Overview of 309S Stainless Steel

  • PGrade: AISI 309/309S
  • 제조: 냉연 판재, 열연 판재, 단조 판재
  • 표준 ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • 유형: 냉간 압연 박판, 열간 압연 후판
  • 표면: 2B, NO.1, NO.4, HL, BA, 8K 등.
  • 길이: 2438mm3048mm6000mm 사용자 정의 가능
  • 원산지: TISCO, 바오스틸, 포항, 칭산, 델롱

Overview of 309S Stainless Steel

309S stainless steel is a low-carbon version of the 309 alloy, specifically designed to enhance ease of fabrication and weldability. As an austenitic heat-resistant alloy, it offers exceptional oxidation resistance and high temperature corrosion resistance, making it a reliable choice for demanding environments. The low carbon content of 309S minimizes carbide precipitation, ensuring stability and performance at elevated temperatures. This combination of properties makes 309S stainless steel an ideal material for applications requiring both durability and high temperature stability.

Properties and Characteristics

309S stainless steel stands out due to its unique blend of properties, making it highly suitable for high-temperature applications. With a high chromium content of 23%, it provides excellent oxidation resistance and high temperature corrosion resistance. The alloy also contains a moderate amount of nickel, contributing to its overall heat resistance and stability. However, it is important to note that 309S has only moderate resistance to carbon absorption, which may limit its use in highly carburizing atmospheres. Despite this, its robust performance in other high-temperature conditions makes it a valuable material in various industrial applications.

Heat Resistance and Applications

기술 데이터

ASTM A240 309/309s Stainless Steel Plates Specification ASTM A240 / ASME SA240
ASTM A240 309/309s Stainless Steel Plates Manufacturing Plate Process 열간 압연(HR)/냉간 압연(CR)
ASTM A240 309/309s Stainless Steel Plates Grades 202 / 304 / 304L / 304H / 309S / 310S / 316 / 316L / 316Ti / 317L / 321 / 321H / 347 / 347H / 904L 등입니다.
UNS 번호 - UNS S30400, UNS S30403, UNS S31008, UNS S31620, UNS S31603, UNS S31603, UNS S31635, UNS S31703, UNS S32100, UNS S34700, UNS S34709, UNS S8904
EN No. – 1.4301, 1.4307, 1.4845, 1.4401, 1.4404, 1.4571, 1.4438, 1.4541, 1.4550, 1.4551, 1.4539
ASTM A240 309/309s Stainless Steel Plates Thickness 0.6 MM TO 80 MM THICKNESS
ASTM A240 309/309s Stainless Steel Plates Width 1250mm / 1500mm / 2000mm / 04피트 / 05피트 및 요구 사항에 따른 맞춤형 절단 폭
ASTM A240 309/309s Stainless Steel Plates Length 2400mm / 2420mm / 6000mm / 08피트 / 10피트 / 요구 사항에 따른 코일 컷 및 맞춤형 컷 길이
ASTM A240 309/309s Stainless Steel Plates Surface Finish 2B, 2D, BA, 매트, 매트 PVC, 4호, 5호, SB, HR, 8호, 거울, 헤어라인, 브러시, 질감, 오일 베이스 습식 광택, 양면 광택 가능.
ASTM A240 309/309s Stainless Steel Plates Coating PVC 코팅 일반 / 레이저, 필름: 100 마이크로미터, 색상: 블랙/화이트.
ASTM A240 309/309s Stainless Steel Plates Other Testing NACE MR0175, 초음파 테스트, IGC 테스트, ASTM A262 실습 E에 따른 입계 부식 테스트, 샤르피 충격 테스트, 매크로, 입자 크기, 경도 등.
ASTM A240 309/309s Stainless Steel Plates Value Added Services 가스 절단 / CNC 플라즈마 절단 / 프로파일링 / 압연 / 절곡 / 판금 제작 / 드릴 / 펀치 / 기계 가공 / 샌드 블라스팅 / 샷 블라스팅 / 열처리
ASTM A240 309/309s Stainless Steel Plates Packaging 루즈 / 캐럿 / 나무 팔레트 / 나무 상자-a / 플라스틱 천 랩
ASTM A240 309/309s Stainless Steel Plates Shipment & Transportation 육로 - 트럭/기차 부분적재, 만재화물, 해상 - 브레이크벌크 일반 선박 / FCL(만재화물) / LCL(소량화물) / 20피트 컨테이너 / 40피트 컨테이너 / 45피트 컨테이너 / 하이 큐브 컨테이너 / 오픈탑 컨테이너, 항공 - 화물기 민간 여객 및 화물 비행기
ASTM A240 309/309s Stainless Steel Platesheet Material Test Certificate Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From聽NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS, Bureau of Indian Standards BIS Approved ETC
요소 % Present (in product form)
C, H, P, L TW2)
탄소(C) 0.2 0.2
실리콘(Si) 1.50 – 2.00 1.50 – 2.50
망간(Mn) 2 2
Phosphorous (P) 0.045 0.045
Sulfur (S) 0.015 0.03
크롬(Cr) 19.00 – 21.00 19.00 – 21.00
니켈(Ni) 11.00 – 13.00 11.00 – 13.00
질소(N) 0.11 -
철(Fe) 잔액 잔액
Product Form
C, H, P L TW*
Thickness a or diamter d (mm) a ≤ 12 d ≤ 25 a=25
Hardness HB max. 1) 2) 3) 216 -
Proof Strength3) Rp0.2 N/mm2 190 230
Rp1.0 N/mm2 230 270
인장 강도 Rm N/mm2 500 – 720 min. 550
Elongation min. in % Long Products 401) -
Flat Products 0.5 ≤ a/d ˂ 3 404)5) 304)5)6)
3 ≤ a/d 404)5) 304)5)6)
밀도(파운드/인치^2) @ RT 0.29
장력 탄성 계수(psi x 10^6) 29
비열(BTU/o F/lb.) 32~212oF 0.12
열 전도성(BTU/hr/ft^2/ft) 212oF 9
932oF 10.8
평균 열팽창 계수(인치 x 10^-6 o F당) 32~212oF 8.3
32 to 600oF 9.3
32 to 1,000oF 9.6
32~1,200oF 10
전기 저항률(마이크로옴 - cm) 70oF에서 39.8
Melting Point Range (oF) 2550 – 2650
Oxidation Resistance – Continuous Service(oF) 2000
Oxidation Resistance – Intermittent Service(oF) 1800
UNS S30900  UNS S30908  UNS S30909
ASTM A240 ASTM A240  ASTM A240
ASTM A480 ASTM A480 ASTM A480
ASME SA240  ASME SA240  ASME SA240
AMS 5523  AMS 5523 AMS 5523

