors, and fuselage superplastic forming components.
2. Military applications include armor, guidance, shell casings, etc.
3. Spacecraft components, including rocket engines and heat shields, etc.
4. Medical and surgical instruments.
5. Sports equipment, including bicycle frames and golf clubs.


Özel Kesim
Daxun Alloy, titanyum plakaların boyut kaybını kontrol etmenize yardımcı olmak için müşterilere çeşitli boyutlarda özelleştirilmiş kesme çözümleri sunar, böylece işleme maliyetlerinizden ve zamandan tasarruf sağlar. Kesme yöntemlerimiz şunları içerir:
- Su jeti ile kesim
- Lazer kesim
- Plazma kesim
- Tel kesme
- Bükme
- Dilme
- Testere
Paketleme
We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- Kutular ve kasalar
- Shrinkwrap
- Ahşap paletler
- Ahşap kutular


Teknik Destek
If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.
Daxun Grade 23 Titanium sheet Let your brand improve rapidly
- Other Titanium Plate Grades
| Aşağıda listelenen ürünler dışında, mevcut diğer metal ürünler burada listelenmemiştir. DAXUN'un üretip tedarik edebileceği diğer metal ürünler arasında ağırlıklı olarak Levha, Çubuk ve Boru şeklinde olan Tantal, Niyobyum, Zirkonyum, Hafniyum, Nikel, Bakır vb. bulunmaktadır. | |
| Ürünler/İşleme Standardı | Sınıf / Boyut |
| Titanyum Levha, Levha, Rulo- ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136 | GR1, GR2, GR3, GR4, GR5, GR7, GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3 (Kalınlık: ( 0.0197”-6”) Maksimum Genişlik: 12 fit, Maksimum Uzunluk: 50 fit) |
| AMS-T-9046 | |
| Titanyum ve Titanyum alaşımlı levha, plaka | |
| Ticari olarak saf titanyum (CP) | |
| Kod tanımı | Akma dayanımı |
| minimum, ksi 1 / | |
| CP-1 Gr1 | 70 |
| CP-2 Gr2 | 55 |
| CP-3 Gr3 | 40 |
| CP-4 Gr4 | 25 |
| Alfa titanyum alaşımları(A) | |
| Kod tanımı | Kompozisyon |
| A-1 | 5A1-2.5Sn |
| A-2 | 5A1-2.5Sn(ELI) 2 / |
| A-3 | 6A1-2Cb-1Ta-0,8Mo |
| A-4 | 8A1-1Mo-1V |
| Alfa-beta titanyum alaşımları (AB) | |
| Kod tanımı | Kompozisyon |
| AB-1 Gr5 | 6A1-4V |
| AB-2 Gr5 | 6A1-4V (ELI) |
| AB-3 | 6A1-6V-2Sn |
| AB-4 | 6A1-2Sn-4Zr-2Mo |
| AB-5 | 3A1-2.5V |
| AB-6 | 8Mn |
| Beta titanyum alaşımları (B) | |
| Kod tanımı | Kompozisyon |
| B-1 | 13V-11Cr-3A1 |
| B-2 | 11.5Mo-6Zr-4.5Sn |
| B-3 | 3A1-8V-6Cr-4Mo-4Zr |
| B-4 | 8Mo-8V-2Fe-3A1 |
| İşleniyor: | |
| Sıcak Haddeleme | Soğuk Haddeleme |
| Mevcut Sınıflar: | |
| CP Sınıf 1 | Sınıf 6Al-2Sn-4Zr-2Mo (6-2-4-2) |
| CP Sınıf 2 | Sınıf 6Al-4V ELI (Eski Sınıf 23) |
| 7. Sınıf | Sınıf 6Al-6V-2Sn (6-62) |
| 19. Sınıf | Sınıf 8Al-1Mo-1V (8-1-1) |
| 5. Sınıf (6Al-4V) | 9. Sınıf (3Al-2,5V) |
| Sınıf 6 (5Al-2,5Sn) | CP Sınıf 3 |
| Uygulama | |
| Kimya Endüstrisi | Deniz Suyunun Tuzdan Arındırılması |
| Petrokimya Endüstrisi | Havacılık ve Uzay |
| Talaşlı İmalat Alanı, Otomobil Alanı | Cep Telefonu Bileşen Alanı. |
Güncel sıcak vaka projeleri ve ürünleri






İlgili Ürünler (6)
Grade 23 titanium (Ti-6Al-4V ELI) is an extra low interstitial version of the popular Grade 5 titanium alloy. It contains reduced levels of oxygen, nitrogen, carbon, and iron, which enhances its ductility and fracture toughness while maintaining excellent strength. This makes it particularly suitable for critical applications where reliability is paramount.
We supply Grade 23 titanium plates in thicknesses ranging from 0.5mm to 100mm, with standard widths of 1000mm, 1500mm, and 2000mm. Custom dimensions can be accommodated based on your specific project requirements. All our plates come with full material certification and traceability documentation.
Yes, all our Grade 23 titanium plates come with full material certification including chemical composition analysis, mechanical properties testing, and traceability to the original mill.
Our Grade 23 titanium plates undergo rigorous quality control including incoming material inspection, in-process monitoring, and final testing. We verify chemical composition, mechanical properties, surface quality, and dimensional accuracy. Additionally, we maintain comprehensive quality records and can accommodate third-party inspection if required by our customers.
Lütfen “Bize Ulaşın” sayfasındaki formu doldurun veya “+86 13382898899” adresinden satış müdürümüzü arayın, en kısa sürede sizinle iletişime geçeceğiz. WhatsApp'ımız çevrimiçidir ve e-posta (Daxunalloy@gmail.com) 6 saat içinde kontrol edilecektir. Her soruya veya mesaja derhal yanıt verilecektir. Ayrıca, her hafta müşterilerimizle pazar bilgilerini paylaşıyoruz
We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.
Kanada, Şili, Kuveyt, Almanya, Güney Kore, Suudi Arabistan, Singapur gibi 42'den fazla ülkeye ihracat yaptık.
Deneme siparişleri bir hafta içinde teslim edilebilir. Normal siparişler için bu süre yaklaşık iki haftadır.