Daxun Alloy - Hastelloy G35 pipe made in China

As a leading supplier of Hastelloy G35 pipes in China, Daxun provides high-performance alloy tubes to the world.
  • Hastelloy G35 types: Seamless tube,  welded tube, forged tube
  • Certification : ASTM,SGS,ISO,CE
  • Delivery Time : 7-15 days
  • Surface finish: Annealed, polished etc.
  • MOQ : ≥300kg

————Daxun produces hastelloy pipe in China to meet the diverse and ——고객의 까다로운 요구 사항!

Characteristics & Properties of Hastelloy G35

Hastelloy G-35 is a high-performance nickel-based alloy designed for extreme corrosive environments and high-temperature conditions. It is particularly suitable for harsh industrial fields such as chemical, petroleum refining and aerospace. The alloy has been optimized in chemical composition, containing a high proportion of nickel (about 46%), chromium (about 22%), molybdenum (about 8%) and tungsten (about 6%), and a small amount of cobalt and iron are added as auxiliary elements, which makes it have excellent corrosion resistance.

The most prominent feature of G-35 alloy is its ability to resist a variety of highly corrosive media, including sulfuric acid, phosphoric acid, hydrochloric acid and high-temperature chloride environments. Its high chromium and molybdenum content gives it excellent resistance to pitting and crevice corrosion, while the addition of tungsten further enhances its stability in oxidizing acids. In addition, the alloy can still maintain good mechanical strength and oxidation resistance at high temperatures and can be used for a long time at temperatures up to 1093°C (2000°F).

Due to these characteristics, Hastelloy G-35 is widely used in chemical equipment (such as reactors, heat exchangers), petroleum refining equipment (such as flue gas desulfurization systems), and aerospace components (such as gas turbine engine parts). Its excellent processing properties (such as weldability and forgeability) also make it more advantageous in manufacturing complex structures.

Hastelloy G35 Parameters

Ni Cr Co W Mo Fe
Remainder 28% – 33% ≤1.0% ≤4.0% 4.0% – 8.0% 1.3% – 2.0%
Cu C Si Mn P S
1.0% – 2.4% ≤0.05% ≤0.6% ≤1.5% ≤0.035% ≤0.02%
속성 밀도 녹는점 열 전도성 비열 용량 열팽창 계수 탄성 계수
가치 8.22 – 8.72 g/cm³ 1325 – 1361°C 10 – 23 W/(m·K) 400 – 600 J/(kg·K) 13.9×10⁻⁶/°C (20 – 100°C) 177 GPa

 

속성 인장 강도 수율 강도 Elongation (A5%) 경도
가치 σb ≥ 524 N/mm² σ0.2 ≥ 200 N/mm² δ ≥ 62% HB ≤ 350

 

프로젝트의 성공을 위해 Daxun을 선택하세요.

지금 Daxun에 문의

Advanced Production:Hastelloy alloy pipe

Hastelloy G35 alloy is an all-around nickel-chromium-molybdenum-tungsten alloy with good resistance to pitting, crevice corrosion and stress corrosion cracking. It has excellent resistance to oxidative aqueous media, including wet chlorine, nitric acid or mixed acids of oxidizing acids containing chloride ions. At the same time, Hastelloy G35 alloy also has ideal resistance to reducing and oxidizing environments encountered in the process. Relying on this versatile performance, it can be used in some troublesome environments or in factories for a variety of production purposes.

지금 Daxun에 문의

Hastelloy G35 Pipe Features

Hastelloy G35 alloy has an exceptional resistance to various chemical environments, including strong oxidizing substances, such as ferric chloride, cupric chloride, chlorine, thermally contaminated solutions (organic and inorganic), formic acid, acetic acid, acetic anhydride, seawater and salt solutions, etc. Hastelloy G35 alloy has the ability to resist the formation of grain boundary precipitation in the heat affected zone of welding, so that it can also be used in many chemical processes in the welding state.

지금 Daxun에 문의

품질, 배송, 검사

Daxun conducts a series of quality assurance tests on Hastelloy G35 pipes. These tests include flattening test, flaring test, ultrasonic flaw detection, crevice corrosion resistance test, mechanical property test, hardness test, material positive identification, and expansion test, etc. All these tests are designed to ensure that the Hastelloy G35 pipes meet the requirements of the intended applications. During the production process, we meticulously measure the outer diameter, wall thickness, and surface quality of the products. Our standard delivery time is 5 – 7 days, and for special sizes, it is 15 – 20 days.

  • 배송 시간은 엄격하게 계약에 따릅니다.
  • 고객 타사 대행사가 공장에 가서 검사할 수 있도록 지원
  • 고객 테스트를 위한 무료 샘플 지원
  • 현장 또는 비디오 공장 검사 지원
지금 Daxun에 문의

패키징

상품이 다양한 경로를 거쳐 최종 목적지에 도착하는 국제화물에서 포장은 중요한 역할을 하기 때문에 대순합금은 포장에 각별한 주의를 기울이고 있으며 최고의 품질을 보장합니다. 제품에 따라 다양한 방법으로 상품을 포장합니다. 다음과 같은 다양한 방법으로 제품을 포장합니다:
- 상자 및 상자
- 수축 포장
- 목재 팔레트
- 나무 상자

지금 Daxun에 문의

기술 지원

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. [지금 문의]Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Daxun is a trustworthy stainless steel tube manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel tubes have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

견적을 받거나 시장 정보를 최대한 빨리 파악하려면 어떻게 해야 하나요?

“문의하기” 페이지의 양식을 작성하거나 영업 관리자(+86 13382898899)에게 전화하시면 최대한 빨리 연락드리겠습니다. WhatsApp은 온라인 상태이며 이메일(Daxunalloy@gmail.com)은 6시간 이내에 확인합니다. 모든 문의나 메시지는 신속하게 답변해 드립니다. 또한 매주 고객과 시장 정보를 공유합니다.

샘플을 받을 수 있나요?

품질을 확인할 수 있도록 스테인리스 강판 샘플을 제공할 수 있습니다. 샘플은 무료이며 운임만 지불하면 됩니다.

이미 수출한 국가는 어디인가요?

캐나다, 칠레, 쿠웨이트, 독일, 한국, 사우디아라비아, 싱가포르 등 42개 이상의 국가에 수출하고 있습니다.

MOQ는 얼마인가요?

The minimum order quantity for our Hastelloy products is 300kg

배송 시간은 얼마나 걸리나요?

체험판 주문은 일주일 이내에 배송됩니다. 일반 주문의 경우 대략 2주 정도 소요됩니다.

오늘 문의 보내기
빠른 견적