Daxun을 선택하고 고객을 만족시키세요.

Properties and Characteristics

309S stainless steel stands out due to its unique blend of properties, making it highly suitable for high-temperature applications. With a high chromium content of 23%, it provides excellent oxidation resistance and high temperature corrosion resistance. The alloy also contains a moderate amount of nickel, contributing to its overall heat resistance and stability. However, it is important to note that 309S has only moderate resistance to carbon absorption, which may limit its use in highly carburizing atmospheres. Despite this, its robust performance in other high-temperature conditions makes it a valuable material in various industrial applications.

Heat Resistance and Applications

Designed for high-temperature environments, 309S stainless steel excels in applications such as furnace components, oven linings, fire box sheets, and catalytic recovery systems. It can withstand peak temperatures up to 1900°F (1038°C) under constant conditions and up to 1850°F (1010°C) during frequent thermal cycling. Additionally, 309S stainless steel is resistant to high temperature sulfur-bearing atmospheres, making it suitable for use in neutral salt pots and other corrosive settings. Its versatility and durability under extreme conditions make it a preferred choice for many industrial applications.

Chemical Composition and Standards

  • The chemical composition of 309S stainless steel includes:

    • Carbon: 0.08% max
    • Chromium: 23.0%
    • Nickel: 14.0%
    • Manganese: 2.0%
    • Silicon: 1.0%
    • Phosphorus: 0.045% max
    • Sulfur: 0.03% max

품질, 배송, 검사

  • Daxun strictly controls product quality. Before placing an order, we will send you the product warranty, or if you need samples for testing, we can also send samples for free.
  • 생산 과정에서 제품의 직경, 두께, 표면을 측정합니다. 표준 배송 기간은 7~15일이며, 일부 특수 사이즈 제품을 제외하고는 배송 기간이 20일로 늘어납니다.
    배송 시간은 엄격하게 계약에 따릅니다.
  • 고객 타사 대행사가 공장에 가서 검사할 수 있도록 지원
  • 고객에게 테스트용 무료 샘플 지원
  • 현장 또는 비디오 공장 검사 지원

This alloy meets several industry standards, including ASTM A240, A276, A312, and A479, as well as ASME SA240, SA276, SA312, and SA479. These standards ensure that 309S stainless steel maintains consistent quality and performance across various applications.

