Grade 23 Ti 6Al-4V ELI Titanium Alloy Plate Manufacturer - Daxun Alloy

As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.

  • Plate Grade:Grade 23 UNS R56401
  • Plate Production type:cold rolling, hot rolling, forging.
  • Standard:ASTM B 265,ASME SB265,AMS4911 etc
  • Features:High strength, Lightweight, High-temperature resistance
  • Surface:bright, polished, pickled, sandblasted, etc.
  • Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request

————Daxun produces titanium sheets in China to meet the diverse and ——고객의 까다로운 요구 사항!

Provide High Quality Grade 23 Titanium Plates to Customers Around The World

Grade 23 titanium plate is a commercial grade of Ti-6Al-4V ELI (Extra Low Interstitial). It is an improved alloy that further reduces the content of interstitial elements such as oxygen, iron, and nitrogen (such as oxygen content ≤ 0.13%) based on the classic Ti-6Al-4V (Grade 5). It is characterized by high strength, light weight, strong corrosion resistance, and is very friendly to the human body (high biocompatibility). This material is both strong and durable and can be used in various harsh environments, such as strong acids, strong alkalis, and seawater. It is not easily damaged. Its density is much smaller than that of steel, but its strength is close to that of steel, so it is often used to manufacture products that require both lightness and high durability.

Where is Grade 23 titanium plate used?
In the medical field, it is used to make artificial joints, bone fixation plates and dental implants because it is harmless to the human body and can be used for a long time without being easily damaged. It is also used to make key parts on aircraft and spacecraft, such as landing gear and engine parts, which can reduce weight and ensure strength. Chemical plants use it to make corrosion-resistant pipes and reactors, which can also be used for a long time in strong acid and alkali environments. In shipbuilding and marine engineering, it is used to make ship parts and seawater treatment equipment, and is not afraid of seawater corrosion. In addition, this material is also used in some parts of high-end sports equipment and nuclear power plants because it is both light and durable and can adapt to various extreme environments.

데이터

요소 Ti Al V O Fe C N H Other elements
구성 범위(% 무게) >89% 5.50 – 6.5% 3.50 – 4.50% ≤ 0.13% ≤ 0.25% ≤ 0.08% ≤ 0.05% ≤ 0.0125% ≤ 0.4%

Key Notes:

ELI (Extra Low Interstitial): Grade 23 has stricter limits on oxygen, nitrogen, hydrogen, and carbon compared to standard Grade 5 (Ti-6Al-4V) to enhance ductility and biocompatibility.

Primary alloying elements: Aluminum (Al) and vanadium (V) contribute to strength and phase stability.

Impurity control: Low iron, carbon, nitrogen, and hydrogen ensure superior corrosion resistance and fatigue performance.

 

Key performance:

High strength + high toughness: tensile strength can reach 895-930 MPa (annealed state), elongation ≥10%, better than ordinary Grade 5, suitable for scenes with dynamic loads.

Excellent corrosion resistance: acid resistance (such as hydrochloric acid, sulfuric acid), alkali resistance, seawater resistance, outstanding performance in medical implants and chemical equipment.

Biocompatibility: non-magnetic, non-toxic, excellent compatibility with human tissue, is the preferred material for orthopedic implants.

Processability: can be formed by forging, rolling, machining, welding performance is better than ordinary titanium alloy.

프로젝트의 성공을 위해 Daxun을 선택하세요.

주요 기능

Grade 23 titanium alloy plate is the most commercially available of all titanium alloys. It combines high strength and toughness. Grade 23 can be cold drawn and extruded, but this process is generally limited to smaller industrial facilities and is more commonly applied to commercially pure grades.

Ti-6Al-4V ELI Grade 23 titanium alloy has good comprehensive properties:

  • 높은 강도
  • Creep resistance
  • Fatigue resistance
  • 열처리 가능
  • Good ductility
  • Good plasticity
  • 우수한 용접성
  • Suitable for service temperatures -196°C-450°C

Common applications

Ti-6AL-4V ELI titanium plates and sheets are primarily used for components that demand superior corrosion resistance, high strength at elevated temperatures (400-450°C), as well as good ductility and lateral strength.

1. Applications include jet engine compressor blades, disks, and rings, fuselage components like wings and doors, turbine disks, bulkheads, military aircraft parts, engine nozzles, landing gear doors, and fuselage superplastic forming components.

2. Military applications include armor, guidance, shell casings, etc.

3. Spacecraft components, including rocket engines and heat shields, etc.

4. Medical and surgical instruments.

5. Sports equipment, including bicycle frames and golf clubs.

맞춤 커팅

Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:

  • 워터젯 절단
  • 레이저 커팅
  • Plasma cutting
  • Wire cutting
  • Bending
  • Slitting
  • 톱질

패키징

We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- 상자 및 상자
• Shrinkwrap
- 목재 팔레트
- 나무 상자

기술 지원

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.