Fabrication and Welding

309S stainless steel is known for its excellent weldability and ease of fabrication using standard shop practices. It can be welded using AWS E309-16 covered electrodes or ER309 bare wire, ensuring strong and reliable joints. The alloy also boasts a machinability rating of 43% relative to AISI B1112 steel, making it relatively easy to machine. Room temperature forming is recommended, and the alloy can be polished to achieve a high finish. These fabrication and welding properties make 309S stainless steel a versatile and practical choice for a wide range of industrial applications.

309/309S plate stainless steel Features

높은 강도
내식성
내열성
저온 저항
환경 보호
용접 성능

Daxun 브랜드가 빠르게 향상되도록 하세요

등급 유형 두께 Surface
오스테나이트 304/304H/304L/304J1 0.25-150mm 2B/BA/NO.4/8K/SB/HL/NO.1
321 0.4-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
316/316L/317L/316Ti 0.3-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
페라이트 430 0.4-3.0mm 2B/BA/NO.4/8K/SB/HL
울트라 퓨어 페라이트 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B、2D
409L 0.4-2.5mm 2B、2D
등급 유형 두께 원본
내열성 강철 309S 0.5-40mm CHN
310S 0.5-40mm CHN
듀플렉스 스틸 2101 1.5-50mm CHN
2304 3.0-50mm CHN
2205 0.5-60mm CHN
2507 1.0-60mm 스웨덴/일본/중국
슈퍼 오스테나이트강 N08904 0.6-50mm 스웨덴/일본/중국
S31254 0.5-50mm 스웨덴/일본/중국
N08926 0.5-50mm 스웨덴/일본/중국
N08367 0.5-50mm 스웨덴/일본/중국
니켈 베이스 합금 N08031 1.0-50mm 미국/일본/독일
N08810/N08800 0.8-50mm 미국/일본/중국
N08028 1.0-20mm US / 독일 / 일본
N08020 1.0-20mm US / 독일 / 일본
N08825 0.8-40mm 미국 / 독일 / 스웨덴 / 일본 / 중국
N10276 0.5-50mm US / 독일 / 일본
N06022 1.0-50mm US / 독일 / 일본
N06625 0.8-20mm US / GER / CHN
N04400 1.0-20mm US / 독일 / 일본
N06600 1.0-50mm US / 독일 / 일본 / 중국
N02201 0.5-20mm 미국/일본
티타늄 TA1/Gr1 0.5-50mm 일본/중국
TA2/Gr2 0.5-50mm 일본/중국
용접 재료 ERNiCrMo-13 1.2, 2.4mm GER
ERNiCrMo-3 2.4mm GER
ERNiCrMo-4 2.4mm US

The surface and shape of 309S stainless steel plate (7)

Daxun은 신뢰할 수 있는 스테인리스 강판 제조업체입니다.

전문 제조업체로서 Daxun은 우리가 생산하는 모든 제품의 고품질을 보장합니다. 따라서 모든 스테인리스 강판은 ISO9001, SGS, CE, OQC 및 기타 국제 품질 표준 인증을 받았으며 스테인리스 강판의 결함이 적도록 엄격한 품질 관리를 실시하고 있습니다. Daxun에서는 모든 제품이 내구성, 고품질 및 고성능이므로 안심하십시오.

최근 인기 있는 사례 프로젝트 및 제품

309/309s plate stainless steel
astm a240 309/309s stainless steel plate
309/309s flat stainless steel plate
310/310S stainless steel sheet suppliers
309/309s 2b stainless steel sheet
309/309s stainless steel sheet
Daxun stainless steel plates are in high demand, have good quality, oxidation resistance, and are honest and trustworthy.