Daxun Grade 23 Titanium sheet Let your brand improve rapidly

아래 나열된 제품 외에 사용 가능한 다른 금속 제품은 여기에 나열되어 있지 않습니다. DAXUN이 제조 및 공급할 수 있는 기타 금속 제품으로는 탄탈륨, 니오븀, 지르코늄, 하프늄, 니켈, 구리 등이 있으며 주로 판재, 바, 튜브 형태입니다.
제품/처리 표준 등급/크기
티타늄 플레이트, 시트, 코일- ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(두께:( 0.0197”-6”)최대 폭: 12피트, 최대 길이: 50피트)
AMS-T-9046
티타늄 및 티타늄 합금 시트, 플레이트
상업적으로 순수한 티타늄(CP)
코드 지정 수율 강도
최소, KSI 1 /
CP-1 Gr1 70
CP-2 Gr2 55
CP-3 Gr3 40
CP-4 Gr4 25
알파 티타늄 합금(A)
코드 지정 구성
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0.8Mo
A-4 8A1-1Mo-1V
알파-베타 티타늄 합금(AB)
코드 지정 구성
AB-1 Gr5 6A1-4V
AB-2 Gr5 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
베타 티타늄 합금(B)
코드 지정 구성
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
처리 중입니다:
열간 압연 냉간 압연
사용 가능한 성적:
CP 1등급 6Al-2Sn-4Zr-2Mo(6-2-4-2) 등급
CP 2등급 6Al-4V ELI 등급(이전 23등급)
7학년 6Al-6V-2Sn(6-62) 등급
19학년 8알-1모-1V 등급(8-1-1)
5등급(6Al-4V) 9등급(3Al-2.5V)
6등급(5Al-2.5Sn) CP 3등급
애플리케이션
화학 산업 해수 담수화
석유화학 산업 항공우주
기계 가공 분야, 자동차 분야 휴대폰 구성 요소 필드.

최근 인기 있는 사례 프로젝트 및 제품

Grade 23 Titanium Plate and sheet
Naval vessels
Grade 23 Titanium Plate and sheet
Aviation and Aerospace
티타늄 플레이트 및 시트
Military armor
티타늄 플레이트 및 시트
Guidance components
티타늄 플레이트 및 시트
새로운 에너지 산업
티타늄 플레이트 및 시트
해양 엔지니어링
What is Grade 23 titanium and how does it differ from other titanium alloys?

Grade 23 titanium (Ti-6Al-4V ELI) is an extra low interstitial version of the popular Grade 5 titanium alloy. It contains reduced levels of oxygen, nitrogen, carbon, and iron, which enhances its ductility and fracture toughness while maintaining excellent strength. This makes it particularly suitable for critical applications where reliability is paramount.

What thicknesses and dimensions of Grade 23 titanium plates do you supply?

We supply Grade 23 titanium plates in thicknesses ranging from 0.5mm to 100mm, with standard widths of 1000mm, 1500mm, and 2000mm. Custom dimensions can be accommodated based on your specific project requirements. All our plates come with full material certification and traceability documentation.

Do you provide material certification and traceability for your Grade 23 titanium plates?

Yes, all our Grade 23 titanium plates come with full material certification including chemical composition analysis, mechanical properties testing, and traceability to the original mill.

What quality control measures do you implement for your Grade 23 titanium products?

Our Grade 23 titanium plates undergo rigorous quality control including incoming material inspection, in-process monitoring, and final testing. We verify chemical composition, mechanical properties, surface quality, and dimensional accuracy. Additionally, we maintain comprehensive quality records and can accommodate third-party inspection if required by our customers.

견적을 받거나 시장 정보를 최대한 빨리 파악하려면 어떻게 해야 하나요?

“문의하기” 페이지의 양식을 작성하거나 영업 관리자(+86 13382898899)에게 전화하시면 최대한 빨리 연락드리겠습니다. WhatsApp은 온라인 상태이며 이메일([email protected])은 6시간 이내에 확인합니다. 모든 문의나 메시지는 신속하게 답변해 드립니다. 또한 매주 고객과 시장 정보를 공유합니다.

샘플을 받을 수 있나요?

We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.

이미 수출한 국가는 어디인가요?

캐나다, 칠레, 쿠웨이트, 독일, 한국, 사우디아라비아, 싱가포르 등 42개 이상의 국가에 수출하고 있습니다.