Daxun International has been in international business for over ten years. In 2022, its export revenue surpassed $100 million, and its export volume was among the top Chinese stainless steel processing enterprises. To serve abroad markets, we have built three export service facilities in China and collaborated with engineering organisations, steel mills, and international trade companies. We continue to enhance our service capabilities, establishing three export service bases in China, and collaborating with engineering firms, steel mills, and international trading firms to grow into new markets.

Daxun has long-standing relationships with dozens of well-known steel mills throughout the world, supplying 30,000 tonnes of standard stainless steel plates and 20,000 tonnes of metals such as duplex steel, nickel-based alloys, and heat-resistant steel. Daxun supplies heat resistant alloys for various high-temperature applications. Daxun’s stainless steel materials are of consistent quality and never counterfeited. The kinds, specifications, and delivery weights strictly adhere to the standards.

Daxun has several stainless steel plate processing equipment, a professional physical and chemical testing centre, and “cutting, grinding, forming, beveling, welding, heat treatment, machining, and spraying” production lines. Daxun’s stainless steel plates are used in components like lead pans for thermal processing equipment. Services are provided in approximately 30 industries, including vehicles, home appliances, lifts, new energy, vacuum semiconductors, food and beverage/biofermentation, petrochemicals, and energy equipment. Collaborate with steel mills, research institutes, and other organisations to offer comprehensive services ranging from project design and material development to processing and manufacturing process optimisation.

Stainless steel materials “more, faster, better, and cheaper” customised services

First, it refers to Daxun’s stainless steel plate kinds and specifications, as well as its spot inventories. Daxun has strategic resource assistance from many large steel mills at home and abroad, ensuring the stability of the stainless steel plate supply chain and meeting clients’ individualised needs on specific materials. Additionally, Daxun’s stainless steel plates can withstand maximum temperature nitriding conditions.

Secondly, Daxun’s processing technology is diverse. processes, including stainless steel plate cutting, grinding, cutting, forming, welding, and machining, to provide customers with “one-stop” service.

Daxun services a large number of consumers in a variety of sectors.

Daxun’s stainless steel company focuses on the key sectors of equipment manufacture. Far, it has served over 30,000 customers, including over 10,000 active customers from more than 30 industries and a big number of major businesses. This demonstrates Daxun’s extensive service experience, as well as its widespread consumer recognition across industries. Daxun also provides materials with enhanced creep resistance for high-temperature applications.

Customers with urgent needs can rest assured that we will supply stainless steel plate products for elevated temperatures on time and quickly.

Behind the speed is the support of the system, including information flow, logistics, and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, seamlessly connected; in terms of logistics, the processing center is close to ports, rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading to ensure that the task is completed on time.

We provide excellent quality and high-quality services.
  • Quality is belief, and integrity is a business card. Daxun pioneered the concept of “excellent performance management” and promoted the “PDCA+Lean” management model, making “Daxun = assured quality” the company’s business card. In terms of materials, Daxun Stainless Steel has achieved full traceability of each steel plate from the ERP system, including varieties, specifications, and origins, and advocated and encouraged industry anti-counterfeiting.
  • Daxun Stainless Steel relies on technology for processing, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, closely monitors during sales, and provides worry-free service guarantees after sales.
We save our customers time, materials and energy, and ultimately save them money.

Daxun’s professional advantages enable us to provide the most cost-effective material recommendations based on customer needs, and minimize costs for customers through methods such as continuous processing and nesting processing.

Daxun Alloys: Premium ASTM A240 309/309s Stainless Steel Plates

We offer a wide range of ASTM A240 309/309s Stainless Steel Plates in stock. Our inventory includes thicknesses from 6mm to 80mm and widths of 1250mm, 1500mm, and 2000mm. We accommodate both large and small orders with no minimum quantity requirement. Our cut-to-size service ensures you get exactly what you need. Daxun’s stainless steel plates perform well under peak temperature oxidizing conditions.

Current Offers: Enjoy a 2% discount on orders over $25,000. We provide free insurance and competitive shipping rates, ensuring the best value without compromising quality.

Customization and Packaging: Our plates are available in various thicknesses, widths, and lengths to suit your specifications. We take utmost care in packaging, using plastic sheets and sturdy wooden containers. Our waterproof packaging includes proper strapping and hanging points for safe transportation.

At Daxun Alloys, we combine top-quality products with flexible ordering options and secure shipping. Choose us for premium stainless steel plates tailored to your needs.

Leading Stainless Steel Sheet Suppliers in China

Daxun Alloys: Premier Stainless Steel Sheet Supplier in China

As a well-recognized manufacturer, trader, and supplier, Daxun Alloys leads the industry in ASTM A240 309/309s Stainless Steel Plates. Our products are crafted with precision, adhering to international quality standards. Our ISO 9001:2008 certification underscores our commitment to excellence. We specialize in exporting high-quality stainless steel plates worldwide. Our ASTM A240 309/309s Stainless Steel Plates come with comprehensive mill test reports and can be customized to your specifications. We offer widths up to 2000 mm and custom lengths to suit your needs. Daxun Alloys excels in sourcing rare grades and non-standard sizes, meeting our clients’ unique requirements. Our expertise extends to processing all ASTM A240 SS 304 Steel Plates, which we can cut to precise dimensions. Choose Daxun for unparalleled quality, customization, and global supply capabilities in stainless steel products.

Order Stainless Steel Sheets by Phone or Online.

There has never been an easier way to get stainless steel sheets. Simply refer to the simple and detailed instructions on our website. Alternatively, our sales staff will be happy to take your order or answer any questions when you call +86 13382898899 or email daxunhejin@gmail.com.

Our delivery time is only one to two days.

 

Daxun Alloys: Customized High Chromium Stainless Steel Sheet Solutions

We pride ourselves on offering tailored stainless steel sheets to match your exact specifications. Our versatile range includes:

Three distinct finishes to suit various applications

A wide array of sizes to meet diverse project needs

Custom sizing options for unique requirements

Our stainless steel sheets are available in thicknesses ranging from 0.3 mm to 30 mm. Sheet dimensions span from compact 50 x 50 mm pieces to expansive 2500 x 1250 mm sheets.

To ensure perfect fit for your projects, we offer a complimentary unlimited cutting service. Our state-of-the-art cutting machine guarantees precision with every cut. This free service allows you to order exactly what you need, eliminating waste and reducing costs.

At Daxun, we combine quality products with unparalleled customization options. Our commitment to meeting your specific needs sets us apart in the industry. Choose Daxun for stainless steel sheets that fit your project requirements precisely.

Exporting ASTM A240 309/309s Stainless Steel Plates Worldwide

We’re thrilled to ship our ASTM A240 309/309s stainless steel plates to countries all around the globe! Whether you’re in Saudi Arabia, Turkey, or the United Arab Emirates; Singapore, Japan, or South Korea; the United States, Canada, or Mexico—we’ve got you covered. Our reach extends to Europe with nations like Germany, France, and the United Kingdom, as well as throughout Africa, Asia, the Middle East, and the Far East. No matter where you are—from bustling cities to serene landscapes—we’re here to meet your stainless steel needs with joy and efficiency!

Daxun Alloys: Premium 309/309s Grade Stainless Steel Sheets

We offer 309/309s grade stainless steel sheets in an array of attractive finishes:

  1. Brushed finish for a sleek, modern look
  2. 2B smooth finish for a clean, uniform appearance
  3. 8K mirror finish for a highly reflective surface

Each sheet comes with a protective film on the finished side. This film safeguards the surface from wear and marks during handling and installation. It’s easily removable after fabrication, ensuring your product remains pristine. The back side is left unfinished for versatility.

Our 309s Grade Stainless Steel Sheet is a popular choice among customers. It boasts excellent weldability and formability, making it ideal for various applications. Its good corrosion resistance adds to its durability and longevity in diverse environments.

Choose Daxun for high-quality, versatile stainless steel sheets that meet your specific needs. Our range of finishes and protective features ensure you receive a product that’s ready for immediate use or further fabrication.

Our innovative nesting processing methods optimize material and cutting utilization.

At the same time, Daxun achieves continuous cost reduction and efficiency improvement by promoting lean improvement activities and passing the benefits to customers. Daxun also has a complete product traceability system and timely quality objection handling, which relieves customers’ concerns.

중요 안전 참고 사항:

The edges of the metal sheets we sell are not polished, ground or finished, so they may be sharp, just like the edges of any stainless steel sheet. We remind users to use, install and handle these devices with care.

오늘 문의 보내기
빠른 견적